Yutao Zhou
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yutao Zhou has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Anping Dong
Shanghai Jiao Tong University
1 shared publication - Jingshe Li
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Shufeng Yang
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing, P.R. China
1 shared publication - Wei Liu
School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication
Latest Publications
- Open Access
Effects of Heat-Treatment Temperature on the Microstructure and Mechanical Properties of Steel by MgO Nanoparticle Additions
The characteristics and formation mechanisms of intragranular acicular ferrite (IAF) in steel with MgO nanoparticle additions were systematically investigated for different isothermal heat-treatment temperatures, and its influence on mechanical properties was also clarified. The results indicate that the inclusions were finely dispersed and refined after adding MgO nanoparticles. In addition, with decreasing heat-treatment temperature, the microstructure changed from grain boundary ferrite (GBF) and polygonal ferrite (PF) to intragranular acicular ferrite. Moreover, the steel with MgO additions had excellent mechanical properties in the temperature range of 973 to 823 K and an average Charpy absorbed energies value of around 174 J at 873 K due to the significant refinement of the microstructure and nucleation of intragranular acicular ferrite.
Open AccessEffects of Heat-Treatment Temperature on the Microstructure and Mechanical Properties of Steel by MgO Nanoparticle Additions
The characteristics and formation mechanisms of intragranular acicular ferrite (IAF) in steel with MgO nanoparticle additions were systematically investigated for different isothermal heat-treatment temperatures, and its influence on mechanical properties was also clarified. The results indicate that the inclusions were finely dispersed and refined after adding MgO nanoparticles. In addition, with decreasing heat-treatment temperature, the microstructure changed from grain boundary ferrite (GBF) and polygonal ferrite (PF) to intragranular acicular ferrite. Moreover, the steel with MgO additions had excellent mechanical properties in the temperature range of 973 to 823 K and an average Charpy absorbed energies value of around 174 J at 873 K due to the significant refinement of the microstructure and nucleation of intragranular acicular ferrite.