Ertan Arda
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Ertan Arda has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Önder Pekcan
Faculty of Engineering and Natural Sciences, Kadir Has University, Istanbul, Turkey
14 shared publications - Ömer Bahadır Mergen
Dokuz Eylul University
9 shared publications Gülşen Akın Evingür
Faculty of Engineering, Piri Reis University, Turkey
4 shared publicationsSelim Kara
Department of Physics, Faculty of Science Trakya University Edirne Turkey
4 shared publications- Selim Kara
Department of Physics, Faculty of Science, Trakya University, Edirne, Turkey
2 shared publications Erhan P K N
Hacettepe University, Chemical Engineering Department and Bioengineering Division, Beytepe, 06532, Ankara, Turkey
1 shared publication
Latest Publications
- 5 May 2026
- Published by SAGE Publications in Journal of Composite Materials
Electrical and optical percolation behavior of carbon nanotube-doped graphene reinforced polyvinylpyrrolidone/polymethyl methacrylate nanocomposite films
In this study, multifunctional poly (vinylpyrrolidone)/poly (methyl methacrylate)/carbon nanotube-doped graphene (PVP/PMMA/CNTG) nanocomposite films were fabricated, and their electrical conductivity and optical transmittance were quantitatively analyzed within the framework of percolation theory. The pure PVP/PMMA blend exhibited an insulating behavior a very low electrical conductivity of 2.7 × 10 -7 S m -1 . Upon the incorporation of CNTG fillers, a dramatic enhancement in electrical conductivity was observed, reaching 2.46 × 10 2 S m -1 at 3.00 vol% loading, corresponding to an increase of approximately nine orders of magnitude. Electrical percolation analysis revealed a low percolation threshold of ϕ σ = 0.30 vol%, which is attributed to the synergistic interaction between one-dimensional carbon nanotubes and two-dimensional graphene sheets forming an efficient three-dimensional conductive network. The critical exponent was determined to be t σ = 2.62, indicating a non-ideal, tunneling assisted three-dimensional percolation mechanism. Optical characterization performed at a fixed wavelength of 600 nm demonstrated a progressive decrease in optical transmittance with increasing CNTG content, due to enhanced photon scattering and absorption arising from refractive index mismatch and increased structural heterogeneity. In contrast to the electrical behavior, optical percolation occurred at a higher filler content, with an optical percolation threshold of ϕ o p = 1.20 vol% and a critical optical exponent t o p = 0.41, which is close to the theoretical site percolation value. A strong inverse correlation between electrical conductivity and optical transmittance was observed, highlighting the inherent trade-off between electrical performance and optical transparency.
- 5 May 2026
- Published by SAGE Publications in Journal of Composite Materials
Electrical and optical percolation behavior of carbon nanotube-doped graphene reinforced polyvinylpyrrolidone/polymethyl methacrylate nanocomposite films
In this study, multifunctional poly (vinylpyrrolidone)/poly (methyl methacrylate)/carbon nanotube-doped graphene (PVP/PMMA/CNTG) nanocomposite films were fabricated, and their electrical conductivity and optical transmittance were quantitatively analyzed within the framework of percolation theory. The pure PVP/PMMA blend exhibited an insulating behavior a very low electrical conductivity of 2.7 × 10 -7 S m -1 . Upon the incorporation of CNTG fillers, a dramatic enhancement in electrical conductivity was observed, reaching 2.46 × 10 2 S m -1 at 3.00 vol% loading, corresponding to an increase of approximately nine orders of magnitude. Electrical percolation analysis revealed a low percolation threshold of ϕ σ = 0.30 vol%, which is attributed to the synergistic interaction between one-dimensional carbon nanotubes and two-dimensional graphene sheets forming an efficient three-dimensional conductive network. The critical exponent was determined to be t σ = 2.62, indicating a non-ideal, tunneling assisted three-dimensional percolation mechanism. Optical characterization performed at a fixed wavelength of 600 nm demonstrated a progressive decrease in optical transmittance with increasing CNTG content, due to enhanced photon scattering and absorption arising from refractive index mismatch and increased structural heterogeneity. In contrast to the electrical behavior, optical percolation occurred at a higher filler content, with an optical percolation threshold of ϕ o p = 1.20 vol% and a critical optical exponent t o p = 0.41, which is close to the theoretical site percolation value. A strong inverse correlation between electrical conductivity and optical transmittance was observed, highlighting the inherent trade-off between electrical performance and optical transparency.
- Open Access
- 19 January 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (2)
Comprehensive Investigation of Linear and Nonlinear Optical Properties and Tunable Band Gaps in CS/PVP-GnP Nanocomposites
The growing demand for low-cost and environmentally friendly polymer nanocomposites has intensified research efforts toward advanced functional materials. In this work, chitosan/polyvinylpyrrolidone (CS/PVP) nanocomposites reinforced with graphene nanoplatelets (GnP) were fabricated using a solution-based method and systematically characterized to evaluate their electrical and optical performance. The study focuses on electrical conductivity, optical band gap energy (Eg), Urbach energy (E_u), reflectance (R), refractive index (n), optical conductivity, and optical dielectric properties. To gain deeper insight into the dispersive and electronic behavior of the nanocomposites, the Wemple–DiDomenico (WD) model, the Spitzer–Fan model, and the Drude free-electron model were employed. In addition, the nonlinear optical (NLO) parameters, including optical susceptibility and nonlinear refractive indices, were analyzed. The results reveal significant enhancements in both linear and nonlinear optical properties with increasing GnP content, highlighting the strong structure–property relationships within the nanocomposite system. These findings demonstrate that CS/PVP-GnP nanocomposites are promising candidates for advanced applications in optoelectronics, energy storage, and photonic technologies.
- 19 January 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (2)
Open AccessComprehensive Investigation of Linear and Nonlinear Optical Properties and Tunable Band Gaps in CS/PVP-GnP Nanocomposites
The growing demand for low-cost and environmentally friendly polymer nanocomposites has intensified research efforts toward advanced functional materials. In this work, chitosan/polyvinylpyrrolidone (CS/PVP) nanocomposites reinforced with graphene nanoplatelets (GnP) were fabricated using a solution-based method and systematically characterized to evaluate their electrical and optical performance. The study focuses on electrical conductivity, optical band gap energy (Eg), Urbach energy (E_u), reflectance (R), refractive index (n), optical conductivity, and optical dielectric properties. To gain deeper insight into the dispersive and electronic behavior of the nanocomposites, the Wemple–DiDomenico (WD) model, the Spitzer–Fan model, and the Drude free-electron model were employed. In addition, the nonlinear optical (NLO) parameters, including optical susceptibility and nonlinear refractive indices, were analyzed. The results reveal significant enhancements in both linear and nonlinear optical properties with increasing GnP content, highlighting the strong structure–property relationships within the nanocomposite system. These findings demonstrate that CS/PVP-GnP nanocomposites are promising candidates for advanced applications in optoelectronics, energy storage, and photonic technologies.
- Open Access
- 6 January 2020
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (18) , 2449-2459
Electrical, mechanical, and optical changes in MWCNT-doped PMMA composite films
In this study, we report the preparation of poly (methyl methacrylate)/multi-walled carbon nanotube (MWCNT) composite thin films by simple and efficient solution mixing and ultrasonic method and the electrical, optical, and mechanical characterizations. Scattered light intensity ( I sc), tensile modulus ( E), and surface conductivity ( σ) of these composites have increased with the addition of MWCNT into the composite. The observed behavior in electrical, optical, and mechanical properties of the poly (methyl methacrylate)/MWCNT composites was interpreted by site and classical percolation theory. The optical mechanical and electrical percolation thresholds of poly (methyl methacrylate)/MWCNT composites were determined as φ op = 3 wt%, φ m = 0 wt%, and φσ = 5 wt%, respectively. The optical ( t op), mechanical ( t m), and electrical ( t σ) critical exponents were calculated as 2.23, 0.43, and 0.11, respectively. Both the tensile modulus and tensile strength of poly (methyl methacrylate)/MWCNT composites were increased with increasing MWCNT content until it reaches to 10 wt%. However, above φ = 10 wt%, the mechanical properties of the composites were decreased due to the aggregation of MWCNTs, while the toughness does not show a significant change until φ = 10 wt% MWCNT content, whereas it was decreased above this value.
- 6 January 2020
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (18) , 2449-2459
Open AccessElectrical, mechanical, and optical changes in MWCNT-doped PMMA composite films
In this study, we report the preparation of poly (methyl methacrylate)/multi-walled carbon nanotube (MWCNT) composite thin films by simple and efficient solution mixing and ultrasonic method and the electrical, optical, and mechanical characterizations. Scattered light intensity ( I sc), tensile modulus ( E), and surface conductivity ( σ) of these composites have increased with the addition of MWCNT into the composite. The observed behavior in electrical, optical, and mechanical properties of the poly (methyl methacrylate)/MWCNT composites was interpreted by site and classical percolation theory. The optical mechanical and electrical percolation thresholds of poly (methyl methacrylate)/MWCNT composites were determined as φ op = 3 wt%, φ m = 0 wt%, and φσ = 5 wt%, respectively. The optical ( t op), mechanical ( t m), and electrical ( t σ) critical exponents were calculated as 2.23, 0.43, and 0.11, respectively. Both the tensile modulus and tensile strength of poly (methyl methacrylate)/MWCNT composites were increased with increasing MWCNT content until it reaches to 10 wt%. However, above φ = 10 wt%, the mechanical properties of the composites were decreased due to the aggregation of MWCNTs, while the toughness does not show a significant change until φ = 10 wt% MWCNT content, whereas it was decreased above this value.
- 24 October 2019
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (11) , 1497-1510
Electrical, optical and mechanical properties of chitosan biocomposites
In this work, chitosan/graphene nanoplatelets (CS/GNP) and chitosan/multi-walled carbon nanotube (CS/MWCNT) biocomposite films were prepared using a simple, eco-friendly and low-cost method. The electrical, optical and mechanical properties of these composite films were investigated. The optical, mechanical and electrical properties of the biocomposites were significantly improved, which make them promising materials for food packaging, ultraviolet protection and biomedical applications. With the increase of carbon filler content (GNP or MWCNT) in CS biocomposites, the surface conductivity ( σ), the scattered light intensity ( I sc) and the tensile modulus ( E) increased significantly. This behaviour in the electrical, optical and mechanical properties of the CS/carbon filler biocomposites was explained by percolation theory. The electrical percolation thresholds were determined as R σ = 25.0 wt.% for CS/GNP and R σ = 10.0 wt.% for CS/MWCNT biocomposites, while the optical percolation thresholds were found as R op =12.0 wt.% for CS/GNP and R op = 2.0 wt.% for CS/MWCNT biocomposites. Conversely, the mechanical percolation thresholds for both CS/GNP and CS/MWCNT biocomposites were found to be negligibly small ( R m = 0.0 wt.%). The electrical ( β σ), optical ( β op) and mechanical ( β m) critical exponents were calculated for both CS/carbon filler biocomposites and found compatible with the applied percolation theory.
- 24 October 2019
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (11) , 1497-1510
Electrical, optical and mechanical properties of chitosan biocomposites
In this work, chitosan/graphene nanoplatelets (CS/GNP) and chitosan/multi-walled carbon nanotube (CS/MWCNT) biocomposite films were prepared using a simple, eco-friendly and low-cost method. The electrical, optical and mechanical properties of these composite films were investigated. The optical, mechanical and electrical properties of the biocomposites were significantly improved, which make them promising materials for food packaging, ultraviolet protection and biomedical applications. With the increase of carbon filler content (GNP or MWCNT) in CS biocomposites, the surface conductivity ( σ), the scattered light intensity ( I sc) and the tensile modulus ( E) increased significantly. This behaviour in the electrical, optical and mechanical properties of the CS/carbon filler biocomposites was explained by percolation theory. The electrical percolation thresholds were determined as R σ = 25.0 wt.% for CS/GNP and R σ = 10.0 wt.% for CS/MWCNT biocomposites, while the optical percolation thresholds were found as R op =12.0 wt.% for CS/GNP and R op = 2.0 wt.% for CS/MWCNT biocomposites. Conversely, the mechanical percolation thresholds for both CS/GNP and CS/MWCNT biocomposites were found to be negligibly small ( R m = 0.0 wt.%). The electrical ( β σ), optical ( β op) and mechanical ( β m) critical exponents were calculated for both CS/carbon filler biocomposites and found compatible with the applied percolation theory.
- 27 June 2019
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (1) , 31-44
Electrical, optical, and mechanical percolations of multi-walled carbon nanotube and carbon mesoporous-doped polystyrene composites
In this study, we have investigated and compared electrical, optical, and mechanical properties of polystyrene thin films with added multi-walled carbon nanotube and carbon mesoporous. Surface conductivity ( σ), scattered light intensity ( I sc), and all the mechanical parameters of these composites have increased with increasing the content of carbon filler (multi-walled carbon nanotube or carbon mesoporous) in the polystyrene composites. This behavior in electrical, mechanical, and optical properties of the polystyrene/carbon fiber composites has been explained by classical and site percolation theory, respectively. The electrical percolation thresholds ( R σ) were determined to be 8.0 wt% for polystyrene/multi-walled carbon nanotube and 25.0 wt% for polystyrene/carbon mesoporous composites. The optical percolation thresholds were found to be R op = 0.8 wt.% for polystyrene/multi-walled carbon nanotube and R op = 3.0 wt.% for polystyrene/carbon mesoporous composites. For the polystyrene/carbon mesoporous composite system, it was determined that the mechanical percolation threshold occurred at lower R values than the polystyrene/multi-walled carbon nanotube composite system. The electrical ( β σ), optical ( β op), and mechanical ( β m) critical exponents have been calculated for both of the polystyrene/carbon fiber composites and obtained as compatible with used percolation theory.
- 27 June 2019
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 54 (1) , 31-44
Electrical, optical, and mechanical percolations of multi-walled carbon nanotube and carbon mesoporous-doped polystyrene composites
In this study, we have investigated and compared electrical, optical, and mechanical properties of polystyrene thin films with added multi-walled carbon nanotube and carbon mesoporous. Surface conductivity ( σ), scattered light intensity ( I sc), and all the mechanical parameters of these composites have increased with increasing the content of carbon filler (multi-walled carbon nanotube or carbon mesoporous) in the polystyrene composites. This behavior in electrical, mechanical, and optical properties of the polystyrene/carbon fiber composites has been explained by classical and site percolation theory, respectively. The electrical percolation thresholds ( R σ) were determined to be 8.0 wt% for polystyrene/multi-walled carbon nanotube and 25.0 wt% for polystyrene/carbon mesoporous composites. The optical percolation thresholds were found to be R op = 0.8 wt.% for polystyrene/multi-walled carbon nanotube and R op = 3.0 wt.% for polystyrene/carbon mesoporous composites. For the polystyrene/carbon mesoporous composite system, it was determined that the mechanical percolation threshold occurred at lower R values than the polystyrene/multi-walled carbon nanotube composite system. The electrical ( β σ), optical ( β op), and mechanical ( β m) critical exponents have been calculated for both of the polystyrene/carbon fiber composites and obtained as compatible with used percolation theory.
- 8 August 2018
- Published by Wiley in Polymer Composites
- Vol. 40 (5) , 1862-1869
Effects of GNP addition on optical properties and band gap energies of PMMA films
In this study, the effects of graphene nanoplatelet (GNP) doping on the optical parameters (absorption coefficient, α and extinction coefficient, k) and the optical transition energies (optical band gap and Urbach energies) of poly(methyl methacrylate)/graphene nanoplatelet (PMMA/GNP) composite films were studied. PMMA/GNP composite films with various GNP mass fractions were prepared by spin coating technique. The absorbance (A) changes of the prepared composites were measured by using UV–Vis technique. The α and k values of the composites were obtained from UV–Vis data. The observed rapid increase in A values in UV‐region were associated with the optical transitions of GNP electrons from valence to conduction band. The direct (Ed) and indirect (Ei) optical band gap energies of the composites were determined by using Tauc method. Both of the band gap energies were decreased when the GNP content in the PMMA matrix is increased. The decrease in the band gap energies was interpreted as evidence of increased conductivity of the composites. Additionally, energies of the band tails (Urbach energy) were calculated. It was seen that the Urbach energy levels were increased with GNP content. POLYM. COMPOS., 40:1862–1869, 2019. © 2018 Society of Plastics Engineers
- 8 August 2018
- Published by Wiley in Polymer Composites
- Vol. 40 (5) , 1862-1869
Effects of GNP addition on optical properties and band gap energies of PMMA films
In this study, the effects of graphene nanoplatelet (GNP) doping on the optical parameters (absorption coefficient, α and extinction coefficient, k) and the optical transition energies (optical band gap and Urbach energies) of poly(methyl methacrylate)/graphene nanoplatelet (PMMA/GNP) composite films were studied. PMMA/GNP composite films with various GNP mass fractions were prepared by spin coating technique. The absorbance (A) changes of the prepared composites were measured by using UV–Vis technique. The α and k values of the composites were obtained from UV–Vis data. The observed rapid increase in A values in UV‐region were associated with the optical transitions of GNP electrons from valence to conduction band. The direct (Ed) and indirect (Ei) optical band gap energies of the composites were determined by using Tauc method. Both of the band gap energies were decreased when the GNP content in the PMMA matrix is increased. The decrease in the band gap energies was interpreted as evidence of increased conductivity of the composites. Additionally, energies of the band tails (Urbach energy) were calculated. It was seen that the Urbach energy levels were increased with GNP content. POLYM. COMPOS., 40:1862–1869, 2019. © 2018 Society of Plastics Engineers
- 3 August 2018
- Published by Taylor & Francis in Phase Transitions
- Vol. 91 (8) , 887-900
Electrical, optical and mechanical properties of PS/GNP composite films
In this study, the electrical, optical and mechanical properties of polystyrene (PS) thin films added graphene nanoplatelet (GNP) have been investigated. Surface conductivity (σ), absorbance intensity (A) and tensile modulus of these composite films have increased with increasing the content of GNP in the composite. The increase in the electrical and optical properties of the PS/GNP composite films has been interpreted by site and classical percolation theory, respectively. The electrical and the optical percolation thresholds of PS/GNP composite films were determined as Rσ = 23.0 wt.% and Rop = 13.0 wt.%, respectively. While the conductivity results have been attributed to the classical percolation theory, the optical results have attributed to the site percolation theory. The electrical (βσ) and the optical (βop) critical exponents were calculated as 2.54 and 0.40, respectively. The tensile modulus and the tensile strength of the PS/GNP composites increased with the increasing of GNP content in the PS. But, the toughness of the composites fluctuated with GNP addition.
- 3 August 2018
- Published by Taylor & Francis in Phase Transitions
- Vol. 91 (8) , 887-900
Electrical, optical and mechanical properties of PS/GNP composite films
In this study, the electrical, optical and mechanical properties of polystyrene (PS) thin films added graphene nanoplatelet (GNP) have been investigated. Surface conductivity (σ), absorbance intensity (A) and tensile modulus of these composite films have increased with increasing the content of GNP in the composite. The increase in the electrical and optical properties of the PS/GNP composite films has been interpreted by site and classical percolation theory, respectively. The electrical and the optical percolation thresholds of PS/GNP composite films were determined as Rσ = 23.0 wt.% and Rop = 13.0 wt.%, respectively. While the conductivity results have been attributed to the classical percolation theory, the optical results have attributed to the site percolation theory. The electrical (βσ) and the optical (βop) critical exponents were calculated as 2.54 and 0.40, respectively. The tensile modulus and the tensile strength of the PS/GNP composites increased with the increasing of GNP content in the PS. But, the toughness of the composites fluctuated with GNP addition.
- 8 February 2018
- Published by Taylor & Francis in Phase Transitions
- Vol. 91 (5) , 546-557
Electrical and optical percolations in PMMA/GNP composite films
Effects of graphene nanoplatelet (GNP) addition on the electrical conductivity and optical absorbance of poly(methyl methacrylate)/graphene nanoplatelet (PMMA/GNP) composite films were studied. Optical absorbance and two point probe resistivity techniques were used to determine the variations of the optical and electrical properties of the composites, respectively. Absorbance intensity, A, and surface resistivity, Rs, of the composite films were monitored as a function of GNP mass fraction (M) at room temperature. Absorbance intensity values of the composites were increased and surface resistivity values were decreased by increasing the content of GNP in the composite. Electrical and optical percolation thresholds of composite films were determined as Mσ = 27.5 wt.% and Mop = 26.6 wt.%, respectively. The conductivity and the optical results were attributed to the classical and site percolation theories, respectively. Optical (βop) and electrical (βσ) critical exponents were calculated as 0.40 and 1.71, respectively.
- 8 February 2018
- Published by Taylor & Francis in Phase Transitions
- Vol. 91 (5) , 546-557
Electrical and optical percolations in PMMA/GNP composite films
Effects of graphene nanoplatelet (GNP) addition on the electrical conductivity and optical absorbance of poly(methyl methacrylate)/graphene nanoplatelet (PMMA/GNP) composite films were studied. Optical absorbance and two point probe resistivity techniques were used to determine the variations of the optical and electrical properties of the composites, respectively. Absorbance intensity, A, and surface resistivity, Rs, of the composite films were monitored as a function of GNP mass fraction (M) at room temperature. Absorbance intensity values of the composites were increased and surface resistivity values were decreased by increasing the content of GNP in the composite. Electrical and optical percolation thresholds of composite films were determined as Mσ = 27.5 wt.% and Mop = 26.6 wt.%, respectively. The conductivity and the optical results were attributed to the classical and site percolation theories, respectively. Optical (βop) and electrical (βσ) critical exponents were calculated as 0.40 and 1.71, respectively.
- 28 October 2014
- Published by Springer Nature in Polymer Bulletin
- Vol. 72 (2) , 157-175
A comparison of fluorescence and UV–visible spectrometry techniques for thermal phase transitions of agarose gels
- 28 October 2014
- Published by Springer Nature in Polymer Bulletin
- Vol. 72 (2) , 157-175
A comparison of fluorescence and UV–visible spectrometry techniques for thermal phase transitions of agarose gels
- 24 December 2012
- Published by Taylor & Francis in Phase Transitions
- Vol. 86 (10) , 1017-1032
Electrical, optical and fluorescence percolations in P(VAc-co-BuA)/MWCNT composite films
Effects of multiwall carbon nanotube (MWCNT) addition on the electrical conductivities, optical transparencies and fluorescence emissions of poly(vinyl acetate-co-butyl acrylate) (P(VAc-co-BuA))/MWCNT composite films were studied. Optical transmission, fluorescence emission and two point probe resistivity techniques were used to determine the variations of the optical, fluorescence and electrical properties of the composites, respectively. Transmitted photon intensity (I tr), fluorescence emission intensity (I fl) and surface resistivity (ρ s) of the composite films were monitored as a function of MWCNT mass fraction (M) at room temperature. All these measured quantities of the composites were decreased by increasing the content of MWCNT in the composite. The conductivity and the optical results were attributed to the classical and site percolation theories, respectively. The fluorescence results, however, possessed both the site and classical percolation theories at low and high MWCNT content regions, respectively.
- 24 December 2012
- Published by Taylor & Francis in Phase Transitions
- Vol. 86 (10) , 1017-1032
Electrical, optical and fluorescence percolations in P(VAc-co-BuA)/MWCNT composite films
Effects of multiwall carbon nanotube (MWCNT) addition on the electrical conductivities, optical transparencies and fluorescence emissions of poly(vinyl acetate-co-butyl acrylate) (P(VAc-co-BuA))/MWCNT composite films were studied. Optical transmission, fluorescence emission and two point probe resistivity techniques were used to determine the variations of the optical, fluorescence and electrical properties of the composites, respectively. Transmitted photon intensity (I tr), fluorescence emission intensity (I fl) and surface resistivity (ρ s) of the composite films were monitored as a function of MWCNT mass fraction (M) at room temperature. All these measured quantities of the composites were decreased by increasing the content of MWCNT in the composite. The conductivity and the optical results were attributed to the classical and site percolation theories, respectively. The fluorescence results, however, possessed both the site and classical percolation theories at low and high MWCNT content regions, respectively.