Xiaolei Xing
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Xiaolei Xing has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- Yefei Zhou
College of Mechanical Engineering, Yanshan University, Qinhuangdao, People’s Republic of China
3 shared publications Qingxiang Yang
State Key Laboratory of Metastable Materials Science & Technology, Yanshan University, Qinhuangdao, China
2 shared publications- Qingxiang Yang
State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao 066004, China
2 shared publications - Dong Yang Li
University of Alberta
1 shared publication G. K. Qin
Yanshan University
1 shared publication- Guangkuo Qin
College of Mechanical Engineering, Yanshan University, Qinhuangdao 066004, China
1 shared publication
Latest Publications
- Open Access
Effects of Ambient Oxygen Concentration on Microstructural Evolution and Mechanical Properties of Wire Arc Additively Manufactured Ti-6Al-4V Thin-Walled Components
Ti-6Al-4V thin-walled specimens were fabricated by gas tungsten arc welding-based wire arc additive manufacturing under controlled oxygen concentrations of 1, 500 and 1000 ppm, with ambient air used as a severe oxygen-exposure reference. The effects of oxygen concentration on oxygen uptake, microstructure, oxidation behavior and mechanical properties were investigated. Within the controlled range, the internal oxygen content increased from 0.07 to 0.15 wt.%, remaining below the ASTM B381-2013 limit. These specimens retained sound interlayer bonding and were mainly composed of α-Ti with a small amount of β-Ti, without detectable crystalline TiO2 by X-ray diffraction. Controlled oxygen uptake refined the α lamellae and increased deformation resistance through interstitial solid-solution strengthening, increasing hardness from approximately 320 HV to 330–350 HV and tensile strength from 880 to 940 MPa, while reducing elongation from 11.5% to 9.5%. In contrast, the ambient-air specimen reached an oxygen content of 0.36 wt.%, developed an approximately 90 μm oxidation-affected layer and showed TiO2-related oxides, α-colony aggregation and interface weakening. Its tensile strength and elongation decreased sharply to 295 MPa and 1.9%, respectively. These results indicate that atmosphere control in WAAM Ti-6Al-4V should prevent the transition from controlled oxygen strengthening to excessive oxygen-induced embrittlement.
Open AccessEffects of Ambient Oxygen Concentration on Microstructural Evolution and Mechanical Properties of Wire Arc Additively Manufactured Ti-6Al-4V Thin-Walled Components
Ti-6Al-4V thin-walled specimens were fabricated by gas tungsten arc welding-based wire arc additive manufacturing under controlled oxygen concentrations of 1, 500 and 1000 ppm, with ambient air used as a severe oxygen-exposure reference. The effects of oxygen concentration on oxygen uptake, microstructure, oxidation behavior and mechanical properties were investigated. Within the controlled range, the internal oxygen content increased from 0.07 to 0.15 wt.%, remaining below the ASTM B381-2013 limit. These specimens retained sound interlayer bonding and were mainly composed of α-Ti with a small amount of β-Ti, without detectable crystalline TiO2 by X-ray diffraction. Controlled oxygen uptake refined the α lamellae and increased deformation resistance through interstitial solid-solution strengthening, increasing hardness from approximately 320 HV to 330–350 HV and tensile strength from 880 to 940 MPa, while reducing elongation from 11.5% to 9.5%. In contrast, the ambient-air specimen reached an oxygen content of 0.36 wt.%, developed an approximately 90 μm oxidation-affected layer and showed TiO2-related oxides, α-colony aggregation and interface weakening. Its tensile strength and elongation decreased sharply to 295 MPa and 1.9%, respectively. These results indicate that atmosphere control in WAAM Ti-6Al-4V should prevent the transition from controlled oxygen strengthening to excessive oxygen-induced embrittlement.
- Open Access
- 13 March 2023
- Published by Tsinghua University Press in Friction
- Vol. 11 (9) , 1708-1723
Metastable hybridized structure transformation in amorphous carbon films during friction—A study combining experiments and MD simulation
Amorphous carbon films have attracted substantial interest due to their exceptional mechanical and tribological properties. Previous studies revealed that the amorphous carbon films exhibited lower coefficient of friction (COF) because of the transformation in bond structure from sp3-C to sp2-C during friction processes. However, the mechanism for such a transformation during friction is not well understood. This study is conducted to get an insight into the metastable transformation in amorphous carbon film during friction by means of experiments and molecular dynamics (MD) simulation. Relevant wear tests showed that wear of the film changed from an abrasive wear mode to a mixture of abrasion and adhesive wear, resulting in a decrease in growth rate of the wear rate after the running-in stage. It is worth noting that the sp3-C atoms were increased during the running-in stage when the films contained lower sp3/sp2 ratios. However, the formed sp3-C atoms could only be short-lived and gradually transformed to sp2-C atoms with the graphitization generated on the wearing surface of the films. The radial distribution function and translational order parameter indicated that the films’ high sp3/sp2 ratio led to an increased sp2-C proportion on the wear scar after friction, which caused an increased structural ordering.
- 13 March 2023
- Published by Tsinghua University Press in Friction
- Vol. 11 (9) , 1708-1723
Open AccessMetastable hybridized structure transformation in amorphous carbon films during friction—A study combining experiments and MD simulation
Amorphous carbon films have attracted substantial interest due to their exceptional mechanical and tribological properties. Previous studies revealed that the amorphous carbon films exhibited lower coefficient of friction (COF) because of the transformation in bond structure from sp3-C to sp2-C during friction processes. However, the mechanism for such a transformation during friction is not well understood. This study is conducted to get an insight into the metastable transformation in amorphous carbon film during friction by means of experiments and molecular dynamics (MD) simulation. Relevant wear tests showed that wear of the film changed from an abrasive wear mode to a mixture of abrasion and adhesive wear, resulting in a decrease in growth rate of the wear rate after the running-in stage. It is worth noting that the sp3-C atoms were increased during the running-in stage when the films contained lower sp3/sp2 ratios. However, the formed sp3-C atoms could only be short-lived and gradually transformed to sp2-C atoms with the graphitization generated on the wearing surface of the films. The radial distribution function and translational order parameter indicated that the films’ high sp3/sp2 ratio led to an increased sp2-C proportion on the wear scar after friction, which caused an increased structural ordering.
- 29 July 2021
- Published by International Union of Crystallography (IUCr) in Acta crystallographica Section B, Structural science, crystal engineering and materials
- Vol. 77 (4) , 649-661
First-principles investigation of V-doping effects on Fe3Cr4C3 carbide in hypereutectic Fe–Cr–C hardfacing coating
The mechanical property improvement of M 7C3 carbides in hypereutectic Fe–Cr–C hardfacing coating is required for its widespread application and longer service life. Vanadium is a frequently used alloying element, while the effects of V doping on the stability and tensile properties of M 7C3 carbide have been rarely reported. In this article, the formation enthalpy, structural stability, anisotropic tensile properties and electronic structure of V-doped M 7C3 (Fe3Cr4C3) carbide were calculated by the first-principles method. The mechanism by which the tensile property of Fe3Cr4C3 carbide can be improved by V-atom doping is discussed. The results show that the formation enthalpy (−0.24 eV/atom) of Fe3Cr3VC3 carbide is lower than that (0.48 eV/atom) of Fe3Cr4C3 carbide, which indicates that the formation of Fe3Cr3VC3 carbide is more facile. The absence of an imaginary frequency in the phonon dispersion spectra reveals that the Fe3Cr3VC3 carbide model is stable. Compared with Fe3Cr4C3 carbide, the tensile strength of Fe3Cr3VC3 carbide in the (0001) crystal face is increased from 44.42 to 48.46 GPa and that in the (1111) crystal face is also increased, from 28.99 to 34.19 GPa. The reasons that the tensile property of Fe3Cr4C3 can be improved by V doping are the electron redistribution and the formation of stronger bonds in Fe3Cr3VC3 carbide.
- 29 July 2021
- Published by International Union of Crystallography (IUCr) in Acta crystallographica Section B, Structural science, crystal engineering and materials
- Vol. 77 (4) , 649-661
First-principles investigation of V-doping effects on Fe3Cr4C3 carbide in hypereutectic Fe–Cr–C hardfacing coating
The mechanical property improvement of M 7C3 carbides in hypereutectic Fe–Cr–C hardfacing coating is required for its widespread application and longer service life. Vanadium is a frequently used alloying element, while the effects of V doping on the stability and tensile properties of M 7C3 carbide have been rarely reported. In this article, the formation enthalpy, structural stability, anisotropic tensile properties and electronic structure of V-doped M 7C3 (Fe3Cr4C3) carbide were calculated by the first-principles method. The mechanism by which the tensile property of Fe3Cr4C3 carbide can be improved by V-atom doping is discussed. The results show that the formation enthalpy (−0.24 eV/atom) of Fe3Cr3VC3 carbide is lower than that (0.48 eV/atom) of Fe3Cr4C3 carbide, which indicates that the formation of Fe3Cr3VC3 carbide is more facile. The absence of an imaginary frequency in the phonon dispersion spectra reveals that the Fe3Cr3VC3 carbide model is stable. Compared with Fe3Cr4C3 carbide, the tensile strength of Fe3Cr3VC3 carbide in the (0001) crystal face is increased from 44.42 to 48.46 GPa and that in the (1111) crystal face is also increased, from 28.99 to 34.19 GPa. The reasons that the tensile property of Fe3Cr4C3 can be improved by V doping are the electron redistribution and the formation of stronger bonds in Fe3Cr3VC3 carbide.
- Open Access
Effects of Polyurethane Substrate Pre-Treatment on Pulsed Cathodic Arc Deposited DLC Films
Diamond-like carbon (DLC) films were deposited by means of pulsed cathodic arc deposition on pretreated polyurethane (PU) rubber substrates. Tetrachloroethylene was chosen as a dissolution method to remove the plasticizer added in the PU substrates. Scanning electron microscopy (SEM) and Raman spectroscopy were applied to observe and characterize the surface morphologies and compositions of the deposited films, respectively. The tribological behaviours of uncoated and coated rubbers were investigated with ring-on-disc tribo experiments under dry sliding conditions. The coefficients of friction (COFs) of the coated rubbers were 40% lower than those of uncoated rubber and the COFs of different samples decreased first and then increased slightly with the increase in temperature and the time of ultrasonic treatment under dry friction. Based on the above experiments, ultrasonic treatment with tetrachloroethylene contributes to the increase in the wear resistance of DLC films deposited on PU rubbers. The most suitable temperature and time of ultrasonic treatment with tetrachloroethylene is 50 °C for 15 min.
Open AccessEffects of Polyurethane Substrate Pre-Treatment on Pulsed Cathodic Arc Deposited DLC Films
Diamond-like carbon (DLC) films were deposited by means of pulsed cathodic arc deposition on pretreated polyurethane (PU) rubber substrates. Tetrachloroethylene was chosen as a dissolution method to remove the plasticizer added in the PU substrates. Scanning electron microscopy (SEM) and Raman spectroscopy were applied to observe and characterize the surface morphologies and compositions of the deposited films, respectively. The tribological behaviours of uncoated and coated rubbers were investigated with ring-on-disc tribo experiments under dry sliding conditions. The coefficients of friction (COFs) of the coated rubbers were 40% lower than those of uncoated rubber and the COFs of different samples decreased first and then increased slightly with the increase in temperature and the time of ultrasonic treatment under dry friction. Based on the above experiments, ultrasonic treatment with tetrachloroethylene contributes to the increase in the wear resistance of DLC films deposited on PU rubbers. The most suitable temperature and time of ultrasonic treatment with tetrachloroethylene is 50 °C for 15 min.
- 26 July 2018
- Published by Springer Nature in Tribology Letters
- Vol. 66 (3) , 108
Dry Sliding Wear Behavior of (Cr, Fe)7C3-γ(Cr, Fe) Metal Matrix Composite (MMC) Coatings: The Influence of High Volume Fraction (Cr, Fe)7C3 Carbide
- 26 July 2018
- Published by Springer Nature in Tribology Letters
- Vol. 66 (3) , 108
Dry Sliding Wear Behavior of (Cr, Fe)7C3-γ(Cr, Fe) Metal Matrix Composite (MMC) Coatings: The Influence of High Volume Fraction (Cr, Fe)7C3 Carbide
- 1 May 2016
- Published by Elsevier in Materials Letters
- Vol. 171, 216-219
Stability of eutectic carbide in Fe-Cr-Mo-W-V-C alloy
- 1 May 2016
- Published by Elsevier in Materials Letters
- Vol. 171, 216-219
Stability of eutectic carbide in Fe-Cr-Mo-W-V-C alloy