Taiwo Ebenezer Abioye
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Taiwo Ebenezer Abioye has a total of 75 co-authors. Here are the top co-authors by number of shared publications:
- Peter Kayode Farayibi
Federal University of Technology
12 shared publications - Adam Thomas Clare
University of Nottingham
11 shared publications - Hussain Zuhailawati
School of Materials and Mineral Resources Engineering, Universiti Sains Malaysia, Engineering Campus, Nibong Tebal, Penang, Malaysia
6 shared publications Tunde Isaac Ogedengbe
Department of Chemical Engineering, Federal University of Technology, Akure, Nigeria
5 shared publications- David Graham McCartney
Department of Mechanical Engineering, University College London, London WC1E 7JE, UK
4 shared publications - Abu Seman Anasyida
School of Materials and Mineral Resources Engineering, Universiti Sains Malaysia, Engineering Campus, Nibong Tebal, Penang, Malaysia
3 shared publications
Latest Publications
- 12 April 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Evaluation of mechanical properties of recycled stainless-steel chips and glass waste particle reinforced AA6061 composites via friction stir processing
This study develops hybrid aluminum matrix composites based on AA6061 reinforced with borosilicate glass waste (GW) and stainless-steel chips (SSCs) using friction stir processing (FSP). GW (<45 µm) and SSC (<200 µm) were incorporated at varying ratios to evaluate their effects on microstructure and mechanical properties. Microstructural analysis confirmed uniform particle distribution and grain refinement in hybrid composites. All reinforced samples exhibited higher hardness (82–107 BHN) than the unreinforced friction stir processed (FSPed) AA6061 (70.2 BHN), with a maximum increase of 52% for the 100 wt.% GW composite. While single-reinforcement composites showed reduced tensile strength (77–82 MPa), hybrid composites demonstrated improved performance. The 50 wt.% GW–50 wt.% SSC composite achieved the highest tensile strength of 139 MPa, representing a 17% improvement over the unreinforced alloy. Impact energy also increased, with a maximum value of 55.4 J for the 60 wt.% GW–40 wt.% SSC composite, corresponding to a 33.5% improvement over the unreinforced FSPed AA6061. Fracture surface analysis revealed predominantly ductile fracture modes in the optimally hybridized composites. These results demonstrate that hybridization of silica-rich industrial waste and metal chips via FSP provides an effective and sustainable route for tailoring the strength–ductility–toughness balance of AA6061 composites.
- 12 April 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Evaluation of mechanical properties of recycled stainless-steel chips and glass waste particle reinforced AA6061 composites via friction stir processing
This study develops hybrid aluminum matrix composites based on AA6061 reinforced with borosilicate glass waste (GW) and stainless-steel chips (SSCs) using friction stir processing (FSP). GW (<45 µm) and SSC (<200 µm) were incorporated at varying ratios to evaluate their effects on microstructure and mechanical properties. Microstructural analysis confirmed uniform particle distribution and grain refinement in hybrid composites. All reinforced samples exhibited higher hardness (82–107 BHN) than the unreinforced friction stir processed (FSPed) AA6061 (70.2 BHN), with a maximum increase of 52% for the 100 wt.% GW composite. While single-reinforcement composites showed reduced tensile strength (77–82 MPa), hybrid composites demonstrated improved performance. The 50 wt.% GW–50 wt.% SSC composite achieved the highest tensile strength of 139 MPa, representing a 17% improvement over the unreinforced alloy. Impact energy also increased, with a maximum value of 55.4 J for the 60 wt.% GW–40 wt.% SSC composite, corresponding to a 33.5% improvement over the unreinforced FSPed AA6061. Fracture surface analysis revealed predominantly ductile fracture modes in the optimally hybridized composites. These results demonstrate that hybridization of silica-rich industrial waste and metal chips via FSP provides an effective and sustainable route for tailoring the strength–ductility–toughness balance of AA6061 composites.
- Open Access
- 17 December 2025
- Published by Elsevier in Next Materials
- Vol. 10
Composition analysis, mechanical properties, and water absorption kinetics of extracted cellulosic fibers from Calamus deerratus cane as biodegradable reinforcement alternatives
- 17 December 2025
- Published by Elsevier in Next Materials
- Vol. 10
Open AccessComposition analysis, mechanical properties, and water absorption kinetics of extracted cellulosic fibers from Calamus deerratus cane as biodegradable reinforcement alternatives
- Open Access
- 18 September 2025
- Published by IOP Publishing in Engineering Research Express
- Vol. 7 (3) , 035438
Optimization of Carbonized Wheat Husk Reinforced AA6061 Composites for Enhanced Mechanical Performance
The increasing demand for lightweight, cost-effective, and high-performance materials in the automotive industry has driven interest in aluminum matrix composites (AMMCs) reinforced with sustainable materials like agricultural waste. While some agro-waste reinforcements, such as rice husk ash, palm kernel shell ash, and coconut shell ash, have been explored, the use of carbonized wheat husk (CWH) remains relatively novel. Wheat husk, an abundantly available agro-waste often disposed of by burning, contributes to environmental pollution and greenhouse gas emissions. Its use as a reinforcement particulate will help mitigate these environmental issues. Moreover, the adoption of CWH aligns with circular economy principles and offers a sustainable pathway for producing lightweight components with improved mechanical properties. In this study, CWH-reinforced AA6061 composites were produced at varying parameters using stir casting. Taguchi’s L9 orthogonal array was employed to optimize three parameters: percentage composition (PC) of the reinforcement, melting temperature (MT) of the alloy, and stirring time (ST), with levels of 5–15 wt.%, 700–800 °C, and 3–9 minutes, respectively. Microstructural examination of the developed AA6061–CWH composites revealed that the CWH particles were well bonded to the matrix and uniformly distributed within the continuous AA6061 matrix. Mechanical testing of the fabricated nine composite samples showed significant improvements over the control sample (unreinforced AA6061), and a confirmatory experiment validated the Taguchi-optimized parameters for AA6061–CWH composites, showing a 61.8% increase in tensile strength and a 59.8% improvement in hardness compared to the unreinforced sample. ANOVA results revealed that CWH composition was the most significant factor influencing the mechanical performance of the developed composites. This research has established the potential of carbonized wheat husk as a sustainable reinforcement material for developing cost-effective and performance-enhanced aluminum matrix composites suitable for lightweight automotive and structural applications.
- 18 September 2025
- Published by IOP Publishing in Engineering Research Express
- Vol. 7 (3) , 035438
Open AccessOptimization of Carbonized Wheat Husk Reinforced AA6061 Composites for Enhanced Mechanical Performance
The increasing demand for lightweight, cost-effective, and high-performance materials in the automotive industry has driven interest in aluminum matrix composites (AMMCs) reinforced with sustainable materials like agricultural waste. While some agro-waste reinforcements, such as rice husk ash, palm kernel shell ash, and coconut shell ash, have been explored, the use of carbonized wheat husk (CWH) remains relatively novel. Wheat husk, an abundantly available agro-waste often disposed of by burning, contributes to environmental pollution and greenhouse gas emissions. Its use as a reinforcement particulate will help mitigate these environmental issues. Moreover, the adoption of CWH aligns with circular economy principles and offers a sustainable pathway for producing lightweight components with improved mechanical properties. In this study, CWH-reinforced AA6061 composites were produced at varying parameters using stir casting. Taguchi’s L9 orthogonal array was employed to optimize three parameters: percentage composition (PC) of the reinforcement, melting temperature (MT) of the alloy, and stirring time (ST), with levels of 5–15 wt.%, 700–800 °C, and 3–9 minutes, respectively. Microstructural examination of the developed AA6061–CWH composites revealed that the CWH particles were well bonded to the matrix and uniformly distributed within the continuous AA6061 matrix. Mechanical testing of the fabricated nine composite samples showed significant improvements over the control sample (unreinforced AA6061), and a confirmatory experiment validated the Taguchi-optimized parameters for AA6061–CWH composites, showing a 61.8% increase in tensile strength and a 59.8% improvement in hardness compared to the unreinforced sample. ANOVA results revealed that CWH composition was the most significant factor influencing the mechanical performance of the developed composites. This research has established the potential of carbonized wheat husk as a sustainable reinforcement material for developing cost-effective and performance-enhanced aluminum matrix composites suitable for lightweight automotive and structural applications.
- 4 October 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (4) , 045509
The effect of pulverized glass waste particle sizes on the mechanical properties of AA6061-T6 friction stir welded joints.
The study sought to investigate the effect of pulverized glass waste (PGW) particle size as reinforcement for AA6061-T6 joints produced by Friction Stir Welding (FSW). The study utilized three particle sizes of 15 microns, 45 microns and 75 microns of the PGW as reinforcement alongside established process parameters of 900 rpm, 1120 rpm, and 1400 rpm for rotational speed, 25 mm /mi n, 40 mm min−1 and 63 mm/min for traverse speed and 1°, 1.5° and 2.5° for tilt angle in a Taguchi L9 orthogonal array experimental design for the welding process. The welding experiments were repeated for each reinforcement particle size utilized in this work. Parallel-hole reinforcement strategy was used on all joints for the application of the PGW. Microstructural analysis, tensile strength and hardness tests were carried out on the welded joints. The volume percentage of the PGW in the aluminum alloy matrix at the welded joint were determined using Image J Processing software. A processing condition of 900 rpm rotational speed, 25 mm/min traverse speed and 1° tilt angle was found to produce the weldment (sample 4) that has a favourable combination of high tensile strength (77.3 MPa) and high hardness (87.3 BHN). The tensile strength was established to increase as the PGW size decreased. This correlation was found to be statistically significant. The hardness of the welded joint did not show any particular trend with the size of the PGW. However, the hardness of the welded joint increased with the increase in the volume percentage of the pulverized glass waste in the welded joint. A moderate Pearson correlation (0.615) between hardness and PGW volume percentage was found.
- 4 October 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (4) , 045509
The effect of pulverized glass waste particle sizes on the mechanical properties of AA6061-T6 friction stir welded joints.
The study sought to investigate the effect of pulverized glass waste (PGW) particle size as reinforcement for AA6061-T6 joints produced by Friction Stir Welding (FSW). The study utilized three particle sizes of 15 microns, 45 microns and 75 microns of the PGW as reinforcement alongside established process parameters of 900 rpm, 1120 rpm, and 1400 rpm for rotational speed, 25 mm /mi n, 40 mm min−1 and 63 mm/min for traverse speed and 1°, 1.5° and 2.5° for tilt angle in a Taguchi L9 orthogonal array experimental design for the welding process. The welding experiments were repeated for each reinforcement particle size utilized in this work. Parallel-hole reinforcement strategy was used on all joints for the application of the PGW. Microstructural analysis, tensile strength and hardness tests were carried out on the welded joints. The volume percentage of the PGW in the aluminum alloy matrix at the welded joint were determined using Image J Processing software. A processing condition of 900 rpm rotational speed, 25 mm/min traverse speed and 1° tilt angle was found to produce the weldment (sample 4) that has a favourable combination of high tensile strength (77.3 MPa) and high hardness (87.3 BHN). The tensile strength was established to increase as the PGW size decreased. This correlation was found to be statistically significant. The hardness of the welded joint did not show any particular trend with the size of the PGW. However, the hardness of the welded joint increased with the increase in the volume percentage of the pulverized glass waste in the welded joint. A moderate Pearson correlation (0.615) between hardness and PGW volume percentage was found.
- 25 December 2023
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 239 (5) , 2677-2687
Enhancing the single-track deposition quality of AISI 308L wire arc additive manufacturing via process optimization and cold forging treatment
Wire arc additive manufacturing (WAAM) has been established as a promising additive manufacturing technique for fabricating and repairing medium-to-large scale metallic engineering parts. However, achieving an excellent geometrical accuracy and high mechanical properties close to the parent metal require an optimal setting of parameters for every material system and, sometimes, post-processing treatment. In this work, WAAM of 308L stainless steel was performed, using gas metal arc welding as the heat source, at varying values of wire feed rate (WFR) and traverse speed (TS) to investigate its effects on the geometry, microstructure and mechanical properties of the deposited track. Thereafter, post-cold forging treatment was performed on the track deposited at the optimum parametric setting. The track width and height decreased with increasing TS due to reduction in the wire deposition volume per unit length of track. The track height increased as the WFR increased from 61.67 to 95 mm/s, after which the process became unstable, leading to a decline in height. The microstructure of the deposited track mainly comprised δ-ferrite and austenite phases while the hardness of the track deposits (ranging between 124–172 HV) was largely influenced by the presence of carbide precipitates and equiaxed grains size which reduced as the TS and WFR increased. The post-cold forging treatment resulted in strain hardening, which resulted in significant improvement in the track hardness (up to 219 HV) but a fall in its impact strength due to loss of ductility.
- 25 December 2023
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 239 (5) , 2677-2687
Enhancing the single-track deposition quality of AISI 308L wire arc additive manufacturing via process optimization and cold forging treatment
Wire arc additive manufacturing (WAAM) has been established as a promising additive manufacturing technique for fabricating and repairing medium-to-large scale metallic engineering parts. However, achieving an excellent geometrical accuracy and high mechanical properties close to the parent metal require an optimal setting of parameters for every material system and, sometimes, post-processing treatment. In this work, WAAM of 308L stainless steel was performed, using gas metal arc welding as the heat source, at varying values of wire feed rate (WFR) and traverse speed (TS) to investigate its effects on the geometry, microstructure and mechanical properties of the deposited track. Thereafter, post-cold forging treatment was performed on the track deposited at the optimum parametric setting. The track width and height decreased with increasing TS due to reduction in the wire deposition volume per unit length of track. The track height increased as the WFR increased from 61.67 to 95 mm/s, after which the process became unstable, leading to a decline in height. The microstructure of the deposited track mainly comprised δ-ferrite and austenite phases while the hardness of the track deposits (ranging between 124–172 HV) was largely influenced by the presence of carbide precipitates and equiaxed grains size which reduced as the TS and WFR increased. The post-cold forging treatment resulted in strain hardening, which resulted in significant improvement in the track hardness (up to 219 HV) but a fall in its impact strength due to loss of ductility.
- 8 April 2023
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 76 (8) , 2009-2031
Review of Parametric Strategies for Enhancing the Mechanical and Wear Properties of Friction Stir Processed Aluminium Alloys Composites
- 8 April 2023
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 76 (8) , 2009-2031
Review of Parametric Strategies for Enhancing the Mechanical and Wear Properties of Friction Stir Processed Aluminium Alloys Composites
- Open Access
- 1 January 2023
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 59 (3) , 443-454
Characterization of cryo-rolled low carbon steel using ferrite-martensite starting microstructure
Cryo-rolling, a technique of severe plastic deformation (SPD) performed at cryogenic temperatures, has proven to be a promising technique for improving the microstructure and mechanical properties of low-carbon steels. Low carbon steel with a two-phase ferrite-martensite starting microstructure was subjected to cryogenic rolling at liquid nitrogen temperature to produce sheets with different deformation rates: 50%, 70%, and 90%. The microstructure, mechanical properties, and corrosion resistance were investigated. The results show that cryo-rolling effectively refines the microstructure and leads to a higher dislocation density and smaller grain size as the deformation rate increases. The cryorolled sample deformed at 90% has the highest grain aspect ratio (35.5), the smallest crystallite size (13.70 nm), the highest lattice strain (74.6 x 10-3), and the highest dislocation density compared to the samples deformed at 50% and 70%. This refined microstructure significantly improves the mechanical properties, with the cryo-rolled sample deformed at 90% exhibiting the highest hardness (152 HV), tensile strength (1020 MPa), and yield strength (950 MPa), corresponding to an increase of 175.6%, 344.0%, and 466.5%, respectively. In addition, cryo-rolling at 90% showed a decrease in corrosion resistance, with the lowest corrosion rate observed at 90% deformation (5.97 mm/year).
- 1 January 2023
- Published by National Library of Serbia in Journal of Mining and Metallurgy, Section B: Metallurgy
- Vol. 59 (3) , 443-454
Open AccessCharacterization of cryo-rolled low carbon steel using ferrite-martensite starting microstructure
Cryo-rolling, a technique of severe plastic deformation (SPD) performed at cryogenic temperatures, has proven to be a promising technique for improving the microstructure and mechanical properties of low-carbon steels. Low carbon steel with a two-phase ferrite-martensite starting microstructure was subjected to cryogenic rolling at liquid nitrogen temperature to produce sheets with different deformation rates: 50%, 70%, and 90%. The microstructure, mechanical properties, and corrosion resistance were investigated. The results show that cryo-rolling effectively refines the microstructure and leads to a higher dislocation density and smaller grain size as the deformation rate increases. The cryorolled sample deformed at 90% has the highest grain aspect ratio (35.5), the smallest crystallite size (13.70 nm), the highest lattice strain (74.6 x 10-3), and the highest dislocation density compared to the samples deformed at 50% and 70%. This refined microstructure significantly improves the mechanical properties, with the cryo-rolled sample deformed at 90% exhibiting the highest hardness (152 HV), tensile strength (1020 MPa), and yield strength (950 MPa), corresponding to an increase of 175.6%, 344.0%, and 466.5%, respectively. In addition, cryo-rolling at 90% showed a decrease in corrosion resistance, with the lowest corrosion rate observed at 90% deformation (5.97 mm/year).
- 1 January 2023
- Published by SAGE Publications in Materials Science and Technology
- Vol. 39 (2) , 129-146
Review of post-processing methods for high-quality wire arc additive manufacturing
The present paper reviews the concept of wire arc additive manufacturing (WAAM), its associated defects, and the existing post-processing methods for product quality enhancement. The application of friction stir processing (a surface modification technique) for enhancing the microstructure and mechanical properties of wire arc additively manufactured parts was considered as a new horizon in this field of research. Finally, the article concludes that the widespread usage of WAAM is still challenged by some obstacles, which may need to be targeted and addressed in unique ways for different materials in order to generate functional systems in a reasonable amount of time. Unifying materials and manufacturing techniques to produce defect-free and structurally robust deposited parts will become increasingly important in the future.
- 1 January 2023
- Published by SAGE Publications in Materials Science and Technology
- Vol. 39 (2) , 129-146
Review of post-processing methods for high-quality wire arc additive manufacturing
The present paper reviews the concept of wire arc additive manufacturing (WAAM), its associated defects, and the existing post-processing methods for product quality enhancement. The application of friction stir processing (a surface modification technique) for enhancing the microstructure and mechanical properties of wire arc additively manufactured parts was considered as a new horizon in this field of research. Finally, the article concludes that the widespread usage of WAAM is still challenged by some obstacles, which may need to be targeted and addressed in unique ways for different materials in order to generate functional systems in a reasonable amount of time. Unifying materials and manufacturing techniques to produce defect-free and structurally robust deposited parts will become increasingly important in the future.