Jun Tian
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Jun Tian has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
- Pinqiang Dai
College of Materials Science and Engineering, Fujian University of Technology, Fuzhou 350118, China
3 shared publications Pinqiang Dai
College of Materials Science and Engineering, FuJian University of Technology, Fuzhou, China
2 shared publications- Biliang Bao
Fujian Minhang Electronics Co., Ltd., Nanping 353000, China
1 shared publication - Chun-Ming Lin
Department of Marine Engineering, National Kaohsiung University of Science and Technology, Kaohsiung City, Taiwan
1 shared publication - Chunfu Hong
Fujian Provincial Key Laboratory of Advanced Materials Processing and Application, Fujian University of Technology, Fuzhou 350118, China
1 shared publication - Fa Chang
College of Materials Science and Engineering, Fujian University of Technology, Fuzhou 350118, China
1 shared publication
Latest Publications
- 6 May 2026
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 55 (7) , 6337-6350
Microstructural Refinement and Interfacial Evolution of Ge addition Sn-Bi-Zn Medium-Entropy Solders
- 6 May 2026
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 55 (7) , 6337-6350
Microstructural Refinement and Interfacial Evolution of Ge addition Sn-Bi-Zn Medium-Entropy Solders
- Open Access
Effects of β-Si3N4 Seeds on Microstructure and Performance of Si3N4 Ceramics in Semiconductor Package
Among the various ceramic substrate materials, Si3N4 ceramics have demonstrated high thermal conductivity, good thermal shock resistance, and excellent corrosion resistance. As a result, they are well-suited for semiconductor substrates in high-power and harsh conditions encountered in automobiles, high-speed rail, aerospace, and wind power. In this work, Si3N4 ceramics with various ratios of α-Si3N4 and β-Si3N4 in raw powder form were prepared by spark plasma sintering (SPS) at 1650 °C for 30 min under 30 MPa. When the content of β-Si3N4 was lower than 20%, with the increase in β-Si3N4 content, the ceramic grain size changed gradually from 1.5 μm to 1 μm and finally resulted in 2 μm mixed grains. However, As the content of β-Si3N4 seed crystal increased from 20% to 50%, with the increase in β-Si3N4 content, the ceramic grain size changed gradually from 1 μm and 2 μm to 1.5 μm. Therefore, when the content of β-Si3N4 in the raw powder is 20%, the sintered ceramics exhibited a double-peak structure distribution and the best overall performance with a density of 97.5%, fracture toughness of 12.1 MPa·m1/2, and a Vickers hardness of 14.5 GPa. The results of this study are expected to provide a new way of studying the fracture toughness of silicon nitride ceramic substrates.
Open AccessEffects of β-Si3N4 Seeds on Microstructure and Performance of Si3N4 Ceramics in Semiconductor Package
Among the various ceramic substrate materials, Si3N4 ceramics have demonstrated high thermal conductivity, good thermal shock resistance, and excellent corrosion resistance. As a result, they are well-suited for semiconductor substrates in high-power and harsh conditions encountered in automobiles, high-speed rail, aerospace, and wind power. In this work, Si3N4 ceramics with various ratios of α-Si3N4 and β-Si3N4 in raw powder form were prepared by spark plasma sintering (SPS) at 1650 °C for 30 min under 30 MPa. When the content of β-Si3N4 was lower than 20%, with the increase in β-Si3N4 content, the ceramic grain size changed gradually from 1.5 μm to 1 μm and finally resulted in 2 μm mixed grains. However, As the content of β-Si3N4 seed crystal increased from 20% to 50%, with the increase in β-Si3N4 content, the ceramic grain size changed gradually from 1 μm and 2 μm to 1.5 μm. Therefore, when the content of β-Si3N4 in the raw powder is 20%, the sintered ceramics exhibited a double-peak structure distribution and the best overall performance with a density of 97.5%, fracture toughness of 12.1 MPa·m1/2, and a Vickers hardness of 14.5 GPa. The results of this study are expected to provide a new way of studying the fracture toughness of silicon nitride ceramic substrates.
- Open Access
Effect of Al Addition on Microstructure and Properties of CoCrNi Medium-Entropy Alloy Prepared by Powder Metallurgy
Powder metallurgy possesses the advantages of low energy consumption, less material consumption, uniform composition, and near-final forming. In order to improve the mechanical properties and high-temperature oxidation resistance of CoCrNi medium-entropy alloy (MEA), CoCrNiAlX (X = 0, 0.1, 0.3, 0.5, 0.7) MEAs were prepared using mechanical alloying (MA) and spark-plasma sintering (SPS). The effect of aluminum content on the microstructure and properties of the MEAs was investigated. The results show that the CoCrNi MEA is composed of face center cubic (fcc) phase and some carbides (Cr23C6). With the increase in Al content, there exists Al2O3 precipitation. When the Al content is increased to Al0.5 and Al0.7, the body center cubic (bcc) phase begins to precipitate. The addition of aluminum significantly enhances the properties of the alloys, especially those containing fcc+bcc dual-phase solid solutions. The yield strength, compressive strength, and hardness of CoCrNiAl0.7 alloy are as high as 2083 MPa, 2498 MPa, and 646 HV, respectively. The high-temperature resistance also reaches the oxidation resistance level. Different oxides include Cr2O3, Al2O3, and (Co, Ni) Cr2O4 and NiCrO3 spinel oxides formed on the surface of alloys. The formation of an Al2O3 oxidation film prevents the further erosion of the matrix by oxygen elements.
Open AccessEffect of Al Addition on Microstructure and Properties of CoCrNi Medium-Entropy Alloy Prepared by Powder Metallurgy
Powder metallurgy possesses the advantages of low energy consumption, less material consumption, uniform composition, and near-final forming. In order to improve the mechanical properties and high-temperature oxidation resistance of CoCrNi medium-entropy alloy (MEA), CoCrNiAlX (X = 0, 0.1, 0.3, 0.5, 0.7) MEAs were prepared using mechanical alloying (MA) and spark-plasma sintering (SPS). The effect of aluminum content on the microstructure and properties of the MEAs was investigated. The results show that the CoCrNi MEA is composed of face center cubic (fcc) phase and some carbides (Cr23C6). With the increase in Al content, there exists Al2O3 precipitation. When the Al content is increased to Al0.5 and Al0.7, the body center cubic (bcc) phase begins to precipitate. The addition of aluminum significantly enhances the properties of the alloys, especially those containing fcc+bcc dual-phase solid solutions. The yield strength, compressive strength, and hardness of CoCrNiAl0.7 alloy are as high as 2083 MPa, 2498 MPa, and 646 HV, respectively. The high-temperature resistance also reaches the oxidation resistance level. Different oxides include Cr2O3, Al2O3, and (Co, Ni) Cr2O4 and NiCrO3 spinel oxides formed on the surface of alloys. The formation of an Al2O3 oxidation film prevents the further erosion of the matrix by oxygen elements.
- Open Access
On the Microstructure and Mechanical Properties of CrNx/Ag Multilayer Films Prepared by Magnetron Sputtering
CrNx/Ag multilayer coatings and a comparative CrNx single layer were deposited via reactive magnetron sputtering. In multilayer coatings, the thickness of each CrNx layer was constant at 60 nm, while that of the Ag layer was adjusted from 3 to 10 nm. Microstructure of the films was characterized by X-ray diffraction and transmission electron spectroscopy. The results suggest that the film containing 3 nm of Ag layer presents a nanocomposite structure comprising fine nano-grains and quasi-amorphous clusters. With Ag layer thickness reaching 4.5 nm and above, Ag grains coalesce to produce continuous an Ag layer and exhibit (111) preferential crystallization. Hardness of the films was detected by nanoindentation and it reveals that with increasing the Ag layer thickness, the hardness continuously decreases from 30.2 to 11.6 GPa. Wear performance of the films was examined by the ball-on-disk test at 500 °C. The result suggests that the out-diffusion of Ag towards film surface contributes to the friction reduction, while the wear performance of films depends on the thickness of the Ag layer.
Open AccessOn the Microstructure and Mechanical Properties of CrNx/Ag Multilayer Films Prepared by Magnetron Sputtering
CrNx/Ag multilayer coatings and a comparative CrNx single layer were deposited via reactive magnetron sputtering. In multilayer coatings, the thickness of each CrNx layer was constant at 60 nm, while that of the Ag layer was adjusted from 3 to 10 nm. Microstructure of the films was characterized by X-ray diffraction and transmission electron spectroscopy. The results suggest that the film containing 3 nm of Ag layer presents a nanocomposite structure comprising fine nano-grains and quasi-amorphous clusters. With Ag layer thickness reaching 4.5 nm and above, Ag grains coalesce to produce continuous an Ag layer and exhibit (111) preferential crystallization. Hardness of the films was detected by nanoindentation and it reveals that with increasing the Ag layer thickness, the hardness continuously decreases from 30.2 to 11.6 GPa. Wear performance of the films was examined by the ball-on-disk test at 500 °C. The result suggests that the out-diffusion of Ag towards film surface contributes to the friction reduction, while the wear performance of films depends on the thickness of the Ag layer.
- 7 August 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (22) , 17185-17192
Interfacial reactions between Cu and Zn20Sn solder doped with minor RE
- 7 August 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (22) , 17185-17192
Interfacial reactions between Cu and Zn20Sn solder doped with minor RE