Fangfang Ge
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Fangfang Ge has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Bingsheng Li
State Key Laboratory for Environment-friendly Energy Materials, Southwest University of Science and Technology, Mianyang 621010, China
3 shared publications Fanping Meng
Ningbo Key Laboratory of Special Energy Materials and Chemistry Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications Ningbo Institute of Materials Technology and Engineering Chinese Academy of Sciences 315201 Ningbo China
2 shared publicationsFeng Huang
Engineering Laboratory of Advanced Energy Materials, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, China
2 shared publicationsRenda Wang
Ningbo Key Laboratory of Special Energy Materials and Chemistry Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications Ningbo Institute of Materials Technology and Engineering Chinese Academy of Sciences 315201 Ningbo China
2 shared publicationsChen Ke
1 shared publicationChunfan Liu
1 shared publication
Latest Publications
- Open Access
Cross-sectional helium irradiation reveals interface-controlled bubble evolution in Cr/CrAlSiN multilayer coatings on zirconium alloys
The irradiation stability of Cr based protective coatings on zirconium alloys is critical for the development of accident-tolerant fuel claddings. However, conventional surface irradiation often produces shallow, nonuniform damage, obscuring interfacial behavior. In this study, we perform cross-sectional He irradiation to directly examine the interfacial response and He bubble evolution across Cr monolayer and Cr and CrAlSiN multilayer coatings on Zr substrates. Irradiation was carried out at 500 C and 750 C to doses of 2 and 3 dpa, enabling a direct comparison of temperature-dependent microstructural evolution. In the Cr monolayer, He implantation produced a homogeneous distribution of nanoscale bubbles throughout the damaged region and large cavities at the Cr and Zr interface, indicating severe Kirkendall-type voiding and interfacial decohesion at elevated temperature. In contrast, the Cr/CrAlSiN multilayer exhibited a periodically modulated bubble distribution, with bubble fragmentation and transformation into nanoscale platelets at CrAlSiN interfaces. A N-enriched Zr(N) interlayer formed spontaneously at the CrAlSiN and Zr interface, effectively suppressing bubble accumulation and interdiffusion. The nanochannel interfaces acted as He sinks and diffusion barriers, enhancing interfacial bonding and mitigating swelling. This work demonstrates that cross-sectional ion irradiation is a powerful approach for probing interfacial stability in multilayer systems, offering new insights into He-defect interactions and radiation tolerance engineering at buried interfaces. The findings highlight the potential of Cr and CrAlSiN multilayers as advanced coating architectures for high-temperature nuclear environments.
Open AccessCross-sectional helium irradiation reveals interface-controlled bubble evolution in Cr/CrAlSiN multilayer coatings on zirconium alloys
The irradiation stability of Cr based protective coatings on zirconium alloys is critical for the development of accident-tolerant fuel claddings. However, conventional surface irradiation often produces shallow, nonuniform damage, obscuring interfacial behavior. In this study, we perform cross-sectional He irradiation to directly examine the interfacial response and He bubble evolution across Cr monolayer and Cr and CrAlSiN multilayer coatings on Zr substrates. Irradiation was carried out at 500 C and 750 C to doses of 2 and 3 dpa, enabling a direct comparison of temperature-dependent microstructural evolution. In the Cr monolayer, He implantation produced a homogeneous distribution of nanoscale bubbles throughout the damaged region and large cavities at the Cr and Zr interface, indicating severe Kirkendall-type voiding and interfacial decohesion at elevated temperature. In contrast, the Cr/CrAlSiN multilayer exhibited a periodically modulated bubble distribution, with bubble fragmentation and transformation into nanoscale platelets at CrAlSiN interfaces. A N-enriched Zr(N) interlayer formed spontaneously at the CrAlSiN and Zr interface, effectively suppressing bubble accumulation and interdiffusion. The nanochannel interfaces acted as He sinks and diffusion barriers, enhancing interfacial bonding and mitigating swelling. This work demonstrates that cross-sectional ion irradiation is a powerful approach for probing interfacial stability in multilayer systems, offering new insights into He-defect interactions and radiation tolerance engineering at buried interfaces. The findings highlight the potential of Cr and CrAlSiN multilayers as advanced coating architectures for high-temperature nuclear environments.
- 1 January 2026
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 41 (6) , 775
Research Progress on Lead-bismuth Eutectic Corrosion Resistant Coatings
- 1 January 2026
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 41 (6) , 775
Research Progress on Lead-bismuth Eutectic Corrosion Resistant Coatings
- Open Access
Ultra-High Spectral Contrast Nanobeam Photonic Crystal Cavity on Bending Waveguide
In this article, one-dimensional photonic crystal cavities on bending waveguides (PCCoBW) used for achieving high-contrast spectra are proposed, analyzed, and experimentally verified on silicon on insulator (SOI). Both air and dielectric modes of the PCCoBW calculated by the finite-difference time-domain (FDTD) method show finger-ring-like mode profiles with the achievement of high-quality factors (Q∼106), even when the bending radius is less than 50 times the lattice constant. Straight waveguides side-coupled to the cavity are used to access and measure mode resonances. The measured spectra show a high extinction ratio over 40 dB for dielectric modes and 20 dB for air modes, respectively. Both dielectric and air resonant modes are revealed with Q-factors over 3.3 × 104 and 7.9 × 104, respectively, for the coupled PCCoBWs. The proposed PCCoBW could be implemented as high-contrast notch filtering and would benefit a broad range of applications such as optical filters, modulators, sensors, or switches.
Open AccessUltra-High Spectral Contrast Nanobeam Photonic Crystal Cavity on Bending Waveguide
In this article, one-dimensional photonic crystal cavities on bending waveguides (PCCoBW) used for achieving high-contrast spectra are proposed, analyzed, and experimentally verified on silicon on insulator (SOI). Both air and dielectric modes of the PCCoBW calculated by the finite-difference time-domain (FDTD) method show finger-ring-like mode profiles with the achievement of high-quality factors (Q∼106), even when the bending radius is less than 50 times the lattice constant. Straight waveguides side-coupled to the cavity are used to access and measure mode resonances. The measured spectra show a high extinction ratio over 40 dB for dielectric modes and 20 dB for air modes, respectively. Both dielectric and air resonant modes are revealed with Q-factors over 3.3 × 104 and 7.9 × 104, respectively, for the coupled PCCoBWs. The proposed PCCoBW could be implemented as high-contrast notch filtering and would benefit a broad range of applications such as optical filters, modulators, sensors, or switches.
- 13 January 2022
- Published by Wiley in Materials and Corrosion
- Vol. 73 (5) , 784-797
Investigation into creep‐to‐rupture of SIMP steel in stagnant LBE at 300–450°C
Ferritic/martensitic steel was chosen as a primary candidate structural material for China Initiative Accelerator Driven System (CiADS) which started in 2015. A new kind of tempered martensitic steel, Steel of Institute of Modern Physics (SIMP), was designed to meet the requirements of the special operating environment. Structural materials suffer from liquid Pb‐Bi corrosion and liquid metal wetting at 450°C. Liquid metal wetting can seriously affect the mechanical properties of structural materials due to the decrease in surface energy and transition from martensitic laths to ferritic grains. Creep‐to‐rupture of SIMP steel was explored in stagnant liquid Pb‐Bi eutectic at 450°C. The possible reasons for creep‐to‐rupture are discussed. The results of the present study provide a new insight into challenges related to the application of SIMP steel in CiADS.
- 13 January 2022
- Published by Wiley in Materials and Corrosion
- Vol. 73 (5) , 784-797
Investigation into creep‐to‐rupture of SIMP steel in stagnant LBE at 300–450°C
Ferritic/martensitic steel was chosen as a primary candidate structural material for China Initiative Accelerator Driven System (CiADS) which started in 2015. A new kind of tempered martensitic steel, Steel of Institute of Modern Physics (SIMP), was designed to meet the requirements of the special operating environment. Structural materials suffer from liquid Pb‐Bi corrosion and liquid metal wetting at 450°C. Liquid metal wetting can seriously affect the mechanical properties of structural materials due to the decrease in surface energy and transition from martensitic laths to ferritic grains. Creep‐to‐rupture of SIMP steel was explored in stagnant liquid Pb‐Bi eutectic at 450°C. The possible reasons for creep‐to‐rupture are discussed. The results of the present study provide a new insight into challenges related to the application of SIMP steel in CiADS.
- Open Access
Lattice Defects and Exfoliation Efficiency of 6H-SiC via H2+ Implantation at Elevated Temperature
Silicon carbide (SiC) is an important material used in semiconductor industries and nuclear power plants. SiC wafer implanted with H ions can be cleaved inside the damaged layer after annealing, in order to facilitate the transfer of a thin SiC slice to a handling wafer. This process is known as “ion-cut” or “Smart-Cut”. It is worth investigating the exfoliation efficiency and residual lattice defects in H-implanted SiC before and after annealing. In the present paper, lattice damage in the 6H-SiC implanted by H2+ to a fluence of 5 × 1016 H2+/cm2 at 450 and 900 °C was investigated by a combination of Raman spectroscopy and transmission electron microscopy. Different levels of damage caused by dynamic annealing were observed by Raman spectroscopy and transmission electron microscopy in the as-implanted sample. Atomic force microscopy and scanning white-light interferometry were used to observe the sample surface morphology. Surface blisters and exfoliations were observed in the sample implanted at 450 °C and then annealed at 1100 °C for 15 min, whereas surface blisters and exfoliation occurred in the sample implanted at 900 °C without further thermal treatment. This finding can be attributed to the increase in the internal pressure of platelets during high temperature implantation. The exfoliation efficiency, location, and roughness after exfoliation were investigated and possible reasons were discussed. This work provides a basis for further understanding and improving the high-efficiency “ion-cut” technology.
Open AccessLattice Defects and Exfoliation Efficiency of 6H-SiC via H2+ Implantation at Elevated Temperature
Silicon carbide (SiC) is an important material used in semiconductor industries and nuclear power plants. SiC wafer implanted with H ions can be cleaved inside the damaged layer after annealing, in order to facilitate the transfer of a thin SiC slice to a handling wafer. This process is known as “ion-cut” or “Smart-Cut”. It is worth investigating the exfoliation efficiency and residual lattice defects in H-implanted SiC before and after annealing. In the present paper, lattice damage in the 6H-SiC implanted by H2+ to a fluence of 5 × 1016 H2+/cm2 at 450 and 900 °C was investigated by a combination of Raman spectroscopy and transmission electron microscopy. Different levels of damage caused by dynamic annealing were observed by Raman spectroscopy and transmission electron microscopy in the as-implanted sample. Atomic force microscopy and scanning white-light interferometry were used to observe the sample surface morphology. Surface blisters and exfoliations were observed in the sample implanted at 450 °C and then annealed at 1100 °C for 15 min, whereas surface blisters and exfoliation occurred in the sample implanted at 900 °C without further thermal treatment. This finding can be attributed to the increase in the internal pressure of platelets during high temperature implantation. The exfoliation efficiency, location, and roughness after exfoliation were investigated and possible reasons were discussed. This work provides a basis for further understanding and improving the high-efficiency “ion-cut” technology.
- 15 October 2019
- Published by Springer Nature in JOM
- Vol. 71 (12) , 4839-4847
Effect of Cr/Al Atomic Ratio on the Oxidation Resistance in 1200°C Steam for the CrAlSiN Coatings Deposited on Zr Alloy Substrates
- 15 October 2019
- Published by Springer Nature in JOM
- Vol. 71 (12) , 4839-4847
Effect of Cr/Al Atomic Ratio on the Oxidation Resistance in 1200°C Steam for the CrAlSiN Coatings Deposited on Zr Alloy Substrates
- 1 September 2017
- Published by Elsevier in Surface and Coatings Technology
- Vol. 324, 429-437
Age hardening of a magnetron sputtered V-Al-Si-N quaternary coating
- 1 September 2017
- Published by Elsevier in Surface and Coatings Technology
- Vol. 324, 429-437
Age hardening of a magnetron sputtered V-Al-Si-N quaternary coating