SGShin-Ichi Goto

Shin-Ichi Goto

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Shin-Ichi Goto has a total of 4 co-authors. Here are the top co-authors by number of shared publications:

  • Hideo Ogura

    Department of Dental Materials Science, School of Life Dentistry at Niigata, The Nippon Dental University

    2 shared publications
  • Chatcharee Suchatlampong

    Department of Prosthodontics, Faculty of Dentistry, Mahidol University, Bangkok, Thailand

    1 shared publication
  • Pornkiat Churnjitapirom

    Department of Dental Materials Science, School of Life Dentistry at Niigata, The Nippon Dental University

    1 shared publication
  • Yukio Miyagawa

    Advanced Research Center, School of Life Dentistry at Niigata, The Nippon Dental University

    1 shared publication

Latest Publications

  • Open Access

    Effect of additive metals, Sn, Ga, and In in Ag-Pd-Au-Cu alloys on initial bond strength of 4-META adhesive cement to these alloys

    by Shin-Ichi Goto, Pornkiat Churnjitapirom, Yukio Miyagawa, Hideo Ogura

    The purpose of this study was to investigate the effects of three additives, Sn, Ga, and In, as well as the main constituents, Pd and Cu, of Ag-Pd-Au-Cu alloys on the initial bond strength of 4-META adhesive cement to these alloys. The Ag-Pd-Au-Cu alloys consisted of 20%, 30% or 40%Pd, and 10%, 15% or 20%Cu, 20%Au, and Ag as balance. Besides, additive metals (Sn, Ga, and In) of 2% and 4% were added to these compositions. The addition of three additives, in general, increased the initial bond strength of the cement in comparison to the mother compositions (0% additives), although the degrees of effectiveness of the three additives were different and varied with their contents. Among these additives, a remarkable increase in bond strength was observed with the addition of In. The increase in Cu content, in many cases, resulted in an increase in bond strength at high Pd contents (30% and 40%), but a decrease at low Pd content (20%) in some cases. The positive effects of the three additives and Cu could be due to the formation of a suitable oxide layer for strong bonding with 4-META.


  • Early Compressive Strength and Phase-Formation of Dental Amalgam

    by Chatcharee Suchatlampong, Shin-Ichi Goto, Hideo Ogura

    The compressive strength of five different amalgams was measured at one hour, six hours, 24 hours, and seven days, and X-ray diffraction analysis was carried out for each amalgam at the same times in order to investigate the early strength characteristics of the amalgams in relation to the formation of different phases. At 24 hours all tested amalgams reached about 90% or more of their seven-day compressive strength, but the increase in the early compressive strength from one hour to 24 hours varied between different amalgams. Two of the five amalgams tested reached about 90% of their seven-day compressive strength at six hours. A significant correlation was found between the ratio of early compressive strength to seven-day compressive strength, and the X-ray diffraction intensity ratio (ratios of one-, six- and 24 hour intensity to seven-day intensity) for the gamma 1 phase, indicating that the increases in early compressive strength are mainly dependent upon the formation of gamma 1.