Guangbing Han
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Guangbing Han has a total of 49 co-authors. Here are the top co-authors by number of shared publications:
Shishou Kang
12 shared publicationsMehran Khan Alam
7 shared publicationsShahzab Raza
6 shared publications- Mehran Khan Alam
Key Laboratory for Liquid–Solid Structural Evolution and Processing of Materials (Ministry of Education), School of Materials Science and Engineering, Shandong University 2 , Jinan 250061
4 shared publications - Shishou Kang
Shandong University
3 shared publications Fei Wei
Shandong University
2 shared publications
Latest Publications
- Open Access
- 30 September 2026
- Published by Elsevier in SSRN Electronic Journal
Enhanced coercivity in Pr10Fe80.5B6.5Nb3 melt-spun ribbons induced by texture and fine microstructure
We report the realization of high coercivity in Nb-doped Pr₁₀Fe₈₀.₅B₆.₅Nb₃ melt-spun ribbons via post-annealing-induced crystallographic texture control. A distinct (00l) fiber texture is achieved, characterized by a preferential alignment of crystallite c-axes at a finite tilt relative to the ribbon plane, while maintaining random in-plane orientation. This unique texture configuration introduces pronounced magnetic anisotropy, yielding a record-high coercivity of 1204 kA m-1 for melt-spun ribbons with a rare-earth content as low as 10 at.%. Mechanistically, segregation at grain boundaries has been found to modify interfacial chemistry and promote preferential stabilization of the (006) orientation during annealing. The synergistic effects of texture-induced anisotropy, refined microstructure, and enhanced intergranular exchange coupling elucidate the superior magnetic hardening. These findings provide a pathway for designing high-performance, rare-earth-deficient permanent magnets via interface engineering.
- 30 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessEnhanced coercivity in Pr10Fe80.5B6.5Nb3 melt-spun ribbons induced by texture and fine microstructure
We report the realization of high coercivity in Nb-doped Pr₁₀Fe₈₀.₅B₆.₅Nb₃ melt-spun ribbons via post-annealing-induced crystallographic texture control. A distinct (00l) fiber texture is achieved, characterized by a preferential alignment of crystallite c-axes at a finite tilt relative to the ribbon plane, while maintaining random in-plane orientation. This unique texture configuration introduces pronounced magnetic anisotropy, yielding a record-high coercivity of 1204 kA m-1 for melt-spun ribbons with a rare-earth content as low as 10 at.%. Mechanistically, segregation at grain boundaries has been found to modify interfacial chemistry and promote preferential stabilization of the (006) orientation during annealing. The synergistic effects of texture-induced anisotropy, refined microstructure, and enhanced intergranular exchange coupling elucidate the superior magnetic hardening. These findings provide a pathway for designing high-performance, rare-earth-deficient permanent magnets via interface engineering.
- Open Access
- 28 September 2026
- Published by Elsevier in SSRN Electronic Journal
Metalloid-Controlled Local Structure, Thermal Stability, and Magnetic Dynamics in Fe-Based Amorphous Alloys
The choice of metalloid strongly influences the local atomic structure and magnetic behavior of Fe-based amorphous alloys. Here we comparatively investigated Fe80P10C10 (FePC), Fe80B10Si10 (FeBSi), and Fe80B10C10 (FeBC) amorphous ribbons to establish the relationship between local structure, thermal stability, and magnetic dynamics. FeBSi showed the most compact short-range atomic structure and the highest crystallization temperature (Tx1 = 753 K), indicating better thermal stability. It also exhibited favorable soft-magnetic behavior, with a saturation magnetization of 1.72 T and the lowest coercivity of 7 A m-1. MOKE, EPR, and FMR studies showed more homogeneous magnetic environments and easier magnetization reversal in FeBSi, while FeBC had stronger magnetic heterogeneity and domain-wall resistance. XPS revealed different Fe-metalloid bonding environments in the three alloys. These findings suggest that metalloid combination controls thermal stability and magnetic dynamics, offering a useful strategy for designing high-performance Fe-based amorphous soft magnets.
- 28 September 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessMetalloid-Controlled Local Structure, Thermal Stability, and Magnetic Dynamics in Fe-Based Amorphous Alloys
The choice of metalloid strongly influences the local atomic structure and magnetic behavior of Fe-based amorphous alloys. Here we comparatively investigated Fe80P10C10 (FePC), Fe80B10Si10 (FeBSi), and Fe80B10C10 (FeBC) amorphous ribbons to establish the relationship between local structure, thermal stability, and magnetic dynamics. FeBSi showed the most compact short-range atomic structure and the highest crystallization temperature (Tx1 = 753 K), indicating better thermal stability. It also exhibited favorable soft-magnetic behavior, with a saturation magnetization of 1.72 T and the lowest coercivity of 7 A m-1. MOKE, EPR, and FMR studies showed more homogeneous magnetic environments and easier magnetization reversal in FeBSi, while FeBC had stronger magnetic heterogeneity and domain-wall resistance. XPS revealed different Fe-metalloid bonding environments in the three alloys. These findings suggest that metalloid combination controls thermal stability and magnetic dynamics, offering a useful strategy for designing high-performance Fe-based amorphous soft magnets.
- 28 March 2026
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 733
Effect of Nb content on texture evolution in Pr2Fe14B/α-Fe melt-spun ribbons
- 28 March 2026
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 733
Effect of Nb content on texture evolution in Pr2Fe14B/α-Fe melt-spun ribbons
- Open Access
- 13 March 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
Nb-doping Induced High Coercivity in Pr2Fe14B/α-Fe Nanocomposite Melt-spun Ribbons
The effect of niobium (Nb) doping on the microstructure and magnetic properties of as-spun Pr10Fe82.5-xB6.5Nbx ribbons was investigated. Nb doping significantly refines the grain size and enhances the coercivity, which increases from 380 kA/m (x = 0) to a remarkable 990 kA/m (x = 3), a top-level performance among Nb‑doped rare-earth-deficient nanocomposite alloys. The improvement is attributed to the microstructural refinement and a shift in the magnetization reversal mechanism toward dominant domain‑wall pinning. Recoil loop measurements further confirm that Nb doping strengthens the intergranular exchange coupling. This work demonstrates that Nb doping is a feasible and efficient approach for producing cost-effective, high-performance permanent magnets with low rare-earth content.
- 13 March 2026
- Published by Kaunas University of Technology (KTU) in Materials Science
Open AccessNb-doping Induced High Coercivity in Pr2Fe14B/α-Fe Nanocomposite Melt-spun Ribbons
The effect of niobium (Nb) doping on the microstructure and magnetic properties of as-spun Pr10Fe82.5-xB6.5Nbx ribbons was investigated. Nb doping significantly refines the grain size and enhances the coercivity, which increases from 380 kA/m (x = 0) to a remarkable 990 kA/m (x = 3), a top-level performance among Nb‑doped rare-earth-deficient nanocomposite alloys. The improvement is attributed to the microstructural refinement and a shift in the magnetization reversal mechanism toward dominant domain‑wall pinning. Recoil loop measurements further confirm that Nb doping strengthens the intergranular exchange coupling. This work demonstrates that Nb doping is a feasible and efficient approach for producing cost-effective, high-performance permanent magnets with low rare-earth content.
- Open Access
- 15 December 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 138 (23)
Asymmetric modulation of photorefractive space-charge fields formation: Theory and experimental validation
The asymmetric modulation of light-induced space-charge fields by axial beam motion (v→∥opticalaxis) in Ce:SBN crystals was investigated through coupled theory-experiment approaches. Theoretically, introducing a direction-sensitive velocity term into the Kukhtarev equations yields analytical solutions that reveal electric field enhancement (v→0) due to asymmetric carrier accumulation, with the critical velocity v→c=μE→0 defining the threshold for dominance of these effects. Experimentally, 0.03 wt. % Ce:SBN demonstrates 81.8% diffraction efficiency gain under reverse motion vs 37.6% reduction in forward motion, while 0.1 wt. % crystals exhibit direction-triggered self-focusing, defocusing, and asymmetric oscillation. The unexpected dielectric breakdown observed at relatively high forward beam velocities (v→>0) directly confirms the simultaneous decay of the space-charge field and amplification of the external field. Theoretical predictions exhibited remarkable concordance with experimental observations, validating the proposed physical model. These findings establish a “velocity–direction–field” co-design paradigm enabling high-speed reconfigurable photonic devices.
- 15 December 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 138 (23)
Open AccessAsymmetric modulation of photorefractive space-charge fields formation: Theory and experimental validation
The asymmetric modulation of light-induced space-charge fields by axial beam motion (v→∥opticalaxis) in Ce:SBN crystals was investigated through coupled theory-experiment approaches. Theoretically, introducing a direction-sensitive velocity term into the Kukhtarev equations yields analytical solutions that reveal electric field enhancement (v→0) due to asymmetric carrier accumulation, with the critical velocity v→c=μE→0 defining the threshold for dominance of these effects. Experimentally, 0.03 wt. % Ce:SBN demonstrates 81.8% diffraction efficiency gain under reverse motion vs 37.6% reduction in forward motion, while 0.1 wt. % crystals exhibit direction-triggered self-focusing, defocusing, and asymmetric oscillation. The unexpected dielectric breakdown observed at relatively high forward beam velocities (v→>0) directly confirms the simultaneous decay of the space-charge field and amplification of the external field. Theoretical predictions exhibited remarkable concordance with experimental observations, validating the proposed physical model. These findings establish a “velocity–direction–field” co-design paradigm enabling high-speed reconfigurable photonic devices.
- 1 October 2025
- Published by American Physical Society (APS) in Physical Review B
- Vol. 112 (14)
Fractal properties and tunable flat band structures in chiral magnonic quasicrystals
- 1 October 2025
- Published by American Physical Society (APS) in Physical Review B
- Vol. 112 (14)
Fractal properties and tunable flat band structures in chiral magnonic quasicrystals
- 1 March 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 126 (12)
Orbital torque in Mn/FM bilayer systems
We investigate the orbital torque generated in ferromagnetic (FM)/manganese (Mn) bilayer systems based on angular-dependent spin-torque ferromagnetic resonance (ST-FMR) experiments. From the ST-FMR results, it is found that a relatively large out-of-plane anti-damping torque can be obtained in Ni/Mn bilayers. The Gilbert damping constant, derived from the resonant linewidth of frequency-dependent ST-FMR experiments, decreases almost linearly with increasing thickness of Mn, further indicating the out-of-plane anti-damping torque in Ni/Mn bilayer systems. The origin of this torque can be attributed to the orbital Rashba–Edelstein effect. Furthermore, the orbital diffusion length (λL) in Mn is determined to be more than 17 nm and larger than spin diffusion length, suggesting that the torque observed in our sample is predominantly influenced by the orbital-related effect. Finally, the insertion of Pt in a Ni/Mn bilayer system significantly enhances the orbital-to-spin conversion efficiency. These results clearly demonstrate that Mn is a promising material for future orbitronics devices.
- 1 March 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 126 (12)
Orbital torque in Mn/FM bilayer systems
We investigate the orbital torque generated in ferromagnetic (FM)/manganese (Mn) bilayer systems based on angular-dependent spin-torque ferromagnetic resonance (ST-FMR) experiments. From the ST-FMR results, it is found that a relatively large out-of-plane anti-damping torque can be obtained in Ni/Mn bilayers. The Gilbert damping constant, derived from the resonant linewidth of frequency-dependent ST-FMR experiments, decreases almost linearly with increasing thickness of Mn, further indicating the out-of-plane anti-damping torque in Ni/Mn bilayer systems. The origin of this torque can be attributed to the orbital Rashba–Edelstein effect. Furthermore, the orbital diffusion length (λL) in Mn is determined to be more than 17 nm and larger than spin diffusion length, suggesting that the torque observed in our sample is predominantly influenced by the orbital-related effect. Finally, the insertion of Pt in a Ni/Mn bilayer system significantly enhances the orbital-to-spin conversion efficiency. These results clearly demonstrate that Mn is a promising material for future orbitronics devices.
- 10 February 2025
- Published by American Physical Society (APS) in Physical Review Applied
- Vol. 23 (2)
Flat band structure in chiral magnonic crystals with tunable indirect band gaps
- 10 February 2025
- Published by American Physical Society (APS) in Physical Review Applied
- Vol. 23 (2)
Flat band structure in chiral magnonic crystals with tunable indirect band gaps
- 22 December 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 222 (8)
High Coercivity and Strong [00l] Crystallographic Texture in Sm(CoFeCuZr)7.4 Nanoflakes Prepared by Surfactant‐Assisted Ball Milling
Sm(Co0.61Fe0.21Cu0.13Zr0.05)7.4 nanoflakes are prepared by surfactant‐assisted ball milling from annealed ingots, and the ingots are synthesized by the arc‐melting process. The X‐ray diffraction (XRD) patterns of nanoflakes exhibit two hard magnetic phases: Sm2Co17 is the primary hard phase, which provides high saturation magnetization, and SmCo5 acts as a minor hard phase, presumably impeding the movement of magnetic domain walls, thereby increasing intrinsic coercivity. The high coercivity value of 7.2 kOe is achieved after 0.5 h ball milling. In addition, the XRD patterns of nanoflakes at different milling times show a strong [00l] crystallographic texture after the magnetic alignment. A remanence value of 1.03 T and a maximum energy product of 123 kJ m−3 achieve in 0.5 h milled nanoflakes. The aligned nanoflakes show strong anisotropic behavior with a degree of anisotropy value of 0.81. Henkel plots indicate the strong exchange coupling interaction in nanoflakes milled for 0.5 h. Based on the analysis of temperature‐dependent hysteresis loops and initial magnetization curves, the coercivity is controlled by the pinning of domain wall movement and the nucleation of the reverse domains.
- 22 December 2024
- Published by Wiley in Physica Status Solidi (a)
- Vol. 222 (8)
High Coercivity and Strong [00l] Crystallographic Texture in Sm(CoFeCuZr)7.4 Nanoflakes Prepared by Surfactant‐Assisted Ball Milling
Sm(Co0.61Fe0.21Cu0.13Zr0.05)7.4 nanoflakes are prepared by surfactant‐assisted ball milling from annealed ingots, and the ingots are synthesized by the arc‐melting process. The X‐ray diffraction (XRD) patterns of nanoflakes exhibit two hard magnetic phases: Sm2Co17 is the primary hard phase, which provides high saturation magnetization, and SmCo5 acts as a minor hard phase, presumably impeding the movement of magnetic domain walls, thereby increasing intrinsic coercivity. The high coercivity value of 7.2 kOe is achieved after 0.5 h ball milling. In addition, the XRD patterns of nanoflakes at different milling times show a strong [00l] crystallographic texture after the magnetic alignment. A remanence value of 1.03 T and a maximum energy product of 123 kJ m−3 achieve in 0.5 h milled nanoflakes. The aligned nanoflakes show strong anisotropic behavior with a degree of anisotropy value of 0.81. Henkel plots indicate the strong exchange coupling interaction in nanoflakes milled for 0.5 h. Based on the analysis of temperature‐dependent hysteresis loops and initial magnetization curves, the coercivity is controlled by the pinning of domain wall movement and the nucleation of the reverse domains.
- 30 October 2024
- Published by IOP Publishing in Chinese Physics B
- Vol. 33 (12)
Cu-doped nanocomposite Pr2Fe14B/α-Fe ribbons with high (BH)max
The melt-spun ribbons of nominal composition Pr9Fe84.2-xB6.2P0.3Zr0.3Cux (x=0, 0.5, 1, 2) were prepared at wheel speeds of 21, 27, 30, and 33 ms-1. The XRD patterns show that as the wheel speed increases, the crystallinity of the 2:14:1 hard phase decreases, while that of the α-Fe soft phase increases. The (BH)max, remanence, and coercivity are improved from 63 kJm-3, 0.85 T, and 515 kAm-1 for the Cu-free ribbons to 171 kJm-3, 1.08 T, and 684 kAm-1 with x=0.5. The high squareness ratio of Jr/Js ~ 0.82 at 0.5 at. % Cu (27 ms-1) indicates strong exchange coupling due to small grain sizes of 15 and 30 nm for soft and hard magnetic phases, respectively. The SEM images revealed smooth morphology and uniform element distribution at 0.5 at. % Cu (27 ms-1), contributing to the high magnetic properties. The low recoil permeability (μ rec ) value of 5.466×10-4 to 1.970×10-4 $\frac{T}{k A m^{-1}}$ confirms the strong exchange coupling with x=0.5 (27 ms-1). The initial magnetization curves show that the coercivity mechanism of the Cu-free alloy evolves from the nucleation of the reverse domain to the domain wall pinning as the wheel speed increases, resulting in a high coercivity value of 818 kAm-1 (33 ms-1). Conversely, for the Cuadded alloy, the coercivity mechanism changes from pinning to the nucleation of the reverse domain from low to high wheel speed.- 30 October 2024
- Published by IOP Publishing in Chinese Physics B
- Vol. 33 (12)
Cu-doped nanocomposite Pr2Fe14B/α-Fe ribbons with high (BH)max
The melt-spun ribbons of nominal composition Pr9Fe84.2-xB6.2P0.3Zr0.3Cux (x=0, 0.5, 1, 2) were prepared at wheel speeds of 21, 27, 30, and 33 ms-1. The XRD patterns show that as the wheel speed increases, the crystallinity of the 2:14:1 hard phase decreases, while that of the α-Fe soft phase increases. The (BH)max, remanence, and coercivity are improved from 63 kJm-3, 0.85 T, and 515 kAm-1 for the Cu-free ribbons to 171 kJm-3, 1.08 T, and 684 kAm-1 with x=0.5. The high squareness ratio of Jr/Js ~ 0.82 at 0.5 at. % Cu (27 ms-1) indicates strong exchange coupling due to small grain sizes of 15 and 30 nm for soft and hard magnetic phases, respectively. The SEM images revealed smooth morphology and uniform element distribution at 0.5 at. % Cu (27 ms-1), contributing to the high magnetic properties. The low recoil permeability (μ rec ) value of 5.466×10-4 to 1.970×10-4 $\frac{T}{k A m^{-1}}$ confirms the strong exchange coupling with x=0.5 (27 ms-1). The initial magnetization curves show that the coercivity mechanism of the Cu-free alloy evolves from the nucleation of the reverse domain to the domain wall pinning as the wheel speed increases, resulting in a high coercivity value of 818 kAm-1 (33 ms-1). Conversely, for the Cuadded alloy, the coercivity mechanism changes from pinning to the nucleation of the reverse domain from low to high wheel speed.