V. I. Putlyaev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
V. I. Putlyaev has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
P. V. Evdokimov
Faculty of Materials Science, Moscow State University, Moscow, Russia
4 shared publicationsE. S. Klimashina
Moscow State University
3 shared publicationsA. V. Garshev
Faculty of Materials Science, Moscow State University, Moscow, Russia
2 shared publicationsN. K. Orlov
Moscow State University
2 shared publications- Tatiana Viktorovna Safronova
Department of Chemistry, Lomonosov Moscow State University, Building, 3, Leninskie Gory, 1, 119991 Moscow, Russia
2 shared publications - Andrei A. Tikhonov
Moscow State University
1 shared publication
Latest Publications
- 1 February 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 59 (2) , 210-220
Stereolithographic Fabrication of Alumina Ceramics from Aluminum Chloride-Containing Polymerizable Precursors
An approach has been proposed for preparing polymerizable precursors to alpha-alumina and aluminum oxynitride ceramics and using them in stereolithographic fabrication of aluminum-containing ceramics. With allowance for their homogeneity (optical transmission), photopolymerizability, and weight loss during thermolysis, three precursors based on aluminum chlorides (anhydrous and hexahydrate) and a basic aluminum chloride were chosen for characterization. We analyzed the behavior of the precursors during firing in an ammonia atmosphere for the preparation of oxynitride ceramics and during firing in air for the preparation of alpha-alumina ceramics from homogeneous precursors. Stereolithographic 3D printing of alpha-alumina ceramics was tested, in particular with the use of the proposed precursors in the form of photopolymerizable binders allowing the fraction of alumina in photosuspensions to be increased.
- 1 February 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 59 (2) , 210-220
Stereolithographic Fabrication of Alumina Ceramics from Aluminum Chloride-Containing Polymerizable Precursors
An approach has been proposed for preparing polymerizable precursors to alpha-alumina and aluminum oxynitride ceramics and using them in stereolithographic fabrication of aluminum-containing ceramics. With allowance for their homogeneity (optical transmission), photopolymerizability, and weight loss during thermolysis, three precursors based on aluminum chlorides (anhydrous and hexahydrate) and a basic aluminum chloride were chosen for characterization. We analyzed the behavior of the precursors during firing in an ammonia atmosphere for the preparation of oxynitride ceramics and during firing in air for the preparation of alpha-alumina ceramics from homogeneous precursors. Stereolithographic 3D printing of alpha-alumina ceramics was tested, in particular with the use of the proposed precursors in the form of photopolymerizable binders allowing the fraction of alumina in photosuspensions to be increased.
- 1 September 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 57 (9) , 958-966
Synthesis of Submicron Са3–хNa2х(PO4)2 Substituted Calcium Phosphate Powders in a Nonaqueous Medium for Stereolithographic Fabrication of Bioceramics
This paper compares the synthesis of tricalcium phosphate (TCP) (β-Са3(РО4)2) and Са3–хNa2х(PO4)2 substituted calcium phosphates (x = 0.5 and 1: solid solution A and β-CaNaPO4 sodium rhenanite, respectively) via precipitation and by a sol–gel process in ethylene glycol (EG). We have determined the phase composition of the synthesized phosphate powders and studied their micromorphology. Slow addition of ammonium (di)hydrogen phosphate to calcium ethylene glycolate at temperatures above 110°C leads to precipitation of crystalline β-TCP (with an average particle size under 200 nm) from the solution. In the synthesis of sodium calcium substituted phosphates, solvolysis of the sodium phosphates prevents congruent precipitation and requires correction of solution composition. The powder precipitated from a solution of sodium ethylate and calcium ethylene glycolate in EG (molar ratio above 2) crystallizes at 800°C in the rhenanite structure (particle size under 500 nm). In sol–gel synthesis, triethyl phosphate (TEP) was used as a phosphate component. For gelation, we used TEP solvolysis in EG and the formation of ester polymers as a result of reaction between citric acid and EG (Pechini process). The gel thermolysis products obtained between 600 and 800°C contained considerable amounts of residual carbon. The particle size characteristics and sinterability of the calcium phosphate powders precipitated from solutions in EG allow them to be used for filling photosuspensions that are employed in the fabrication of osteoconductive bioceramics with the use of stereolithographic 3D printing.
- 1 September 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 57 (9) , 958-966
Synthesis of Submicron Са3–хNa2х(PO4)2 Substituted Calcium Phosphate Powders in a Nonaqueous Medium for Stereolithographic Fabrication of Bioceramics
This paper compares the synthesis of tricalcium phosphate (TCP) (β-Са3(РО4)2) and Са3–хNa2х(PO4)2 substituted calcium phosphates (x = 0.5 and 1: solid solution A and β-CaNaPO4 sodium rhenanite, respectively) via precipitation and by a sol–gel process in ethylene glycol (EG). We have determined the phase composition of the synthesized phosphate powders and studied their micromorphology. Slow addition of ammonium (di)hydrogen phosphate to calcium ethylene glycolate at temperatures above 110°C leads to precipitation of crystalline β-TCP (with an average particle size under 200 nm) from the solution. In the synthesis of sodium calcium substituted phosphates, solvolysis of the sodium phosphates prevents congruent precipitation and requires correction of solution composition. The powder precipitated from a solution of sodium ethylate and calcium ethylene glycolate in EG (molar ratio above 2) crystallizes at 800°C in the rhenanite structure (particle size under 500 nm). In sol–gel synthesis, triethyl phosphate (TEP) was used as a phosphate component. For gelation, we used TEP solvolysis in EG and the formation of ester polymers as a result of reaction between citric acid and EG (Pechini process). The gel thermolysis products obtained between 600 and 800°C contained considerable amounts of residual carbon. The particle size characteristics and sinterability of the calcium phosphate powders precipitated from solutions in EG allow them to be used for filling photosuspensions that are employed in the fabrication of osteoconductive bioceramics with the use of stereolithographic 3D printing.
- 2 October 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (10) , 1062-1070
Synthesis of Substituted Octacalcium Phosphate for Filling Composite Implants Based on Polymer Hydrogels Produced by Stereolithographic 3D Printing
Based on theoretical and experimental analysis of ionic equilibria in buffer solutions, we have found conditions for octacalcium phosphate (OCP), Ca8(HPO4)2(PO4)4 ∙ 5H2O, synthesis....
- 2 October 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (10) , 1062-1070
Synthesis of Substituted Octacalcium Phosphate for Filling Composite Implants Based on Polymer Hydrogels Produced by Stereolithographic 3D Printing
Based on theoretical and experimental analysis of ionic equilibria in buffer solutions, we have found conditions for octacalcium phosphate (OCP), Ca8(HPO4)2(PO4)4 ∙ 5H2O, synthesis....
- 4 May 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (5) , 500-508
Resorption of Ca3 – xM2x(PO4)2 (M = Na, K) Calcium Phosphate Bioceramics in Model Solutions
The resorbability of bioceramics in the Ca3(PO4)2–CaNaPO4–CaKPO4system is evaluated in an approach involving thermodynamic assessment of solubility and investigation of the dissolution kinetics in...
- 4 May 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (5) , 500-508
Resorption of Ca3 – xM2x(PO4)2 (M = Na, K) Calcium Phosphate Bioceramics in Model Solutions
The resorbability of bioceramics in the Ca3(PO4)2–CaNaPO4–CaKPO4system is evaluated in an approach involving thermodynamic assessment of solubility and investigation of the dissolution kinetics in...
- 23 April 2017
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 53 (5) , 529-535
Fabrication of osteoconductive Ca3–x M2x (PO4)2 (M = Na, K) calcium phosphate bioceramics by stereolithographic 3D printing
Osteoconductive ceramic implants based on Ca3–xM2x(PO4)2 (M = Na, K) double phosphates and having the Kelvin structure, tailored macropore size (in the range 50–750 μm), and a total porosity of 70–80% have been produced by stereolithographic 3D printing. We demonstrate that, to maintain the initial geometry of a model and reach sufficiently high strength characteristics of macroporous ceramics (compressive strength up to 9 MPa and fracture toughness up to 0.7 MPa m1/2), the polymer component should be removed under specially tailored heat treatment conditions. Based on our results on polymer matrix destruction kinetics, we have found heat treatment conditions that ensure a polymer removal rate no higher than 0.1 wt%/min and allow one to avoid implant cracking during the firing process.
- 23 April 2017
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 53 (5) , 529-535
Fabrication of osteoconductive Ca3–x M2x (PO4)2 (M = Na, K) calcium phosphate bioceramics by stereolithographic 3D printing
Osteoconductive ceramic implants based on Ca3–xM2x(PO4)2 (M = Na, K) double phosphates and having the Kelvin structure, tailored macropore size (in the range 50–750 μm), and a total porosity of 70–80% have been produced by stereolithographic 3D printing. We demonstrate that, to maintain the initial geometry of a model and reach sufficiently high strength characteristics of macroporous ceramics (compressive strength up to 9 MPa and fracture toughness up to 0.7 MPa m1/2), the polymer component should be removed under specially tailored heat treatment conditions. Based on our results on polymer matrix destruction kinetics, we have found heat treatment conditions that ensure a polymer removal rate no higher than 0.1 wt%/min and allow one to avoid implant cracking during the firing process.