Gbenga Asala
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Gbenga Asala has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
O.A. Ojo
5 shared publications- Joel Andersson
Department of Engineering Science, University West, Trollhättan, Sweden
4 shared publications - Akindele G. Odeshi
University of Saskatchewan
3 shared publications O.T. Ola
3 shared publicationsO. A. Ojo
University of Manitoba
2 shared publications- Toan Dang Truong
Department of Mechanical Engineering, Texas A&M University, College Station, TX 77843, USA
2 shared publications
Latest Publications
- Open Access
- 14 November 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 920
The effects of loading direction on the dynamic impact response of additively manufactured M350 maraging steel-Al0.5CoCrFeNi1.5 hybrid plates
- 14 November 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 920
Open AccessThe effects of loading direction on the dynamic impact response of additively manufactured M350 maraging steel-Al0.5CoCrFeNi1.5 hybrid plates
- Open Access
Influence of Heat Treatments on Heat Affected Zone Cracking of Gas Tungsten Arc Welded Additive Manufactured Alloy 718
The weldability of additive manufactured Alloy 718 was investigated in various heat-treated conditions. The microstructure of the base metal was examined in detail in order to understand the effect of different pre-weld heat treatments; i.e., solution, solution and aging, and hot isostatic pressing. After welding, the variation in total crack lengths, maximum crack length and the total number of cracks in the heat affected zone (HAZ) were used as criteria for the cracking susceptibility of each material condition where wrought Alloy 718 was used as the reference material. Selective laser melting (SLM) manufactured Alloy 718 was susceptible to HAZ cracking in all material conditions. Total crack lengths in HAZ were highest in the SLM as-built condition and lowest in the SLM hot isostatic pressed condition. The cracks that were found in the HAZ of the welded materials consisted of liquation cracks, with eutectic product surrounding the cracks, as well as cracks from which liquation products were absent.
Open AccessInfluence of Heat Treatments on Heat Affected Zone Cracking of Gas Tungsten Arc Welded Additive Manufactured Alloy 718
The weldability of additive manufactured Alloy 718 was investigated in various heat-treated conditions. The microstructure of the base metal was examined in detail in order to understand the effect of different pre-weld heat treatments; i.e., solution, solution and aging, and hot isostatic pressing. After welding, the variation in total crack lengths, maximum crack length and the total number of cracks in the heat affected zone (HAZ) were used as criteria for the cracking susceptibility of each material condition where wrought Alloy 718 was used as the reference material. Selective laser melting (SLM) manufactured Alloy 718 was susceptible to HAZ cracking in all material conditions. Total crack lengths in HAZ were highest in the SLM as-built condition and lowest in the SLM hot isostatic pressed condition. The cracks that were found in the HAZ of the welded materials consisted of liquation cracks, with eutectic product surrounding the cracks, as well as cracks from which liquation products were absent.
- 5 April 2019
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 103 (1-4) , 1419-1431
Analysis and constitutive modelling of high strain rate deformation behaviour of wire–arc additive-manufactured ATI 718Plus superalloy
- 5 April 2019
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 103 (1-4) , 1419-1431
Analysis and constitutive modelling of high strain rate deformation behaviour of wire–arc additive-manufactured ATI 718Plus superalloy
- 1 December 2018
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 738, 111-124
Improved dynamic impact behaviour of wire-arc additive manufactured ATI 718Plus®
- 1 December 2018
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 738, 111-124
Improved dynamic impact behaviour of wire-arc additive manufactured ATI 718Plus®
- 7 November 2018
- Published by Taylor & Francis in Philosophical Magazine
- Vol. 99 (4) , 419-437
A study of the dynamic impact behaviour of IN 718 and ATI 718Plus® superalloys
The dynamic impact response of IN 718 and ATI 718Plus®, in both the solution heat treated and age-hardened conditions, were investigated at different deformation temperatures and strain rates using a direct impact Hopkinson pressure bar. Analyses of the results provide a vital but previously not reported information that the ATI 718Plus® offers a higher resistance to damage during high strain rate ballistic impact deformation compared to the most widely used Iron-nickel based superalloy, Inconel 718. ATI 718Plus® showed higher strain hardening and strain rate sensitivity, in both heat treatment conditions, than IN 718. The difference in the deformation behaviour of both alloys, in the annealed condition, is attributable to the compositional modification in ATI 718Plus® which has been reported to lower its stacking fault energy and increases the tendency for deformation twinning. However, in the age-hardened condition, the difference is believed to be related to the disparity in the operative strengthening mechanism, of the precipitates present in both alloys. Furthermore, a higher susceptibility to strain location and the formation of adiabatic shear band, in aged IN 718, is attributable to the stronger temperature-softening characteristics observed in the alloy and to the limited strain hardening tendency under dynamic impact loading.
- 7 November 2018
- Published by Taylor & Francis in Philosophical Magazine
- Vol. 99 (4) , 419-437
A study of the dynamic impact behaviour of IN 718 and ATI 718Plus® superalloys
The dynamic impact response of IN 718 and ATI 718Plus®, in both the solution heat treated and age-hardened conditions, were investigated at different deformation temperatures and strain rates using a direct impact Hopkinson pressure bar. Analyses of the results provide a vital but previously not reported information that the ATI 718Plus® offers a higher resistance to damage during high strain rate ballistic impact deformation compared to the most widely used Iron-nickel based superalloy, Inconel 718. ATI 718Plus® showed higher strain hardening and strain rate sensitivity, in both heat treatment conditions, than IN 718. The difference in the deformation behaviour of both alloys, in the annealed condition, is attributable to the compositional modification in ATI 718Plus® which has been reported to lower its stacking fault energy and increases the tendency for deformation twinning. However, in the age-hardened condition, the difference is believed to be related to the disparity in the operative strengthening mechanism, of the precipitates present in both alloys. Furthermore, a higher susceptibility to strain location and the formation of adiabatic shear band, in aged IN 718, is attributable to the stronger temperature-softening characteristics observed in the alloy and to the limited strain hardening tendency under dynamic impact loading.
- Open Access
- 1 January 2016
- Published by Elsevier in Results in Physics
- Vol. 6, 196-198
On post-weld heat treatment cracking in tig welded superalloy ATI 718Plus
- 1 January 2016
- Published by Elsevier in Results in Physics
- Vol. 6, 196-198
Open AccessOn post-weld heat treatment cracking in tig welded superalloy ATI 718Plus