Xiuwen Zhou
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Xiuwen Zhou has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Weidong Wu
Science and Technology on Plasma Physics Laboratory, Research Center of Laser Fusion, China Academy of Engineering Physics, Mianyang 621900, China
3 shared publications - Jinzhi Jia
Lanzhou University
2 shared publications - Xudong Liu
Research Centre of Laser Fusion China Academy of Engineering Physics Mianyang 621900 P. R. China
2 shared publications Bin Yu
Research Center of Laser Fusion, China Academy of Engineering Physics, Mianyang 621900, China
1 shared publicationBo Yang
Research Center of Laser Fusion, China Academy of Engineering Physics, Mianyang 621900, China
1 shared publicationBotao Wu
1 shared publication
Latest Publications
- Open Access
- 3 January 2019
- Published by MDPI AG in Nanomaterials
- Vol. 9 (1) , 53
A Controllability Investigation of Magnetic Properties for FePt Alloy Nanocomposite Thin Films
An appropriate writing field is very important for magnetic storage application of L10 FePt nanocomposite thin films. However, the applications of pure L10 FePt are limited due to its large coercivity. In this paper, the ratios of L10 and non-L10 phase FePt alloy nanoparticles in FePt/MgO (100) nanocomposite thin films were successfully tuned by pulsed laser deposition method. By adjusting the pulsed laser energy density from 3 to 7 J/cm2, the ordering parameter initially increased, and then decreased. The highest ordering parameter of 0.9 was obtained at the pulsed laser energy density of 5 J/cm2. At this maximum value, the sample had the least amount of the soft magnetic phase of almost 0%, as analyzed by a magnetic susceptibility study. The saturation magnetization decreased with the increase in the content of soft magnetic phase. Therefore, the magnetic properties of FePt nanocomposite thin films can be controlled, which would be beneficial for the magnetic applications of these thin films.
- 3 January 2019
- Published by MDPI AG in Nanomaterials
- Vol. 9 (1) , 53
Open AccessA Controllability Investigation of Magnetic Properties for FePt Alloy Nanocomposite Thin Films
An appropriate writing field is very important for magnetic storage application of L10 FePt nanocomposite thin films. However, the applications of pure L10 FePt are limited due to its large coercivity. In this paper, the ratios of L10 and non-L10 phase FePt alloy nanoparticles in FePt/MgO (100) nanocomposite thin films were successfully tuned by pulsed laser deposition method. By adjusting the pulsed laser energy density from 3 to 7 J/cm2, the ordering parameter initially increased, and then decreased. The highest ordering parameter of 0.9 was obtained at the pulsed laser energy density of 5 J/cm2. At this maximum value, the sample had the least amount of the soft magnetic phase of almost 0%, as analyzed by a magnetic susceptibility study. The saturation magnetization decreased with the increase in the content of soft magnetic phase. Therefore, the magnetic properties of FePt nanocomposite thin films can be controlled, which would be beneficial for the magnetic applications of these thin films.
- 16 July 2018
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 6 (31) , 15330-15339
Self-assembled pancake-like hexagonal tungsten oxide with ordered mesopores for supercapacitors
Hexagonal WO3 with well-ordered mesopores was achieved using a one-pot hydrothermal method, and it exhibited excellent capacitive performance.
- 16 July 2018
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 6 (31) , 15330-15339
Self-assembled pancake-like hexagonal tungsten oxide with ordered mesopores for supercapacitors
Hexagonal WO3 with well-ordered mesopores was achieved using a one-pot hydrothermal method, and it exhibited excellent capacitive performance.
- 3 January 2018
- Published by Royal Society of Chemistry (RSC) in Nanoscale
- Vol. 10 (9) , 4209-4217
Hybrid nanowires and nanoparticles of WO 3 in a carbon aerogel for supercapacitor applications
WO 3 was incorporated into a carbon aerogel with controllable single or hybrid structure, and the latter structure exhibited better capacitive performance.
- 3 January 2018
- Published by Royal Society of Chemistry (RSC) in Nanoscale
- Vol. 10 (9) , 4209-4217
Hybrid nanowires and nanoparticles of WO 3 in a carbon aerogel for supercapacitor applications
WO 3 was incorporated into a carbon aerogel with controllable single or hybrid structure, and the latter structure exhibited better capacitive performance.
- 1 September 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (91) , 88656-88663
Preparation of size controllable porous polymethylmethacrylate template and Cu micro/nanowire arrays
Preparation of a size controllable porous polymethylmethacrylate template and Cu micro/nanowire arrays by an iterative melt co-drawing and bundling technique.
- 1 September 2016
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 6 (91) , 88656-88663
Preparation of size controllable porous polymethylmethacrylate template and Cu micro/nanowire arrays
Preparation of a size controllable porous polymethylmethacrylate template and Cu micro/nanowire arrays by an iterative melt co-drawing and bundling technique.
- Open Access
- 24 May 2016
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 36 (5) , 485-493
Mechanical Properties and Microstructures of Ni20Cr Micro-wires with Abnormal Plastic Deformation
Ni80Cr20 (Ni20Cr, wt%) micro-wires were fabricated by the cold-drawing method with single die. Abnormal engineering strains were approximately 17.3–46.6 % for each pass. The relationship between mechanical properties and microstructures of Ni20Cr micro-wires were investigated under different engineering strains and annealing conditions. Experiment results indicate that the as-drawn NiCr micro-wires present obviously brittle fractures. The ultimate tensile strength (UTS) significantly increases from 781 to 1,147 MPa and the elongation decreases from 17.2 % to 1 % with engineering strains increasing. The deformed microstructures of Ni20Cr micro-wire were analyzed in detail including two-phase (solid solution/amorphous phase), edge dislocations and twins. With the annealing temperature increasing, specimens had experienced three stages and their mechanical properties were improved. After annealing at 890 °C (with 6.5 g stress) for 7.3 s in N2, the Ni20Cr micro-wires benefited for the second drawing pass. The results are very importance in fabricating Ni20Cr micro-wire with the diameter from 25 to 10 μm.
- 24 May 2016
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 36 (5) , 485-493
Open AccessMechanical Properties and Microstructures of Ni20Cr Micro-wires with Abnormal Plastic Deformation
Ni80Cr20 (Ni20Cr, wt%) micro-wires were fabricated by the cold-drawing method with single die. Abnormal engineering strains were approximately 17.3–46.6 % for each pass. The relationship between mechanical properties and microstructures of Ni20Cr micro-wires were investigated under different engineering strains and annealing conditions. Experiment results indicate that the as-drawn NiCr micro-wires present obviously brittle fractures. The ultimate tensile strength (UTS) significantly increases from 781 to 1,147 MPa and the elongation decreases from 17.2 % to 1 % with engineering strains increasing. The deformed microstructures of Ni20Cr micro-wire were analyzed in detail including two-phase (solid solution/amorphous phase), edge dislocations and twins. With the annealing temperature increasing, specimens had experienced three stages and their mechanical properties were improved. After annealing at 890 °C (with 6.5 g stress) for 7.3 s in N2, the Ni20Cr micro-wires benefited for the second drawing pass. The results are very importance in fabricating Ni20Cr micro-wire with the diameter from 25 to 10 μm.
- 8 October 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (110) , 90852-90857
Investigation on the microstructure of as-deformed NiCr microwires using TEM
The deformed microstructures of Ni20Cr wires include amorphous GB, crystal GB, edge dislocations, and twins. Edge dislocations exist in GB and grain interiors. Twinning angles is approximately 141° and 146°, respectively.
- 8 October 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (110) , 90852-90857
Investigation on the microstructure of as-deformed NiCr microwires using TEM
The deformed microstructures of Ni20Cr wires include amorphous GB, crystal GB, edge dislocations, and twins. Edge dislocations exist in GB and grain interiors. Twinning angles is approximately 141° and 146°, respectively.