IBIgor P. Balabanov

Igor P. Balabanov

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Igor P. Balabanov has a total of 25 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Increase of resistance of steel moulds using the complex modifier INSTEEL-7

    by V. A. Korovin, I. O. Leushin, I. P. Balabanov, I. A. Savin

    In this paper the authors examined the problem of insufficient operating resistance of moulds which are used for manufacture of steel ingots. Massive moulds, usually made from cast iron and sometimes from carbon steel, are used conventionally for production of steel ingots. Operating resistance of moulds depends of many factors and it can be maximized when three most important requirements are executed: structural strength; resistance to slopping of internal surface of mould walls during contact with liquid steel melt; ability of mould walls to hold thermal and mechanical effects. Satisfaction of the first two requirements is achieved via varying the mould wall thickness, while meeting the third requirement is determined by correct material choice. This choice, in its turn, is impossible without deep analysis of the problems occurring during mould operation and signs of their reject, such as cracks, erosion nets and burn-backs. Improvement of mould material parameters during their manufacture via casting seems to be the most prospective solution for increase of mould resistance. In this connection, the described research was aimed on formulating the scientifically substantiated choice of the initial material for moulds, which are used for manufacture of steel ingots in the conditions of the operating industrial production facilities (1), and the complex of experimental investigations in order to improve parameters of this material via technological methods of liquid phase treatment (2). The ingots made from carbon steel were chosen as initial material, while modifying and microalloying by the complex modifier INSTEEL-7 (produced by NPP “Tekhnologiya”, Chelyabinsk) were used for liquid phase treatment of initial material for improvement of its properties. Based on the results of conducted pilot-experimental work, the following parameters were obtained: increase of impact toughness for modified metal almost by two times (in comparison with conventional metal), rise of tensile strength and yield strength by 8.5 % and 20 % respectively, decrease of relative elongation and area reduction by 27 % and by three times respectively, what provided increase of operating resistance of a mould more than by 2 times as a result.

  • Manufacture of thin-walled steel castings via consumable additive patterns

    by I. O. Leushin, O. M. Yavtushenko, I. P. Balabanov, I. A. Savin

    The problems of thin-walled steel casting are usually connected with insufficient level of alloy fluidity in the field of operating casting temperatures, as well as with appearing counter-pressure for the alloy which fills the narrow mould sections. These sections correspond to thin walls of the future casting, depending on restricted gas permeability of a mould. To solve these problems, the methods of precise casting via thermodeleting patterns, as well as the methods of external effect on metallic melt which fills the mould. This work analyzes the accumulated experience of casting via lost and consumable patterns, the features of their practical realization in the conditions of a casting mould vacuum treatment; their disadvantages are shown as well. The authors formulated the task to eliminate the revealed disadvantages, to provide stability of the technological process and high quality of manufactured castings (in particular for surface defects, non-metallic inclusions, violations of geometrical shape and dimension accuracy) together with lowering of labour intensity and energy intensity of casting in comparison with Replicast–CS-process as a prototype. The innovative technology of casting via consumable patterns was suggested and successfully tested in the conditions of operating production facilities. This technology differs from the prototype in such way, that the patterns are fabricated via additive technologies providing obtaining of internal cellular adjustable structure from the material which is burnt at the temperature not more than the lower temperature threshold of polymorphic transformations of a filling agent of refractory suspension. This refractory suspension is applied on the pattern block with 1-2 layers, sintering of ceramic shell and burning of a pattern block are carried out after placing the pattern block in a moulding box and its filling by fluid self-hardening mixture. Then mould filling by metallic melt is conducted after solidification and restoration of the required gas permeability of fluid self-hardening mixture, while vacuum treatment of the mould is stopped after reaching the solidus temperature by metal. The authors believe that the suggested technology can be used for manufacture of castings of special duty from low-carbon steels and other alloys, which are sensitive to destruction of consumable patterns manufactured via additive technologies (additive patterns).The research was carried out at the expenses of subvention within the framework of Kazan(Privolzhskiy) Federal University in order to rise its competitiveness among the leading global scientific and education centers.


  • Production of moulding cores and waterglass mixtures using “dry ice” for steel and iron casting

    by I. O. Leushin, L. I. Leushina, I. P. Balabanov, I. A. Savin

    Increased interest of industrial enterprises to manufacture of moulding cores and moulds of mixtures based on waterglass binder is connected with acceptability and high ecological safety of this material. It stipulated more active work for searching technical solutions that can decrease or exclude deficiencies of such technologies as carbon dioxide blowing and thermal effect that are mostly popular at Russian enterprises. Among these deficiencies, the following can be mentioned for example: low setting rates during blowing of waterglass mixtures in the normal temperature conditions as well as the effect of noncontrolled moisture migration in a moulding core of mould body during heating. Their appearances lead to deterioration of operation parameters of core or mould, such as lowering of surface strength, increase of friability, elevation of strength of internal parts of core or mould, what enlarges the risk of their poor knock-out ability from steel and iron castings. Analytical survey of accessible information data was conducted by the authors of this paper; they revealed two directions in searching the solution of the a.m. problem that were supported by overwhelming majority of the researchers. These directions include directed vacuum treatment of technological accessories for increase of control abilities of moisture migration in a body of core or mould, as well as technological additives of different origination in the mixture composition for provision of timely softening of core or mould during knock-out operation out of casting. However, their use does not guarantee always the stable positive effect, thereby this task is still not solved. The authors of this paper concentrated their attention on the problem of development and testing the innovative technology of production of moulding cores and moulds of waterglass mixtures in the conditions of operating enterprise. This technology allows to improve their operating properties and parameters, to lower the mentioned deficiencies and as a result to stabilize the quality of cast metallic billets of steel and iron at the high level. Solving of this task is based on well-known combination of chemical and physical mechanisms of setting of waterglass mixtures together with directed vacuum treatment of technological accessories during acquiring of the required geometrical shape by a moulding core or mould. In this case the following consequent operations tale place: filling of moulding core or moulding box accessories by mixture; its compacting and strengthening via passing of heated setting gas through the mixture from the one side of core or mould with simultaneous its consumption from the other side due to adjustable exhausting. The authors substantiated scientifically and proved experimentally expedience of introduction of small amount of solid carbon dioxide (“dry ice”) in the form of particles with preset size and compensation of inevitably occurring undesirable endothermic effect of setting gas heating (air in this case) up to higher temperature in comparison with well-known prototype. Testing of the suggested solution in the conditions of operating production facilities confirmed its practical efficiency. The research was conducted at the expenses of subvention within the framework of the state support of Kazan Federal University among the leading global science and education centers.


  • Open Access

    Experience in the application of nitriding in a glow discharge to increase the efficiency of gear processing by the method of grinding

    by V N Gilman, A I Fashutdinov, I P Balabanov

    The article presents the experience of increasing the resistance by nitriding the gear tool using the method of grinding, using the Skywing technology. Tool material P6M5K5 with hardness 62-64HRC (analog: 1.3243, HS6-5-2-5 – Germany, W6Mo5Cr4V2Co5-China). Gear material is 20crnimoh structural alloy steel (analog 1.6523, 21NiCrMo2 – Germany). Nitriding was carried out by ionoplasmic nitriding, in an ammonia gas environment, at a temperature of 450 degrees Celsius, for 40 hours, to a depth of 0.6 mm. In addition, a wear-resistant coating based on alumotite carbonitrides was applied, with the activation of the surfaces by a hydroabrasive installation based on aluminum oxide. Washing was carried out in an environment of alkaline surfactants. This experience led to rapid destruction of the cutting edges. Experience has shown that the saturation of tool steel with nitrogen did not yield the expected dispersed nitrides. The material has become fragle. This is due to the oversaturation of tool steel with alloying elements. In continuation, it is recommended to conduct a new experiment with heating to 500-520 degrees Celsius and nitrogen in a glow discharge lasting 2-3 hours for an expected layer of 20-40 microns. In order to avoid loss of adhesion of the wear-resistant coating for some nitrogen etching, it is assumed that an argon volume is introduced into the gas mixture.


  • Open Access

    Development of a parametric model for calculating cutting forces for external cylindrical turning of steel 20CrMNTi

    by I P Balabanov, O N Balabanova, V N Gilman

    The paper presents a mathematical model for calculating the cutting force when processing 20crmnti steel with the Sandvik CNMG 120408 16P25T tool. The stand based on the 16d25 machine is presented. It allows measuring the actual values of the spindle speed, longitudinal feed, cutting depth, and cutting force. The results are transmitted to the computer via the LTR-EU-8 workstation with galvanically isolated LTE modules and a synchronization interface. According to the test results, the obtained theoretical model has a deviation from the actual measurements of no more than 0.12%. It is shown that the calculation results provided by the leading tool manufacturers are expected to be overstated. The difference in cutting forces can be more than 1.5 times.


  • Open Access

    Improving the efficiency of shaving through the use of wear-resistant coatings

    by V N Gilman, I P Balabanov, A I Faskhutdinov

    The influence of the preparation and use of various types of wear-resistant coatings on the tool shaver of high-speed steel R6M5K5 with a hardness of 60-65HRc for shavinging parts such as gear driven made of steel 20HGNMTA with a hardness of 160-210 HB. The use of hydroabrasive cleaning with ceramic balls made it possible to obtain a clean surface with a rounding of the cutting edge to 7 microns. For the analysis of durability, coatings based on titanium nitride (TiN) and a multi-component coating of titanium and aluminum (AlTiN) were used. The coating on the basis of titanium nitride (TiN) increased the resistance 1.35 times. Multi-component coating of titanium and aluminum (AlTiN) increased resistance 1.61 (AlTiN) times.


  • Modeling of the Cutting Edge Rounding Influence on the Tool Life in Processing A Gear Wheel by the Power Skiving Method

    by Igor P. Balabanov, Vitaliy N. Gilman, Tatyana S. Timofeeva, Airat I. Faskhutdinov

    Modeling of the shaping by a milling cutter is made while forming the internal gear teeth of the driven gear wheel. The estimate of the cutting edge rounding influence on the tool life taking into account the wear-resistant coating. The effects of radii of 10 μm, 15 μm, 20 μm, 25 μm are simulated. At the edge radius of 10 μm, the coating layer is rapidly collapses. At a radius of 15 μm, the highest tool life is obtained. At the more high radii, the tools durability is decreases. A practical experiment was carried out on a cupped skiving cutter with AlTiCN-coating (PVD). Processed steel 41CrAlMo7 with hardness 241-287НВ. The simulation results were confirmed, the highest tools lifetime at a radius of 16.13 microns for 60 parts. As a result, for this type of processing and for this coating type of the cutting tool, the most optimal cutting edge rounding can be considered as the value of 15-18 μm. It can be concluded that, perhaps, a more sharp edge from 10 to 15 μm can be a positive effect on tools lifetime, in the case of uniform rounding over the entire cutter edge of the tools tooth (on the top and side tooth profile).


  • Open Access

    Implementation of Iso 9001, Iso 14001, Iso 45001 Requirements with the Systems of Electronic Document Turnover

    by Igor P. Balabanov, Fail F. Davletshin

    In the modern actively developing conditions of globalization and informatization of production, and emergence of new technologies, only those firms have chances to remain at the market which find ways and means of optimization of processes in time. Adhering to the basic principles of the integrated system of management ensures the most natural and trouble-free functioning of all organizational structure. This paper covers the specifics of work with documentation, or the system of paper and electronic document flow, and with the application of an electronic document management system taking into account observance of requirements of documentary information management system. Adherence to ISM requirements for documentary information management is quite real with options of conducting document flow. Nevertheless, it is much simpler and more effective to perform with already introduced EDMS, and the effect of its use of subjects is higher when the enterprise scale and a number of staff involved in work with documentation are bigger. The maximum output can be achieved from electronic document flow introduction with an optimum ratio of the functions demanded in operation and if opportunities of the chosen system correspond to them. Â


  • Selecting optimal cutting tools for lathes

    by R. M. Khusainov, A. N. Golovko, S. M. Petrov, S. Yu. Yurasov, I. P. Balabanov, V. A. Grechishnikov, V. B. Romanov, P. M. Pivkin

    A method is proposed for selecting optimal tool geometry and identifying the best lathe tool for specific applications from a catalog or database.