Yu Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yu Liu has a total of 76 co-authors. Here are the top co-authors by number of shared publications:
- Guangqiang Li
Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan, China
25 shared publications Cheng Yuan
8 shared publicationsXijie Wang
8 shared publicationsGuangqiang Li
The State Key Laboratory of Refractories and Metallurgy Wuhan University of Science and Technology Wuhan Hubei 430081 China
7 shared publicationsPengzhao Zhang
7 shared publicationsYufeng Tian
Hubei Provincial Key Laboratory for New Processes of Ironmaking and Steelmaking, Wuhan University of Science and Technology, Wuhan, People’s Republic of China
5 shared publications
Latest Publications
- 15 June 2026
- Published by Springer Nature in Journal of Iron and Steel Research International
- Vol. 33 (7) , 208
Preparation of phosphorous-rich iron via hydrogen reduction–melting separation of high-phosphorus oolitic hematite
- 15 June 2026
- Published by Springer Nature in Journal of Iron and Steel Research International
- Vol. 33 (7) , 208
Preparation of phosphorous-rich iron via hydrogen reduction–melting separation of high-phosphorus oolitic hematite
- 12 May 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (7) , 3879-3894
Deep Iron-Phosphorus Separation in Hydrogen Reduction-Melting of High-phosphorus Oolitic Hematite
- 12 May 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (7) , 3879-3894
Deep Iron-Phosphorus Separation in Hydrogen Reduction-Melting of High-phosphorus Oolitic Hematite
- 10 October 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (28) , 59291-59296
Dissolution behavior of MgO in CaF2-CaO-Al2O3-La2O3 slag
- 10 October 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (28) , 59291-59296
Dissolution behavior of MgO in CaF2-CaO-Al2O3-La2O3 slag
- 15 July 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (25) , 44317-44325
Dissolution behavior of Al2O3 in CaF2-CaO-Al2O3-La2O3 slag and interface characteristics
- 15 July 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (25) , 44317-44325
Dissolution behavior of Al2O3 in CaF2-CaO-Al2O3-La2O3 slag and interface characteristics
- 15 March 2025
- Published by Springer Nature in Journal of Iron and Steel Research International
- Vol. 32 (9) , 3089-3095
Rapid lime dissolution for efficient dephosphorization by self-disintegrating effect of core–shell structured lime in converter slag
- 15 March 2025
- Published by Springer Nature in Journal of Iron and Steel Research International
- Vol. 32 (9) , 3089-3095
Rapid lime dissolution for efficient dephosphorization by self-disintegrating effect of core–shell structured lime in converter slag
- 24 November 2024
- Published by Wiley in Steel Research International
- Vol. 96 (6)
Oxidation Kinetics and Oxide Scale Characteristics of Ni‐Containing Steel at High Temperature under Air
Oxidation kinetics and oxide scale characteristics of two steels with 7.5 wt% Ni (7.5Ni) and 8.4 wt% Ni (8.4Ni) are investigated in temperature range of 1100–1250 °C by the thermogravimetric analysis, scanning electron microscope, and X‐ray diffraction. In the results, it is shown that oxidation kinetics for both steels obey the parabolic rate law, and oxidation activation energy of 8.4Ni steel is slightly larger than 7.5Ni steel. Thickness of outer oxide scale has an important effect on thickness of inner scale. The inner oxide scale is entangled with the steel matrix, and consists of Ni metal and its surrounding Fe oxide. Compared with 7.5Ni steel, the thicker inner oxide scale of 8.4Ni steel implies that the severer internal oxidation occurs in the 8.4Ni steel than 7.5Ni steel when the temperature exceeds 1200 °C. The decreases in Ni content and heat‐treatment temperature contribute to alleviating surface quality defects of Ni‐containing steel caused by surface oxidation.
- 24 November 2024
- Published by Wiley in Steel Research International
- Vol. 96 (6)
Oxidation Kinetics and Oxide Scale Characteristics of Ni‐Containing Steel at High Temperature under Air
Oxidation kinetics and oxide scale characteristics of two steels with 7.5 wt% Ni (7.5Ni) and 8.4 wt% Ni (8.4Ni) are investigated in temperature range of 1100–1250 °C by the thermogravimetric analysis, scanning electron microscope, and X‐ray diffraction. In the results, it is shown that oxidation kinetics for both steels obey the parabolic rate law, and oxidation activation energy of 8.4Ni steel is slightly larger than 7.5Ni steel. Thickness of outer oxide scale has an important effect on thickness of inner scale. The inner oxide scale is entangled with the steel matrix, and consists of Ni metal and its surrounding Fe oxide. Compared with 7.5Ni steel, the thicker inner oxide scale of 8.4Ni steel implies that the severer internal oxidation occurs in the 8.4Ni steel than 7.5Ni steel when the temperature exceeds 1200 °C. The decreases in Ni content and heat‐treatment temperature contribute to alleviating surface quality defects of Ni‐containing steel caused by surface oxidation.
- Open Access
- 4 November 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 33, 6756-6766
Dephosphorization study on hydrogen reduction-melting separation of high-phosphorus oolitic hematite
- 4 November 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 33, 6756-6766
Open AccessDephosphorization study on hydrogen reduction-melting separation of high-phosphorus oolitic hematite
- 21 October 2024
- Published by SAGE Publications in Ironmaking & Steelmaking: Processes, Products and Applications
- Vol. 53 (4) , 757-765
Comparative study on the cleanliness and compositional change of alloy steels processed by electroslag remelting and vacuum arc remelting
The cleanliness and compositional change of Ni containing alloy steel processed by electroslag remelting (ESR) and vacuum arc remelting (VAR) were studied. The results show that compared with the electrode steel, the total oxygen content increases in the steel processed by ESR. On the contrary, the total oxygen and total nitrogen content in the steel processed by VAR can be significantly decreased due to the vacuum environment. The number and size of inclusions in steel processed by VAR are significantly decreased, which indicates that the VAR is conducive to improving the cleanliness of steel. Single TiN inclusions are found in both steels processed by ESR and VAR, and oxide inclusions in two steels are (Mg,Al,Ca)O and (Mg,Al)O, respectively. The growth time of TiN inclusions is relatively shorter in the steel processed by VAR, which leads to the thinner TiN layer surrounding the oxide inclusions. During the VAR process, the high temperature and high vacuum conditions promote the volatilization of Mn in steel, leading to decrease of the Mn content in steel. Therefore, extra Mn should be added to the electrode steel before VAR.
- 21 October 2024
- Published by SAGE Publications in Ironmaking & Steelmaking: Processes, Products and Applications
- Vol. 53 (4) , 757-765
Comparative study on the cleanliness and compositional change of alloy steels processed by electroslag remelting and vacuum arc remelting
The cleanliness and compositional change of Ni containing alloy steel processed by electroslag remelting (ESR) and vacuum arc remelting (VAR) were studied. The results show that compared with the electrode steel, the total oxygen content increases in the steel processed by ESR. On the contrary, the total oxygen and total nitrogen content in the steel processed by VAR can be significantly decreased due to the vacuum environment. The number and size of inclusions in steel processed by VAR are significantly decreased, which indicates that the VAR is conducive to improving the cleanliness of steel. Single TiN inclusions are found in both steels processed by ESR and VAR, and oxide inclusions in two steels are (Mg,Al,Ca)O and (Mg,Al)O, respectively. The growth time of TiN inclusions is relatively shorter in the steel processed by VAR, which leads to the thinner TiN layer surrounding the oxide inclusions. During the VAR process, the high temperature and high vacuum conditions promote the volatilization of Mn in steel, leading to decrease of the Mn content in steel. Therefore, extra Mn should be added to the electrode steel before VAR.
- 12 September 2024
- Published by Wiley in Steel Research International
- Vol. 96 (1)
Industrial Trials on the Cleanliness Improvement, Microstructure Refinement and Performance Enhancement of Rare‐Earth‐Treated 75Cr1 Steel
The effects of rare‐earth treatment on cleanliness, corrosion resistance, microstructure, and mechanical properties of 75Cr1 steel are investigated by industrial trial. In the results, it is shown that the appropriate La–Ce addition can effectively remove oxygen and sulfur elements in steel, and total oxygen (T.O) and S contents decrease by 45% and 33%, respectively. After La–Ce treatment, the typical inclusions in steel are transformed from (Mg–Al–O)–CaS composite inclusions to RExSy–CaS inclusion with a small amount of Al2O3. The number and average size of inclusions in steel are significantly reduced, and the morphology of inclusions changes from irregular shape to spherical shape, which contributes to the improvement of the corrosion resistance of 75Cr1 steel. Furthermore, the pearlite spacing and the grain size are refined, the tensile and yield strengths are significantly enhanced in the test of La–Ce‐treated steel. The 75Cr1 steels are fabricated in small batches, which avoids the nozzle clogging resulted by rare‐earth treatment during continuous casting. It implies that rare‐earth treatment to improve the quality of 75Cr1 steel shows the strong industrial applicability.
- 12 September 2024
- Published by Wiley in Steel Research International
- Vol. 96 (1)
Industrial Trials on the Cleanliness Improvement, Microstructure Refinement and Performance Enhancement of Rare‐Earth‐Treated 75Cr1 Steel
The effects of rare‐earth treatment on cleanliness, corrosion resistance, microstructure, and mechanical properties of 75Cr1 steel are investigated by industrial trial. In the results, it is shown that the appropriate La–Ce addition can effectively remove oxygen and sulfur elements in steel, and total oxygen (T.O) and S contents decrease by 45% and 33%, respectively. After La–Ce treatment, the typical inclusions in steel are transformed from (Mg–Al–O)–CaS composite inclusions to RExSy–CaS inclusion with a small amount of Al2O3. The number and average size of inclusions in steel are significantly reduced, and the morphology of inclusions changes from irregular shape to spherical shape, which contributes to the improvement of the corrosion resistance of 75Cr1 steel. Furthermore, the pearlite spacing and the grain size are refined, the tensile and yield strengths are significantly enhanced in the test of La–Ce‐treated steel. The 75Cr1 steels are fabricated in small batches, which avoids the nozzle clogging resulted by rare‐earth treatment during continuous casting. It implies that rare‐earth treatment to improve the quality of 75Cr1 steel shows the strong industrial applicability.