Xuanru Ren
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xuanru Ren has a total of 61 co-authors. Here are the top co-authors by number of shared publications:
Peizhong Feng
6 shared publicationsYuexing Chen
5 shared publicationsBaojing Zhang
4 shared publications- Peizhong Feng
China University of Mining and Technology
4 shared publications Xueqin Kang
4 shared publicationsEvgeny A. Levashov
3 shared publications
Latest Publications
- Open Access
- 1 May 2026
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 15 (7)
Oxidation-driven glass evolution enabling self-sealing protection in HfB 2 -based boride–silicide coatings at high temperatures
At high temperatures, oxidation is generally regarded as an unavoidable degradation process for ceramic protective coatings. Here, oxidation is shown to drive dynamic glass evolution and form a robust self-sealing barrier under extreme thermal conditions. An in situ alloyed boride-silicide composite coating is constructed, and the controlled incorporation of HfSi2 is found to change oxide-scale development by providing additional Hf and Si sources during oxidation and promoting the early formation and continuous reconstruction of a highly sealing Hf-Si-O glassy layer. The optimized coating exhibits exceptional oxidation resistance at 1700 °C, with oxygen permeability and carbon loss rate reduced by 61.67% and 75.26%, respectively, corresponding to an average protection efficiency of 99.94%. Mechanistically, oxidation-driven glass evolution seals pores and microcracks and slows inward oxygen diffusion, whereas appropriate HfSi2 incorporation helps compact and stabilize the glassy layer, while excessive glass stiffening reduces high-temperature fluidity and weakens scale integrity. These findings provide a general design method for improving self-sealing oxidation protection at high temperatures.
- 1 May 2026
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 15 (7)
Open AccessOxidation-driven glass evolution enabling self-sealing protection in HfB 2 -based boride–silicide coatings at high temperatures
At high temperatures, oxidation is generally regarded as an unavoidable degradation process for ceramic protective coatings. Here, oxidation is shown to drive dynamic glass evolution and form a robust self-sealing barrier under extreme thermal conditions. An in situ alloyed boride-silicide composite coating is constructed, and the controlled incorporation of HfSi2 is found to change oxide-scale development by providing additional Hf and Si sources during oxidation and promoting the early formation and continuous reconstruction of a highly sealing Hf-Si-O glassy layer. The optimized coating exhibits exceptional oxidation resistance at 1700 °C, with oxygen permeability and carbon loss rate reduced by 61.67% and 75.26%, respectively, corresponding to an average protection efficiency of 99.94%. Mechanistically, oxidation-driven glass evolution seals pores and microcracks and slows inward oxygen diffusion, whereas appropriate HfSi2 incorporation helps compact and stabilize the glassy layer, while excessive glass stiffening reduces high-temperature fluidity and weakens scale integrity. These findings provide a general design method for improving self-sealing oxidation protection at high temperatures.
- 11 January 2025
- Published by Elsevier in Applied Surface Science
- Vol. 688
Enhanced oxidation resistance of LaB6-modified HfB2-SiC coating at 1700 °C by low-loss film-forming treatment
- 11 January 2025
- Published by Elsevier in Applied Surface Science
- Vol. 688
Enhanced oxidation resistance of LaB6-modified HfB2-SiC coating at 1700 °C by low-loss film-forming treatment
- 25 November 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (3)
Enhancing oxygen‐blocking properties of HfB 2 ‐MoSi 2 ‐SiC coating by CeO 2 modification
To alleviate the destructive alteration of the glass layer surface caused by gas evolution during the oxygen‐blocking process of the HfB 2 ‐MoSi 2 ‐SiC coating, CeO 2 was incorporated to modify HfB 2 ‐MoSi 2 ‐SiC coating, and the anti‐oxidation mechanism at 1700°C in air was investigated. Compared with the unmodified HfB 2 ‐MoSi 2 ‐SiC coating, the addition of the refractory CeO 2 to the Hf‐B‐Si‐O system leads to the formation of a stable Hf‐Ce‐B‐Si‐O complex phase glass, which substantially enhances the viscosity, stability, and self‐healing sealing properties of the glass layer. The introduction of 0.75 vol.% CeO 2 significantly lowers the oxidative activity of the HfB 2 ‐MoSi 2 ‐SiC coating, boosting its average protective efficiency to 99.96% and reducing the maximal oxygen permeability by 43.48%, thus exhibiting superior oxygen‐blocking performance. However, excessive addition of CeO 2 leads to an overabundance of oxygen release through its distinctive oxygen vacancy mechanism, which accelerates the formation of Hf‐oxides, resulting in excessive viscosity on the coating surface and leaving oxidation defects unrepaired.
- 25 November 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (3)
Enhancing oxygen‐blocking properties of HfB 2 ‐MoSi 2 ‐SiC coating by CeO 2 modification
To alleviate the destructive alteration of the glass layer surface caused by gas evolution during the oxygen‐blocking process of the HfB 2 ‐MoSi 2 ‐SiC coating, CeO 2 was incorporated to modify HfB 2 ‐MoSi 2 ‐SiC coating, and the anti‐oxidation mechanism at 1700°C in air was investigated. Compared with the unmodified HfB 2 ‐MoSi 2 ‐SiC coating, the addition of the refractory CeO 2 to the Hf‐B‐Si‐O system leads to the formation of a stable Hf‐Ce‐B‐Si‐O complex phase glass, which substantially enhances the viscosity, stability, and self‐healing sealing properties of the glass layer. The introduction of 0.75 vol.% CeO 2 significantly lowers the oxidative activity of the HfB 2 ‐MoSi 2 ‐SiC coating, boosting its average protective efficiency to 99.96% and reducing the maximal oxygen permeability by 43.48%, thus exhibiting superior oxygen‐blocking performance. However, excessive addition of CeO 2 leads to an overabundance of oxygen release through its distinctive oxygen vacancy mechanism, which accelerates the formation of Hf‐oxides, resulting in excessive viscosity on the coating surface and leaving oxidation defects unrepaired.
- 4 June 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 107 (10) , 6678-6691
Enhanced oxidation resistance of HfB 2 ‐SiC‐ZrSi 2 coating at 1700°C through low‐loss film‐forming treatment
To enhance the oxidation resistance of HfB 2 ‐SiC‐ZrSi 2 coating, low‐loss film‐forming treatment (LFT) was employed to generate high‐quality oxygen barrier glass layers, and the modification effect of varying formation temperature on the oxidation resistance was investigated at 1700°C. The results demonstrated that, with LFT at 1500°C, the relatively modest oxidation activity and complete dispersion of metal oxide nanocrystals generated a compact and continuous composite glass layer, which caused a decreased oxidation activity at 1700°C. The excessive formation temperature might result in oxidized and porous coatings, while lower temperatures could lead to poor fluidity of the glass layer, rendering it challenging to achieve compact composite glass layers. The coating sample with LFT at 1500°C exhibited a carbon loss rate of 0.33 × 10 −6 g·cm −2 ·s −1 and an oxygen permeability level of 0.28%, respectively, when oxidized at 1700°C. These results provide fundamental insights into the oxidation resistance mechanisms within the modified HfB 2 ‐SiC‐ZrSi 2 coating system.
- 4 June 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 107 (10) , 6678-6691
Enhanced oxidation resistance of HfB 2 ‐SiC‐ZrSi 2 coating at 1700°C through low‐loss film‐forming treatment
To enhance the oxidation resistance of HfB 2 ‐SiC‐ZrSi 2 coating, low‐loss film‐forming treatment (LFT) was employed to generate high‐quality oxygen barrier glass layers, and the modification effect of varying formation temperature on the oxidation resistance was investigated at 1700°C. The results demonstrated that, with LFT at 1500°C, the relatively modest oxidation activity and complete dispersion of metal oxide nanocrystals generated a compact and continuous composite glass layer, which caused a decreased oxidation activity at 1700°C. The excessive formation temperature might result in oxidized and porous coatings, while lower temperatures could lead to poor fluidity of the glass layer, rendering it challenging to achieve compact composite glass layers. The coating sample with LFT at 1500°C exhibited a carbon loss rate of 0.33 × 10 −6 g·cm −2 ·s −1 and an oxygen permeability level of 0.28%, respectively, when oxidized at 1700°C. These results provide fundamental insights into the oxidation resistance mechanisms within the modified HfB 2 ‐SiC‐ZrSi 2 coating system.
- 17 November 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (3) , 2155-2168
Effect of La 2 O 3 content on the oxygen barrier ability of the HfB 2 ‐SiC coating at 1973 K
To inhibit the destructive evolution of the HfB 2 ‐SiC coating during oxidation, La 2 O 3 was added to modify the oxygen‐blocking capability of the HfB 2 ‐SiC coating. The effect of La 2 O 3 content on the oxygen barrier capacity of HfB 2 ‐SiC was investigated. The addition of 5 vol.% La 2 O 3 lowered the oxidation activity and strengthened the inert oxygen barrier capacity of the HfB 2 ‐SiC coating, which made the oxygen permeability and maximum weight change rate of the coating decrease by 30.32% and 73.97%, respectively. Due to the solid solution reaction of the dispersed La 2 O 3 , HfO 2 , and SiO 2 nanoparticles, a stable Hf‐B‐La‐Si‐O multiphase glass was formed on the surface of the coating. Besides, the high‐melting‐point particles, such as HfO 2 , La 2 Hf 2 O 7 , and HfSiO 4 , dispersed in the glass layer as hard particles and formed a mosaic structure based on the Hf‐B‐La‐Si‐O compound, which increased the cumulative protection efficiency of the HfB 2 ‐SiC coating to 98.5% and reduced the inert factor value by 84.57%. However, the excessive consumption of SiO 2 glass by La 2 O 3 results in dendritization of the generated glass when the La 2 O 3 content is above 10 vol.%, which reduced the self‐healing capability of the generated glass and instead weakened the oxygen barrier properties of the HfB 2 ‐SiC‐La 2 O 3 coatings.
- 17 November 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (3) , 2155-2168
Effect of La 2 O 3 content on the oxygen barrier ability of the HfB 2 ‐SiC coating at 1973 K
To inhibit the destructive evolution of the HfB 2 ‐SiC coating during oxidation, La 2 O 3 was added to modify the oxygen‐blocking capability of the HfB 2 ‐SiC coating. The effect of La 2 O 3 content on the oxygen barrier capacity of HfB 2 ‐SiC was investigated. The addition of 5 vol.% La 2 O 3 lowered the oxidation activity and strengthened the inert oxygen barrier capacity of the HfB 2 ‐SiC coating, which made the oxygen permeability and maximum weight change rate of the coating decrease by 30.32% and 73.97%, respectively. Due to the solid solution reaction of the dispersed La 2 O 3 , HfO 2 , and SiO 2 nanoparticles, a stable Hf‐B‐La‐Si‐O multiphase glass was formed on the surface of the coating. Besides, the high‐melting‐point particles, such as HfO 2 , La 2 Hf 2 O 7 , and HfSiO 4 , dispersed in the glass layer as hard particles and formed a mosaic structure based on the Hf‐B‐La‐Si‐O compound, which increased the cumulative protection efficiency of the HfB 2 ‐SiC coating to 98.5% and reduced the inert factor value by 84.57%. However, the excessive consumption of SiO 2 glass by La 2 O 3 results in dendritization of the generated glass when the La 2 O 3 content is above 10 vol.%, which reduced the self‐healing capability of the generated glass and instead weakened the oxygen barrier properties of the HfB 2 ‐SiC‐La 2 O 3 coatings.
- 5 October 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (2) , 1568-1580
Oxidation inhibition behaviors of HfB 2 ‐MoSi 2 ‐SiC oxygen blocking coating prepared by spark plasma sintering
The HfB 2 ‐MoSi 2 ‐SiC oxygen blocking coatings were prepared by the spark plasma sintering (SPS) technique, whose oxidation inhibition ability was further strengthened by the pre‐oxidation treatment. The effect of MoSi 2 content and pre‐oxidation treatment process on the oxygen blocking ability of the HfB 2 ‐MoSi 2 ‐SiC coating at 1973 K were conducted. After SPS, for the HfB 2 ‐MoSi 2 ‐SiC coatings with 20 wt%, 40 wt%, and 60 wt% MoSi 2 , the relative density of the coatings are 92.6%, 93.9%, and 85.6%, respectively. Owing to the enhanced compactness of the coatings, increasing MoSi 2 content can significantly improve the protection efficiency of the coatings during the activation oxidation stage. However, due to the increased formation of gaseous by‐products during the inerting oxidation stage, excessive MoSi 2 weaken the oxidation inhibition ability of the coatings. The sufficient dispersion of Hf‐oxides nanocrystals in the glass layer conduces to enhance the oxygen blocking ability of the glass layer, making the 40HfB 2 ‐40MoSi 2 ‐20SiC coating present the best oxidation protective ability. The pre‐oxidation treatment at 1773 K conduces to form the steady glass layer with fewer defects at the cost of a lower oxidation consumption of the coating, which enhanced the protection efficiency of the coating from 96.9% to 99.8% and reduced the oxygen permeability from 0.13% to 0.028%.
- 5 October 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (2) , 1568-1580
Oxidation inhibition behaviors of HfB 2 ‐MoSi 2 ‐SiC oxygen blocking coating prepared by spark plasma sintering
The HfB 2 ‐MoSi 2 ‐SiC oxygen blocking coatings were prepared by the spark plasma sintering (SPS) technique, whose oxidation inhibition ability was further strengthened by the pre‐oxidation treatment. The effect of MoSi 2 content and pre‐oxidation treatment process on the oxygen blocking ability of the HfB 2 ‐MoSi 2 ‐SiC coating at 1973 K were conducted. After SPS, for the HfB 2 ‐MoSi 2 ‐SiC coatings with 20 wt%, 40 wt%, and 60 wt% MoSi 2 , the relative density of the coatings are 92.6%, 93.9%, and 85.6%, respectively. Owing to the enhanced compactness of the coatings, increasing MoSi 2 content can significantly improve the protection efficiency of the coatings during the activation oxidation stage. However, due to the increased formation of gaseous by‐products during the inerting oxidation stage, excessive MoSi 2 weaken the oxidation inhibition ability of the coatings. The sufficient dispersion of Hf‐oxides nanocrystals in the glass layer conduces to enhance the oxygen blocking ability of the glass layer, making the 40HfB 2 ‐40MoSi 2 ‐20SiC coating present the best oxidation protective ability. The pre‐oxidation treatment at 1773 K conduces to form the steady glass layer with fewer defects at the cost of a lower oxidation consumption of the coating, which enhanced the protection efficiency of the coating from 96.9% to 99.8% and reduced the oxygen permeability from 0.13% to 0.028%.
- Open Access
- 15 September 2021
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 10 (5) , 1011-1024
Preparation of ZrB2-MoSi2 high oxygen resistant coating using nonequilibrium state powders by self-propagating high-temperature synthesis
To achieve high oxygen blocking structure of the ZrB2-MoSi2 coating applied on carbon structural material, ZrB2-MoSi2 coating was prepared by spark plasma sintering (SPS) method utilizing ZrB2-MoSi2 composite powders synthesized by self-propagating high-temperature synthesis (SHS) technique as raw materials. The oxygen blocking mechanism of the ZrB2-MoSi2 coatings at 1973 K was investigated. Compared with commercial powders, the coatings prepared by SHS powders exhibited superior density and inferior oxidation activity, which significantly heightened the structural oxygen blocking ability of the coatings in the active oxidation stage, thus characterizing higher oxidation protection efficiency. The rise of MoSi2 content facilitated the dispersion of transition metal oxide nanocrystals (5–20 nm) in the SiO2 glass layer and conduced to the increasing viscosity, thus strengthening the inerting impact of the compound glass layer in the inert oxidation stage. Nevertheless, the ZrB2-40 vol%MoSi2 coating sample prepared by SHS powders presented the lowest oxygen permeability of 0.3% and carbon loss rate of 0.29×10−6 g·cm−2·s−1. Owing to the gradient oxygen partial pressure inside the coatings, the Si-depleted layer was developed under the compound glass layer, which brought about acute oxygen erosion.
- 15 September 2021
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 10 (5) , 1011-1024
Open AccessPreparation of ZrB2-MoSi2 high oxygen resistant coating using nonequilibrium state powders by self-propagating high-temperature synthesis
To achieve high oxygen blocking structure of the ZrB2-MoSi2 coating applied on carbon structural material, ZrB2-MoSi2 coating was prepared by spark plasma sintering (SPS) method utilizing ZrB2-MoSi2 composite powders synthesized by self-propagating high-temperature synthesis (SHS) technique as raw materials. The oxygen blocking mechanism of the ZrB2-MoSi2 coatings at 1973 K was investigated. Compared with commercial powders, the coatings prepared by SHS powders exhibited superior density and inferior oxidation activity, which significantly heightened the structural oxygen blocking ability of the coatings in the active oxidation stage, thus characterizing higher oxidation protection efficiency. The rise of MoSi2 content facilitated the dispersion of transition metal oxide nanocrystals (5–20 nm) in the SiO2 glass layer and conduced to the increasing viscosity, thus strengthening the inerting impact of the compound glass layer in the inert oxidation stage. Nevertheless, the ZrB2-40 vol%MoSi2 coating sample prepared by SHS powders presented the lowest oxygen permeability of 0.3% and carbon loss rate of 0.29×10−6 g·cm−2·s−1. Owing to the gradient oxygen partial pressure inside the coatings, the Si-depleted layer was developed under the compound glass layer, which brought about acute oxygen erosion.
- 5 February 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (7) , 3682-3694
Preparation and high‐temperature oxidation resistance of multilayer MoSi 2 /MoB coating by spent MoSi 2 ‐based materials
Spent MoSi 2 and MoB were used as raw materials to prepare multilayer MoSi 2 /MoB coating on molybdenum by the two‐step method of slurry deposition and spark plasma sintering. The results showed dense MoSi 2 /MoB coating after sintering while penetrated cracks appeared in MoSi 2 coating due to coefficient of thermal expansion mismatch between the Mo substrate and coating. After the sintering of MoSi 2 /MoB coatings, MoB and Mo 2 B diffusion layers were formed between MoB transition layer and Mo substrate without defects, exhibiting good metallurgical bonding. The high‐temperature oxidation behavior of coatings (1500°C) was also explored. After oxidation of 50 h at 1500°C, lowest mass gain (0.035 mg/cm 2 ) was obtained for MoSi 2 /MoB coating, and the oxide scale was dense and complete without voids, making the oxygen diffusion at elevated temperature inhibited. Compared with MoSi 2 coating under the same oxidation conditions, relatively thinner silica oxide scale was acquired by MoSi 2 /MoB coating because of the reduction of cracks, and the multilayer coating exhibits better anti‐oxidation properties at high temperature.
- 5 February 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (7) , 3682-3694
Preparation and high‐temperature oxidation resistance of multilayer MoSi 2 /MoB coating by spent MoSi 2 ‐based materials
Spent MoSi 2 and MoB were used as raw materials to prepare multilayer MoSi 2 /MoB coating on molybdenum by the two‐step method of slurry deposition and spark plasma sintering. The results showed dense MoSi 2 /MoB coating after sintering while penetrated cracks appeared in MoSi 2 coating due to coefficient of thermal expansion mismatch between the Mo substrate and coating. After the sintering of MoSi 2 /MoB coatings, MoB and Mo 2 B diffusion layers were formed between MoB transition layer and Mo substrate without defects, exhibiting good metallurgical bonding. The high‐temperature oxidation behavior of coatings (1500°C) was also explored. After oxidation of 50 h at 1500°C, lowest mass gain (0.035 mg/cm 2 ) was obtained for MoSi 2 /MoB coating, and the oxide scale was dense and complete without voids, making the oxygen diffusion at elevated temperature inhibited. Compared with MoSi 2 coating under the same oxidation conditions, relatively thinner silica oxide scale was acquired by MoSi 2 /MoB coating because of the reduction of cracks, and the multilayer coating exhibits better anti‐oxidation properties at high temperature.
- Open Access
- 13 August 2020
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 9 (6) , 703-715
Influence of MoSi2 on oxidation protective ability of TaB2-SiC coating in oxygen-containing environments within a broad temperature range
TaB2-SiC coating modified by different content of MoSi2 was fabricated on graphite substrate with SiC inner coating by liquid phase sintering to elevate the anti-oxidation capability of the TaB2-SiC coatings. As compared to the sample with the TaB2—40wt%SiC coating, the coating sample modified with MoSi2 exhibited a weight gain trend at lower temperatures, the fastest weight loss rate went down by 76%, and the relative oxygen permeability value reduced from about 1% to near 0. More importantly, the large amount of SiO2 glass phase produced over the coating during oxidation was in contact with the modification of MoSi2, which was proved to be beneficial to the dispersion of Ta-oxides. A concomitantly formed continuous Ta-Si-O-B compound glass layer showed excellent capacity to prevent oxygen penetration. However, when the TaB2 content was sacrificed to increase the MoSi2 content, the relative oxygen permeability of the coating increased instead of decreased. Thus, on the basis of ample TaB2 content, increasing the MoSi2 content of the coating is conducive to reducing the relative oxygen permeability of the coatings in a broad temperature region.
- 13 August 2020
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 9 (6) , 703-715
Open AccessInfluence of MoSi2 on oxidation protective ability of TaB2-SiC coating in oxygen-containing environments within a broad temperature range
TaB2-SiC coating modified by different content of MoSi2 was fabricated on graphite substrate with SiC inner coating by liquid phase sintering to elevate the anti-oxidation capability of the TaB2-SiC coatings. As compared to the sample with the TaB2—40wt%SiC coating, the coating sample modified with MoSi2 exhibited a weight gain trend at lower temperatures, the fastest weight loss rate went down by 76%, and the relative oxygen permeability value reduced from about 1% to near 0. More importantly, the large amount of SiO2 glass phase produced over the coating during oxidation was in contact with the modification of MoSi2, which was proved to be beneficial to the dispersion of Ta-oxides. A concomitantly formed continuous Ta-Si-O-B compound glass layer showed excellent capacity to prevent oxygen penetration. However, when the TaB2 content was sacrificed to increase the MoSi2 content, the relative oxygen permeability of the coating increased instead of decreased. Thus, on the basis of ample TaB2 content, increasing the MoSi2 content of the coating is conducive to reducing the relative oxygen permeability of the coatings in a broad temperature region.
- 17 June 2020
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 49 (9) , 5346-5352
Solution Combustion Synthesis of Bi2Mo3O12 and Bi2Mo3O12/MoO3 Composites with Enhanced Photocatalytic Properties
- 17 June 2020
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 49 (9) , 5346-5352
Solution Combustion Synthesis of Bi2Mo3O12 and Bi2Mo3O12/MoO3 Composites with Enhanced Photocatalytic Properties