Latest Publications

  • Comparison of sodium dichloroisocyanurate and trichloroisocyanuric acid for gold dissolution in hydrochloric acid solutions

    by Raisa E. Khabibulina, Vladimir G. Lobanov, Elvira B. Kolmachikhina, Olga B. Kolmachikhina, Lev V. Sokolov

  • Open Access

    Assessment of the prospects for processing oxidized nickel ores using microwave energy

    by S. E. Polygalov, V. G. Lobanov, Д. С. Седельникова, O. B. Kolmachikhina, O. Yu. Makovskaya, О. Ю. Маковская

    The Ural region holds an estimated 1.5 million tons of nickel reserves, located in the industrially developed Chelyabinsk, Sverdlovsk, and Orenburg regions. At present, however, these deposits are not being exploited, and metallic nickel is not produced in the Urals, as metallurgical facilities have been completely shut down. The reserves are represented by oxidized nickel ores (ONO) – a complex raw material with low nickel and cobalt contents, whose processing by existing technologies is economically unfeasible. The challenge is compounded by the absence of a beneficiation method for ONO that yields a concentrate; therefore, all current technologies require processing the entire ore mass, which results in high reagent consumption and substantial energy costs. Research is ongoing to develop new technological approaches, including alternative methods for extracting nickel and cobalt from ONO in the Ural deposits. One promising option is the use of microwave (MW) energy to unlock nickel-bearing minerals and accelerate the dissolution of nickel and cobalt. This study evaluates the effect of microwave energy on nickel recovery from oxidized nickel ores of the Ural region. Comparative data are presented for conventional sulfuric acid leaching and for the process with microwave energy applied. A series of test studies was carried out to assess the feasibility of using microwave energy for ONO processing. The comparison of technological parameters demonstrated the advantage of atmospheric sulfuric acid leaching with microwave energy, which achieved nickel recovery of up to 95 % in a relatively short time. These results identify this approach as the most promising for practical implementation.

  • Open Access

    Investigation of the behavior of sodium dichloroisocyanurate in aqueous solutions

    by R. E. Khabibulina, E. B. Kolmachikhina, V. G. Lobanov, O. B. Kolmachikhina

    Global gold consumption has steadily increased in recent decades, driven by expanding industrial applications and reserve accumulation by many countries. In parallel, depletion of high-grade deposits has shifted processing toward low-grade and refractory ores. These trends—together with tighter environmental regulations—highlight the need for alternative lixiviants for gold extraction. Although cyanide remains the industry standard, it is highly toxic and often ineffective for refractory sulfide ores. Other systems—thiosulfate (including ammoniacal thiosulfate), thiourea, and bromide/iodide lixiviants—are used far less frequently due to significant disadvantages. Among acidic chloride lixiviants, sodium dichloroisocyanurate (NaDCC) was investigated as a promising candidate. Use of NaDCC requires strongly acidic solutions (pH < 1.0) and an excess of Cl–, i.e., conditions consistent with the stability domain of the Au(III) chloride complex (AuCl4–). Using the rotating-disk technique, we examined the effects of temperature, disk rotation rate, and HCl concentration on the specific dissolution rate of the reagent (NaDCC), as well as on solution pH and redox potential (Eh). NaDCC hydrolyzes in water to form hypochlorous acid (HClO)—the primary source of active chlorine—while the concurrent pH decrease arises from formation of weak acids (hypochlorous and cyanuric). Adding HCl to NaDCC solutions generates molecular chlorine (Cl2), which evolves once its solubility limit is exceeded. Gold-dissolution tests across NaDCC and HCl concentrations identified an optimum at [HCI] = 14.4 g/dm3 and [NaDCC] = 3.0 g/dm3, yielding a maximum gold dissolution rate of υAu = 0.118 mg/(cm2·min).

  • Open Access

    Combined scheme for conditioning circulating cyanide solutions

    by A. M. Samofeev, V. G. Lobanov, F. M. Nabiullin, A. V. Tretyakov

    Due to the specific features of hydrometallurgical processing, where cyanide solutions are used, the composition of the leaching solution undergoes periodic changes referred to in the literature as “fatigue.” This adversely affects the rate of gold recovery and cementation, and therefore the overall efficiency of cyanide leaching technology. One of the most important markers determining the “fatigue” of the solution is copper. This study examined the possibility of applying a combined scheme for the purification of circulating cyanide solutions with high concentrations of copper (1196 mg/dm3), iron (111 mg/dm3), arsenic (19 mg/dm3), and sodium cyanide (0.94 g/dm3). A two-stage technology (reverse osmosis + chemical precipitation) was developed for the reduction of treated solution volumes and the removal of impurities. At the first stage, the solution was separated in a reverse osmosis unit equipped with LP22-8040 membranes, producing permeate and concentrate in a 1 : 1 ratio. The permeate (12 mg/dm3 Cu and 0.01 mg/dm3 Fe, pH = 11.13) was returned to the process cycle. At the second stage, the concentrate, which contained 99 % of the initial impurities, was further purified by the stepwise addition of a CuSO4 solution (70 g/dm3 Cu) in 1–11 cm3 doses under stirring (500 rpm, 10 min). The results showed that the optimal CuSO4 dose (11 cm3) provided removal of more than 86 % of Cu from the initial solution, as well as 100 % of Fe and more than 96 % of As. The precipitate obtained in the process consisted of 68.3 % copper, with CuCN and Cu(OH)2 as the main components.

  • Study on the influence of temperature on a baddeleyite concentrate chlorination process

    by A. A. Babintsev, O. Yu. Makovskaya, V. G. Lobanov

    The article describes the chlorination process of baddeleyite concentrates in the melt of chlorides of alkali and alkali-earth metals. A method of chlorination in the melt has technological advantages in comparison with dry chlorination. The authors studied the concentrate of grade PB-0 from Kovdor Mining and Beneficiation Plant, amounting to a total of 99.5% zirconium and hafnium dioxides. The baddeleyite concentrate, unlike the zirconium concentrate, contains low impurities, making easier subsequent recovery ope rations of zirconium and hafnium tetrachlorides. To chlorate the baddeleyite concentrate, the authors used melts of КСl, NaCl – KCl, NaCl – KCl – MgCl2, KCl – MgCl2, NaCl and СаCl2. It has been established that the best parameters of both the percentage of the transition of zirconium into tetrachloride (over 65%), and the chlorination rate (2.07·10–3 g/(g·min)) are attributed to the NaCl – KCl melt. The authors studied the relation between the chlorination process in the NaCl – KCl melt and temperature. Experimentally determined apparent activation energy within a temperature range of 800–1000 oC was 18.49 kJ/mol, and within a temperature range of 750–800 oC, 176.07 kJ/mol. Thus, at 750–800 oC the chlorination process takes place in a kinetic mode, and at 800–1000 oC — in a diffusion mode. It has been established that when the process temperature increases over 900 oC, there is no significant increase in weight of obtained zirconium tetrachloride. Moreover, an increase in chlorination temperature entails a greater transition of impurity elements into zirconium tetrachloride. In view of this, to conduct the process, the recommended temperature range is 900–950 oC. The research was sponsored by funds, amounting to income from trust management of the Endowment Fund of the Institute of New Materials and Technologies, Ural Federal University, established with a participation of JSC Chelyabinsk Zinc Plant.


  • Open Access

    Selection of a leaching system for the extraction of gold from the ore of the Byn’govskoye deposit

    by V. G. Lobanov, R. E. Khabibulina, O. B. Kolmachikhina, O. Yu. Makovskaia, О. Ю. Маковская

    A theoretical substantiation of an environmentally friendly technology for extracting gold from mineral raw materials is presented. In terms of an alternative to conventional cyanide, the authors propose chlorine-bearing derivatives of organic isocyanuric acid (C3H3N3O3). In the studied process, this reagent combines the roles of a long-acting oxidant and complexing agent due to the resulting Cl– ion. For experimental purposes, the rotating disc technique was applied. Experimental results were evaluated by measuring the concentration of gold in solutions using the atomic adsorption method. The theoretical characteristics of gold dissolution using the proposed reagent were studied. In order to evaluate the applicability of the revealed regularities for practical purposes, comparative indicators for leaching gold from the ore of the Byn’govskoye deposit (Sverdlovsk Oblast) using the proposed reagent, cyanide and CYCAD cyanide substitute (China) were evaluated. The dependence of the gold disc dissolution rate on temperature, as well as leaching reagent and hydrochloric acid concentrations, were studied. In disc sample experiments, the exponential dependence of the dissolution rate on the concentration of the studied reagent was established. In this case, the maximum intensity of the process is achieved at a concentration higher than 50 g/dm3. The optimum acidity level comprises 0.3–0.4 g ion/dm3 of hydrochloric acid. Despite an increase in temperature being shown to accelerate the dissolution process, this appears to be technologically unjustified. Under optimal conditions, the gold disc dissolution rate reaches 0.5•10-3 g ion/(cm2•min), which is approximately one hundred times higher than during the dissolution by the cyanic solutions in conventional modes. Close gold extraction values were achieved in the solutions of cyanides and chlorine-bearing derivatives of isocyanuric acid during the leaching of gold from the ore under the comparable conditions. For CYCAD solutions, the same indicator is two times lower. The results of the performed studies demonstrate the high dissolution rate of gold using the proposed reagent along with the technological possibility of leaching gold from ores using this environmentally friendly reagent.


  • Features of the Presence of Precious Metals in the Zinc Production Clinker

    by V. G. Lobanov, O. B. Kolmachikhina, S. E. Polygalov, R. E. Khabibulina, L. V. Sokolov

    The features of forms of occurrence of gold in technogenic raw materials—lying clinker of zinc production of the Belovsky Zinc Plant (Belovo, Kemerov


  • Open Access

    Features of the presence of precious metals in the zinc production clinker

    by V. G. Lobanov, O. B. Kolmachikhina, S. E. Polygalov, R. E. Khabibulina, L. V. Sokolov

    The paper considers the features of gold deportments in technogenic raw materials – aged clinker of zinc production at the Belovsky zinc plant (Belovo, Kemerovo Region). The Belovsky plant operated from 1930 to 2003 using zinc concentrates from the Salairsky ore mining and processing plant. After the plant shutdown, clinker dumps were stored at the plant’s mill site and were repeatedly washed with acidic solutions to isolate copper. This form of storage and leaching led to the transformation of precious metal deportments in clinker, which currently makes it difficult to extract gold. The gold content in clinker is at the level of 2–3 g/t, which makes gold recovery profitable. The presence of carbon in clinker complicates the use of known methods of both analytical detection of gold and its recovery. A method is proposed for determining the deportment and content of gold taking into account the fact that gold may be present in the form of free fine gold, as well as gold finely disseminated in iron and its oxides, in sulfide phases, in the quartz-silicate part of clinker and in the carbonaceous phase. It was shown that gold deportments in clinker change depending on the storage conditions and preceding acid treatment, and this affects the choice of the material processing flow chart. The share of gold available for leaching is at least 40 %. The increased associativity of gold with the coal (flotation-active) phase and the sorption activity of coal significantly interfere with the study into the properties of gold deportments in clinker, which requires preliminary carbon removal.

  • Fine Gold Extraction Problem from Industrial Sludge

    by R.E. Khabibulina, Vladimir G. Lobanov, Konstantin D. Naumov

    Error reasons of gold analytical determination in the chemical plant sludge are studied. The studied sludge is waste of BaCl2 production. According to preliminary estimates it contains gold in sufficient quantity for industrial extraction. Comparison of direct sludge fire assay analysis and sludge dissolution in aqua regia, followed by gold atomic absorption determination in solution is made. The negative effect of Na+, Ca2+, Ba2+, Zn2+ ions presence in studied solutions was shown. Error quantitative estimate at alkali metals introducing into standard solutions is given. It is shown that Ca2+ and Ba2+ ions contribute the most error. Error increases linearly at addition of Ca2+ and Ba2+ ions. Growth error gradually slow down at increasing Na+, Zn2+ ion content.