Antonio Mulone
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Antonio Mulone has a total of 43 co-authors. Here are the top co-authors by number of shared publications:
- Uta Klement
Division of Materials and Manufacture, Department of Mechanical Engineering Chalmers University of Technology Göteborg Sweden
4 shared publications - Jordi Sort
Departament de Física, Universitat Autònoma de Barcelona, E-08193 Cerdanyola del Vallès, Spain
3 shared publications Uta Klement
3 shared publicationsU. Klement
Department of Industrial and Materials Science, Chalmers University of Technology Gothenburg, Sweden
2 shared publications- Wolfgang Kautek
Department of Physical Chemistry, University of Vienna, Vienna, Austria
2 shared publications A. Nicolenco
1 shared publication
Latest Publications
- Open Access
Synchrotron X-ray spectromicroscopy analysis of wear tested graphene-containing alumina coatings
- Open Access
Electrodeposition of Soft Magnetic Fe-W-P Alloy Coatings from an Acidic Electrolyte
Fe-W-P coatings were deposited from a newly developed electrolytic bath. The effect of plating parameters, such as electrolyte current density and pH has been studied. It was found that the pH has a very strong effect on the phosphorous content of the coatings. Metallic-like, non-powdery alloys of Fe-W-P deposits with no cracks (lowly stressed) can be obtained at a lower pH (3), the composition changes to low phosphorus and high tungsten content, showing a matte, greyish, and rough surface. The applied current density also influences the morphology and the amount of phosphorous content. The deposits showed an amorphous structure for all samples with soft ferromagnetic properties.
Open AccessElectrodeposition of Soft Magnetic Fe-W-P Alloy Coatings from an Acidic Electrolyte
Fe-W-P coatings were deposited from a newly developed electrolytic bath. The effect of plating parameters, such as electrolyte current density and pH has been studied. It was found that the pH has a very strong effect on the phosphorous content of the coatings. Metallic-like, non-powdery alloys of Fe-W-P deposits with no cracks (lowly stressed) can be obtained at a lower pH (3), the composition changes to low phosphorus and high tungsten content, showing a matte, greyish, and rough surface. The applied current density also influences the morphology and the amount of phosphorous content. The deposits showed an amorphous structure for all samples with soft ferromagnetic properties.
- Open Access
- 19 December 2022
- Published by MDPI AG in Applied Sciences
- Vol. 12 (24) , 13018
An Integrated Approach for Structural Health Monitoring and Damage Detection of Bridges: An Experimental Assessment
The issue of monitoring the structural condition of bridges is becoming a top priority worldwide. As is well known, any infrastructure undergoes a progressive deterioration of its structural conditions due to aging by normal service loads and environmental conditions. At the same time, it may suffer serious damages or collapse due to natural phenomena such as earthquakes or strong winds. For this reason, it is essential to rely on efficient and widespread monitoring techniques applied throughout the entire road network. This paper aims to introduce an integrated procedure for structural and material monitoring. With regard to structural monitoring, an innovative approach for monitoring based on Vehicle by Bridge Interaction (VBI) will be proposed. Furthermore, with regard to material monitoring, to evaluate concrete degradation, a non-invasive method based on the continuous monitoring of the pH, as well as chloride and sulfate ions concentration in the concrete, is presented.
- 19 December 2022
- Published by MDPI AG in Applied Sciences
- Vol. 12 (24) , 13018
Open AccessAn Integrated Approach for Structural Health Monitoring and Damage Detection of Bridges: An Experimental Assessment
The issue of monitoring the structural condition of bridges is becoming a top priority worldwide. As is well known, any infrastructure undergoes a progressive deterioration of its structural conditions due to aging by normal service loads and environmental conditions. At the same time, it may suffer serious damages or collapse due to natural phenomena such as earthquakes or strong winds. For this reason, it is essential to rely on efficient and widespread monitoring techniques applied throughout the entire road network. This paper aims to introduce an integrated procedure for structural and material monitoring. With regard to structural monitoring, an innovative approach for monitoring based on Vehicle by Bridge Interaction (VBI) will be proposed. Furthermore, with regard to material monitoring, to evaluate concrete degradation, a non-invasive method based on the continuous monitoring of the pH, as well as chloride and sulfate ions concentration in the concrete, is presented.
- 1 January 2021
- Published by Elsevier in Surface and Coatings Technology
- Vol. 406
Carbide-laden coatings deposited using a hand-held high-velocity air-fuel (HVAF) spray gun
- 1 January 2021
- Published by Elsevier in Surface and Coatings Technology
- Vol. 406
Carbide-laden coatings deposited using a hand-held high-velocity air-fuel (HVAF) spray gun
- Open Access
- 30 October 2020
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (5) , 4006-4012
In-situ TEM annealing of amorphous Fe-24at.%W coatings and the effect of crystallization on hardness
This paper describes the crystallization which occurs upon annealing of an amorphous Fe-24at.%W coatings, electrodeposited from a glycolate-citrate plating bath. A combination of Differential Scanning Calorimetry and in-situ Transmission Electron Microscopy annealing is used to study the onset of crystallization of the amorphous coating. The in-situ TEM analyses reveal the formation of first crystallites after annealing at 400 °C for 30 min. Upon a temperature increase to 500–600 °C, the crystallites develop into Fe-rich nanocrystals with ~ 40 nm grain size. The nanocrystals are dispersed in the remaining amorphous Fe-W matrix, which results in the formation of a mixed nanocrystalline-amorphous structure. The observed crystallization can be held responsible for the increase in the hardness obtained upon annealing of Fe-24at.%W coatings. In fact, the hardness of the as-deposited material increases from 11 to 13 GPa after annealing at 400 °C, and it reaches the maximum value of 16.5 GPa after annealing at 600 °C.
- 30 October 2020
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (5) , 4006-4012
Open AccessIn-situ TEM annealing of amorphous Fe-24at.%W coatings and the effect of crystallization on hardness
This paper describes the crystallization which occurs upon annealing of an amorphous Fe-24at.%W coatings, electrodeposited from a glycolate-citrate plating bath. A combination of Differential Scanning Calorimetry and in-situ Transmission Electron Microscopy annealing is used to study the onset of crystallization of the amorphous coating. The in-situ TEM analyses reveal the formation of first crystallites after annealing at 400 °C for 30 min. Upon a temperature increase to 500–600 °C, the crystallites develop into Fe-rich nanocrystals with ~ 40 nm grain size. The nanocrystals are dispersed in the remaining amorphous Fe-W matrix, which results in the formation of a mixed nanocrystalline-amorphous structure. The observed crystallization can be held responsible for the increase in the hardness obtained upon annealing of Fe-24at.%W coatings. In fact, the hardness of the as-deposited material increases from 11 to 13 GPa after annealing at 400 °C, and it reaches the maximum value of 16.5 GPa after annealing at 600 °C.
- 3 May 2020
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 98 (3) , 108-113
Electrodeposition: three steps towards sustainability
In the field of electrodeposition, it is becoming extremely important to integrate the technological progress with sustainability concerns expressed through recent environmental restrictions and regulations. This is especially relevant in consideration of the research dedicated to finding sustainable alternatives for coatings deposited with environmentally hazardous processes such as chromium plating. In this paper, the authors discuss different aspects of a proposed sustainable approach that could be applied as a guideline for future research.
- 3 May 2020
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 98 (3) , 108-113
Electrodeposition: three steps towards sustainability
In the field of electrodeposition, it is becoming extremely important to integrate the technological progress with sustainability concerns expressed through recent environmental restrictions and regulations. This is especially relevant in consideration of the research dedicated to finding sustainable alternatives for coatings deposited with environmentally hazardous processes such as chromium plating. In this paper, the authors discuss different aspects of a proposed sustainable approach that could be applied as a guideline for future research.
- Open Access
Improvement in the Wear Resistance under Dry Friction of Electrodeposited Fe-W Coatings through Heat Treatments
The influence of the microstructural transformations upon heat treatments on the wear resistance of Fe-W coatings is studied. The coatings are electrodeposited from a glycolate-citrate plating bath with 24 at.% of W, and the wear resistance is investigated under dry friction conditions using ball-on-disc sliding tests. The samples were annealed in Ar atmosphere at different temperatures up to 800 °C. The microstructural transformations were studied by means of X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), and Electron Backscattered Diffraction (EBSD) technique. Except for the coating annealed at 800 °C, all the tested coatings suffered severe tribo-oxidation which resulted in the formation of deep cracks, i.e., ~15 μm in depth, within the wear track. The precipitation of the secondary phases, i.e., Fe2W and FeWO4, on the surface of the sample annealed at 800 °C increased the resistance to tribo-oxidation leading to wear tracks with an average depth of ~3 μm. Hence, the Fe-W coating annealed at 800 °C was characterized with a higher wear resistance resulting in a wear rate comparable to electrodeposited hard chromium coatings, i.e., 3 and 4 × 10−6 mm3/N m, respectively.
Open AccessImprovement in the Wear Resistance under Dry Friction of Electrodeposited Fe-W Coatings through Heat Treatments
The influence of the microstructural transformations upon heat treatments on the wear resistance of Fe-W coatings is studied. The coatings are electrodeposited from a glycolate-citrate plating bath with 24 at.% of W, and the wear resistance is investigated under dry friction conditions using ball-on-disc sliding tests. The samples were annealed in Ar atmosphere at different temperatures up to 800 °C. The microstructural transformations were studied by means of X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), and Electron Backscattered Diffraction (EBSD) technique. Except for the coating annealed at 800 °C, all the tested coatings suffered severe tribo-oxidation which resulted in the formation of deep cracks, i.e., ~15 μm in depth, within the wear track. The precipitation of the secondary phases, i.e., Fe2W and FeWO4, on the surface of the sample annealed at 800 °C increased the resistance to tribo-oxidation leading to wear tracks with an average depth of ~3 μm. Hence, the Fe-W coating annealed at 800 °C was characterized with a higher wear resistance resulting in a wear rate comparable to electrodeposited hard chromium coatings, i.e., 3 and 4 × 10−6 mm3/N m, respectively.
- Open Access
- 1 September 2018
- Published by Elsevier in Surface and Coatings Technology
- Vol. 350, 20-30
Enhanced mechanical properties and microstructural modifications in electrodeposited Fe-W alloys through controlled heat treatments
- 1 September 2018
- Published by Elsevier in Surface and Coatings Technology
- Vol. 350, 20-30
Open AccessEnhanced mechanical properties and microstructural modifications in electrodeposited Fe-W alloys through controlled heat treatments
- Open Access
Alkoxylated β-Naphthol as an Additive for Tin Plating from Chloride and Methane Sulfonic Acid Electrolytes
β-naphthol was one of the first additives introduced for smooth and homogeneous tin electrodeposition. Although it can be oxidized under the plating conditions, forming either 1,2-napthoquinone or polymeric materials based on naphthioxides, it is still in use. In this work, an investigation of its more stable form, alkoxylated β-naphthol (ABN), on tin plating is undertaken. For this purpose, chloride based (pH ~5) and methane sulfonic acid (MSA, pH ~0.5) electrolytes, including ABN, were prepared. Reaction kinetics were studied by polarization, Tafel measurements, and cyclic voltammetry. Tin electrodeposits were obtained on flat brass substrates. Surface morphology and preferred crystal orientation were studied by Scanning Electron Microscopy (SEM) and X-ray Diffraction (XRD). In both studied electrolytes ABN acts as an inhibitor but in the case of the chloride electrolyte it is more pronounced. In the MSA electrolyte this effect was overlaid by the presence of tin-citrate complexes. In the chloride-based electrolyte, ABN has a grain refining effect, while in the MSA electrolyte an increase of ABN concentration leads to a slight enlargement of the average grain size. X-ray analysis shows a constant decrease of the (101) intensity with increasing concentration of ABN for the sample deposited from both baths.
Open AccessAlkoxylated β-Naphthol as an Additive for Tin Plating from Chloride and Methane Sulfonic Acid Electrolytes
β-naphthol was one of the first additives introduced for smooth and homogeneous tin electrodeposition. Although it can be oxidized under the plating conditions, forming either 1,2-napthoquinone or polymeric materials based on naphthioxides, it is still in use. In this work, an investigation of its more stable form, alkoxylated β-naphthol (ABN), on tin plating is undertaken. For this purpose, chloride based (pH ~5) and methane sulfonic acid (MSA, pH ~0.5) electrolytes, including ABN, were prepared. Reaction kinetics were studied by polarization, Tafel measurements, and cyclic voltammetry. Tin electrodeposits were obtained on flat brass substrates. Surface morphology and preferred crystal orientation were studied by Scanning Electron Microscopy (SEM) and X-ray Diffraction (XRD). In both studied electrolytes ABN acts as an inhibitor but in the case of the chloride electrolyte it is more pronounced. In the MSA electrolyte this effect was overlaid by the presence of tin-citrate complexes. In the chloride-based electrolyte, ABN has a grain refining effect, while in the MSA electrolyte an increase of ABN concentration leads to a slight enlargement of the average grain size. X-ray analysis shows a constant decrease of the (101) intensity with increasing concentration of ABN for the sample deposited from both baths.