Navid Sayyar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Navid Sayyar has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
Vidar Hansen
Department of Mechanical and Structural Engineering and Materials Science, University of Stavanger, Stavanger, Norway
4 shared publications- Wakshum Mekonnen Tucho
Department of Mechanical and Structural Engineering and Materials Science, University of Stavanger, 4036 Stavanger, Norway
4 shared publications Morteza Shamanian
3 shared publications- Anders Thon Sletsjøe
Department of Mechanical and Structural Engineering and Materials Science, Faculty of Science and Technology, University of Stavanger, 4036 Stavanger, Norway
2 shared publications - Jalal Kangazian
Department of Materials Engineering, Isfahan University of Technology, Isfahan, Iran
2 shared publications Mona Wetrhus Minde
University of Stavanger
2 shared publications
Latest Publications
- Open Access
- 30 October 2025
- Published by Springer Nature in Progress in Additive Manufacturing
- Vol. 11 (1) , 1203-1226
Controlled grain refinement in super duplex stainless steel via laser-based directed energy deposition: effect of microstructure on post-annealing corrosion and mechanical properties
Adoption of pulsed laser irradiation during laser-based directed energy deposition (DED-LB) resulted in substantial microstructural modifications of super duplex stainless steel, leading to significant enhancements in mechanical and corrosion properties after solution annealing. Inherent coarse and columnar grain structure, typical of conventional DED-LB, was inhibited by pulsed high-energy laser input and a refined solidification microstructure was developed. Low-speed high-frequency deposition by the pulsed process promoted strong < 001 > bcc epitaxy of ferrite toward laser paths, rather than vertical building direction, and induced pronounced texture components in both phases. The modified grain morphology and associated crystallographic orientations were largely retained after the annealing operation, demonstrating a strong microstructural and texture memory from as-built condition. The alloy developed by pulsed DED-LB exhibited enhanced mechanical performance, particularly in terms of ductility and toughness, compared to its conventionally processed counterpart. Elemental analysis and quantitative measurements revealed significantly fewer and smaller Mn- and Si-enriched oxide inclusions in the specimen produced by pulsed laser process, which contributed to reduced pit initiation tendency under corrosive environment. The grain-refined specimen exhibited more noble open-circuit potential and reduced corrosion rate. However, its repassivation was slightly delayed, likely due to lower atomic density of crystallographic planes ({001} bcc , {101} fcc , and {001} fcc ) exposed at the test surface during potentiodynamic polarization. This highlights a trade-off between enhanced general corrosion resistance and localized film recovery. The results underscore a complex interplay between microstructure, inclusions, and passivity.
- 30 October 2025
- Published by Springer Nature in Progress in Additive Manufacturing
- Vol. 11 (1) , 1203-1226
Open AccessControlled grain refinement in super duplex stainless steel via laser-based directed energy deposition: effect of microstructure on post-annealing corrosion and mechanical properties
Adoption of pulsed laser irradiation during laser-based directed energy deposition (DED-LB) resulted in substantial microstructural modifications of super duplex stainless steel, leading to significant enhancements in mechanical and corrosion properties after solution annealing. Inherent coarse and columnar grain structure, typical of conventional DED-LB, was inhibited by pulsed high-energy laser input and a refined solidification microstructure was developed. Low-speed high-frequency deposition by the pulsed process promoted strong < 001 > bcc epitaxy of ferrite toward laser paths, rather than vertical building direction, and induced pronounced texture components in both phases. The modified grain morphology and associated crystallographic orientations were largely retained after the annealing operation, demonstrating a strong microstructural and texture memory from as-built condition. The alloy developed by pulsed DED-LB exhibited enhanced mechanical performance, particularly in terms of ductility and toughness, compared to its conventionally processed counterpart. Elemental analysis and quantitative measurements revealed significantly fewer and smaller Mn- and Si-enriched oxide inclusions in the specimen produced by pulsed laser process, which contributed to reduced pit initiation tendency under corrosive environment. The grain-refined specimen exhibited more noble open-circuit potential and reduced corrosion rate. However, its repassivation was slightly delayed, likely due to lower atomic density of crystallographic planes ({001} bcc , {101} fcc , and {001} fcc ) exposed at the test surface during potentiodynamic polarization. This highlights a trade-off between enhanced general corrosion resistance and localized film recovery. The results underscore a complex interplay between microstructure, inclusions, and passivity.
- Open Access
- 28 June 2025
- Published by Springer Nature in Metals and Materials International
- Vol. 32 (1) , 195-229
Adaptive Control of Additive Manufacturing Parameters in Pulsed Laser-Based Directed Energy Deposition of Super Duplex Stainless Steel: Hybrid Taguchi-Grey Relational Approach
Process parameters determine the quality characteristics of additively manufactured (AMed) parts. During Laser-based Directed Energy Deposition (DED-LB), an elaborated parametric analysis is required to control the materials’ behaviour precisely. This work deals with the effect of process parameters on process stability in terms of consistent melt pool geometrical features, such as aspect ratio of the bead and dilution, formation of pores, and ductility of super duplex stainless steel (SDSS) during pulsed laser and powder DED-LB. Independent variables including laser power, deposition speed, pulse frequency, and flow rate of the shielding gas were selected as controlling factors to deposit single tracks and plates of SDSS. Experiments have been designed and conducted according to L16 orthogonal array of Taguchi methodology. Relative density was estimated using Archimedes method. Ductility was estimated by tensile testing of the builds. For geometrical evaluation, phase characterization, and microstructural assessment, specimens were subjected to optical and Scanning Electron Microscopies, and Electron Backscattered Diffraction. Overall results were interpreted and explained using the Taguchi approach and analysis of signal-to-noise ratio. Single objective parameter-property relationships were achieved and discussed. Conclusive parametric remarks under the multi-attribute optimization were derived using weighted Grey Relational Analysis. A desirable parametric combination was extracted, and the associated quality responses were verified by the satisfying confirmatory deposition. The key role of parameters on the process stability, microstructure, and mechanical behaviour was further discussed. This work offers a practical solution to the multi-response optimization problems that can be used in AM and surface treatment of SDSS. Graphical Abstract
- 28 June 2025
- Published by Springer Nature in Metals and Materials International
- Vol. 32 (1) , 195-229
Open AccessAdaptive Control of Additive Manufacturing Parameters in Pulsed Laser-Based Directed Energy Deposition of Super Duplex Stainless Steel: Hybrid Taguchi-Grey Relational Approach
Process parameters determine the quality characteristics of additively manufactured (AMed) parts. During Laser-based Directed Energy Deposition (DED-LB), an elaborated parametric analysis is required to control the materials’ behaviour precisely. This work deals with the effect of process parameters on process stability in terms of consistent melt pool geometrical features, such as aspect ratio of the bead and dilution, formation of pores, and ductility of super duplex stainless steel (SDSS) during pulsed laser and powder DED-LB. Independent variables including laser power, deposition speed, pulse frequency, and flow rate of the shielding gas were selected as controlling factors to deposit single tracks and plates of SDSS. Experiments have been designed and conducted according to L16 orthogonal array of Taguchi methodology. Relative density was estimated using Archimedes method. Ductility was estimated by tensile testing of the builds. For geometrical evaluation, phase characterization, and microstructural assessment, specimens were subjected to optical and Scanning Electron Microscopies, and Electron Backscattered Diffraction. Overall results were interpreted and explained using the Taguchi approach and analysis of signal-to-noise ratio. Single objective parameter-property relationships were achieved and discussed. Conclusive parametric remarks under the multi-attribute optimization were derived using weighted Grey Relational Analysis. A desirable parametric combination was extracted, and the associated quality responses were verified by the satisfying confirmatory deposition. The key role of parameters on the process stability, microstructure, and mechanical behaviour was further discussed. This work offers a practical solution to the multi-response optimization problems that can be used in AM and surface treatment of SDSS. Graphical Abstract
- Open Access
- 13 December 2024
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 136 (3-4) , 983-1008
Pulsed laser directed energy deposition of super duplex stainless steel: engineering microstructure and improving mechanical properties
Alloys developed by fusion-based additive manufacturing often suffer from the coarse columnar grain structure and their effect on properties. This work involves the practical application of pulsed laser in laser-based directed energy deposition (DED-LB) of super duplex stainless steel which led to engineering the microstructure, improving the mechanical properties, and changing the dominant texture. Pulsed laser DED-LB (here P-DED) with laser spot sizes of 1 and 2 mm and different frequencies were used. Refine-grained ferritic steels containing porosity were produced when using a small laser spot size. Ferrite-to-austenite (α → γ) transformation was constrained to the grain boundaries under the effect of small excitation overlaps. Using broader laser, higher energy input, and ultra-short pulse intervals encouraged γ nucleation, promoted the density, and decreased the content of undesirable oxides that are typically formed during the conventional DED-LB (here C-DED). The local ferritization under the fusion lines of C-DED was avoided by P-DED. Directionally solidified α, extending into several layers, was inhibited by P-DED with optimum overlap. Enhanced supercooling resulted in an in situ grain refinement and columnar-to-equiaxed morphological transition. Defect-free microstructure and effective distribution of interphase boundary surface by P-DED, with a laser spot size of 2 mm and ⁓99% excitation overlap, largely improved the toughness and elongation (with acceptable strength). Pulse-induced convection and isotropic heat flow during P-DED with smaller laser spot size subsided the trend of preferred orientation. However, an alignment of < 001 > α with deposition direction during P-DED with the broader laser preserved the typical {001} < 100 > solidification texture and, consequently, the transformation texture.
- 13 December 2024
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 136 (3-4) , 983-1008
Open AccessPulsed laser directed energy deposition of super duplex stainless steel: engineering microstructure and improving mechanical properties
Alloys developed by fusion-based additive manufacturing often suffer from the coarse columnar grain structure and their effect on properties. This work involves the practical application of pulsed laser in laser-based directed energy deposition (DED-LB) of super duplex stainless steel which led to engineering the microstructure, improving the mechanical properties, and changing the dominant texture. Pulsed laser DED-LB (here P-DED) with laser spot sizes of 1 and 2 mm and different frequencies were used. Refine-grained ferritic steels containing porosity were produced when using a small laser spot size. Ferrite-to-austenite (α → γ) transformation was constrained to the grain boundaries under the effect of small excitation overlaps. Using broader laser, higher energy input, and ultra-short pulse intervals encouraged γ nucleation, promoted the density, and decreased the content of undesirable oxides that are typically formed during the conventional DED-LB (here C-DED). The local ferritization under the fusion lines of C-DED was avoided by P-DED. Directionally solidified α, extending into several layers, was inhibited by P-DED with optimum overlap. Enhanced supercooling resulted in an in situ grain refinement and columnar-to-equiaxed morphological transition. Defect-free microstructure and effective distribution of interphase boundary surface by P-DED, with a laser spot size of 2 mm and ⁓99% excitation overlap, largely improved the toughness and elongation (with acceptable strength). Pulse-induced convection and isotropic heat flow during P-DED with smaller laser spot size subsided the trend of preferred orientation. However, an alignment of < 001 > α with deposition direction during P-DED with the broader laser preserved the typical {001} < 100 > solidification texture and, consequently, the transformation texture.
- Open Access
Optimizing Tensile Properties and Hardness of Inconel 718 by Cold Rolling
The as-received commercial Inconel 718 material was solid solution heat treated (ST), cold-rolled (CR), and precipitation-hardened (PH) to investigate the effects of deformation on the tensile properties, hardness, and texture. Three sets of specimens (0%, 20%, and 50% CR) were ST at 1100 °C/1 h, CR, and aged (720 °C/8 h + 650 °C/8 h) for the analysis. The ultimate tensile strength (UTS), 0.2% yield strength (YS), and elongation of 50% deformed condition were 1645 MPa, 1512 MPa, and 3.8%, respectively. The 20% deformation resulted in a balanced UTS (1348 MPa), YS (1202 MPa), and elongation (11%). The contribution of precipitation hardening to the strength decreased, while the contribution of CR increased with an increasing percentage of deformation. As the level of deformation increased, the size and quantity of γ″ decreased proportionally. The CR specimens produced a high density of nano/micro twins with twin planes oriented perpendicular to the RD-ND surface. The gradient of crystal orientation and internal features of large austenitic grains were generated by their preferred rotation. The cross-slip of screw dislocations induced a complete β-fiber consisting of {110}, {112}, and {123}, with doubled intensity at the higher deformation. Additionally, the specimens were highly susceptible to the twinning-induced orientation emerged by a predominant //ND. In the as-deformed condition, an incomplete but intense α-fiber, clustered between {110} and {110}, was characterized. Apart from achieving the highest strength, the current work demonstrates the effects of CR on the material strength without the complex influences of δ precipitates.
Open AccessOptimizing Tensile Properties and Hardness of Inconel 718 by Cold Rolling
The as-received commercial Inconel 718 material was solid solution heat treated (ST), cold-rolled (CR), and precipitation-hardened (PH) to investigate the effects of deformation on the tensile properties, hardness, and texture. Three sets of specimens (0%, 20%, and 50% CR) were ST at 1100 °C/1 h, CR, and aged (720 °C/8 h + 650 °C/8 h) for the analysis. The ultimate tensile strength (UTS), 0.2% yield strength (YS), and elongation of 50% deformed condition were 1645 MPa, 1512 MPa, and 3.8%, respectively. The 20% deformation resulted in a balanced UTS (1348 MPa), YS (1202 MPa), and elongation (11%). The contribution of precipitation hardening to the strength decreased, while the contribution of CR increased with an increasing percentage of deformation. As the level of deformation increased, the size and quantity of γ″ decreased proportionally. The CR specimens produced a high density of nano/micro twins with twin planes oriented perpendicular to the RD-ND surface. The gradient of crystal orientation and internal features of large austenitic grains were generated by their preferred rotation. The cross-slip of screw dislocations induced a complete β-fiber consisting of {110}, {112}, and {123}, with doubled intensity at the higher deformation. Additionally, the specimens were highly susceptible to the twinning-induced orientation emerged by a predominant //ND. In the as-deformed condition, an incomplete but intense α-fiber, clustered between {110} and {110}, was characterized. Apart from achieving the highest strength, the current work demonstrates the effects of CR on the material strength without the complex influences of δ precipitates.
- Open Access
- 7 March 2024
- Published by MDPI AG in Preprints.org
Optimizing Tensile Properties and Hardness of Inconel 718 by Cold Rolling
The as-received commercial Inconel 718 material was solid solution heat treated (ST), cold rolled (CR), and precipitation hardened (PH) to investigate the effects of deformation on tensile properties, hardness, and texture. Three sets of specimens (0%, 20% and 50% CR) were STed at 1100 C/1h, CR and aged (720 °C/8 h + 650 °C/8 h) for the analysis. Ultimate tensile strength (UTS), 0.2% yield strength (YS) and elongation of 50% deformed condition were 1645 MPa, 1512 MPa, and 3.8 %, respectively. The 20 % deformation resulted in a balanced UTS (1348 MPa), YS (1202 MPa) and elongation (11%). Contributions of precipitation hardening to the strength was decreasing, while contribution of CR increases with increasing percentage of deformation. Correspondingly, the size and quantities of decreased with increasing deformation level. In CR specimens, a high density of nano/micro twins were generated with the twin planes oriented perpendicular to the RD-ND surface. The preferred rotation of the crystals generated the gradient of orientation and internal features of the large austenitic grains. The cross-slip of screw dislocations induced a complete β-fibre, consisting of {110}, {112}, and{123}, with doubled intensity at higher deformation. In addition, the specimens tended to be highly susceptible to the twinning-induced orientation emerged by a predominant ⫽ND. An incomplete but intense α-fibre clustered between {110} and {110} was characterized in the as-deformed condition. Besides achieving highest strength, the current work demonstrates the effects of CR on the material strength without the complex influences of precipitate.
- 7 March 2024
- Published by MDPI AG in Preprints.org
Open AccessOptimizing Tensile Properties and Hardness of Inconel 718 by Cold Rolling
The as-received commercial Inconel 718 material was solid solution heat treated (ST), cold rolled (CR), and precipitation hardened (PH) to investigate the effects of deformation on tensile properties, hardness, and texture. Three sets of specimens (0%, 20% and 50% CR) were STed at 1100 C/1h, CR and aged (720 °C/8 h + 650 °C/8 h) for the analysis. Ultimate tensile strength (UTS), 0.2% yield strength (YS) and elongation of 50% deformed condition were 1645 MPa, 1512 MPa, and 3.8 %, respectively. The 20 % deformation resulted in a balanced UTS (1348 MPa), YS (1202 MPa) and elongation (11%). Contributions of precipitation hardening to the strength was decreasing, while contribution of CR increases with increasing percentage of deformation. Correspondingly, the size and quantities of decreased with increasing deformation level. In CR specimens, a high density of nano/micro twins were generated with the twin planes oriented perpendicular to the RD-ND surface. The preferred rotation of the crystals generated the gradient of orientation and internal features of the large austenitic grains. The cross-slip of screw dislocations induced a complete β-fibre, consisting of {110}, {112}, and{123}, with doubled intensity at higher deformation. In addition, the specimens tended to be highly susceptible to the twinning-induced orientation emerged by a predominant ⫽ND. An incomplete but intense α-fibre clustered between {110} and {110} was characterized in the as-deformed condition. Besides achieving highest strength, the current work demonstrates the effects of CR on the material strength without the complex influences of precipitate.
- 1 February 2024
- Published by Springer Nature
- p. 13-26
Microstructural Investigations on Super Duplex Stainless Steel UNS S32750 Fabricated by Blown-Powder Directed Laser Deposition
- 1 February 2024
- Published by Springer Nature
- p. 13-26
Microstructural Investigations on Super Duplex Stainless Steel UNS S32750 Fabricated by Blown-Powder Directed Laser Deposition
- 1 December 2020
- Published by Elsevier in Journal of Manufacturing Processes
- Vol. 60, 86-95
EBSD observations of microstructural features and mechanical assessment of INCOLOY 825 alloy/AISI 321 stainless steel dissimilar welds
- 1 December 2020
- Published by Elsevier in Journal of Manufacturing Processes
- Vol. 60, 86-95
EBSD observations of microstructural features and mechanical assessment of INCOLOY 825 alloy/AISI 321 stainless steel dissimilar welds
- 1 December 2018
- Published by Elsevier in Journal of Materials Processing Technology
- Vol. 262, 562-570
Arc weldability of Incoloy 825 to AISI 321 stainless steel welds
- 1 December 2018
- Published by Elsevier in Journal of Materials Processing Technology
- Vol. 262, 562-570
Arc weldability of Incoloy 825 to AISI 321 stainless steel welds
- 5 May 2017
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 6 (3) , 190-199
Influence of Microstructural Features on the Mechanical Behavior of Incoloy 825 Welds
- 5 May 2017
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 6 (3) , 190-199
Influence of Microstructural Features on the Mechanical Behavior of Incoloy 825 Welds