Ghent University, Ghent, Belgium
5 shared publications - Tom Depover
Ghent University
5 shared publications - Arne R. D. Verliefde
Ghent University
3 shared publications - Ellen Lambrechts
Research Unit Sustainable Materials Science, Department of Materials, Textiles and Chemical Engineering, Ghent University, Technologiepark 46, 9052 Zwijnaarde, Belgium
2 shared publications - Aurélie Laureys
Department of Materials, Textiles and Chemical Engineering, Ghent University, Technologiepark-Zwijnaarde 70A, 9052 Ghent, Belgium
1 shared publication - Evelyn De Meyer
Faculty of Veterinary Medicine, Ghent University Department of Veterinary and Biosciences Merelbeke
1 shared publication
Latest Publications
- Open Access
Stress Corrosion Cracking of Steam Turbine Steel: The Influence of Organic Acid Characteristics
This work evaluates the impact of different organic acids on the corrosion sensitivity and stress-corrosion cracking (SCC) of NiCrMoV steam turbine steel. For all organic acids, potentiodynamic measurements shows linear relationships between corrosion rate and hydrogen proton concentration between pH 2.4 and 3.9. For solutions with the same pH, i.e., similar conductivity, the corrosion rate differs depending on the type of organic acid. The anodic dissolution in formic acid is the highest, followed by acetic, propanoic and nonanoic acid. The acid dissociation reaction is identified as the rate determining step in the corrosion process. Nonanoic acid, alternatively, clearly acts as a corrosion inhibitor. In situ four-point constant-extension tests in formic acid, acetic acid and nonanoic acid, at a pH value of 3.4 were performed to evaluate their impact on the SSC sensitivity. The general degradation followed the trend of the corrosion rate, although the synergetic effect of corrosion and stress resulted in a higher degradation depth. Though nonanoic acid induced little visible corrosion, still stress-corrosion cracks were still detected. It was shown that solutions of different organic acids with the same pH do not have the same influence on stress-induced degradation.
Open AccessStress Corrosion Cracking of Steam Turbine Steel: The Influence of Organic Acid Characteristics
This work evaluates the impact of different organic acids on the corrosion sensitivity and stress-corrosion cracking (SCC) of NiCrMoV steam turbine steel. For all organic acids, potentiodynamic measurements shows linear relationships between corrosion rate and hydrogen proton concentration between pH 2.4 and 3.9. For solutions with the same pH, i.e., similar conductivity, the corrosion rate differs depending on the type of organic acid. The anodic dissolution in formic acid is the highest, followed by acetic, propanoic and nonanoic acid. The acid dissociation reaction is identified as the rate determining step in the corrosion process. Nonanoic acid, alternatively, clearly acts as a corrosion inhibitor. In situ four-point constant-extension tests in formic acid, acetic acid and nonanoic acid, at a pH value of 3.4 were performed to evaluate their impact on the SSC sensitivity. The general degradation followed the trend of the corrosion rate, although the synergetic effect of corrosion and stress resulted in a higher degradation depth. Though nonanoic acid induced little visible corrosion, still stress-corrosion cracks were still detected. It was shown that solutions of different organic acids with the same pH do not have the same influence on stress-induced degradation.
- 1 February 2021
- Published by SAGE Publications in Materials Science and Technology
- Vol. 37 (3) , 250-257
Assessment of the hydrogen interaction on the mechanical integrity of a welded martensitic steel
This work evaluates the effect of hydrogen on the mechanical integrity of a weld in a martensitic base metal. Different regions in the heat-affected zone (HAZ) are reproduced to investigate the interaction of the local microstructure with hydrogen. The hardness strongly depends on the distance from the welding joint due to the different phases present. The HAZ contains zones of acicular ferrite, coarse martensite and tempered martensite. Additionally, the entire weld is subjected to a constant load while being simultaneously electrochemically charged with hydrogen. During this test, a crack initiates in the filler, showing the highest hydrogen solubility as demonstrated by thermal desorption spectroscopy, while propagation occurs along the microstructure of the HAZ with the highest hardness level.
- 1 February 2021
- Published by SAGE Publications in Materials Science and Technology
- Vol. 37 (3) , 250-257
Assessment of the hydrogen interaction on the mechanical integrity of a welded martensitic steel
This work evaluates the effect of hydrogen on the mechanical integrity of a weld in a martensitic base metal. Different regions in the heat-affected zone (HAZ) are reproduced to investigate the interaction of the local microstructure with hydrogen. The hardness strongly depends on the distance from the welding joint due to the different phases present. The HAZ contains zones of acicular ferrite, coarse martensite and tempered martensite. Additionally, the entire weld is subjected to a constant load while being simultaneously electrochemically charged with hydrogen. During this test, a crack initiates in the filler, showing the highest hydrogen solubility as demonstrated by thermal desorption spectroscopy, while propagation occurs along the microstructure of the HAZ with the highest hardness level.
- Open Access
Effect of Film-Forming Amines on the Acidic Stress-Corrosion Cracking Resistance of Steam Turbine Steel
This work evaluates the effect of film-forming amines (FFA) on the acidic stress-corrosion cracking (SCC) resistance of NiCrMoV turbine steel. Contact angle measurements show an increased hydrophobicity of the surface when coating the steel with oleyl propylene diamine (OLDA). According to potentiodynamic measurements and post-mortem scanning electron microscopy (SEM) analysis, anodic dissolution and hydrogen embrittlement still occur when the steel is FFA coated. In situ constant extension rate testing (CERT) in acidic aqueous environment at elevated temperature of FFA-coated steel shows a ductility gain compared to non-coated steel, explained by a decrease in both corrosion rate and hydrogen uptake.
Open AccessEffect of Film-Forming Amines on the Acidic Stress-Corrosion Cracking Resistance of Steam Turbine Steel
This work evaluates the effect of film-forming amines (FFA) on the acidic stress-corrosion cracking (SCC) resistance of NiCrMoV turbine steel. Contact angle measurements show an increased hydrophobicity of the surface when coating the steel with oleyl propylene diamine (OLDA). According to potentiodynamic measurements and post-mortem scanning electron microscopy (SEM) analysis, anodic dissolution and hydrogen embrittlement still occur when the steel is FFA coated. In situ constant extension rate testing (CERT) in acidic aqueous environment at elevated temperature of FFA-coated steel shows a ductility gain compared to non-coated steel, explained by a decrease in both corrosion rate and hydrogen uptake.
- Open Access
- 14 March 2020
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 14 (52) , 113-127
Initiation of hydrogen induced cracks at secondary phase particles
The goal of this work is to propose a general mechanism for hydrogen induced crack initiation in steels based on a microstructural study of multiple steel grades. Four types of steels with strongly varying microstructures are studied for this purpose, i.e. ultra low carbon (ULC) steel, TRIP (transformation induced plasticity) steel, Fe-C-Ti generic alloy, and pressure vessel steel. A strong dependency of the initiation of hydrogen induced cracks on the microstructural features in the materials is observed. By use of SEM-EBSD characterization, initiation is found to always occur at the hard secondary phase particles in the materials.
- 14 March 2020
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 14 (52) , 113-127
Open AccessInitiation of hydrogen induced cracks at secondary phase particles
The goal of this work is to propose a general mechanism for hydrogen induced crack initiation in steels based on a microstructural study of multiple steel grades. Four types of steels with strongly varying microstructures are studied for this purpose, i.e. ultra low carbon (ULC) steel, TRIP (transformation induced plasticity) steel, Fe-C-Ti generic alloy, and pressure vessel steel. A strong dependency of the initiation of hydrogen induced cracks on the microstructural features in the materials is observed. By use of SEM-EBSD characterization, initiation is found to always occur at the hard secondary phase particles in the materials.