George Abdel-Sayed
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
George Abdel-Sayed has a total of 2 co-authors. Here are the top co-authors by number of shared publications:
- Nataliya Hearn
Department of Civil and Environmental Engineering, Faculty of Engineering, University of Windsor, 401 Sunset Avenue, Windsor, ON N9B 3P4, Canada
4 shared publications - Safiuddin
Angelo DelZotto School of Construction Management, Centre for Construction and Engineering Technologies, George Brown College, 160 Kendal Avenue, Toronto, ON M5R 1M3, Canada
4 shared publications
Latest Publications
- Open Access
Flexural and Impact Behaviors of Mortar Composite Including Carbon Fibers
This study investigated the flexural and impact performances of mortar composite made with carbon fibers (MCCF). Four mortar composites (MCCF1, MCCF2, MCCF3, and MCCF4) were produced, using 1%, 2%, 3%, and 4% carbon fibers by volume, respectively. Another mortar composite without any carbon fibers (MCCF0) was prepared for its use as a control mix. The freshly mixed mortar composites were tested for inverted slump cone flow time to ensure they had an adequate workability to cast test specimens under vibration. In addition, all fresh mortar composites were examined for density and air content. The hardened mortar composites were tested for their first-crack flexural strength, ultimate flexural strength, first-crack impact resistance, and ultimate impact resistance. Moreover, the first-crack flexural toughness, ultimate flexural toughness, first-crack impact toughness, and ultimate impact toughness were determined for all hardened mortar composites. The correlations among the hardened properties of the mortar composites were also sought. Finally, the optimum fiber content was defined from the overall test results and considering the costs of the mortar composites. The test results showed that the workability and density of the fresh mortar composite decreased, whereas its air content increased due to the inclusion of carbon fibers. However, MCCF3 possessed the highest density and lowest air content among all MCCF mixes. It also had a higher workability than MCCF4. In the hardened state, the first-crack flexural strength and impact resistance, as well as the ultimate flexural strength and impact resistance of mortar composite, increased significantly with the increasing volume content of carbon fibers. In addition, the first-crack flexural toughness, ultimate flexural toughness, first-crack impact toughness, and ultimate impact toughness increased greatly with the higher volume content of carbon fibers. Strong correlations between the flexural strength and impact resistance, and between the flexural toughness and impact toughness of the mortar composites, were observed. Above all, excellent flexural strength, flexural toughness, impact resistance, and impact toughness values were observed for MCCF4 (4% carbon fibers). The 28-day ultimate flexural strength and impact resistance of MCCF4 increased by 4.6 MPa and 134 blows, respectively, as compared to MCCF0. Moreover, the 28-day ultimate flexural toughness and ultimate impact toughness values of MCCF4 were higher than that of MCCF0, by 3739.7 N-mm and 2703.3 J, respectively. However, MCCF3 (3% carbon fibers) also exhibited a good performance under flexural and impact loadings. Based on the costs of all mortar composites and their performances in both fresh and hardened states, MCCF3 was derived as the best mortar mix. This implies that 3% carbon fibers can be defined as the optimum fiber content in the context of the present study.
Open AccessFlexural and Impact Behaviors of Mortar Composite Including Carbon Fibers
This study investigated the flexural and impact performances of mortar composite made with carbon fibers (MCCF). Four mortar composites (MCCF1, MCCF2, MCCF3, and MCCF4) were produced, using 1%, 2%, 3%, and 4% carbon fibers by volume, respectively. Another mortar composite without any carbon fibers (MCCF0) was prepared for its use as a control mix. The freshly mixed mortar composites were tested for inverted slump cone flow time to ensure they had an adequate workability to cast test specimens under vibration. In addition, all fresh mortar composites were examined for density and air content. The hardened mortar composites were tested for their first-crack flexural strength, ultimate flexural strength, first-crack impact resistance, and ultimate impact resistance. Moreover, the first-crack flexural toughness, ultimate flexural toughness, first-crack impact toughness, and ultimate impact toughness were determined for all hardened mortar composites. The correlations among the hardened properties of the mortar composites were also sought. Finally, the optimum fiber content was defined from the overall test results and considering the costs of the mortar composites. The test results showed that the workability and density of the fresh mortar composite decreased, whereas its air content increased due to the inclusion of carbon fibers. However, MCCF3 possessed the highest density and lowest air content among all MCCF mixes. It also had a higher workability than MCCF4. In the hardened state, the first-crack flexural strength and impact resistance, as well as the ultimate flexural strength and impact resistance of mortar composite, increased significantly with the increasing volume content of carbon fibers. In addition, the first-crack flexural toughness, ultimate flexural toughness, first-crack impact toughness, and ultimate impact toughness increased greatly with the higher volume content of carbon fibers. Strong correlations between the flexural strength and impact resistance, and between the flexural toughness and impact toughness of the mortar composites, were observed. Above all, excellent flexural strength, flexural toughness, impact resistance, and impact toughness values were observed for MCCF4 (4% carbon fibers). The 28-day ultimate flexural strength and impact resistance of MCCF4 increased by 4.6 MPa and 134 blows, respectively, as compared to MCCF0. Moreover, the 28-day ultimate flexural toughness and ultimate impact toughness values of MCCF4 were higher than that of MCCF0, by 3739.7 N-mm and 2703.3 J, respectively. However, MCCF3 (3% carbon fibers) also exhibited a good performance under flexural and impact loadings. Based on the costs of all mortar composites and their performances in both fresh and hardened states, MCCF3 was derived as the best mortar mix. This implies that 3% carbon fibers can be defined as the optimum fiber content in the context of the present study.
- Open Access
Performance and Cost-Effectiveness of Short Pitch-Based Carbon Fiber Reinforced Mortar Composite
This paper discusses the performance of the short pitch-based carbon fiber reinforced mortar (CFRM) composite considering its key properties and cost-effectiveness. Five different types of mortar composite were produced using 0–4% volume contents of short pitch-based carbon fibers. The mortar composites were tested for inverted slump cone flow (flow time and volume flow), unit weight, air content, compressive strength, flexural strength, impact resistance, and water absorption. The cost-effectiveness of CFRM was assessed based on the performance to cost ratio (PCR), which was calculated for each mortar composite, considering its workability, mechanical properties, and durability. The inverted slump cone volume flow was counted as a measure of workability, whereas the compressive strength, flexural strength, and impact resistance were considered as the major attributes of the mechanical behavior. In addition, the water absorption was used as a measure of durability. The test results revealed that the mortar composite made with 3% carbon fibers provided adequate workability, a relatively high unit weight and low air content, the highest compressive strength, excellent flexural strength, good impact resistance, and the lowest water absorption. It was also found that the PCR increased up to 3% carbon fibers. Beyond a 3% fiber content, the PCR significantly decreased. The overall research findings revealed that the mortar with 3% carbon fibers was the optimum and most cost-effective mortar composite.
Open AccessPerformance and Cost-Effectiveness of Short Pitch-Based Carbon Fiber Reinforced Mortar Composite
This paper discusses the performance of the short pitch-based carbon fiber reinforced mortar (CFRM) composite considering its key properties and cost-effectiveness. Five different types of mortar composite were produced using 0–4% volume contents of short pitch-based carbon fibers. The mortar composites were tested for inverted slump cone flow (flow time and volume flow), unit weight, air content, compressive strength, flexural strength, impact resistance, and water absorption. The cost-effectiveness of CFRM was assessed based on the performance to cost ratio (PCR), which was calculated for each mortar composite, considering its workability, mechanical properties, and durability. The inverted slump cone volume flow was counted as a measure of workability, whereas the compressive strength, flexural strength, and impact resistance were considered as the major attributes of the mechanical behavior. In addition, the water absorption was used as a measure of durability. The test results revealed that the mortar composite made with 3% carbon fibers provided adequate workability, a relatively high unit weight and low air content, the highest compressive strength, excellent flexural strength, good impact resistance, and the lowest water absorption. It was also found that the PCR increased up to 3% carbon fibers. Beyond a 3% fiber content, the PCR significantly decreased. The overall research findings revealed that the mortar with 3% carbon fibers was the optimum and most cost-effective mortar composite.
- Open Access
Absorption and Strength Properties of Short Carbon Fiber Reinforced Mortar Composite
This paper presents the water absorption and strength properties of short carbon fiber reinforced mortar (CFRM) composite. Four CFRM composites with 1%, 2%, 3%, and 4% short pitch-based carbon fibers were produced in this study. Normal Portland cement mortar (NCPM) was also prepared for use as the control mortar. The freshly mixed mortar composites were tested for workability, wet density, and entrapped air content. In addition, the hardened mortar composites were examined for compressive strength, splitting tensile strength, flexural strength, and water absorption at the ages of 7 and 28 days. The effects of different carbon fiber contents on the tested properties were observed. Test results showed that the incorporation of carbon fibers decreased the workability and wet density, but increased the entrapped air content in mortar composite. Most interestingly, the compressive strength of CFRM composite increased up to 3% carbon fiber content and then it declined significantly for 4% fiber content, depending on the workability and compaction of the mortar. In contrast, the splitting tensile strength and flexural strength of the CFRM composite increased for all fiber contents due to the greater cracking resistance and improved bond strength of the carbon fibers in the mortar. The presence of short pitch-based carbon fibers significantly strengthened the mortar by bridging the microcracks, resisting the propagation of these minute cracks, and impeding the growth of macrocracks. Furthermore, the water absorption of CFRM composite decreased up to 3% carbon fiber content and then it increased substantially for 4% fiber content, depending on the entrapped air content of the mortar. The overall test results suggest that the mortar with 3% carbon fibers is the optimum CFRM composite based on the tested properties.
Open AccessAbsorption and Strength Properties of Short Carbon Fiber Reinforced Mortar Composite
This paper presents the water absorption and strength properties of short carbon fiber reinforced mortar (CFRM) composite. Four CFRM composites with 1%, 2%, 3%, and 4% short pitch-based carbon fibers were produced in this study. Normal Portland cement mortar (NCPM) was also prepared for use as the control mortar. The freshly mixed mortar composites were tested for workability, wet density, and entrapped air content. In addition, the hardened mortar composites were examined for compressive strength, splitting tensile strength, flexural strength, and water absorption at the ages of 7 and 28 days. The effects of different carbon fiber contents on the tested properties were observed. Test results showed that the incorporation of carbon fibers decreased the workability and wet density, but increased the entrapped air content in mortar composite. Most interestingly, the compressive strength of CFRM composite increased up to 3% carbon fiber content and then it declined significantly for 4% fiber content, depending on the workability and compaction of the mortar. In contrast, the splitting tensile strength and flexural strength of the CFRM composite increased for all fiber contents due to the greater cracking resistance and improved bond strength of the carbon fibers in the mortar. The presence of short pitch-based carbon fibers significantly strengthened the mortar by bridging the microcracks, resisting the propagation of these minute cracks, and impeding the growth of macrocracks. Furthermore, the water absorption of CFRM composite decreased up to 3% carbon fiber content and then it increased substantially for 4% fiber content, depending on the entrapped air content of the mortar. The overall test results suggest that the mortar with 3% carbon fibers is the optimum CFRM composite based on the tested properties.
- Open Access
Effects of Pitch-Based Short Carbon Fibers on the Workability, Unit Weight, and Air Content of Mortar Composite
Pitch is a viscoelastic polymer material consisting of aromatic hydrocarbons. It is used to produce carbon fibers with sheet-like crystal structures. The aim of the work presented in this paper was to evaluate the effects of pitch-based short carbon fibers on the workability, unit weight, and air content of freshly mixed mortar composite. Experimental investigation was carried out on five different types of mortar composite, including a control mortar. Four mortar composites were prepared including pitch-based short carbon fibers with 1–4% volume contents. The fresh mortar composites were tested to determine their slump, inverted slump cone flow (flow time, mass flow, and volume flow), unit weight, and air content. In addition, the correlation between the slump and flow time of various mortar composites was determined. It was found that the slump decreased with the increasing volume content of carbon fibers. The flow time of mortar composite increased, and therefore its mass flow and volume flow decreased with a greater volume content of carbon fibers. The slump was strongly correlated with the flow time, with a correlation coefficient of 0.9782. Furthermore, the unit weight of the fresh mortar composite decreased due to the incorporation of carbon fibers. However, amongst the different carbon fiber reinforced mortar composites, the mortar with 3% fiber volume content provided the highest unit weight. The air content results were consistent with the unit weight results. The change in air content of various mortar composites followed a trend reciprocal to that of unit weights. When the overall effects of carbon fibers were compared, it was observed that the fiber volume content higher than 3% resulted in a significantly low workability and provided a much lower unit weight with greater entrapped air content.
Open AccessEffects of Pitch-Based Short Carbon Fibers on the Workability, Unit Weight, and Air Content of Mortar Composite
Pitch is a viscoelastic polymer material consisting of aromatic hydrocarbons. It is used to produce carbon fibers with sheet-like crystal structures. The aim of the work presented in this paper was to evaluate the effects of pitch-based short carbon fibers on the workability, unit weight, and air content of freshly mixed mortar composite. Experimental investigation was carried out on five different types of mortar composite, including a control mortar. Four mortar composites were prepared including pitch-based short carbon fibers with 1–4% volume contents. The fresh mortar composites were tested to determine their slump, inverted slump cone flow (flow time, mass flow, and volume flow), unit weight, and air content. In addition, the correlation between the slump and flow time of various mortar composites was determined. It was found that the slump decreased with the increasing volume content of carbon fibers. The flow time of mortar composite increased, and therefore its mass flow and volume flow decreased with a greater volume content of carbon fibers. The slump was strongly correlated with the flow time, with a correlation coefficient of 0.9782. Furthermore, the unit weight of the fresh mortar composite decreased due to the incorporation of carbon fibers. However, amongst the different carbon fiber reinforced mortar composites, the mortar with 3% fiber volume content provided the highest unit weight. The air content results were consistent with the unit weight results. The change in air content of various mortar composites followed a trend reciprocal to that of unit weights. When the overall effects of carbon fibers were compared, it was observed that the fiber volume content higher than 3% resulted in a significantly low workability and provided a much lower unit weight with greater entrapped air content.