Sergey Rodin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Sergey Rodin has a total of 63 co-authors. Here are the top co-authors by number of shared publications:
- Igor G. Kononov
Russian Academy of Sciences
11 shared publications - Sergey Yu Kazantsev
Moscow Technical University of Communications and Informatics, Moscow, Russia
11 shared publications E M Gavrishchuk
8 shared publicationsE. M. Gavrishchuk
Devyatykh Institute of Chemistry of High-Purity Substances, Russian Academy of Sciences, ul. Tropinina 49, 603951, Nizhny Novgorod, Russia
6 shared publicationsD V Savin
5 shared publicationsD. V. Savin
Devyatykh Institute of Chemistry of High-Purity Substances, Russian Academy of Sciences, ul. Tropinina 49, 603951, Nizhny Novgorod, Russia
5 shared publications
Latest Publications
- 24 December 2019
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 55 (12) , 1201-1205
Fe2+ Diffusion in CVD ZnSe during Annealing in Different (Ar, Zn, and Se) Atmospheres
We have studied Fe2+ diffusion in polycrystalline CVD ZnSe during high-temperature (900–1100°C) annealing in different atmospheres, determined effective Fe2+ diffusion coefficients in CVD ZnSe, and evaluated the activation energy for the diffusion process. Distinctive features of the doping process in Zn vapor have been identified that are responsible for the observed order-of-magnitude increase in Fe diffusion rate in comparison with annealing in Ar and Se. The effect of annealing conditions on Fe diffusion mechanisms is discussed.
- 24 December 2019
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 55 (12) , 1201-1205
Fe2+ Diffusion in CVD ZnSe during Annealing in Different (Ar, Zn, and Se) Atmospheres
We have studied Fe2+ diffusion in polycrystalline CVD ZnSe during high-temperature (900–1100°C) annealing in different atmospheres, determined effective Fe2+ diffusion coefficients in CVD ZnSe, and evaluated the activation energy for the diffusion process. Distinctive features of the doping process in Zn vapor have been identified that are responsible for the observed order-of-magnitude increase in Fe diffusion rate in comparison with annealing in Ar and Se. The effect of annealing conditions on Fe diffusion mechanisms is discussed.
- 20 August 2019
- Published by IOP Publishing in Laser Physics Letters
- Vol. 16 (9) , 095002
Luminescent and lasing characteristics of polycrystalline Cr:Fe:ZnSe exited at 2.09 and 2.94 µ m wavelengths
The luminescence of Cr 2+ and Fe 2+ in Cr:Fe:ZnSe polycrystals excited at room temperature by pulsed lasers at wavelengths of 2.09 and 2.94 m was studied. For comparison, we also studied the luminescence in single crystals and polycrystals of Fe:ZnSe with iron ion concentration in the range from 5.6 × 10 18 to 5.7 × 10 19 cm −3 . Doping of the polycrystalline samples was carried out using a high-temperature diffusion process with subsequent control of the dopants concentration distribution over the crystal depth. The dependence of the luminescence lifetime τ lt of Fe 2+ ions on the dopants concentration in crystals excited at a wavelength of 2.94 m was obtained. It was found that chromium quenches the luminescence of Fe 2+ no less actively (if no more) than iron itself. The τ lt values were measured for Fe:ZnSe excited at a wavelength of 2.94 m and Cr:Fe:ZnSe samples with the same maximum Fe 2+ ions concentrations (≈0.9 × 10 19 cm −3 ) at wavelengths of 2.94 m and 2.09 m. A noticeable increase in τ lt value and luminescence rise time was observed in Cr:Fe:ZnSe crystals excited at a wavelength of 2.09 m ( τ lt ≈ 460 ns) compared to 2.94 m ( τ lt ≈ 240 ns). For comparison, the value of τ lt in Fe:ZnSe was about 340 ns. The obtained results confirm the fast energy transfer in Cr:Fe:ZnSe crystals from excited chromium ions to iron ions. The output characteristics of lasers on Fe:ZnSe and Cr:Fe:ZnSe polycrystalline active elements with pumping by HF laser radiation were compared. The slope efficiency with respect to the absorbed energy of Cr:Fe:ZnSe lasers was significantly lower, and the generation threshold was two times higher than for Fe:ZnSe lasers. The prospects for creating a room temperature laser, in which the excitation of iron ions will be carried out through energy transfer from chromium ions, are analyzed.
- 20 August 2019
- Published by IOP Publishing in Laser Physics Letters
- Vol. 16 (9) , 095002
Luminescent and lasing characteristics of polycrystalline Cr:Fe:ZnSe exited at 2.09 and 2.94 µ m wavelengths
The luminescence of Cr 2+ and Fe 2+ in Cr:Fe:ZnSe polycrystals excited at room temperature by pulsed lasers at wavelengths of 2.09 and 2.94 m was studied. For comparison, we also studied the luminescence in single crystals and polycrystals of Fe:ZnSe with iron ion concentration in the range from 5.6 × 10 18 to 5.7 × 10 19 cm −3 . Doping of the polycrystalline samples was carried out using a high-temperature diffusion process with subsequent control of the dopants concentration distribution over the crystal depth. The dependence of the luminescence lifetime τ lt of Fe 2+ ions on the dopants concentration in crystals excited at a wavelength of 2.94 m was obtained. It was found that chromium quenches the luminescence of Fe 2+ no less actively (if no more) than iron itself. The τ lt values were measured for Fe:ZnSe excited at a wavelength of 2.94 m and Cr:Fe:ZnSe samples with the same maximum Fe 2+ ions concentrations (≈0.9 × 10 19 cm −3 ) at wavelengths of 2.94 m and 2.09 m. A noticeable increase in τ lt value and luminescence rise time was observed in Cr:Fe:ZnSe crystals excited at a wavelength of 2.09 m ( τ lt ≈ 460 ns) compared to 2.94 m ( τ lt ≈ 240 ns). For comparison, the value of τ lt in Fe:ZnSe was about 340 ns. The obtained results confirm the fast energy transfer in Cr:Fe:ZnSe crystals from excited chromium ions to iron ions. The output characteristics of lasers on Fe:ZnSe and Cr:Fe:ZnSe polycrystalline active elements with pumping by HF laser radiation were compared. The slope efficiency with respect to the absorbed energy of Cr:Fe:ZnSe lasers was significantly lower, and the generation threshold was two times higher than for Fe:ZnSe lasers. The prospects for creating a room temperature laser, in which the excitation of iron ions will be carried out through energy transfer from chromium ions, are analyzed.
- 1 July 2019
- Published by Allerton Press in Physics of Wave Phenomena
- Vol. 27 (3) , 211-216
Lasing Characteristics of Fe:Cr:ZnSe Polycrystals
The characteristics of a laser based on Fe:Cr:ZnSe polycrystals, excited at room temperature by a non-chain HF laser (2.6 to 3.1 µm) have been investigated. High-temperature diffusion doping of zinc...
- 1 July 2019
- Published by Allerton Press in Physics of Wave Phenomena
- Vol. 27 (3) , 211-216
Lasing Characteristics of Fe:Cr:ZnSe Polycrystals
The characteristics of a laser based on Fe:Cr:ZnSe polycrystals, excited at room temperature by a non-chain HF laser (2.6 to 3.1 µm) have been investigated. High-temperature diffusion doping of zinc...
- 1 June 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 109
Cr2+:ZnSe active media with inhomogeneous doping profiles: modeling and experimental results
Cr 2+ :ZnSe polycrystalline active elements with different distribution profiles of Cr 2+ ions concentration over their thicknesses were fabricated. Dependences of the output laser powers on the incident pump power of Tm 3+ -laser in continuous and pulse modes were obtained. There was found to be a correlation between the generation slope efficiency and the shape of the concentration profile. There was proposed a numerical model to explain the experimental results by the influence of thermo-optical distortions caused by uneven heating of the active elements due to the pumping process.
- 1 June 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 109
Cr2+:ZnSe active media with inhomogeneous doping profiles: modeling and experimental results
Cr 2+ :ZnSe polycrystalline active elements with different distribution profiles of Cr 2+ ions concentration over their thicknesses were fabricated. Dependences of the output laser powers on the incident pump power of Tm 3+ -laser in continuous and pulse modes were obtained. There was found to be a correlation between the generation slope efficiency and the shape of the concentration profile. There was proposed a numerical model to explain the experimental results by the influence of thermo-optical distortions caused by uneven heating of the active elements due to the pumping process.
- 16 January 2018
- Published by IOP Publishing in Laser Physics Letters
- Vol. 15 (2) , 025002
Doping profile influence on a polycrystalline Cr 2+ :ZnSe laser efficiency
Cr 2+ :ZnSe polycrystalline active elements were fabricated, with different distribution profiles of Cr ions concentration over their thicknesses and an equal absorption at a pump wavelength of 1.9 µ m. The lasing characteristics of the obtained samples in short cavity schemes were determined, using a CW Tm 3+ -doped fiber laser and a Tm 3+ :YLF pulsed laser as the sources of pumping. There was found to be a correlation between the generation slope efficiency and the shape of the concentration profile. It was determined that bilateral doping samples achieved better laser performance. The maximum values of the slope efficiencies with respect to the absorbed power were η =73% in the pulse-periodic mode, and η = 37% in the continuous-wave mode.
- 16 January 2018
- Published by IOP Publishing in Laser Physics Letters
- Vol. 15 (2) , 025002
Doping profile influence on a polycrystalline Cr 2+ :ZnSe laser efficiency
Cr 2+ :ZnSe polycrystalline active elements were fabricated, with different distribution profiles of Cr ions concentration over their thicknesses and an equal absorption at a pump wavelength of 1.9 µ m. The lasing characteristics of the obtained samples in short cavity schemes were determined, using a CW Tm 3+ -doped fiber laser and a Tm 3+ :YLF pulsed laser as the sources of pumping. There was found to be a correlation between the generation slope efficiency and the shape of the concentration profile. It was determined that bilateral doping samples achieved better laser performance. The maximum values of the slope efficiencies with respect to the absorbed power were η =73% in the pulse-periodic mode, and η = 37% in the continuous-wave mode.
- 1 January 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (1) , 21-25
Effect of Annealing Atmosphere on Chromium Diffusion in CVD ZnSe
This paper examines the effect of high-temperature doping conditions on Cr2+diffusion in polycrystalline zinc selenide. The activation energy for the diffusion process is determined in the...
- 1 January 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 54 (1) , 21-25
Effect of Annealing Atmosphere on Chromium Diffusion in CVD ZnSe
This paper examines the effect of high-temperature doping conditions on Cr2+diffusion in polycrystalline zinc selenide. The activation energy for the diffusion process is determined in the...
- 17 October 2017
- Published by Wiley in Physica Status Solidi (a)
- Vol. 215 (4)
Investigations of Nanoscale Defects in Crystalline and Powder ZnSe Doped With Fe for Laser Application
The theoretical and experimental analysis of the ternary system Zn‐Se‐Fe for obtaining new fundamental information on phase using X‐ray analysis and inductively coupled plasma mass‐spectrometry is carried out. New experimental data of isothermal annealing in the Zn‐Se‐Fe system at the temperatures 730, 814, 1073 K by X‐ray studies confirms the reliability of theoretical isothermal sections. The information on Fe solubility and concentrations of native point defects of atomic scale at bi‐ and monovariant conditions at 1073 and 1273 K have been carried out. Taking into account the new data on phase equilibria, it is possible to fabricate active ZnSe:Fe2+ elements to create an effective laser operating at the temperature of 300 K with 1.52 Joule emission energy with efficiency of ≈50% relative to the absorbed energy.
- 17 October 2017
- Published by Wiley in Physica Status Solidi (a)
- Vol. 215 (4)
Investigations of Nanoscale Defects in Crystalline and Powder ZnSe Doped With Fe for Laser Application
The theoretical and experimental analysis of the ternary system Zn‐Se‐Fe for obtaining new fundamental information on phase using X‐ray analysis and inductively coupled plasma mass‐spectrometry is carried out. New experimental data of isothermal annealing in the Zn‐Se‐Fe system at the temperatures 730, 814, 1073 K by X‐ray studies confirms the reliability of theoretical isothermal sections. The information on Fe solubility and concentrations of native point defects of atomic scale at bi‐ and monovariant conditions at 1073 and 1273 K have been carried out. Taking into account the new data on phase equilibria, it is possible to fabricate active ZnSe:Fe2+ elements to create an effective laser operating at the temperature of 300 K with 1.52 Joule emission energy with efficiency of ≈50% relative to the absorbed energy.
- 1 October 2017
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 53 (11) , 1115-1119
Recrystallization behavior of zinc selenide during chromium diffusion doping
We have studied the effect of high-temperature diffusion doping with chromium (Cr2+) ions on the microstructure of polycrystalline zinc selenide (ZnSe). We have determined energy and kinetic characteristics of solid-state recrystallization in ZnSe and assessed the effect of chromium concentration on the rate of grain growth during the doping process.
- 1 October 2017
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 53 (11) , 1115-1119
Recrystallization behavior of zinc selenide during chromium diffusion doping
We have studied the effect of high-temperature diffusion doping with chromium (Cr2+) ions on the microstructure of polycrystalline zinc selenide (ZnSe). We have determined energy and kinetic characteristics of solid-state recrystallization in ZnSe and assessed the effect of chromium concentration on the rate of grain growth during the doping process.
- 30 March 2017
- Published by IOP Publishing in Laser Physics Letters
- Vol. 14 (5) , 055805
CVD-grown Fe2+:ZnSe polycrystals for laser applications
A technique for growing bulk zinc selenide polycrystals, doped with iron ions, by chemical vapor deposition (CVD), has been developed. It has been shown that iron is embedded in the crystal lattice of deposited zinc selenide in the optically active state of Fe 2+ . To improve the optical quality, the grown material was subjected to postgrowth hot isostatic pressing (HIP) treatment. It was experimentally demonstrated that the synthesised bulk crystals can be used as the active media of Fe 2+ :ZnSe lasers and as the passive Q-switches for three-micron lasers. The letter goes on to discuss the prospect of extending the proposed method to the synthesis of zinc sulphide doped with iron ions.
- 30 March 2017
- Published by IOP Publishing in Laser Physics Letters
- Vol. 14 (5) , 055805
CVD-grown Fe2+:ZnSe polycrystals for laser applications
A technique for growing bulk zinc selenide polycrystals, doped with iron ions, by chemical vapor deposition (CVD), has been developed. It has been shown that iron is embedded in the crystal lattice of deposited zinc selenide in the optically active state of Fe 2+ . To improve the optical quality, the grown material was subjected to postgrowth hot isostatic pressing (HIP) treatment. It was experimentally demonstrated that the synthesised bulk crystals can be used as the active media of Fe 2+ :ZnSe lasers and as the passive Q-switches for three-micron lasers. The letter goes on to discuss the prospect of extending the proposed method to the synthesis of zinc sulphide doped with iron ions.