Kei Sawata
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Kei Sawata has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
Yoshihisa Sasaki
Research Faculty of Agriculture, Hokkaido University, Sapporo, Japan
13 shared publicationsAkio Koizumi
Hokkaido University
5 shared publicationsTakanobu Sasaki
Research Faculty of Agriculture, Hokkaido University, Sapporo, Japan
5 shared publicationsTakuro Hirai
Hokkaido University
5 shared publicationsOkumu Gordon Wanyama
Hokkaido University
3 shared publicationsRintaro Ueda
Gifu Academy of Forest Science and Culture, Mino, Japan
3 shared publications
Latest Publications
- 16 July 2024
- Published by Taylor & Francis in Journal of Forest Research
- Vol. 29 (6) , 425-431
Regional variation in branch morphological and physical traits in Abies sachalinensis associated with winter climatic conditions
- 16 July 2024
- Published by Taylor & Francis in Journal of Forest Research
- Vol. 29 (6) , 425-431
Regional variation in branch morphological and physical traits in Abies sachalinensis associated with winter climatic conditions
- Open Access
- 16 April 2023
- Published by Springer Nature in International Journal of Civil Engineering
- Vol. 21 (8) , 1305-1314
Experimental Investigation on Bonded and Screwed Carbon Fiber-Reinforced Plastic Plates on Timber Column–Sill Joints
In this study, timber column–sill joints strengthened with carbon fiber-reinforced plastic (CFRP) plates using bonds and screws were subjected to loading tests. Twelve joint specifications were considered depending on different combinations of the CFRP plate surface finish and thickness and the type of bond, and the corresponding effects on the load–displacement behavior of the joints were investigated. Three failure modes were observed in addition to the peeling of the CFRP plate. The specimens that failed owing to screw tear out and screw head pull-through in the CFRP plate or splitting of the sill showed load–displacement curves of a similar shape. Those that failed owing to buckling of the CFRP plate showed a rapid and substantial load decrease due to failure. This failure mode was only observed in 0.50 mm thick CFRP plate specimens. When a peel-ply CFRP plate was installed in the column–sill joint specimens, similar secant stiffnesses were observed in the silicon and epoxy resin-bonded specimens, both with high shear strength. Although the specimens with bonds with a high shear strength showed lower deformation performance, the specimens' maximum load increased with the bond's shear strength. The maximum load improved for a 0.75 mm thick peel-ply silicon- or epoxy-bonded CFRP plate. The load's maximum value after peeling the CFRP plate was 0.79–1.23 times as large as the maximum load of the no-bond specimens and did not change significantly.
- 16 April 2023
- Published by Springer Nature in International Journal of Civil Engineering
- Vol. 21 (8) , 1305-1314
Open AccessExperimental Investigation on Bonded and Screwed Carbon Fiber-Reinforced Plastic Plates on Timber Column–Sill Joints
In this study, timber column–sill joints strengthened with carbon fiber-reinforced plastic (CFRP) plates using bonds and screws were subjected to loading tests. Twelve joint specifications were considered depending on different combinations of the CFRP plate surface finish and thickness and the type of bond, and the corresponding effects on the load–displacement behavior of the joints were investigated. Three failure modes were observed in addition to the peeling of the CFRP plate. The specimens that failed owing to screw tear out and screw head pull-through in the CFRP plate or splitting of the sill showed load–displacement curves of a similar shape. Those that failed owing to buckling of the CFRP plate showed a rapid and substantial load decrease due to failure. This failure mode was only observed in 0.50 mm thick CFRP plate specimens. When a peel-ply CFRP plate was installed in the column–sill joint specimens, similar secant stiffnesses were observed in the silicon and epoxy resin-bonded specimens, both with high shear strength. Although the specimens with bonds with a high shear strength showed lower deformation performance, the specimens' maximum load increased with the bond's shear strength. The maximum load improved for a 0.75 mm thick peel-ply silicon- or epoxy-bonded CFRP plate. The load's maximum value after peeling the CFRP plate was 0.79–1.23 times as large as the maximum load of the no-bond specimens and did not change significantly.
- Open Access
- 1 January 2023
- Published by Japan Society of Civil Engineers in Japanese Journal of JSCE
- Vol. 79 (28) , 22-28003
CLT床版を用いた林道橋の補修設計と解析
CLT(直交集成板)はその軽さの特徴から土木分野への利用も期待されている。例えば、既設橋梁の劣化したコンクリート床板を取替える際に、軽量なCLTで代替することができれば、コンクリート床板の増厚に伴う重量増加に対応するための鋼桁の補強が不要となり、安価に改修を行うことができる可能性がある。本研究では、床版取替の補修工事が計画されている北海道内の林道橋を対象に、CLT床版への取替えにの可能性について、有限要素法を用いた解析により検討した。
- 1 January 2023
- Published by Japan Society of Civil Engineers in Japanese Journal of JSCE
- Vol. 79 (28) , 22-28003
Open AccessCLT床版を用いた林道橋の補修設計と解析
CLT(直交集成板)はその軽さの特徴から土木分野への利用も期待されている。例えば、既設橋梁の劣化したコンクリート床板を取替える際に、軽量なCLTで代替することができれば、コンクリート床板の増厚に伴う重量増加に対応するための鋼桁の補強が不要となり、安価に改修を行うことができる可能性がある。本研究では、床版取替の補修工事が計画されている北海道内の林道橋を対象に、CLT床版への取替えにの可能性について、有限要素法を用いた解析により検討した。
- 25 October 2022
- Published by Japan Wood Society in Mokuzai Gakkaishi
- Vol. 68 (4) , 179-187
Evaluation of Out-of-plane Shear Strength of CLT made from Japanese Larch
カラマツ3層3プライ直交集成板(CLT)に対して3種類のせん断試験を実施し,試験方法がCLTのせん断強度に与える影響と,CLTの直交層を構成するラミナの欠点および幅はぎ接着がせん断強度に与える影響を調べた。その結果,3点曲げ破壊試験と逆対称4点曲げ破壊試験間でせん断強度に差は見られなかったが,圧縮型試験から得られたせん断強度は3点曲げ破壊試験で得られた値と比較して低い値を示した。ラミナの節や幅はぎ接着の存在によるせん断強度への影響は確認されなかった。モンテカルロシミュレーションによって直交層の破壊程度とCLTの最大せん断耐力の関係を調べた結果,CLTの最大せん断耐力は複数枚の直交層ラミナが順次破壊して決定されることが明らかとなった。
- 25 October 2022
- Published by Japan Wood Society in Mokuzai Gakkaishi
- Vol. 68 (4) , 179-187
Evaluation of Out-of-plane Shear Strength of CLT made from Japanese Larch
カラマツ3層3プライ直交集成板(CLT)に対して3種類のせん断試験を実施し,試験方法がCLTのせん断強度に与える影響と,CLTの直交層を構成するラミナの欠点および幅はぎ接着がせん断強度に与える影響を調べた。その結果,3点曲げ破壊試験と逆対称4点曲げ破壊試験間でせん断強度に差は見られなかったが,圧縮型試験から得られたせん断強度は3点曲げ破壊試験で得られた値と比較して低い値を示した。ラミナの節や幅はぎ接着の存在によるせん断強度への影響は確認されなかった。モンテカルロシミュレーションによって直交層の破壊程度とCLTの最大せん断耐力の関係を調べた結果,CLTの最大せん断耐力は複数枚の直交層ラミナが順次破壊して決定されることが明らかとなった。
- 16 September 2022
- Published by Springer Nature in European Journal of Wood and Wood Products
- Vol. 81 (1) , 111-124
Elastoplastic performance of wood under compression load considering cross-grain orientation and moisture content
- 16 September 2022
- Published by Springer Nature in European Journal of Wood and Wood Products
- Vol. 81 (1) , 111-124
Elastoplastic performance of wood under compression load considering cross-grain orientation and moisture content
- Open Access
- 15 December 2021
- Published by Springer Nature in Journal of Wood Science
- Vol. 67 (1) , 1-9
Effects of decay on the shear properties of nailed joints parallel and perpendicular to the grain
Information on the properties of nailed joints with decayed member is necessary to evaluate the remaining structural properties of timber constructions. In this study, loading tests were conducted on nailed joints parallel and perpendicular to the grain with decayed members, and the relationship between the decrease in shear properties and the loading direction to the grain was investigated. After the loading tests, the extent of decay of the specimens was evaluated by the penetration depth of Pilodyn and the decay depth, and these were compared with the shear properties of the nailed joints. The nailed joints with decay had a low load at the initial deformation, regardless of the loading direction to the grain. The initial stiffness, yield resistance, and maximum resistance of the nailed joints parallel to the grain were negatively correlated with the Pilodyn penetration depth, and those of the nailed joints perpendicular to the grain showed no significant correlation with the Pilodyn penetration depth at the 5% level. The initial stiffness, yield resistance, and maximum resistance of the nailed joints parallel to the grain tended to decrease with increasing decay depth, and those of the nailed joints perpendicular to the grain did not exhibit this tendency. The shear properties of the nailed joints significantly decreased at small decay depths.
- 15 December 2021
- Published by Springer Nature in Journal of Wood Science
- Vol. 67 (1) , 1-9
Open AccessEffects of decay on the shear properties of nailed joints parallel and perpendicular to the grain
Information on the properties of nailed joints with decayed member is necessary to evaluate the remaining structural properties of timber constructions. In this study, loading tests were conducted on nailed joints parallel and perpendicular to the grain with decayed members, and the relationship between the decrease in shear properties and the loading direction to the grain was investigated. After the loading tests, the extent of decay of the specimens was evaluated by the penetration depth of Pilodyn and the decay depth, and these were compared with the shear properties of the nailed joints. The nailed joints with decay had a low load at the initial deformation, regardless of the loading direction to the grain. The initial stiffness, yield resistance, and maximum resistance of the nailed joints parallel to the grain were negatively correlated with the Pilodyn penetration depth, and those of the nailed joints perpendicular to the grain showed no significant correlation with the Pilodyn penetration depth at the 5% level. The initial stiffness, yield resistance, and maximum resistance of the nailed joints parallel to the grain tended to decrease with increasing decay depth, and those of the nailed joints perpendicular to the grain did not exhibit this tendency. The shear properties of the nailed joints significantly decreased at small decay depths.
- Open Access
Effects of Moisture Content and Grain Direction on the Elastic Properties of Beech Wood Based on Experiment and Finite Element Method
Beech wood (Fagus sylvatica L.) is used in a wide range of wood products. However, the influence of the wood’s moisture content on its mechanical functions will affect its structural strength. It would be complicated and time-consuming to experimentally measure wood’s mechanical functions under different moisture contents. Therefore, it is necessary to establish a prediction formula between the moisture content and elastic constants, and then verify whether its mechanical functions within a wide range of moisture content can be studied by using FEM (finite element method). In this study, which was based on experimentation, we studied the influence of a wide range of moisture contents and grain direction on the compressive yield strength, modulus of elasticity and shear modulus of beech wood. The relationship between the moisture content and elastic constants was established; the moisture sensitivities of different elastic parameters were obtained. Ultimately, compression curves under different moisture contents were plotted out, using both FEM and experimentation. According to the results, the interaction of moisture with the grain direction had a significant effect on the elastic constants of wood, with grain direction having a greater effect on the elastic properties than the moisture content. Moreover, the decay function can be used to fit these experimental results well. The elastic constants of beech wood responded differently to the moisture content, depending on whether it was in the longitude or transverse directions. Finally, this study proved the feasibility of using FEM to simulate wood’s compressive performance with a wide range of moisture contents.
Open AccessEffects of Moisture Content and Grain Direction on the Elastic Properties of Beech Wood Based on Experiment and Finite Element Method
Beech wood (Fagus sylvatica L.) is used in a wide range of wood products. However, the influence of the wood’s moisture content on its mechanical functions will affect its structural strength. It would be complicated and time-consuming to experimentally measure wood’s mechanical functions under different moisture contents. Therefore, it is necessary to establish a prediction formula between the moisture content and elastic constants, and then verify whether its mechanical functions within a wide range of moisture content can be studied by using FEM (finite element method). In this study, which was based on experimentation, we studied the influence of a wide range of moisture contents and grain direction on the compressive yield strength, modulus of elasticity and shear modulus of beech wood. The relationship between the moisture content and elastic constants was established; the moisture sensitivities of different elastic parameters were obtained. Ultimately, compression curves under different moisture contents were plotted out, using both FEM and experimentation. According to the results, the interaction of moisture with the grain direction had a significant effect on the elastic constants of wood, with grain direction having a greater effect on the elastic properties than the moisture content. Moreover, the decay function can be used to fit these experimental results well. The elastic constants of beech wood responded differently to the moisture content, depending on whether it was in the longitude or transverse directions. Finally, this study proved the feasibility of using FEM to simulate wood’s compressive performance with a wide range of moisture contents.
- Open Access
- 29 May 2020
- Published by Springer Nature in Journal of Wood Science
- Vol. 66 (1) , 1-11
Degradation of shear performance of screwed joints caused by wood decay
Shear tests were conducted on screwed joints with decayed main members, and the degradation of shear performance of screwed joints by wood decay was investigated. The differences between decayed and control specimens in yield load (Py), and maximum load (Pmax) were both significant at the 1% level, while the difference in the initial stiffness (Ks) was not significant at the 5% level. The extent of decay was evaluated through Pilodyn penetration depth and the decay depth. Pilodyn penetration depth had no significant relationships with Ks, Py, or Pmax of screwed joints. It is inferred that no significant relationship was found between Pilodyn penetration depth and the strength properties because the range of the measured Pilodyn penetration depth was narrow (16–23.5 mm). The decay depth had a significant inverse correlation with Ks of the decayed specimens. There was no significant relationship between the decay depth and Py, or Pmax. Multiple regression analysis was conducted on Ks, Py, and Pmax using the decay depth and sound wood density (WDh) as 2 explanatory variables. The multiple regression of Ks, Py, and Pmax on the decay depth and WDh were significant at the 1%, 5%, and 1% level, respectively. Ks, Py, and Pmax are inferred to be determined by both the decay depth and WDh. The strength properties of screwed joints with one screw obtained in this study were compared with those of screwed joints with seven screws obtained in a previous study. The difference between Ks, Py, and Pmax of the screwed joints with one screw and those of the screwed joints with seven screws was not significant at the 5% level. It is inferred that shear performance of screw joints with multiple screws are sufficiently estimated from those of screw joints with one screw by simply multiplying the strength properties, even if the main members were decayed.
- 29 May 2020
- Published by Springer Nature in Journal of Wood Science
- Vol. 66 (1) , 1-11
Open AccessDegradation of shear performance of screwed joints caused by wood decay
Shear tests were conducted on screwed joints with decayed main members, and the degradation of shear performance of screwed joints by wood decay was investigated. The differences between decayed and control specimens in yield load (Py), and maximum load (Pmax) were both significant at the 1% level, while the difference in the initial stiffness (Ks) was not significant at the 5% level. The extent of decay was evaluated through Pilodyn penetration depth and the decay depth. Pilodyn penetration depth had no significant relationships with Ks, Py, or Pmax of screwed joints. It is inferred that no significant relationship was found between Pilodyn penetration depth and the strength properties because the range of the measured Pilodyn penetration depth was narrow (16–23.5 mm). The decay depth had a significant inverse correlation with Ks of the decayed specimens. There was no significant relationship between the decay depth and Py, or Pmax. Multiple regression analysis was conducted on Ks, Py, and Pmax using the decay depth and sound wood density (WDh) as 2 explanatory variables. The multiple regression of Ks, Py, and Pmax on the decay depth and WDh were significant at the 1%, 5%, and 1% level, respectively. Ks, Py, and Pmax are inferred to be determined by both the decay depth and WDh. The strength properties of screwed joints with one screw obtained in this study were compared with those of screwed joints with seven screws obtained in a previous study. The difference between Ks, Py, and Pmax of the screwed joints with one screw and those of the screwed joints with seven screws was not significant at the 5% level. It is inferred that shear performance of screw joints with multiple screws are sufficiently estimated from those of screw joints with one screw by simply multiplying the strength properties, even if the main members were decayed.
- Open Access
- 27 November 2018
- Published by Springer Nature in Journal of Wood Science
- Vol. 64 (6) , 882
Correction to: Effect of decay on shear performance of dowel-type timber joints
- 27 November 2018
- Published by Springer Nature in Journal of Wood Science
- Vol. 64 (6) , 882
Open AccessCorrection to: Effect of decay on shear performance of dowel-type timber joints
- 6 June 2018
- Published by Springer Nature in Journal of Wood Science
- Vol. 64 (5) , 601-611
Lateral strength of nailed timber connections with decay
- 6 June 2018
- Published by Springer Nature in Journal of Wood Science
- Vol. 64 (5) , 601-611
Lateral strength of nailed timber connections with decay