Milton Sergio Fernandes De Lima
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Milton Sergio Fernandes De Lima has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Adilson Rodrigues da Costa
UFOP
1 shared publication - David Dias
Postgraduate Program in Aeronautical and Mechanical Engineering, Aeronautical Institute of Technology, Vila das Acácias, Sao José dos Campos 12200-000, Brazil
1 shared publication - Filipe Augusto Santos Rocha
Instituto Tecnológico Vale (ITV)—Avenida Juscelino Kubitschek, 31, Bauxita, 35400-000 Ouro Preto, Brazil
1 shared publication - Gabriel Carvalho Garcia
Instituto Tecnológico Vale (ITV)—Avenida Juscelino Kubitschek, 31, Bauxita, 35400-000 Ouro Preto, Brazil
1 shared publication - Geraldo Lúcio de Faria
Campus Universitário do Morro do Cruzeiro, Universidade Federal de Ouro Preto, Ouro Preto, Brazil
1 shared publication - Gustavo Medeiros Freitas
Instituto Tecnológico Vale (ITV), Avenida Juscelino Kubitschek, 31, Bauxita, 35400-000 Ouro Preto, MG, Brazil
1 shared publication
Latest Publications
- Open Access
Fiber Laser Surface Melting of a NiTi Superelastic Alloy: Influence on Structural and Mechanical Properties
The surface melting of a NiTi superelastic alloy using a high-power laser Yb:Fiber was investigated. The influence of this process on the microstructural and mechanical properties was also examined. The reference material was a 3 mm nitinol strip with a homogeneous austenitic B2 phase. For the laser surface melting process, input fluences were applied from 17.5 to 45 J/mm2. The morphology of the structure and the chemical composition of several regions were determined by optical microscopy, scanning electron microscopy, dispersive energy spectra, and X-ray diffraction techniques. The mechanical properties, such as modulus of elasticity and hardness, were determined using nanoindentation and microindentation techniques. The greatest surface finishing of the fusion zone was observed for the condition 35 J/mm2. Three well-defined regions (fusion zone (FZ), heat-affected zone (HAZ), base metal (BM)) could be observed and dimensions of grain size, width, and depth of the melted pool were directly affected by the laser fluence. The geometry of the molten pool could be controlled by the optimization of the laser parameters. High laser fluence caused preferential volatilization of nickel, dynamic precipitation of intermetallic phases, including Ti2Ni, Ni3Ti, and Ni4Ti3, as well as solubilization of TiC in the matrix, which led to grain refinement. Thus, high laser fluence is a suitable technique to enhance mechanical properties such as hardness and Young’s modulus.
Open AccessFiber Laser Surface Melting of a NiTi Superelastic Alloy: Influence on Structural and Mechanical Properties
The surface melting of a NiTi superelastic alloy using a high-power laser Yb:Fiber was investigated. The influence of this process on the microstructural and mechanical properties was also examined. The reference material was a 3 mm nitinol strip with a homogeneous austenitic B2 phase. For the laser surface melting process, input fluences were applied from 17.5 to 45 J/mm2. The morphology of the structure and the chemical composition of several regions were determined by optical microscopy, scanning electron microscopy, dispersive energy spectra, and X-ray diffraction techniques. The mechanical properties, such as modulus of elasticity and hardness, were determined using nanoindentation and microindentation techniques. The greatest surface finishing of the fusion zone was observed for the condition 35 J/mm2. Three well-defined regions (fusion zone (FZ), heat-affected zone (HAZ), base metal (BM)) could be observed and dimensions of grain size, width, and depth of the melted pool were directly affected by the laser fluence. The geometry of the molten pool could be controlled by the optimization of the laser parameters. High laser fluence caused preferential volatilization of nickel, dynamic precipitation of intermetallic phases, including Ti2Ni, Ni3Ti, and Ni4Ti3, as well as solubilization of TiC in the matrix, which led to grain refinement. Thus, high laser fluence is a suitable technique to enhance mechanical properties such as hardness and Young’s modulus.
- Open Access
- 21 September 2017
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 20 (suppl 1) , 8-14
Surface Modification of Ti6Al4V Alloy by Pulsed Lasers: Microstructure and Hydrophobic Behavior
In many aerospace applications, it is important to produce hydro-repellent surfaces because water and ice accumulation could lead to malfunctioning of the part or component with a potential critical failure. In this study, it was investigated the texturing of a titanium alloy (Ti6Al4V) by applying a pulsed Nd:YAG laser, aimed at the surface characterization by microscopy, X-ray diffraction, roughness and nano-indentation tests as well as free fall drop test. The experimental procedure aimed to understand the influence of three variables: (N) the number of laser runs 1, 2, 5 and 10; (V) laser speeds of 25, 50 and 100 cm/s and (P) laser power of 5, 10 and 20 W on the microstructure and the hydrophobic behavior. The Vickers hardness and elastic modulus of laser processed surfaces were similar to the untreated surfaces. When the number of the laser runs (N) increased, a TiO phase amount increases as a result of increasing heat input. The measured roughnesses decreased with increasing P as a direct result of remelting. As the number of runs (N) increases the surface became more and more flat, consequently the overlapping runs induced polishing of the titanium surfaces. The mean roughness Ra attained 0.23 µm after 10 runs at V=100m/s and P=10W, compared to Ra=0.41 µm of the virgin surface. The water repellent conditions were N1V50P05, N1V100P05, N2V25P05, N2V50P05, N5V25P05, N5V50P05, N5V100P10 and N10V25P10. These conditions were associated with a homogeneous remelted layer, low power, partial superposition of the laser shots of 50% or 75%, and a surface finish slightly rougher than the original material.
- 21 September 2017
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 20 (suppl 1) , 8-14
Open AccessSurface Modification of Ti6Al4V Alloy by Pulsed Lasers: Microstructure and Hydrophobic Behavior
In many aerospace applications, it is important to produce hydro-repellent surfaces because water and ice accumulation could lead to malfunctioning of the part or component with a potential critical failure. In this study, it was investigated the texturing of a titanium alloy (Ti6Al4V) by applying a pulsed Nd:YAG laser, aimed at the surface characterization by microscopy, X-ray diffraction, roughness and nano-indentation tests as well as free fall drop test. The experimental procedure aimed to understand the influence of three variables: (N) the number of laser runs 1, 2, 5 and 10; (V) laser speeds of 25, 50 and 100 cm/s and (P) laser power of 5, 10 and 20 W on the microstructure and the hydrophobic behavior. The Vickers hardness and elastic modulus of laser processed surfaces were similar to the untreated surfaces. When the number of the laser runs (N) increased, a TiO phase amount increases as a result of increasing heat input. The measured roughnesses decreased with increasing P as a direct result of remelting. As the number of runs (N) increases the surface became more and more flat, consequently the overlapping runs induced polishing of the titanium surfaces. The mean roughness Ra attained 0.23 µm after 10 runs at V=100m/s and P=10W, compared to Ra=0.41 µm of the virgin surface. The water repellent conditions were N1V50P05, N1V100P05, N2V25P05, N2V50P05, N5V25P05, N5V50P05, N5V100P10 and N10V25P10. These conditions were associated with a homogeneous remelted layer, low power, partial superposition of the laser shots of 50% or 75%, and a surface finish slightly rougher than the original material.
- Open Access
- 1 June 2017
- Published by FapUNIFESP (SciELO) in REM - International Engineering Journal
- Vol. 70 (2) , 181-186
Evaluation of hydrogen-Induced cracking resistance of the In625 laser coating system on a C-Mn steel substrate
The corrosion of C-Mn steels in the presence of hydrogen sulfide (H2S) represents a significant challenge to oil production and natural gas treatment facilities. The failure mechanism induced by hydrogen-induced cracking (HIC) in a Inconel 625 coating / C-Mn steel has not been extensively investigated in the past. In the present work, an API 5CT steel was coated with In625 alloy using laser cladding and the HIC resistance of different regions, such as the coating surface, the substrate and HAZ, were evaluated. SEM observations illustrated that all HIC cracks were formed at the hard HAZ after 96h of exposure. No HIC cracks were observed in the substrate and the In625 coating after the same exposure duration. Pitting was recorded in the substrate caused by non-metallic inclusion dissolving.
- 1 June 2017
- Published by FapUNIFESP (SciELO) in REM - International Engineering Journal
- Vol. 70 (2) , 181-186
Open AccessEvaluation of hydrogen-Induced cracking resistance of the In625 laser coating system on a C-Mn steel substrate
The corrosion of C-Mn steels in the presence of hydrogen sulfide (H2S) represents a significant challenge to oil production and natural gas treatment facilities. The failure mechanism induced by hydrogen-induced cracking (HIC) in a Inconel 625 coating / C-Mn steel has not been extensively investigated in the past. In the present work, an API 5CT steel was coated with In625 alloy using laser cladding and the HIC resistance of different regions, such as the coating surface, the substrate and HAZ, were evaluated. SEM observations illustrated that all HIC cracks were formed at the hard HAZ after 96h of exposure. No HIC cracks were observed in the substrate and the In625 coating after the same exposure duration. Pitting was recorded in the substrate caused by non-metallic inclusion dissolving.
- Open Access
Discontinuity Detection in the Shield Metal Arc Welding Process
This work proposes a new methodology for the detection of discontinuities in the weld bead applied in Shielded Metal Arc Welding (SMAW) processes. The detection system is based on two sensors—a microphone and piezoelectric—that acquire acoustic emissions generated during the welding. The feature vectors extracted from the sensor dataset are used to construct classifier models. The approaches based on Artificial Neural Network (ANN) and Support Vector Machine (SVM) classifiers are able to identify with a high accuracy the three proposed weld bead classes: desirable weld bead, shrinkage cavity and burn through discontinuities. Experimental results illustrate the system’s high accuracy, greater than 90% for each class. A novel Hierarchical Support Vector Machine (HSVM) structure is proposed to make feasible the use of this system in industrial environments. This approach presented 96.6% overall accuracy. Given the simplicity of the equipment involved, this system can be applied in the metal transformation industries.
Open AccessDiscontinuity Detection in the Shield Metal Arc Welding Process
This work proposes a new methodology for the detection of discontinuities in the weld bead applied in Shielded Metal Arc Welding (SMAW) processes. The detection system is based on two sensors—a microphone and piezoelectric—that acquire acoustic emissions generated during the welding. The feature vectors extracted from the sensor dataset are used to construct classifier models. The approaches based on Artificial Neural Network (ANN) and Support Vector Machine (SVM) classifiers are able to identify with a high accuracy the three proposed weld bead classes: desirable weld bead, shrinkage cavity and burn through discontinuities. Experimental results illustrate the system’s high accuracy, greater than 90% for each class. A novel Hierarchical Support Vector Machine (HSVM) structure is proposed to make feasible the use of this system in industrial environments. This approach presented 96.6% overall accuracy. Given the simplicity of the equipment involved, this system can be applied in the metal transformation industries.