Kota Kadoi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Kota Kadoi has a total of 24 co-authors. Here are the top co-authors by number of shared publications:
Hiroshige Inoue
Joining and Welding Research Institute, Osaka University, Osaka, Japan
3 shared publicationsKenji Shinozaki
3 shared publicationsShotaro Yamashita
IHI Corporation, Japan
2 shared publicationsAkira Takemori
Shinko Welding Service Co. Ltd, Japan
1 shared publicationAtsushi Takada
JFE Steel Corporation, Japan
1 shared publication- Daiki Shiozawa
Department of Mechanical Engineering, Kobe University, Kobe 657-8501, Japan
1 shared publication
Latest Publications
- Open Access
- 19 November 2021
- Published by MDPI AG in Engineering Proceedings
- Vol. 8 (1) , 6
Evaluation of Fatigue Strength Based on Dissipated Energy for Laser Welds
To optimize welding conditions that ensure the safety and reliability of laser welds, this study established an evaluation method of the fatigue strength for the laser welds of steel sheets over a short period of time. This study focuses on a fatigue limit estimation based on dissipated energy which is caused by micro plastic deformation. As a result, the area at which the temperature changes, due to dissipated energy, is locally high is the fracture origin of the laser welds. The fatigue limit of the laser welds is almost the same as the stress amplitude at which a temperature change occurs due to dissipated energy.
- 19 November 2021
- Published by MDPI AG in Engineering Proceedings
- Vol. 8 (1) , 6
Open AccessEvaluation of Fatigue Strength Based on Dissipated Energy for Laser Welds
To optimize welding conditions that ensure the safety and reliability of laser welds, this study established an evaluation method of the fatigue strength for the laser welds of steel sheets over a short period of time. This study focuses on a fatigue limit estimation based on dissipated energy which is caused by micro plastic deformation. As a result, the area at which the temperature changes, due to dissipated energy, is locally high is the fracture origin of the laser welds. The fatigue limit of the laser welds is almost the same as the stress amplitude at which a temperature change occurs due to dissipated energy.
- 2 June 2020
- Published by Taylor & Francis in Welding International
- Vol. 34 (4-6) , 176-184
Influence of microstructural morphology on pitting corrosion resistance of duplex stainless steel weld metals
The formation mechanism of microstructure of duplex stainless steel weld metals with different N content and heat input and the effects of microstructural factors on pitting corrosion resistance of them were investigated. As N content of weld metal increased, ferrite content decreased and Cr nitride content increased. However, once N content exceeded a certain value, Cr nitride content decreased. As the ferrite content of the weld metal decreased, the critical pitting temperature (CPT) increased, and as N content increased, CPT increased. Thus, the pitting corrosion resistance of duplex stainless steel weld metals must be affected by both of N content and Cr nitride, and the precipitation of Cr nitride must also be affected by N content and the ferrite content due to N content and the weld heat input. The results indicated that these microstructural factors were an important index to evaluate the pitting corrosion resistance of duplex stainless steel weld metals.
- 2 June 2020
- Published by Taylor & Francis in Welding International
- Vol. 34 (4-6) , 176-184
Influence of microstructural morphology on pitting corrosion resistance of duplex stainless steel weld metals
The formation mechanism of microstructure of duplex stainless steel weld metals with different N content and heat input and the effects of microstructural factors on pitting corrosion resistance of them were investigated. As N content of weld metal increased, ferrite content decreased and Cr nitride content increased. However, once N content exceeded a certain value, Cr nitride content decreased. As the ferrite content of the weld metal decreased, the critical pitting temperature (CPT) increased, and as N content increased, CPT increased. Thus, the pitting corrosion resistance of duplex stainless steel weld metals must be affected by both of N content and Cr nitride, and the precipitation of Cr nitride must also be affected by N content and the ferrite content due to N content and the weld heat input. The results indicated that these microstructural factors were an important index to evaluate the pitting corrosion resistance of duplex stainless steel weld metals.
- 23 May 2020
- Published by Elsevier in Materials Characterization
- Vol. 165, 110402
Relationship between solidification sequence and toughness of carbon steel weld metal
- 23 May 2020
- Published by Elsevier in Materials Characterization
- Vol. 165, 110402
Relationship between solidification sequence and toughness of carbon steel weld metal
- Open Access
- 15 July 2019
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 59 (7) , 1323-1329
Relationship between Alloy Element and Weld Solidification Cracking Susceptibility of Austenitic Stainless Steel
The effect of alloy elements such as niobium, titanium, and zirconium on the weld solidification cracking susceptibility in fully austenitic stainless steel was investigated. Niobium, titanium, or zirconium was added as an alloy element to Fe-24 mass%Cr-26 mass%Ni stainless steel. The cracking susceptibility was evaluated by crack length, number of cracks, and brittle temperature range (BTR) corresponding to results of the Trans-Varestraint test. Depending on the addition of the alloy element, the crack length increased; the length ordering tendencies between the total crack length (TCL) and the maximum crack length (MCL) differed with the alloy addition. The BTR was obtained by corresponding the MCL to the temperature range using the measured temperature history of the weld metal and was increased by the addition of the alloy element. The maximum BTR for the specimen with titanium was 266.9°C, which was three times that of the specimen without the alloy element. The MC carbide and the Laves phase formed at the dendrite cell boundaries as secondary phases. Solidification calculation based on the Scheil model was used to investigate the effect of the type of the alloy element on the solidification temperature range. Depending on the type of the alloy element, the solidification temperature range varied. A significant difference was found between the solidification temperature range and BTR in the case of the specimen with niobium.
- 15 July 2019
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 59 (7) , 1323-1329
Open AccessRelationship between Alloy Element and Weld Solidification Cracking Susceptibility of Austenitic Stainless Steel
The effect of alloy elements such as niobium, titanium, and zirconium on the weld solidification cracking susceptibility in fully austenitic stainless steel was investigated. Niobium, titanium, or zirconium was added as an alloy element to Fe-24 mass%Cr-26 mass%Ni stainless steel. The cracking susceptibility was evaluated by crack length, number of cracks, and brittle temperature range (BTR) corresponding to results of the Trans-Varestraint test. Depending on the addition of the alloy element, the crack length increased; the length ordering tendencies between the total crack length (TCL) and the maximum crack length (MCL) differed with the alloy addition. The BTR was obtained by corresponding the MCL to the temperature range using the measured temperature history of the weld metal and was increased by the addition of the alloy element. The maximum BTR for the specimen with titanium was 266.9°C, which was three times that of the specimen without the alloy element. The MC carbide and the Laves phase formed at the dendrite cell boundaries as secondary phases. Solidification calculation based on the Scheil model was used to investigate the effect of the type of the alloy element on the solidification temperature range. Depending on the type of the alloy element, the solidification temperature range varied. A significant difference was found between the solidification temperature range and BTR in the case of the specimen with niobium.
- 3 June 2019
- Published by Taylor & Francis in Welding International
- Vol. 33 (4-6) , 189-199
Investigation of standardizing for evaluation method of transverse-Varestraint test
Varestraint test is one of the most-used methods to evaluate weld solidification cracking susceptibility. However, the standard about the detailed test method and the evaluation method has not been clearly defined. Thus, it is required to standardize the methods of Varestraint test and the evaluation indexes in order to compare the results tested by each researcher. In this study, the round-robin test of transverse-Varestraint test with GTAW was carried out under identical specimens and test conditions using five test machines to clarify the influence of the test machine and human factor on the test result. Crack number and crack length were measured using a scanning electron microscope (SEM) and an optical microscope. Six evaluators measured the crack number and length. The maximum crack lengths measured by the evaluators were nearly the same. In contrast, there were big di-erences in the crack numbers and the total crack lengths. Thus, the influence of the human factor on the maximum crack length was relatively low and that on the crack number and the total crack length was high. This should be caused by different judgement depending on the evaluators for the crack opening and the propagated crack tip. Using SEM was an adequate measuring method for the crack length since the measurement using an optical microscope tended to cause false judgement of wrinkle as cracks. Maximum crack length must be appropriate to be used as an evaluation index for solidification cracking susceptibility compared to the total crack length and the crack number.
- 3 June 2019
- Published by Taylor & Francis in Welding International
- Vol. 33 (4-6) , 189-199
Investigation of standardizing for evaluation method of transverse-Varestraint test
Varestraint test is one of the most-used methods to evaluate weld solidification cracking susceptibility. However, the standard about the detailed test method and the evaluation method has not been clearly defined. Thus, it is required to standardize the methods of Varestraint test and the evaluation indexes in order to compare the results tested by each researcher. In this study, the round-robin test of transverse-Varestraint test with GTAW was carried out under identical specimens and test conditions using five test machines to clarify the influence of the test machine and human factor on the test result. Crack number and crack length were measured using a scanning electron microscope (SEM) and an optical microscope. Six evaluators measured the crack number and length. The maximum crack lengths measured by the evaluators were nearly the same. In contrast, there were big di-erences in the crack numbers and the total crack lengths. Thus, the influence of the human factor on the maximum crack length was relatively low and that on the crack number and the total crack length was high. This should be caused by different judgement depending on the evaluators for the crack opening and the propagated crack tip. Using SEM was an adequate measuring method for the crack length since the measurement using an optical microscope tended to cause false judgement of wrinkle as cracks. Maximum crack length must be appropriate to be used as an evaluation index for solidification cracking susceptibility compared to the total crack length and the crack number.
- 11 April 2019
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 756, 92-97
Ductility-dip cracking susceptibility in dissimilar weld metals of alloy 690 filler metal and low alloy steel
- 11 April 2019
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 756, 92-97
Ductility-dip cracking susceptibility in dissimilar weld metals of alloy 690 filler metal and low alloy steel
- Open Access
- 1 January 2018
- Published by Sumart Processing Society for Minerals, Environment and Energy in Journal of Smart Processing
- Vol. 7 (1) , 8-13
High Accurate Evaluation of Weld Solidification Cracking Susceptibility by In-situ Observation Technique
- 1 January 2018
- Published by Sumart Processing Society for Minerals, Environment and Energy in Journal of Smart Processing
- Vol. 7 (1) , 8-13
Open AccessHigh Accurate Evaluation of Weld Solidification Cracking Susceptibility by In-situ Observation Technique
- 25 September 2017
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 48 (12) , 5860-5869
Effect of Chemical Composition on Susceptibility to Weld Solidification Cracking in Austenitic Weld Metal
- 25 September 2017
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 48 (12) , 5860-5869
Effect of Chemical Composition on Susceptibility to Weld Solidification Cracking in Austenitic Weld Metal
- 1 January 2017
- Published by Japan Welding Society in QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
- Vol. 35 (1) , 45-50
Effect of Wire Feeding Conditions on Grain Refinement in Weld Metal of Type 310S Stainless Steel
The aim of this study was to investigate the influence of wire feeding conditions such as wire feeding position and power supply distance on the fine grain formation in weld metal of type 310S stainless steel. When the wire feeding position was far from electrode of GTAW, area ratio of fine grain in weld metal increased. The maximum area ratio was obtained when the filler wire was fed to the back of weld pool and the wire melting depended on the joule heating. When the power supply distance was short, the wire wasn't fed to the back of weld pool. On the other hands, when the power supply distance was long, the wire wasn't also fed to the back of weld pool. Because, this phenomenon was related to the local melting region in the wire corresponding to the temperature gradient of wire. Therefore, the adequate feeding conditions was required to form the fine grain by hot-wire GTAW process.
- 1 January 2017
- Published by Japan Welding Society in QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
- Vol. 35 (1) , 45-50
Effect of Wire Feeding Conditions on Grain Refinement in Weld Metal of Type 310S Stainless Steel
The aim of this study was to investigate the influence of wire feeding conditions such as wire feeding position and power supply distance on the fine grain formation in weld metal of type 310S stainless steel. When the wire feeding position was far from electrode of GTAW, area ratio of fine grain in weld metal increased. The maximum area ratio was obtained when the filler wire was fed to the back of weld pool and the wire melting depended on the joule heating. When the power supply distance was short, the wire wasn't fed to the back of weld pool. On the other hands, when the power supply distance was long, the wire wasn't also fed to the back of weld pool. Because, this phenomenon was related to the local melting region in the wire corresponding to the temperature gradient of wire. Therefore, the adequate feeding conditions was required to form the fine grain by hot-wire GTAW process.