Angela Brys Osório
Research Subjects
Research Interests
Angela Brys Osório has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Flávio Fernando Demarco
Federal University of Pelotas, Pelotas, Brazil
1 shared publication Guilherme Brião Camacho
1 shared publicationGuilherme Briäo Camacho
1 shared publicationJohn M Powers
1 shared publicationMariane Gonçalves
1 shared publicationTomio Nonaka
1 shared publication
Latest Publications
- 26 April 2007
- Vol. 20 (2) , 123-4
Microleakage in full-crown all-ceramic restorations: influence of internal surface treatment, silane application, alumina system, and substrate.
This study investigated the influence of internal surface treatment and margin location on the microleakage of 2 alumina-reinforced ceramic crown systems: In-Ceram (VITA Zahnfabrik) and Procera (Nobel Biocare). Full crowns were produced for each of the 2 systems (n = 24) in human premolars, with margins located in enamel and dentin, and luted with Single Bond and RelyX ARC (3M ESPE). Four internal ceramic treatments were tested: (1) aluminum oxide blasting (AO), (2) AO plus silane, (3) hydrofluoric acid etching (HF), and (4) HF plus silane. After thermal cycling, leakage was measured quantitatively. Statistical analysis (P < .05) showed higher leakage in dentin margins compared to enamel. In enamel, Procera showed greater leakage compared to In-Ceram. Generally, lower microleakage was observed for the AO plus silane treatment.
- 26 April 2007
- Vol. 20 (2) , 123-4
Microleakage in full-crown all-ceramic restorations: influence of internal surface treatment, silane application, alumina system, and substrate.
This study investigated the influence of internal surface treatment and margin location on the microleakage of 2 alumina-reinforced ceramic crown systems: In-Ceram (VITA Zahnfabrik) and Procera (Nobel Biocare). Full crowns were produced for each of the 2 systems (n = 24) in human premolars, with margins located in enamel and dentin, and luted with Single Bond and RelyX ARC (3M ESPE). Four internal ceramic treatments were tested: (1) aluminum oxide blasting (AO), (2) AO plus silane, (3) hydrofluoric acid etching (HF), and (4) HF plus silane. After thermal cycling, leakage was measured quantitatively. Statistical analysis (P < .05) showed higher leakage in dentin margins compared to enamel. In enamel, Procera showed greater leakage compared to In-Ceram. Generally, lower microleakage was observed for the AO plus silane treatment.
- 1 April 2007
- Vol. 20 (2) , 121-4
Fracture strength of restored premolars.
To evaluate the fracture resistance (axial compressive strength) of premolars restored with different dental materials under two axial loads. Fracture strength was performed using two metal spheres with 3 mm and 9 mm diameter. Five restorative techniques were chosen for MOD cavity preparations (n = 10): (1) direct resin composite restorations (Z-250); (2) indirect resin composite restorations (Z-250 and RelyX); (3) ceramic inlays (Vitadur Alpha); (4) conventional amalgam restorations (GS-80); (5) bonded amalgam restorations. The restored teeth were compared to human caries-free premolars (Group 6/control). Enforce resin cement was used for ceramic and amalgam adhesive restorative techniques, according to the manufacturers' instructions. Whenever required, the teeth were conditioned by the total etch technique. The ANOVA analysis pointed out a significant difference among the groups (P < 0.01) and the "site" factor (P < 0.1). The ceramic restorations presented the highest values for fracture strength and were similar to the control group. The statistical results of direct and indirect resin composite restorations were similar but inferior to the control group. The amalgam restorations (conventional and bonded) presented the lowest values, with no difference between them. All amalgam groups displayed lower strengths when the load was applied on the central fossa (3 mm 0 sphere) compared to load applied on cusps (9 mm 0 sphere).
- 1 April 2007
- Vol. 20 (2) , 121-4
Fracture strength of restored premolars.
To evaluate the fracture resistance (axial compressive strength) of premolars restored with different dental materials under two axial loads. Fracture strength was performed using two metal spheres with 3 mm and 9 mm diameter. Five restorative techniques were chosen for MOD cavity preparations (n = 10): (1) direct resin composite restorations (Z-250); (2) indirect resin composite restorations (Z-250 and RelyX); (3) ceramic inlays (Vitadur Alpha); (4) conventional amalgam restorations (GS-80); (5) bonded amalgam restorations. The restored teeth were compared to human caries-free premolars (Group 6/control). Enforce resin cement was used for ceramic and amalgam adhesive restorative techniques, according to the manufacturers' instructions. Whenever required, the teeth were conditioned by the total etch technique. The ANOVA analysis pointed out a significant difference among the groups (P < 0.01) and the "site" factor (P < 0.1). The ceramic restorations presented the highest values for fracture strength and were similar to the control group. The statistical results of direct and indirect resin composite restorations were similar but inferior to the control group. The amalgam restorations (conventional and bonded) presented the lowest values, with no difference between them. All amalgam groups displayed lower strengths when the load was applied on the central fossa (3 mm 0 sphere) compared to load applied on cusps (9 mm 0 sphere).