HWHeli Wan

Heli Wan

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Heli Wan has a total of 17 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Study on Al Evaporation during AlV55 Melting and Alloy Preparation

    by Bin Sun, Heli Wan, Baoqiang Xu, Xianjun Lei, Lanjie Li

    Vacuum induction melting is a commonly used method for preparing AlV55 alloys. However, this method results in high Al evaporation losses, leading to poor cost control. Moreover, the influence of the process parameters on the alloy composition remains unclear. In this study, the evaporation pattern of Al in the melting and preparation processes of AlV55 alloys is studied, and measures for controlling the system pressure are proposed to effectively reduce Al evaporation. The experimental results show that smelting under an Ar gas atmosphere of 2000 Pa can reduce the evaporation loss of Al from 11.48% under vacuum conditions (60 Pa) to 0.58% of the amount of raw material added, effectively improving the metal utilization rate and reducing production costs. The influence of various process parameters on the alloy composition and Al volatilization are investigated to enable the effective control of the compositional uniformity and impurity content of the resulting alloys. Under optimal conditions, the impurity contents of C, O, and N are 0.03%, 0.0073%, and 0.013%, respectively; this reduces the amount of Al lost by evaporation compared to conventional methods, and the alloy produced meets commercial standards.


  • Open Access

    Microstructure Evolution and Work Hardening Behavior of Hot-Rolled DP780 Ferrite/Bainite Dual-Phase Steel

    by Zhengtuan Li, Chunjing Wu, Heli Wan

    In this article, by optimizing the alloy composition, the DP780 grade hot-rolled duplex steel was obtained by TMCP (thermo-mechanical control process) combined with medium temperature coiling procedure. The microstructure evolution and mechanical properties of the experimental steel were analyzed by means of optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), room temperature tensile experiment, and low-temperature impact experiment. When the coiling temperature was 540°C, the yield strength, tensile strength, and elongation of the experimental steel were 663 MPa, 785 MPa, and 23%, respectively, and the product of the strength and elongation was as high as 18.1 GPa%, which accords with the mechanical properties of the national standard for DP780 dual-phase steel. The experimental steel exhibits significant work hardening effect at higher strain, and can still guarantee a certain work hardening index and good formability. When the coiling temperature was high (570°C), the strength of the experimental steel decreased and the work hardening effect was also weakened due to the coarsening of microstructure. The results of this article provide theoretical guidance for the production of DP780 dual-phase steel by hot rolling.


  • Open Access

    Study on the Behavior Mechanism of K and Na during the Synthesis of VN Alloy

    by Lanjie Li, Xindong Wang, Caidong Zhang, Mingliang Lu, Haixu Wang, Heli Wan

    In this paper, the sources of K and Na in vanadium-nitrogen (VN) alloys and their effects on the furnace structure were studied. The results show that K and Na are mainly present as counter-ions of decavanadate and dodecanadate in ammonium polyvanadate (APV) and vanadium trioxide (V2O3). In the production process of VN, the concentration of K in the scab produced in the kiln is 25 times higher than that of the vanadium raw material, the concentration of Na is 15 times higher than that of the raw material, and the degree of enrichment of K is stronger than that of Na. Additionally, in the VN products, K and Na are mainly distributed uniformly in the form of KCN and NaCN. The results also found that the K and Na vapors during the production of VN promoted the formation of VN. However, K, Na steam, KCN, NaCN, K2CO3, Na2CO3 and other potassium-sodium high-temperature corrosive substances cause strong corrosion of the furnace lining, graphite sagger, push plate, and heating elements. Therefore, in the process of synthesizing VN, the raw materials of K and Na content of impurity elements must be reasonably controlled. The results not only analyzed the source of K and Na, but also analyzed the characteristics of their enrichment and the influence on the equipment.

  • Open Access

    A Novel Method of Fabricating Al-V Intermetallic Alloy through Electrode Heating

    by Heli Wan, Baoqiang Xu, Lanjie Li, Bin Yang, Dongming Li, Yongnian Dai

    A novel method was developed to produce AlV55 alloy through reducing impurities content and component segregation with electrode assisted heating technology. This new process synergistically integrates a few low-cost process techniques, including granulation, mixing, and electro-heating to produce AlV55 alloy. During the heating process, the CaO is used as an additive in the raw materials. The uniform of AlV55 alloy composition and low impurities content are effectively controlled by this process. The analysis results show that Si (0.13 wt%), Fe (0.22 wt%), N (0.007 wt%), C (0.078 wt%), and O (0.051 wt%) impurities in the AlV55 products were reduced, which met the commercial standard (TS/T 579-2014), and V content ranged from 57.5 to 58.5 wt% when the Al/V2O5 mass ratio was 0.94:1. This method can realize the controllability of the reaction process and is suitable for large-scale industrial production.


  • Open Access

    Effect of CaCl2 on Microstructure of Calciothermic Reduction Products of Ti2O3 to Prepare Porous Titanium

    by Guobo Yang, Baoqiang Xu, Heli Wan, Fengkang Wang, Bin Yang, Zhijun Wang

    The compound CaCl2 plays a significant role in the process of direct calciothermic reduction of Ti2O3 to prepare porous titanium. In this paper, the effect of CaCl2 on reduction products by calciothermic reduction of Ti2O3 was investigated. Results show that the distribution of CaCl2 in reduction preform influences particle size and morphology differences in reduction products both on the surface and the inside. The CaCl2 is transferred to the surface of the Ti2O3 preform due to its volatilization before and throughout reduction. The content of CaCl2 in the surface zone of Ti2O3 preform is significantly higher than that in the interior during the reduction process, contributing to the formation of large Ti particles with a smooth shape on the surface, and small Ti particles with inherited morphology of Ti2O3 inside. More CaCl2 causes the aggregation of Ti particles to form large Ti particles which are advantageous as they connect and form a more solid porous titanium structure. The presence of a small amount of CaCl2 in the interior also results in the coexistence of small Ti and CaO particles, forming a loose structure with uniform distribution.