Yuma Horio
Research Subjects
Yuma Horio has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
Takahiro Hayashi
Materials & Components Development Center, YAMAHA Corporation, 203 Matsunokijima, Iwata-shi, 438-0192, Japan
4 shared publicationsHiroyuki Yamashita
Material & Components Development Center, YAMAHA Corporation
3 shared publicationsNaoki Kamimura
Materials & Components Development Center, YAMAHA Corporation, 203 Matsunokijima, Iwata-shi, 438-0192, Japan
1 shared publicationNobuaki Tomita
Materials & Components Development Center, YAMAHA Corporation, 203 Matsunokijima, Iwata-shi, 438-0192, Japan
1 shared publicationTakahisa Tachibana
Materials & Components Development Center, YAMAHA Corporation, 203 Matsunokijima, Iwata-shi, 438-0192, Japan
1 shared publication
Latest Publications
- 1 January 2006
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 363-366
Application of Thermoelectric Modules Fabricated with (Bi,Sb)2(Te,Se)3 using Rapid Solidification Technique for the Projector System
A thermoelectric generator system was developed to convert low grade waste heat from a bulb inside an optical projection system into electricity. A new type of thermoelectric module with (Bi,Sb)2(Te,Se)3 compounds and intended for consumer use was installed in the system. Bismuth-telluride-based thermoelectric compounds with fine grains and unidirectional crystal orientation prepared using a rapid solidification technique, exhibited high performance at temperatures ranging from 298 to 473 K. Thermoelectric properties were optimized by controlling the microstructure and oxygen content of the specimens. A maximum conversion efficiency of 5.7% was obtained from the developed thermoelectric module at a temperature differential of 150 K (Tc = 323 K, Th = 473 K). A thermoelectric power generating system using a new type of aluminum alloy reflector was developed and evaluated for the prototype projection system
- 1 January 2006
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 363-366
Application of Thermoelectric Modules Fabricated with (Bi,Sb)2(Te,Se)3 using Rapid Solidification Technique for the Projector System
A thermoelectric generator system was developed to convert low grade waste heat from a bulb inside an optical projection system into electricity. A new type of thermoelectric module with (Bi,Sb)2(Te,Se)3 compounds and intended for consumer use was installed in the system. Bismuth-telluride-based thermoelectric compounds with fine grains and unidirectional crystal orientation prepared using a rapid solidification technique, exhibited high performance at temperatures ranging from 298 to 473 K. Thermoelectric properties were optimized by controlling the microstructure and oxygen content of the specimens. A maximum conversion efficiency of 5.7% was obtained from the developed thermoelectric module at a temperature differential of 150 K (Tc = 323 K, Th = 473 K). A thermoelectric power generating system using a new type of aluminum alloy reflector was developed and evaluated for the prototype projection system
- Open Access
- 1 January 2005
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 46 (11) , 2525-2529
Microstructure and Thermoelectric Properties of Hot-Pressed n-Type Bi1.9Sb0.1Te2.6Se0.4 Alloys Prepared Using a Rapid Solidification Technique
N-type Bi1.9Sb0.1Te2.6Se0.4 alloys were prepared by a rapid solidification technique and subsequent hot-pressing method. The microstructure and thermoelectric properties of the alloys were investigated as a function of the hot-pressing temperature and pressure. The X-ray diffraction measurements indicate that the grains are preferably aligned with the c-axis perpendicular to the direction of the hot-pressing force by the hot-pressing. Hot-pressing at higher temperature promotes the grain growth in the alloys. The Seebeck coefficient (α) and electrical resistivity (ρ) decrease with an increase in the hot-pressing temperature, whereas the thermal conductivity (κ) increases. The specimens prepared at higher temperature greater than 733 K show better thermoelectric performance: the largest dimensionless figure of merit (ZT) is 1.08 at room temperature.
- 1 January 2005
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 46 (11) , 2525-2529
Open AccessMicrostructure and Thermoelectric Properties of Hot-Pressed n-Type Bi1.9Sb0.1Te2.6Se0.4 Alloys Prepared Using a Rapid Solidification Technique
N-type Bi1.9Sb0.1Te2.6Se0.4 alloys were prepared by a rapid solidification technique and subsequent hot-pressing method. The microstructure and thermoelectric properties of the alloys were investigated as a function of the hot-pressing temperature and pressure. The X-ray diffraction measurements indicate that the grains are preferably aligned with the c-axis perpendicular to the direction of the hot-pressing force by the hot-pressing. Hot-pressing at higher temperature promotes the grain growth in the alloys. The Seebeck coefficient (α) and electrical resistivity (ρ) decrease with an increase in the hot-pressing temperature, whereas the thermal conductivity (κ) increases. The specimens prepared at higher temperature greater than 733 K show better thermoelectric performance: the largest dimensionless figure of merit (ZT) is 1.08 at room temperature.
- 1 January 2004
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 45 (12) , 3309-3313
Microstructure and Thermoelectric Properties of Hot-Pressed p-Type Bi0.5Sb1.5Te3 Alloys Prepared by Rapid Solidification Technique
Rapidly solidified bismuth-telluride based alloy foil; fabricated using the single roller melt spinning method exhibits a fine microstructure with unidirectional crystals. Meanwhile, a hot-pressing process, using rapidly solidified foils, was used to prepare the consolidated samples. The fine microstructure of this alloy is extremely effective in decreasing thermal conductivity because of the grain boundary scattering of the phonons, a key factor improving the thermoelectric properties of thermoelectric materials. Hot-pressed samples using these rapidly solidified foils display lower thermal conductivity values than the alloys made by the conventional hot-consolidating method using pulverized ingot powder. In this case, thermoelectric properties were investigated comparatively in terms of hot-pressed rapidly solidified foil specimens and pulverized powders of these foils under 53 μm in size, evaluating the dependence of the hot-pressing temperature and consequent pressure on the thermoelectric properties of these specimens. The maximum figure of merit (Z) obtained was 3.34 × 10−3 K−1.
- 1 January 2004
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 45 (12) , 3309-3313
Microstructure and Thermoelectric Properties of Hot-Pressed p-Type Bi0.5Sb1.5Te3 Alloys Prepared by Rapid Solidification Technique
Rapidly solidified bismuth-telluride based alloy foil; fabricated using the single roller melt spinning method exhibits a fine microstructure with unidirectional crystals. Meanwhile, a hot-pressing process, using rapidly solidified foils, was used to prepare the consolidated samples. The fine microstructure of this alloy is extremely effective in decreasing thermal conductivity because of the grain boundary scattering of the phonons, a key factor improving the thermoelectric properties of thermoelectric materials. Hot-pressed samples using these rapidly solidified foils display lower thermal conductivity values than the alloys made by the conventional hot-consolidating method using pulverized ingot powder. In this case, thermoelectric properties were investigated comparatively in terms of hot-pressed rapidly solidified foil specimens and pulverized powders of these foils under 53 μm in size, evaluating the dependence of the hot-pressing temperature and consequent pressure on the thermoelectric properties of these specimens. The maximum figure of merit (Z) obtained was 3.34 × 10−3 K−1.
- 1 January 2004
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 45 (8) , 2757-2760
Microstructure and Crystal Orientation of Rapidly Solidified (Bi,Sb)2(Te,Se)3 Alloys by the Liquid Quenching Technique
A rapid solidification process was found to form unidirectional crystal structures in (Bi,Sb)2Te3 and (Bi,Sb)2(Te,Se)3 based thermoelectric alloys. This fine microstructure with its unidirectional crystal orientation is expected to yield high value thermoelectric properties because the fine grain size is extremely effective in decreasing thermal conductivity by boundary scattering of phonons and because this crystal orientation is extremely effective in decreasing the electrical resistivity (increasing the carrier mobility). The rapidly solidified alloys were prepared by a single-roller liquid quenching method. These alloys were shaped as a thin foil with thicknesses ranging from 5 to 20 μm. The crystal orientation was analyzed by the x-ray diffraction method and the microstructure was observed by optical microscopy and SEM of the thin foil samples. The crystal grains of the rapidly solidified foils were very fine and highly oriented. The thermoelectric properties were measured for p-type Bi0.4Sb1.6Te3 and the n-type Bi1.9Sb0.1Te2.6Se0.4 compacted alloys. The figures of merit of 3.5 × 10−3 K−1 for p-type alloy and 3.3 × 10−3 K−1 for n-type alloy were obtains. It is proposed that the rapid solidification is very useful technique for the improvement of thermoelectric properties.
- 1 January 2004
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 45 (8) , 2757-2760
Microstructure and Crystal Orientation of Rapidly Solidified (Bi,Sb)2(Te,Se)3 Alloys by the Liquid Quenching Technique
A rapid solidification process was found to form unidirectional crystal structures in (Bi,Sb)2Te3 and (Bi,Sb)2(Te,Se)3 based thermoelectric alloys. This fine microstructure with its unidirectional crystal orientation is expected to yield high value thermoelectric properties because the fine grain size is extremely effective in decreasing thermal conductivity by boundary scattering of phonons and because this crystal orientation is extremely effective in decreasing the electrical resistivity (increasing the carrier mobility). The rapidly solidified alloys were prepared by a single-roller liquid quenching method. These alloys were shaped as a thin foil with thicknesses ranging from 5 to 20 μm. The crystal orientation was analyzed by the x-ray diffraction method and the microstructure was observed by optical microscopy and SEM of the thin foil samples. The crystal grains of the rapidly solidified foils were very fine and highly oriented. The thermoelectric properties were measured for p-type Bi0.4Sb1.6Te3 and the n-type Bi1.9Sb0.1Te2.6Se0.4 compacted alloys. The figures of merit of 3.5 × 10−3 K−1 for p-type alloy and 3.3 × 10−3 K−1 for n-type alloy were obtains. It is proposed that the rapid solidification is very useful technique for the improvement of thermoelectric properties.