Gholam Hossein Borhani
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Gholam Hossein Borhani has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Hassan Sheikh
Department of Materials Science and Engineering, Shiraz University, Shiraz University, Shiraz, 71946-84636
2 shared publicationsSaeed Reza Bakhshi
Department of Materials Engineering, Malek-Ashtar University of Technology, Isfahan
2 shared publications- Saeed Reza Bakhshi
Malek Ashtar University of Technology
2 shared publications - Ali Ghasemi
Power Plant Control Engineering Management, MAPNA Electric & Control Engineering & Manufacturing Company (MECO), Karaj, Iran
1 shared publication - Ali Hedayati
Energy Safety Research Institute, Swansea University, Bay Campus, Swansea SA1 8EN, UK
1 shared publication E. Haghshenas Jazi
Department of Materials Engineering, Faculty of Mechanical Engineering, K.N. Toosi University of Technology, No. 17, Pardis St, Molasadra Ave., Vanaq Square, Tehran, Iran
1 shared publication
Latest Publications
- 12 June 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (8) , 0865h5
Development of high densified tantalum-tungsten alloy by powder metallurgy route
In this study, Ta and premixed Ta-3wt%W powders were consolidated through spark plasma sintering (SPS) and hot pressing (HP) techniques at 2200 and 2000°C, respectively. After density measurements, the samples were heat treated at 1100°C for 4 hours in vacuum atmosphere. The high densified PM tantalum and tantalum alloy were subjected to X-ray diffraction (XRD) examination, hardness, and Split Hopkinson Pressure Bar (SHPB) testing. The decrease in lattice parameter measurement of Ta-3wt%W composition showed the alloying process has taken place during heat treatment procedure. The microstructure and hardness testing showed the uniform distribution of W within Ta-3wt%W samples. The dynamic compressive yield strengths were 2203 and 2156 MPa for Ta-3wt%W samples produced by HP and SPS, respectively. Also, the heat treatment improved ductility while high strength was maintained.
- 12 June 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (8) , 0865h5
Development of high densified tantalum-tungsten alloy by powder metallurgy route
In this study, Ta and premixed Ta-3wt%W powders were consolidated through spark plasma sintering (SPS) and hot pressing (HP) techniques at 2200 and 2000°C, respectively. After density measurements, the samples were heat treated at 1100°C for 4 hours in vacuum atmosphere. The high densified PM tantalum and tantalum alloy were subjected to X-ray diffraction (XRD) examination, hardness, and Split Hopkinson Pressure Bar (SHPB) testing. The decrease in lattice parameter measurement of Ta-3wt%W composition showed the alloying process has taken place during heat treatment procedure. The microstructure and hardness testing showed the uniform distribution of W within Ta-3wt%W samples. The dynamic compressive yield strengths were 2203 and 2156 MPa for Ta-3wt%W samples produced by HP and SPS, respectively. Also, the heat treatment improved ductility while high strength was maintained.
- 10 May 2019
- Published by SAGE Publications in Powder Metallurgy
- Vol. 62 (3) , 162-168
Investigation on microstructure and high strain rate behaviour of pure tantalum prepared by hot press and subsequent annealing treatment
Among refractory metals, tantalum has long been the primary material of use in high strain rate applications. Hot pressing (HP) is a technique to produce specimens with high density and homogeneous microstructure. The individual effect of the HP or annealing heat treatment on high strain rate properties of tantalum powder compacts has been investigated, but little attention has been paid to the combined effect of subsequent annealing. In this study, the effect of annealing on the microstructure and mechanical properties of tantalum subjected to hardness and Split Pressure Hopkinson Bar (SHPB) test was investigated. After annealing at 1100°C, the grains are coarsened, thereby hardness and upper yield strength decreased to value 199 VHN and 1833 MPa, respectively. Moreover, an obvious increase in plasticity and toughness is detected at this temperature, indicating subsequent annealing is beneficial to improve the deformation properties of HPed powder compacts; the maximum plasticity of tantalum was 31.74% after annealing.
- 10 May 2019
- Published by SAGE Publications in Powder Metallurgy
- Vol. 62 (3) , 162-168
Investigation on microstructure and high strain rate behaviour of pure tantalum prepared by hot press and subsequent annealing treatment
Among refractory metals, tantalum has long been the primary material of use in high strain rate applications. Hot pressing (HP) is a technique to produce specimens with high density and homogeneous microstructure. The individual effect of the HP or annealing heat treatment on high strain rate properties of tantalum powder compacts has been investigated, but little attention has been paid to the combined effect of subsequent annealing. In this study, the effect of annealing on the microstructure and mechanical properties of tantalum subjected to hardness and Split Pressure Hopkinson Bar (SHPB) test was investigated. After annealing at 1100°C, the grains are coarsened, thereby hardness and upper yield strength decreased to value 199 VHN and 1833 MPa, respectively. Moreover, an obvious increase in plasticity and toughness is detected at this temperature, indicating subsequent annealing is beneficial to improve the deformation properties of HPed powder compacts; the maximum plasticity of tantalum was 31.74% after annealing.
- 3 April 2017
- Published by World Scientific Pub Co Pte Ltd in Functional Materials Letters
- Vol. 10 (02) , 1750003
Sintering and kinetic mechanism of Si3N4-SiC micro-nano composite by spark plasma sintering
Si3N4–SiC composites were fabricated by spark plasma sintering at 1700[ ]C for 480 S with MgSiN2 and Y2O3 as additives. The morphology and phase characterization of the composites were characterized using scanning electron microscopy (SEM) and X-ray diffraction (XRD). The values of [ ] parameter indicate that the grain boundary reaction is the rate controller at 1500[ ]C and diffusion becomes the controlling step at 1550[ ]C. The nanohardness and Young’s modulus attained the maximum value of 18.5 and 316[ ]GPa, respectively.
- 3 April 2017
- Published by World Scientific Pub Co Pte Ltd in Functional Materials Letters
- Vol. 10 (02) , 1750003
Sintering and kinetic mechanism of Si3N4-SiC micro-nano composite by spark plasma sintering
Si3N4–SiC composites were fabricated by spark plasma sintering at 1700[ ]C for 480 S with MgSiN2 and Y2O3 as additives. The morphology and phase characterization of the composites were characterized using scanning electron microscopy (SEM) and X-ray diffraction (XRD). The values of [ ] parameter indicate that the grain boundary reaction is the rate controller at 1500[ ]C and diffusion becomes the controlling step at 1550[ ]C. The nanohardness and Young’s modulus attained the maximum value of 18.5 and 316[ ]GPa, respectively.
- Open Access
- 1 December 2016
- Published by CASRP: Center of Advanced Scientific Research and Publications in Journal of Advanced Materials In Engineering
- Vol. 35 (3) , 1-12
Synthesis and Characterization of Hybrid Silica-Zirconia Coatings with Cerium Inhibitor on Aluminum 6061
- 1 December 2016
- Published by CASRP: Center of Advanced Scientific Research and Publications in Journal of Advanced Materials In Engineering
- Vol. 35 (3) , 1-12
Open AccessSynthesis and Characterization of Hybrid Silica-Zirconia Coatings with Cerium Inhibitor on Aluminum 6061
- 31 May 2012
- Published by Institution of Engineering and Technology (IET) in Micro & Nano Letters
- Vol. 7 (5) , 448-452
Preparation of Al–Fe/TiB 2 nanocomposite powder by ball milling and subsequent heat treatment
In this study, mechanical alloying (MA) was used to synthesise Al–Fe/TiB2 nanocomposites using aluminium, ferrotitanium and acid boric as raw materials. The powders were mixed and subjected to MA in an attritor ball mill under argon (Ar) atmosphere. Then, the milled powders were heat-treated under Ar atmosphere. The phase transformation, microstructure and morphology of MA powders were investigated by X-ray diffraction and scanning electron microscopy. The results showed that the heat-treated powders lead to the in situ formation of nanosized TiB2 particles in the Al matrix with an average grain size of 45 nm. It was also found that after heat-treating, TiB2 phase and other intermetallics such as Al13Fe4 and Al3Ti have been formed.
- 31 May 2012
- Published by Institution of Engineering and Technology (IET) in Micro & Nano Letters
- Vol. 7 (5) , 448-452
Preparation of Al–Fe/TiB 2 nanocomposite powder by ball milling and subsequent heat treatment
In this study, mechanical alloying (MA) was used to synthesise Al–Fe/TiB2 nanocomposites using aluminium, ferrotitanium and acid boric as raw materials. The powders were mixed and subjected to MA in an attritor ball mill under argon (Ar) atmosphere. Then, the milled powders were heat-treated under Ar atmosphere. The phase transformation, microstructure and morphology of MA powders were investigated by X-ray diffraction and scanning electron microscopy. The results showed that the heat-treated powders lead to the in situ formation of nanosized TiB2 particles in the Al matrix with an average grain size of 45 nm. It was also found that after heat-treating, TiB2 phase and other intermetallics such as Al13Fe4 and Al3Ti have been formed.
- 23 September 2011
- Published by Springer Nature in Powder Metallurgy and Metal Ceramics
- Vol. 50 (5-6) , 268-274
Effect of ball milling on formation of ZnAl2O4 by reduction reaction of ZnO and Al powder mixture
- 23 September 2011
- Published by Springer Nature in Powder Metallurgy and Metal Ceramics
- Vol. 50 (5-6) , 268-274
Effect of ball milling on formation of ZnAl2O4 by reduction reaction of ZnO and Al powder mixture