Adam Szafron
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Adam Szafron has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Maria Richert
Management Faculty, AGH University, Gramatyka 10 str., 30-067 Kraków, Poland
2 shared publications - Aleksandra Węglowska
LUKASIEWICZ Research Network– Welding Institute, Gliwice, Poland
1 shared publication - Anna Wąsik
Faculty of Non-Ferrous Metals, AGH University of Science and Technology, Krakow Mickiewicza 30 Av., 30-059 Krakow, Poland
1 shared publication - Beata Leszczyńska-Madej
Faculty of Non-Ferrous Metals, AGH University of Krakow, 30 Mickiewicza Ave, 30-059 Krakow, Poland
1 shared publication - D. Miara
Instytut Spawalnictwa (Institute of Welding), Bl. Czeslawa Str. 16-18, Gliwice 44-100, Poland
1 shared publication - G. Ziobro
Maflow Member of Boryszew Group, Serdeczna Str. 42, 43-100 Tychy, Poland
1 shared publication
Latest Publications
- Open Access
Analysis of the Microstructure and Selected Properties of the Aluminium Alloys Used in Automotive Air-Conditioning Systems
The results of microstructure examinations and studies of selected mechanical properties of four aluminium alloys used in the production of automotive air-conditioning ducts (AA3103, AA5049, AA6060, AA6063) before and after the ASTM G85:A3 SWAAT Test (Sea Water Acetic Acid Test) for corrosion resistance are presented. Materials used for the manufacture of such components should be temperature stable, and therefore thermal resistance tests were carried out in a wide range of temperatures, i.e., −25 °C, 25 °C, 40 °C, 60 °C, 80 °C, 100 °C, 140 °C, 180 °C, and 220 °C. Annealing was performed for 72 h and 240 h, followed by cooling in water. The obtained results have proved that the non-precipitation-hardenable AA3103 and AA5049 alloys remain stable in the entire range of the investigated temperatures. The measured microhardness of these alloys was 43–46 HV0.1 for AA3103 and 56–64 HV0.1 for AA5049. The microhardness of the 6xxx series aluminium alloys was not stable in the investigated range of temperatures. The maximum was observed in the temperature range of 100–140 °C, which corresponded to the precipitation process of intermetallic phases, as further confirmed by microstructure observations. After the corrosion test, the mechanical properties and elongation decreased by about 5–20%.
Open AccessAnalysis of the Microstructure and Selected Properties of the Aluminium Alloys Used in Automotive Air-Conditioning Systems
The results of microstructure examinations and studies of selected mechanical properties of four aluminium alloys used in the production of automotive air-conditioning ducts (AA3103, AA5049, AA6060, AA6063) before and after the ASTM G85:A3 SWAAT Test (Sea Water Acetic Acid Test) for corrosion resistance are presented. Materials used for the manufacture of such components should be temperature stable, and therefore thermal resistance tests were carried out in a wide range of temperatures, i.e., −25 °C, 25 °C, 40 °C, 60 °C, 80 °C, 100 °C, 140 °C, 180 °C, and 220 °C. Annealing was performed for 72 h and 240 h, followed by cooling in water. The obtained results have proved that the non-precipitation-hardenable AA3103 and AA5049 alloys remain stable in the entire range of the investigated temperatures. The measured microhardness of these alloys was 43–46 HV0.1 for AA3103 and 56–64 HV0.1 for AA5049. The microhardness of the 6xxx series aluminium alloys was not stable in the investigated range of temperatures. The maximum was observed in the temperature range of 100–140 °C, which corresponded to the precipitation process of intermetallic phases, as further confirmed by microstructure observations. After the corrosion test, the mechanical properties and elongation decreased by about 5–20%.
- 1 January 2017
- Published by AIP Publishing in AIP Conference Proceedings
The characteristics of welded joints for air conditioning application
In the paper the results of metallographic examination of welded joints for air–conditioning elements are presented. The European directives 2006/40/EC on the greenhouse gasses elimination demand to stop using traditional refrigerant and to change it to R744 (CO2) medium in air conditioning installation. The R744 refrigerant is environmental friendly medium if compared with standard solution such as R12, R134a or R1234yf and safer for passengers than R1234yf. The non-standard thermodynamic parameters of the R744 which translate into high pressure and high temperature require specific materials to develop the shape and to specify the technology of manufacturing for the particular elements of the conduits and moreover the technologies of joining for the whole structure, which would meet the exploitation requirements of the new air–conditioning system. To produce the test welded joints of stainless steels four different joining technologies were applied: laser welding, plasma welding, electron beam welding as well as high speed rotation welding. This paper describes the influence of the selected welding process on the macrostructure and microstructure of welded joints of AISI 304 and AISI 316L steels. The results indicated that plasma welding laser welding and electron beam welding technologies guaranty the proper quality of welded joints and can be used for the air conditioning application in automotive industry. However, high speed rotation welding not guarantee the good quality of welded joints and cannot be used for above application.
- 1 January 2017
- Published by AIP Publishing in AIP Conference Proceedings
The characteristics of welded joints for air conditioning application
In the paper the results of metallographic examination of welded joints for air–conditioning elements are presented. The European directives 2006/40/EC on the greenhouse gasses elimination demand to stop using traditional refrigerant and to change it to R744 (CO2) medium in air conditioning installation. The R744 refrigerant is environmental friendly medium if compared with standard solution such as R12, R134a or R1234yf and safer for passengers than R1234yf. The non-standard thermodynamic parameters of the R744 which translate into high pressure and high temperature require specific materials to develop the shape and to specify the technology of manufacturing for the particular elements of the conduits and moreover the technologies of joining for the whole structure, which would meet the exploitation requirements of the new air–conditioning system. To produce the test welded joints of stainless steels four different joining technologies were applied: laser welding, plasma welding, electron beam welding as well as high speed rotation welding. This paper describes the influence of the selected welding process on the macrostructure and microstructure of welded joints of AISI 304 and AISI 316L steels. The results indicated that plasma welding laser welding and electron beam welding technologies guaranty the proper quality of welded joints and can be used for the air conditioning application in automotive industry. However, high speed rotation welding not guarantee the good quality of welded joints and cannot be used for above application.