Mayerling Martinez Celis
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Mayerling Martinez Celis has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Eric Hug
CRISMAT Laboratory, UNICAEN—Normandy University, UMR CNRS 6508, Boulevard Maréchal Juin, 14000 Caen, France
6 shared publications Eric Hug
Laboratoire CRISMAT Normandie Universite ENSICAEN, UNICAEN, CNRS, 6 Boulevard du Marechal Juin 14050 Caen Cedex 4 France
4 shared publicationsFlorent Picot
ACOME BP 45 Usines de Romagny 50140 Mortain Bocage France
3 shared publicationsJozef Veselý
Faculty of Mathematics and Physics Charles University in Prague Ke Karlovu 5 CZ‐12116 Prague 2 Czech Republic
3 shared publications- Clément Keller
Univ Rouen, INSA Rouen, Grp Phys Mat, UMR CNRS 6634, F-76800 St Etienne Du Rouvray, France
2 shared publications - Lucía García de la Cruz
Departamento Ciencia e Ingeniería de Materiales e Ingeniería Química Universidad Carlos III de Madrid
2 shared publications
Latest Publications
- 22 February 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (7)
Effect of Tool Geometry on the Microstructure of Friction Stir Welding of Copper and 316L Stainless Steel
The microstructure evolution during dissimilar friction stir welding of copper with stainless steel 316L is studied. The welding is performed in transparence configuration using tools of two different geometries. The joints are characterized by optical microscopy, scanning and transmission electron microscopy, electron backscattered diffraction, and microhardness. The microstructure and crystallographic texture of base metals are significantly affected. The joint produced using a shoulder of 8 mm in diameter is characterized by a copper nugget with refined grains. The texture of copper is dominated by component of the shear texture. The steel beneath the tool shows a grain refinement with grains of sub‐micron size and a texture which is close to the ideal simple shear texture. For the joint produced by the 16 mm diameter tool shoulder, the nugget consists of large grains of copper, while the steel beneath the tool shows small recrystallized grains of micrometer size. The texture in the steel is dominated by the component of the shear texture. The Cu/316L interface in both types of joint is of very good quality. In a detailed study of the interface, it is revealed that the welding of metals is achieved by mutual intense mechanical interlocking without formation of any intermetallic compounds.
- 22 February 2024
- Published by Wiley in Advanced Engineering Materials
- Vol. 26 (7)
Effect of Tool Geometry on the Microstructure of Friction Stir Welding of Copper and 316L Stainless Steel
The microstructure evolution during dissimilar friction stir welding of copper with stainless steel 316L is studied. The welding is performed in transparence configuration using tools of two different geometries. The joints are characterized by optical microscopy, scanning and transmission electron microscopy, electron backscattered diffraction, and microhardness. The microstructure and crystallographic texture of base metals are significantly affected. The joint produced using a shoulder of 8 mm in diameter is characterized by a copper nugget with refined grains. The texture of copper is dominated by component of the shear texture. The steel beneath the tool shows a grain refinement with grains of sub‐micron size and a texture which is close to the ideal simple shear texture. For the joint produced by the 16 mm diameter tool shoulder, the nugget consists of large grains of copper, while the steel beneath the tool shows small recrystallized grains of micrometer size. The texture in the steel is dominated by the component of the shear texture. The Cu/316L interface in both types of joint is of very good quality. In a detailed study of the interface, it is revealed that the welding of metals is achieved by mutual intense mechanical interlocking without formation of any intermetallic compounds.
- 10 March 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (12) , 5516-5529
Identification of a pseudo-ternary intermetallic compound in the stirred zone of friction-stir-welded 5083 aluminum alloy with 316L steel
- 10 March 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (12) , 5516-5529
Identification of a pseudo-ternary intermetallic compound in the stirred zone of friction-stir-welded 5083 aluminum alloy with 316L steel
- Open Access
Synthesis and physical properties of uranium thin-film hydrides UH2 and \b{eta}-UH3
Formation of thin uranium hydrides films, UH2 and \b{eta}-UH3, synthesized by a reactive dc sputtering of uranium metal, was explored using variable deposition conditions. Obtained stable oxygen-free hydride films were studied by a variety of methods, both in situ (photoelectron spectroscopy - XPS), and ex-situ (x-ray diffraction - XRD, transmission electron microscopy - TEM), electrical resistivity, and magnetometry). Both types of hydrides are ferromagnetic, the Curie temperatures of UH2 and \b{eta}-UH3 are approx. 120 and 170 K, respectively. Ferromagnetism in the thin films is robust and does not depend on structure details while electrical resistivity data reflect disorder in both types of hydrides.
Open AccessSynthesis and physical properties of uranium thin-film hydrides UH2 and \b{eta}-UH3
Formation of thin uranium hydrides films, UH2 and \b{eta}-UH3, synthesized by a reactive dc sputtering of uranium metal, was explored using variable deposition conditions. Obtained stable oxygen-free hydride films were studied by a variety of methods, both in situ (photoelectron spectroscopy - XPS), and ex-situ (x-ray diffraction - XRD, transmission electron microscopy - TEM), electrical resistivity, and magnetometry). Both types of hydrides are ferromagnetic, the Curie temperatures of UH2 and \b{eta}-UH3 are approx. 120 and 170 K, respectively. Ferromagnetism in the thin films is robust and does not depend on structure details while electrical resistivity data reflect disorder in both types of hydrides.
- 21 July 2022
- Published by Springer Nature in MRS Advances
- Vol. 7 (31) , 818-823
Interface microstructure of friction stir welded aluminum alloy and stainless steel
- 21 July 2022
- Published by Springer Nature in MRS Advances
- Vol. 7 (31) , 818-823
Interface microstructure of friction stir welded aluminum alloy and stainless steel
- 21 January 2021
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (12) , 7740-7752
Analysis of the twin variant selection in polycrystalline cobalt
- 21 January 2021
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (12) , 7740-7752
Analysis of the twin variant selection in polycrystalline cobalt
- Open Access
Exploring the Strain Hardening Mechanisms of Ultrafine Grained Nickel Processed by Spark Plasma Sintering
Ultrafine grained (UFG) materials in the bigger grain size range (0.5–1) µm display a good combination of strength and ductility, unlike smaller size UFG and nanostructured metals, which usually exhibit high strength but low ductility. Such difference can be attributed to a change in plasticity mechanisms that modifies their strain hardening capability. The purpose of this work is to investigate the work hardening mechanisms of UFG nickel considering samples with grain sizes ranging from 0.82 to 25 µm. Specimens processed combining ball milling and spark plasma sintering were subjected to monotonous tensile testing up to fracture. Then, microstructural observations of the deformed state of the samples were carried out by electron backscattered diffraction and transmission electron microscopy. A lower strain hardening capability is observed with decreasing grain size. Samples in the submicrometric range display the three characteristic stages of strain hardening with a short second stage and the third stage beginning soon after yielding. Microstructural observations display a low fraction of low angle grain boundaries and dislocation density for the sample with d = 0.82 µm, suggesting changes in plasticity mechanisms early in the UFG range.
Open AccessExploring the Strain Hardening Mechanisms of Ultrafine Grained Nickel Processed by Spark Plasma Sintering
Ultrafine grained (UFG) materials in the bigger grain size range (0.5–1) µm display a good combination of strength and ductility, unlike smaller size UFG and nanostructured metals, which usually exhibit high strength but low ductility. Such difference can be attributed to a change in plasticity mechanisms that modifies their strain hardening capability. The purpose of this work is to investigate the work hardening mechanisms of UFG nickel considering samples with grain sizes ranging from 0.82 to 25 µm. Specimens processed combining ball milling and spark plasma sintering were subjected to monotonous tensile testing up to fracture. Then, microstructural observations of the deformed state of the samples were carried out by electron backscattered diffraction and transmission electron microscopy. A lower strain hardening capability is observed with decreasing grain size. Samples in the submicrometric range display the three characteristic stages of strain hardening with a short second stage and the third stage beginning soon after yielding. Microstructural observations display a low fraction of low angle grain boundaries and dislocation density for the sample with d = 0.82 µm, suggesting changes in plasticity mechanisms early in the UFG range.
- Open Access
The Effect of Different Thermal Treatment on the Allotropic fcc↔hcp Transformation and Compression Behavior of Polycrystalline Cobalt
Pure polycrystalline cobalt is systematically thermally treated in order to assess the effect of the microstructure on the compression behavior. Isothermal annealing of the as-drawn material leads to recrystallization and grain growth dependent on the annealing temperature (600–1100 C). Consequently, the yield strength decreases and the fracture strain increases as a function of rising grain size; the content of the residual fcc phase is ~6–11%. Subsequent thermal cycling around the transition temperature is applied to further modify the microstructure, especially in terms of the fcc phase content. With the increasing number of cycles, the grain size further increases and the fraction of the fcc phase significantly drops. At the same time, the values of both the yield strength and fracture strain somewhat decrease. An atypical decrease in the fracture strain as a function of grain size is explained in terms of decreasing fcc phase content; the stress-induced fcc→hcp transformation can accommodate a significant amount of plastic strain. Besides controlling basic material parameters (e.g., grain size and texture), adjusting the content of the fcc phase can thus provide an effective means of mechanical performance optimization with respect to particular applications.Open AccessThe Effect of Different Thermal Treatment on the Allotropic fcc↔hcp Transformation and Compression Behavior of Polycrystalline Cobalt
Pure polycrystalline cobalt is systematically thermally treated in order to assess the effect of the microstructure on the compression behavior. Isothermal annealing of the as-drawn material leads to recrystallization and grain growth dependent on the annealing temperature (600–1100 C). Consequently, the yield strength decreases and the fracture strain increases as a function of rising grain size; the content of the residual fcc phase is ~6–11%. Subsequent thermal cycling around the transition temperature is applied to further modify the microstructure, especially in terms of the fcc phase content. With the increasing number of cycles, the grain size further increases and the fraction of the fcc phase significantly drops. At the same time, the values of both the yield strength and fracture strain somewhat decrease. An atypical decrease in the fracture strain as a function of grain size is explained in terms of decreasing fcc phase content; the stress-induced fcc→hcp transformation can accommodate a significant amount of plastic strain. Besides controlling basic material parameters (e.g., grain size and texture), adjusting the content of the fcc phase can thus provide an effective means of mechanical performance optimization with respect to particular applications. - Open Access
- 1 June 2018
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 925, 173-180
Analysis of Nuclei in a Heavy-Section Nodular Iron Casting
The microstructure of heavy section nodular graphite cast irons often presents a bimodal distribution of nodule size associated with so-called primary and secondary graphite nucleation. It has been found that the nuclei in both types of nodules consist mainly in magnesium sulphide. However, nuclei in primary nodules contain some traces of calcium and are thus related with the inoculation treatment. On the contrary, nuclei in secondary nodules do not contain any element that could be associated to inoculation. It is suggested they form in the late stage of the eutectic reaction as a result of microsegregation build-up in magnesium and sulphur.
- 1 June 2018
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 925, 173-180
Open AccessAnalysis of Nuclei in a Heavy-Section Nodular Iron Casting
The microstructure of heavy section nodular graphite cast irons often presents a bimodal distribution of nodule size associated with so-called primary and secondary graphite nucleation. It has been found that the nuclei in both types of nodules consist mainly in magnesium sulphide. However, nuclei in primary nodules contain some traces of calcium and are thus related with the inoculation treatment. On the contrary, nuclei in secondary nodules do not contain any element that could be associated to inoculation. It is suggested they form in the late stage of the eutectic reaction as a result of microsegregation build-up in magnesium and sulphur.
- Open Access
A Correlation between the Ultimate Shear Stress and the Thickness Affected by Intermetallic Compounds in Friction Stir Welding of Dissimilar Aluminum Alloy–Stainless Steel Joints
In this work, Friction Stir Welding (FSW) was applied to join a stainless steel 316L and an aluminum alloy 5083. Ranges of rotation and translation speeds of the tool were used to obtain welding samples with different heat input coefficients. Depending on the process parameters, the heat generated by FSW creates thin layers of Al-rich InterMetallic Compound (IMC) mainly composed of FeAl3, identified by energy dispersive spectrometry. Traces of Fe2Al5 were also depicted in some samples by X-ray diffraction analysis and transmission electron microscopy. Monotonous tensile tests performed on the weld joint show the existence of a maximum mechanical resistance for a judicious choice of rotation and translation speeds. It can be linked to an affected zone of average thickness of 15 µm which encompass the presence of IMC and the chaotic mixing caused by plastic deformation in this area. A thickness of less than 15 µm is not sufficient to ensure a good mechanical resistance of the joint. For a thickness higher than 15 µm, IMC layers become more brittle and less adhesive due to high residual stresses which induces numerous cracks after cooling. This leads to a progressive decrease of the ultimate shear stress supported by the bond.
Open AccessA Correlation between the Ultimate Shear Stress and the Thickness Affected by Intermetallic Compounds in Friction Stir Welding of Dissimilar Aluminum Alloy–Stainless Steel Joints
In this work, Friction Stir Welding (FSW) was applied to join a stainless steel 316L and an aluminum alloy 5083. Ranges of rotation and translation speeds of the tool were used to obtain welding samples with different heat input coefficients. Depending on the process parameters, the heat generated by FSW creates thin layers of Al-rich InterMetallic Compound (IMC) mainly composed of FeAl3, identified by energy dispersive spectrometry. Traces of Fe2Al5 were also depicted in some samples by X-ray diffraction analysis and transmission electron microscopy. Monotonous tensile tests performed on the weld joint show the existence of a maximum mechanical resistance for a judicious choice of rotation and translation speeds. It can be linked to an affected zone of average thickness of 15 µm which encompass the presence of IMC and the chaotic mixing caused by plastic deformation in this area. A thickness of less than 15 µm is not sufficient to ensure a good mechanical resistance of the joint. For a thickness higher than 15 µm, IMC layers become more brittle and less adhesive due to high residual stresses which induces numerous cracks after cooling. This leads to a progressive decrease of the ultimate shear stress supported by the bond.
- 1 January 2017
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 1892, 200002
Nanostructuration of metals via spark plasma sintering using activated powder obtained by ball-milling: Impact on the strain-hardening mechanisms
Powder metallurgy is a good option when coupled with pressure as a method to obtain nanostructured materials (NsM). The samples obtained by these means are nearly fully dense specimens that present low internal stresses. In this work, nickel is chosen to study the possibilities of nanostructuration via Spark Plasma Sintering (SPS) of ball-milled powders. The enhancement of the mechanical properties of the sintered samples are studied and compared with the results obtained for 316L austenitic stainless steel in a previous work.
- 1 January 2017
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 1892, 200002
Nanostructuration of metals via spark plasma sintering using activated powder obtained by ball-milling: Impact on the strain-hardening mechanisms
Powder metallurgy is a good option when coupled with pressure as a method to obtain nanostructured materials (NsM). The samples obtained by these means are nearly fully dense specimens that present low internal stresses. In this work, nickel is chosen to study the possibilities of nanostructuration via Spark Plasma Sintering (SPS) of ball-milled powders. The enhancement of the mechanical properties of the sintered samples are studied and compared with the results obtained for 316L austenitic stainless steel in a previous work.