Linjun Xie
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Linjun Xie has a total of 24 co-authors. Here are the top co-authors by number of shared publications:
Chunhua Bian
CNNC Nuclear Power Operation Management Co., Ltd. , Haiyan 314300 , China
2 shared publicationsHanbo Lin
School of Mechanical Engineering, Zhejiang University of Technology, Hangzhou, China
2 shared publicationsMinglei Hu
CNNC Nuclear Power Operation Management Co., Ltd. , Haiyan 314300 , China
2 shared publicationsWei Zhang
CNNC Nuclear Power Operation Management Co., Ltd. , Haiyan 314300 , China
2 shared publicationsChangxun Wang
Zhejiang University of Technology, College of Mechanical Engineering, Hangzhou 310023, China
1 shared publicationDong Ning
Shanghai Nuclear Engineering Research & Design Institute, Shanghai, China
1 shared publication
Latest Publications
- Open Access
- 17 June 2024
- Published by MDPI AG in Preprints.org
Data analysis and inflection point generation algorithm for RPN intermediate range detectors in active nuclear power plants
The nuclear reactor measurement system is a crucial component of the nuclear measurement system in a nuclear power plant. Its primary function is to measure the power distribution within the reactor core using detectors, calibrate, and provide data on core fuel consumption. Therefore, the study of the detectors' reliability is crucial for ensuring the safe operation of the nuclear power system. The article describes the operational mechanism of the gas ionization chamber detector utilized in the intermediate-range detector of the off-board nuclear measurement system. It also analyzes the movement of particles between the plates during the ionization process of the nuclear reaction taking place in the detector. The functional relationship between the current in the recombination region and the ionization region involved in the actual working condition, and the change with the increase of voltage between the plates, is deduced. A mathematical model is established for the number of pulses generated between the plates and the magnitude of the voltage between the plates. Subsequently, the change in the offset of the voltage corresponding to the inflection point of the ping curve and the change rule of the slope of the ping curve are investigated. Combined with the analysis of experimental data, the results show that the initial particle energy of Ar+, the primary sensitive particle on the detector surface, follows a normal distribution and is influenced by the energy loss associated with the initial velocity and the voltage between the plates. The trends of the inflection points and slopes of the ping curves can be utilized to evaluate the performance and operational status of the detector. Combined with the results of the experimental data analysis, the fit is good, and the inflection point currents in the normal state decrease by about 1.5% annually. The intelligent diagnostic system, based on the method studied in this paper, has been successfully implemented in the RPN digital retrofit and upgrade project at Qinshan No. 2 Plant.
- 17 June 2024
- Published by MDPI AG in Preprints.org
Open AccessData analysis and inflection point generation algorithm for RPN intermediate range detectors in active nuclear power plants
The nuclear reactor measurement system is a crucial component of the nuclear measurement system in a nuclear power plant. Its primary function is to measure the power distribution within the reactor core using detectors, calibrate, and provide data on core fuel consumption. Therefore, the study of the detectors' reliability is crucial for ensuring the safe operation of the nuclear power system. The article describes the operational mechanism of the gas ionization chamber detector utilized in the intermediate-range detector of the off-board nuclear measurement system. It also analyzes the movement of particles between the plates during the ionization process of the nuclear reaction taking place in the detector. The functional relationship between the current in the recombination region and the ionization region involved in the actual working condition, and the change with the increase of voltage between the plates, is deduced. A mathematical model is established for the number of pulses generated between the plates and the magnitude of the voltage between the plates. Subsequently, the change in the offset of the voltage corresponding to the inflection point of the ping curve and the change rule of the slope of the ping curve are investigated. Combined with the analysis of experimental data, the results show that the initial particle energy of Ar+, the primary sensitive particle on the detector surface, follows a normal distribution and is influenced by the energy loss associated with the initial velocity and the voltage between the plates. The trends of the inflection points and slopes of the ping curves can be utilized to evaluate the performance and operational status of the detector. Combined with the results of the experimental data analysis, the fit is good, and the inflection point currents in the normal state decrease by about 1.5% annually. The intelligent diagnostic system, based on the method studied in this paper, has been successfully implemented in the RPN digital retrofit and upgrade project at Qinshan No. 2 Plant.
- 24 April 2023
- Published by Taylor & Francis in Journal of Nuclear Science and Technology
- Vol. 60 (9) , 1100-1115
Fretting wear behavior test and numerical simulation of Inconel 690 alloy
A steam generator heat transfer tube is important for energy exchange between the primary circuit and secondary circuit . The changes in friction and wear properties of Inconel 690 alloy and 403 stainless-steel anti-vibration strips in different media (air, deionized water, and boric acid solution) were compared and analyzed. Friction and wear tests were conducted in different media environments and under different loads, and finite element simulation was performed in different media environments.Results show that the main wear mechanisms in the air are delamination wear and oxidation friction. The oxygen content in the water is reduced, and the oxide formed is reduced. Because the solution replaces the abrasive particles to form the third body, which can reduce friction and lubricate, the abrasive particles and abrasive particles can be easily removed or dissolved. The wear mechanism in a water environment is delamination wear and abrasive wear. In boric acid, a passive film is formed on the contact wear surface of the Inconel 690 alloy after the previous fretting wear. The passivation film is worn first in the next fretting wear, which slows down wearing. The wear mechanism in a boric acid environment primarily includes abrasive wear and corrosion wear.
- 24 April 2023
- Published by Taylor & Francis in Journal of Nuclear Science and Technology
- Vol. 60 (9) , 1100-1115
Fretting wear behavior test and numerical simulation of Inconel 690 alloy
A steam generator heat transfer tube is important for energy exchange between the primary circuit and secondary circuit . The changes in friction and wear properties of Inconel 690 alloy and 403 stainless-steel anti-vibration strips in different media (air, deionized water, and boric acid solution) were compared and analyzed. Friction and wear tests were conducted in different media environments and under different loads, and finite element simulation was performed in different media environments.Results show that the main wear mechanisms in the air are delamination wear and oxidation friction. The oxygen content in the water is reduced, and the oxide formed is reduced. Because the solution replaces the abrasive particles to form the third body, which can reduce friction and lubricate, the abrasive particles and abrasive particles can be easily removed or dissolved. The wear mechanism in a water environment is delamination wear and abrasive wear. In boric acid, a passive film is formed on the contact wear surface of the Inconel 690 alloy after the previous fretting wear. The passivation film is worn first in the next fretting wear, which slows down wearing. The wear mechanism in a boric acid environment primarily includes abrasive wear and corrosion wear.
- 22 February 2022
- Published by Walter de Gruyter GmbH in Kerntechnik
- Vol. 87 (3) , 278-286
Frictional wear characteristics of nickel-based alloy and reactor material in pressure vessel reactor
The reactor pressure vessel was contact sealed with a double-channel O-ring made of Inconel 718 alloy and nuclear power material SA508. The fretting wear characteristics of Inconel 718 O-tube and SA508 plate friction pair were tested by fretting wear testing machine to explore the failure mechanism of reactor pressure vessel seal system. The test conditions are as follows: normal temperature, normal loads of 10, 20, and 40 N, displacement amplitude of 600 μm, the number of cycles of 10,000, and frequency of 4 Hz. Results show that the coefficient of friction (COF) increased with increasing normal force. Significant material losses were detected during the relative sliding of the contact surface of SA508. A large number of abrasive dust accumulated at the edge of the contact zone, forming a large number of oxides. During the friction of Inconel 718 O-ring, plastic deformation occurred, and a plastic flow layer was formed. The plastic deformation flow at the contact point formed an adhesive connection point, producing adhesive wear and oxidative wear. The wear mechanism was characterized by the combination of oxidative wear and abrasive wear.
- 22 February 2022
- Published by Walter de Gruyter GmbH in Kerntechnik
- Vol. 87 (3) , 278-286
Frictional wear characteristics of nickel-based alloy and reactor material in pressure vessel reactor
The reactor pressure vessel was contact sealed with a double-channel O-ring made of Inconel 718 alloy and nuclear power material SA508. The fretting wear characteristics of Inconel 718 O-tube and SA508 plate friction pair were tested by fretting wear testing machine to explore the failure mechanism of reactor pressure vessel seal system. The test conditions are as follows: normal temperature, normal loads of 10, 20, and 40 N, displacement amplitude of 600 μm, the number of cycles of 10,000, and frequency of 4 Hz. Results show that the coefficient of friction (COF) increased with increasing normal force. Significant material losses were detected during the relative sliding of the contact surface of SA508. A large number of abrasive dust accumulated at the edge of the contact zone, forming a large number of oxides. During the friction of Inconel 718 O-ring, plastic deformation occurred, and a plastic flow layer was formed. The plastic deformation flow at the contact point formed an adhesive connection point, producing adhesive wear and oxidative wear. The wear mechanism was characterized by the combination of oxidative wear and abrasive wear.
- 18 October 2021
- Published by Taylor & Francis in Nuclear Science and Engineering
- Vol. 196 (2) , 221-233
Stress Distribution and Safety Evaluation of Pipeline in Ice Plug of Nuclear Power
Nuclear power pipeline ice plug technology, as the main technical method of nuclear power safety maintenance and innovative design, plays a protective role in the long-term safe operation of nuclear power plants. During the ice plug process, pipelines have complex stress states, which can easily lead to problems such as material yielding, cracking, and even damage. In this study, by building an ice plug test platform for nuclear power pipelines, an ice plug test and a numerical analysis of nuclear power pipelines are carried out to explore the stress distribution of nuclear power pipelines during the ice plug process and its impact on the performance of pipeline materials and to analyze the safety of pipelines in the ice plug process. This study shows that the distribution of stress in the pipeline during ice plug is related to the temperature change and cooling rate of the pipe wall. The stress distribution in different parts is uneven, and the maximum stress appears near the edge of the jacket. According to the temperature data of the pipe wall, the stress distribution of the pipe wall can be obtained by the finite element method. From the test and finite element results, it can be seen that when the frost line length of the pipeline is less than 200 mm, the pipeline ice plug method is safe and feasible.
- 18 October 2021
- Published by Taylor & Francis in Nuclear Science and Engineering
- Vol. 196 (2) , 221-233
Stress Distribution and Safety Evaluation of Pipeline in Ice Plug of Nuclear Power
Nuclear power pipeline ice plug technology, as the main technical method of nuclear power safety maintenance and innovative design, plays a protective role in the long-term safe operation of nuclear power plants. During the ice plug process, pipelines have complex stress states, which can easily lead to problems such as material yielding, cracking, and even damage. In this study, by building an ice plug test platform for nuclear power pipelines, an ice plug test and a numerical analysis of nuclear power pipelines are carried out to explore the stress distribution of nuclear power pipelines during the ice plug process and its impact on the performance of pipeline materials and to analyze the safety of pipelines in the ice plug process. This study shows that the distribution of stress in the pipeline during ice plug is related to the temperature change and cooling rate of the pipe wall. The stress distribution in different parts is uneven, and the maximum stress appears near the edge of the jacket. According to the temperature data of the pipe wall, the stress distribution of the pipe wall can be obtained by the finite element method. From the test and finite element results, it can be seen that when the frost line length of the pipeline is less than 200 mm, the pipeline ice plug method is safe and feasible.
- 20 October 2017
- Published by Walter de Gruyter GmbH in Kerntechnik
- Vol. 82 (5) , 579-585
Friction coefficient and limiter load test analysis by flexibility coefficient model of Hold-Down Spring of nuclear reactor vessel internals
The friction force between the contact surfaces of a reactor internal hold-down spring (HDS) and core barrel flanges can directly influence the axial stiffness of an HDS. However, friction coefficient cannot be obtained through theoretical analysis. This study performs a mathematical deduction of the physical model of an HDS. Moreover, a mathematical model of axial load P, displacement δ, and flexibility coefficient is established, and a set of test apparatuses is designed to simulate the preloading process of the HDS. According to the experimental research and theoretical analysis, P-δ curves and the flexibility coefficient λ are obtained in the loading processes of the HDS. The friction coefficient f of the M1000 HDS is further calculated as 0.224. The displacement limit load value (4,638 kN) can be obtained through a displacement limit experiment. With the friction coefficient considered, the theoretical load is 4,271 kN, which is relatively close to the experimental result. Thus, the friction coefficient exerts an influence on the displacement limit load P. The friction coefficient should be considered in the design analysis for HDS.
- 20 October 2017
- Published by Walter de Gruyter GmbH in Kerntechnik
- Vol. 82 (5) , 579-585
Friction coefficient and limiter load test analysis by flexibility coefficient model of Hold-Down Spring of nuclear reactor vessel internals
The friction force between the contact surfaces of a reactor internal hold-down spring (HDS) and core barrel flanges can directly influence the axial stiffness of an HDS. However, friction coefficient cannot be obtained through theoretical analysis. This study performs a mathematical deduction of the physical model of an HDS. Moreover, a mathematical model of axial load P, displacement δ, and flexibility coefficient is established, and a set of test apparatuses is designed to simulate the preloading process of the HDS. According to the experimental research and theoretical analysis, P-δ curves and the flexibility coefficient λ are obtained in the loading processes of the HDS. The friction coefficient f of the M1000 HDS is further calculated as 0.224. The displacement limit load value (4,638 kN) can be obtained through a displacement limit experiment. With the friction coefficient considered, the theoretical load is 4,271 kN, which is relatively close to the experimental result. Thus, the friction coefficient exerts an influence on the displacement limit load P. The friction coefficient should be considered in the design analysis for HDS.
- 9 January 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (2) , 644-652
Experimental Study on Creep Characterization and Lifetime Estimation of RPV Material at 723-1023 K
- 9 January 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (2) , 644-652
Experimental Study on Creep Characterization and Lifetime Estimation of RPV Material at 723-1023 K