Onkar Nath Srivastava
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Onkar Nath Srivastava has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Radhey Shyam Tiwari
Department of Physics, Institute of Science, Banaras Hindu University, Varanasi 221005,India
2 shared publications - Nilay Krishna Mukhopadhyay
Department of Metallurgical Engineering, Indian Institute of Technology (BHU) Varanasi, Varanasi, India
1 shared publication - Rajesh Kumar
Institute of Materials Science Technical University of Darmstadt Darmstadt Germany
1 shared publication - Ram Manohar Yadav
Department of Physics, University of Allahabad, Prayagraj, 211002, U. P., India
1 shared publication
Latest Publications
- 1 January 2016
- Published by Walter de Gruyter GmbH
Synthesis of nanocrystalline spinel phase by mechanical milling of Al–Cu–Fe and Al–Cu–Cr–Fe quasicrystalline alloys
In the present study, a low-temperature synthesis of (Cu,Fe)Al2O4 and (Cu,Cr,Fe)Al2O4 spinels from the quasicrystalline phases was investigated with the variation of process parameters during milling and annealing. The milling of the quasicrystalline materials was carried out in an attritor mill at 400 rpm for 40 hours with ball to powder ratio of 40 : 1 in hexane medium. Subsequently, annealing was performed in an air ambience for 10, 20, and 40 h at 400, 500, 600 and 700°C inside a furnace in order to oxidize the mechanically milled quasicrystalline phase for the possible formation of the spinel phase. It was found that after annealing at higher temperatures (∼500°C), mechanically milled quasicrystalline alloy transformed to a spinel phase whereas annealing at lower temperatures (<500°C) led to the formation of B2 phase as a major one along withminor amount of oxide phase. The X-ray diffraction and transmission electron microscopy of the annealed samples confirmed the formation of the spinel phase with an average grain size of ∼20–40 nm. It is interesting to note that the nanospinel phases showed the different colors during various annealing time and temperature. The optical properties of nanospinel materials, investigated employing UV visible spectrometer exhibited absorption characteristics.
- 1 January 2016
- Published by Walter de Gruyter GmbH
Synthesis of nanocrystalline spinel phase by mechanical milling of Al–Cu–Fe and Al–Cu–Cr–Fe quasicrystalline alloys
In the present study, a low-temperature synthesis of (Cu,Fe)Al2O4 and (Cu,Cr,Fe)Al2O4 spinels from the quasicrystalline phases was investigated with the variation of process parameters during milling and annealing. The milling of the quasicrystalline materials was carried out in an attritor mill at 400 rpm for 40 hours with ball to powder ratio of 40 : 1 in hexane medium. Subsequently, annealing was performed in an air ambience for 10, 20, and 40 h at 400, 500, 600 and 700°C inside a furnace in order to oxidize the mechanically milled quasicrystalline phase for the possible formation of the spinel phase. It was found that after annealing at higher temperatures (∼500°C), mechanically milled quasicrystalline alloy transformed to a spinel phase whereas annealing at lower temperatures (<500°C) led to the formation of B2 phase as a major one along withminor amount of oxide phase. The X-ray diffraction and transmission electron microscopy of the annealed samples confirmed the formation of the spinel phase with an average grain size of ∼20–40 nm. It is interesting to note that the nanospinel phases showed the different colors during various annealing time and temperature. The optical properties of nanospinel materials, investigated employing UV visible spectrometer exhibited absorption characteristics.
- Open Access
- 18 January 2011
- Published by Springer Nature in Discover Nano
- Vol. 6 (1) , 92
Scalable synthesis of aligned carbon nanotubes bundles using green natural precursor: neem oil
Practical application of aligned carbon nanotubes (ACNTs) would have to be determined by a matter of its economical and large-scale preparation. In this study, neem oil (also named Margoaa oil, extracted from the seeds of the neem--Azadirachta indica) was used as carbon source to fabricate the bundles of ACNTs. ACNTs have been synthesized by spray pyrolysis of neem oil and ferrocene mixture at 825°C. The major components of neem oil are hydrocarbon with less amount of oxygen, which provided the precursor species in spray pyrolysis growth of CNTs. The bundles of ACNTs have been grown directly inside the quartz tube. The as-grown ACNTs have been characterized through Raman spectroscopy, scanning and transmission electron microscopic (SEM/TEM) techniques. SEM images reveal that the bundles of ACNTs are densely packed and are of several microns in length. High-resolution TEM analysis reveals these nanotubes to be multi-walled CNTs. These multi-walled CNTs were found to have inner diameter between 15 and 30 nm. It was found that present technique gives high yield with high density of bundles of ACNTs.
- 18 January 2011
- Published by Springer Nature in Discover Nano
- Vol. 6 (1) , 92
Open AccessScalable synthesis of aligned carbon nanotubes bundles using green natural precursor: neem oil
Practical application of aligned carbon nanotubes (ACNTs) would have to be determined by a matter of its economical and large-scale preparation. In this study, neem oil (also named Margoaa oil, extracted from the seeds of the neem--Azadirachta indica) was used as carbon source to fabricate the bundles of ACNTs. ACNTs have been synthesized by spray pyrolysis of neem oil and ferrocene mixture at 825°C. The major components of neem oil are hydrocarbon with less amount of oxygen, which provided the precursor species in spray pyrolysis growth of CNTs. The bundles of ACNTs have been grown directly inside the quartz tube. The as-grown ACNTs have been characterized through Raman spectroscopy, scanning and transmission electron microscopic (SEM/TEM) techniques. SEM images reveal that the bundles of ACNTs are densely packed and are of several microns in length. High-resolution TEM analysis reveals these nanotubes to be multi-walled CNTs. These multi-walled CNTs were found to have inner diameter between 15 and 30 nm. It was found that present technique gives high yield with high density of bundles of ACNTs.