Francisco J. Chaparro
Francisco J. Chaparro has a total of 58 co-authors. Here are the top co-authors by number of shared publications:
- John Joseph Lannutti
Department of Materials Science and Engineering, The Ohio State University, Columbus, OH 43210, USA
4 shared publications John J. Lannutti
Department of Materials Science and Engineering, The Ohio State University, 2041 N. College Rd., Columbus, OH 43210, USA
2 shared publicationsKayla F. Presley
Air Force Research Laboratory Materials and Manufacturing Directorate Wright‐Patterson AFB Ohio USA
2 shared publicationsMarco A. Coutinho da Silva
Department of Veterinary Clinical Sciences, The Ohio State University, 601 Vernon Tharp St., Columbus, OH 43210, USA
2 shared publicationsT. Dull
2 shared publications- Yi-Xiao Liu
Department of Materials Science and Engineering, The Ohio State University, Columbus, OH, United States of America
2 shared publications
Latest Publications
- Open Access
- 9 March 2023
- Published by Public Library of Science (PLoS) in PLOS ONE
- Vol. 18 (3) , e0282903
Visualization of porosity and pore size gradients in electrospun scaffolds using laser metrology
We applied a recently developed method, laser metrology, to characterize the influence of collector rotation on porosity gradients of electrospun polycaprolactone (PCL) widely investigated for use in tissue engineering. The prior- and post-sintering dimensions of PCL scaffolds were compared to derive quantitative, spatially-resolved porosity ‘maps’ from net shrinkage. Deposited on a rotating mandrel (200 RPM), the central region of deposition reaches the highest porosity, ~92%, surrounded by approximately symmetrical decreases to ~89% at the edges. At 1100 RPM, a uniform porosity of ~88–89% is observed. At 2000 RPM, the lowest porosity, ~87%, is found in the middle of the deposition, rebounding to ~89% at the edges. Using a statistical model of random fiber network, we demonstrated that these relatively small changes in porosity values produce disproportionately large variations in pore size. The model predicts an exponential dependence of pore size on porosity when the scaffold is highly porous (e.g., >80%) and, accordingly, the observed porosity variation is associated with dramatic changes in pore size and ability to accommodate cell infiltration. Within the thickest regions most likely to ‘bottleneck’ cell infiltration, pore size decreases from ~37 to 23 μm (38%) when rotational speeds increased from 200 to 2000 RPM. This trend is corroborated by electron microscopy. While faster rotational speeds ultimately overcome axial alignment induced by cylindrical electric fields associated with the collector geometry, it does so at the cost of eliminating larger pores favoring cell infiltration. This puts the bio-mechanical advantages associated with collector rotation-induced alignment at odds with biological goals. A more significant decrease in pore size from ~54 to ~19 μm (65%), well below the minimum associated with cellular infiltration, is observed from enhanced collector biases. Finally, similar predictions show that sacrificial fiber approaches are inefficient in achieving cell-permissive pore sizes.
- 9 March 2023
- Published by Public Library of Science (PLoS) in PLOS ONE
- Vol. 18 (3) , e0282903
Open AccessVisualization of porosity and pore size gradients in electrospun scaffolds using laser metrology
We applied a recently developed method, laser metrology, to characterize the influence of collector rotation on porosity gradients of electrospun polycaprolactone (PCL) widely investigated for use in tissue engineering. The prior- and post-sintering dimensions of PCL scaffolds were compared to derive quantitative, spatially-resolved porosity ‘maps’ from net shrinkage. Deposited on a rotating mandrel (200 RPM), the central region of deposition reaches the highest porosity, ~92%, surrounded by approximately symmetrical decreases to ~89% at the edges. At 1100 RPM, a uniform porosity of ~88–89% is observed. At 2000 RPM, the lowest porosity, ~87%, is found in the middle of the deposition, rebounding to ~89% at the edges. Using a statistical model of random fiber network, we demonstrated that these relatively small changes in porosity values produce disproportionately large variations in pore size. The model predicts an exponential dependence of pore size on porosity when the scaffold is highly porous (e.g., >80%) and, accordingly, the observed porosity variation is associated with dramatic changes in pore size and ability to accommodate cell infiltration. Within the thickest regions most likely to ‘bottleneck’ cell infiltration, pore size decreases from ~37 to 23 μm (38%) when rotational speeds increased from 200 to 2000 RPM. This trend is corroborated by electron microscopy. While faster rotational speeds ultimately overcome axial alignment induced by cylindrical electric fields associated with the collector geometry, it does so at the cost of eliminating larger pores favoring cell infiltration. This puts the bio-mechanical advantages associated with collector rotation-induced alignment at odds with biological goals. A more significant decrease in pore size from ~54 to ~19 μm (65%), well below the minimum associated with cellular infiltration, is observed from enhanced collector biases. Finally, similar predictions show that sacrificial fiber approaches are inefficient in achieving cell-permissive pore sizes.
- Open Access
Manganese Oxide Loaded Carbon Fiber for Solar Energy Harvesting and Oil Decomposition
In this work, a manganese oxide electrode, containing carbon nanofiber composites (MnO2/CNF), has been made through electrospinning, oxidization, and partial carbonization high-temperature treatment. Scanning electron microscopy (SEM) was used to observe the morphology of the nanofiber and analyze the composition of the fiber. The fiber size range and element distribution were determined. The oxide nanoparticles were modeled as electrorheological suspensions in the polyacrylonitrile polymer solution during electrospinning. The dielectrophoretic behavior of the particles subjected to non-uniform electric fields were analyzed and the motion of the oxide particles under the actions from fluctuating electric fields was investigated to explain the sporadic distribution of nanoparticles within the composite nanofibers. A photoactive anode was made from the composite nanofiber and the decomposition of spilled oil was performed under sunlight illumination. It was observed that the manganese oxide containing carbon nanofiber composite electrode can generate electricity and clean the spilled oil under sunlight. Both energy conversion and environment cleaning concepts were demonstrated.
Open AccessManganese Oxide Loaded Carbon Fiber for Solar Energy Harvesting and Oil Decomposition
In this work, a manganese oxide electrode, containing carbon nanofiber composites (MnO2/CNF), has been made through electrospinning, oxidization, and partial carbonization high-temperature treatment. Scanning electron microscopy (SEM) was used to observe the morphology of the nanofiber and analyze the composition of the fiber. The fiber size range and element distribution were determined. The oxide nanoparticles were modeled as electrorheological suspensions in the polyacrylonitrile polymer solution during electrospinning. The dielectrophoretic behavior of the particles subjected to non-uniform electric fields were analyzed and the motion of the oxide particles under the actions from fluctuating electric fields was investigated to explain the sporadic distribution of nanoparticles within the composite nanofibers. A photoactive anode was made from the composite nanofiber and the decomposition of spilled oil was performed under sunlight illumination. It was observed that the manganese oxide containing carbon nanofiber composite electrode can generate electricity and clean the spilled oil under sunlight. Both energy conversion and environment cleaning concepts were demonstrated.
- Open Access
- 20 November 2020
- Published by Wiley in MEDICAL DEVICES & SENSORS
- Vol. 4 (1) , e10149
Biodegradable oxygen biosensors via electrospinning
Monitoring oxygenation in vivo is critical to ensuring human health, particularly in the context of ‘silent’ hypoxia. Utilizing blends of biodegradable polycaprolactone (PCL) and gelatine, we sought to develop an electrospun oxygen sensor that maintains the advantages of robust, phosphorescent oxygen‐sensing chromophores while providing resorbable polymeric scaffolds benefiting from tailorable degradation times ranging from hours to weeks. Electrospun sensors successfully provide accurate oxygen measurements for periods >1 month. In vitro testing took place in a custom aqueous testing system over five weeks in 37°C phosphate‐buffered saline (PBS); dissolved oxygen concentrations were maintained at 0–5% O2 where physoxia characteristic of the subdermal environment is defined as 2–5% O2. Excited state chromophore lifetime (τ) is quenched in the presence of dissolved diatomic oxygen and is influenced by characteristics of the surrounding matrix. The observed final deoxygenated τ (τ0) values were split into 3 groups: polysulphone (PSU)‐PCL (~397 µs) >75:25, 50:50 and 25:75 PCL:gelatine (~191–182 µs) > PCL, 10:90 PCL:gelatine, 1:99 crosslinked PCL:gelatine (~145–135 µs). Highly linear Stern–Volmer activity enabling accurate and precise calibration was observed even after 35 days of exposure; this proves that non‐core–shell fibres consisting of blends of PCL and gelatine can yield predictable lifetime values for >30 days in vitro. Scanning electron microscopy and mass loss data revealed that sensor degradation is highly tailorable, allowing for the fabrication of sensors engineered for a specific biomedical time frame. In contrast, core–shell fibre sensors showed more variability in lifetime following internal degradation likely caused by caproic acid entrapment by the PCL ‘shell’. This work demonstrates that biodegradable and biocompatible optically monitored sensors can be fabricated to provide direct, accurate assessments of oxygenation, even as the sensor platform degrades in a controlled manner. Such technologies have the potential to substantially change respiratory disease management.
- 20 November 2020
- Published by Wiley in MEDICAL DEVICES & SENSORS
- Vol. 4 (1) , e10149
Open AccessBiodegradable oxygen biosensors via electrospinning
Monitoring oxygenation in vivo is critical to ensuring human health, particularly in the context of ‘silent’ hypoxia. Utilizing blends of biodegradable polycaprolactone (PCL) and gelatine, we sought to develop an electrospun oxygen sensor that maintains the advantages of robust, phosphorescent oxygen‐sensing chromophores while providing resorbable polymeric scaffolds benefiting from tailorable degradation times ranging from hours to weeks. Electrospun sensors successfully provide accurate oxygen measurements for periods >1 month. In vitro testing took place in a custom aqueous testing system over five weeks in 37°C phosphate‐buffered saline (PBS); dissolved oxygen concentrations were maintained at 0–5% O2 where physoxia characteristic of the subdermal environment is defined as 2–5% O2. Excited state chromophore lifetime (τ) is quenched in the presence of dissolved diatomic oxygen and is influenced by characteristics of the surrounding matrix. The observed final deoxygenated τ (τ0) values were split into 3 groups: polysulphone (PSU)‐PCL (~397 µs) >75:25, 50:50 and 25:75 PCL:gelatine (~191–182 µs) > PCL, 10:90 PCL:gelatine, 1:99 crosslinked PCL:gelatine (~145–135 µs). Highly linear Stern–Volmer activity enabling accurate and precise calibration was observed even after 35 days of exposure; this proves that non‐core–shell fibres consisting of blends of PCL and gelatine can yield predictable lifetime values for >30 days in vitro. Scanning electron microscopy and mass loss data revealed that sensor degradation is highly tailorable, allowing for the fabrication of sensors engineered for a specific biomedical time frame. In contrast, core–shell fibre sensors showed more variability in lifetime following internal degradation likely caused by caproic acid entrapment by the PCL ‘shell’. This work demonstrates that biodegradable and biocompatible optically monitored sensors can be fabricated to provide direct, accurate assessments of oxygenation, even as the sensor platform degrades in a controlled manner. Such technologies have the potential to substantially change respiratory disease management.
- 1 April 2020
- Published by Elsevier in Journal of Controlled Release
- Vol. 320, 442-456
Injectable biodegradable bi-layered capsule for sustained delivery of bevacizumab in treating wet age-related macular degeneration
- 1 April 2020
- Published by Elsevier in Journal of Controlled Release
- Vol. 320, 442-456
Injectable biodegradable bi-layered capsule for sustained delivery of bevacizumab in treating wet age-related macular degeneration
- 1 June 2019
- Published by Elsevier in Materials Science and Engineering: C
- Vol. 99, 112-120
Sintered electrospun polycaprolactone for controlled model drug delivery
- 1 June 2019
- Published by Elsevier in Materials Science and Engineering: C
- Vol. 99, 112-120
Sintered electrospun polycaprolactone for controlled model drug delivery
- 12 March 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 136 (26)
Sintered electrospun poly(ɛ‐caprolactone)–poly(ethylene terephthalate) for drug delivery
Electrospinning has the inherent advantage of being able to achieve molecular mixing of polymers having substantially different melting points. Electrospun poly(ɛ‐caprolactone)–poly(ethylene terephthalate) (PCL:PET) capsules are densified by sintering to enable drug encapsulation. Proton and diffusive nuclear magnetic resonance, as well as a selective dissolution, suggest an absence of reaction between the two polymers. Sintering at 100 °C successfully densifies 88.89:11.11 and 75:25 PCL:PET blends. Following sintering, the otherwise dense 75:25 composition retains electrospun features and exhibits some “memory” of its previous state. Sintering increases UTS approximately eightfold versus as‐spun values for 88.89:11.11 and 75:25. Elongation increases sixfold and twofold and modulus 44‐ and 69‐fold for the 75:25 and 88.89:11.11 samples, respectively. Differential scanning calorimetry suggests a postsintering structure of nanoscale PET dispersed in PCL along the original fiber directions. Selective PCL removal from dense blends shows that fibrous characteristics remain. An internal shish–kebab‐like structure is also present in as‐spun 75:25 PCL:PET. Water absorption of hydrophobic oil‐containing capsules is approximately zero after 49 days. In contrast, hydrophilic (HPI) oils allow substantial water uptake. Unsurprisingly, there is no release of a model drug from the hydrophobic carrier. HPI oil provides linear (zero‐order) release inversely proportional to PET from the 88.89:11.11 and 75:25 ratios. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019, 136, 47731.
- 12 March 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 136 (26)
Sintered electrospun poly(ɛ‐caprolactone)–poly(ethylene terephthalate) for drug delivery
Electrospinning has the inherent advantage of being able to achieve molecular mixing of polymers having substantially different melting points. Electrospun poly(ɛ‐caprolactone)–poly(ethylene terephthalate) (PCL:PET) capsules are densified by sintering to enable drug encapsulation. Proton and diffusive nuclear magnetic resonance, as well as a selective dissolution, suggest an absence of reaction between the two polymers. Sintering at 100 °C successfully densifies 88.89:11.11 and 75:25 PCL:PET blends. Following sintering, the otherwise dense 75:25 composition retains electrospun features and exhibits some “memory” of its previous state. Sintering increases UTS approximately eightfold versus as‐spun values for 88.89:11.11 and 75:25. Elongation increases sixfold and twofold and modulus 44‐ and 69‐fold for the 75:25 and 88.89:11.11 samples, respectively. Differential scanning calorimetry suggests a postsintering structure of nanoscale PET dispersed in PCL along the original fiber directions. Selective PCL removal from dense blends shows that fibrous characteristics remain. An internal shish–kebab‐like structure is also present in as‐spun 75:25 PCL:PET. Water absorption of hydrophobic oil‐containing capsules is approximately zero after 49 days. In contrast, hydrophilic (HPI) oils allow substantial water uptake. Unsurprisingly, there is no release of a model drug from the hydrophobic carrier. HPI oil provides linear (zero‐order) release inversely proportional to PET from the 88.89:11.11 and 75:25 ratios. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019, 136, 47731.
- 10 August 2015
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 104 (8) , 1525-1534
Biomimetic microstructural reorganization during suture retention strength evaluation of electrospun vascular scaffolds
Suture retention strength (SRS) is commonly used as a measure the ability of sutures to adhere implants to surrounding tissue. While SRS is widely employed, surprisingly its effects on graft microstructure have not been characterized. This is particularly germane to the broad utilization of electrospun implants in tissue engineering. These implants need to retain their initial nanoscale topography while simultaneously preserving clinically critical mechanical properties. We examined the suture‐driven microstructural deformation of polycaprolactone electrospun to form both square and tubular SRS samples. The impact of fiber orientation (generally parallel or random orientation, orthogonally aligned) on the SRS of these vascular tissue equivalents was analyzed and compared to native and decellularized porcine vasculature. The initial state of the fiber clearly dictates the overall efficiency of scaffold utilization. SRS values for as‐spun fibers at a thickness of 300 μm were found to be in the range of 1.59–4.78 N for the three orientations. Unexpectedly, random fibers provided the optimal SRS values based on both resistance to suture motion and the percentage of scaffold involvement. A “V‐shaped” failure morphology is observed for both electrospun scaffolds and native tissue during SRS testing. Post‐test fiber alignment in the tensile direction was visible in all initial fiber orientations similar to that of native tissue. These findings are significant as they allow us to employ new, counterintuitive biomimetic design criteria for nanofiber‐based scaffolds in which reliable mechanical integration with the surrounding tissues via suture‐based methods is important. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 104B: 1525–1534, 2016.
- 10 August 2015
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 104 (8) , 1525-1534
Biomimetic microstructural reorganization during suture retention strength evaluation of electrospun vascular scaffolds
Suture retention strength (SRS) is commonly used as a measure the ability of sutures to adhere implants to surrounding tissue. While SRS is widely employed, surprisingly its effects on graft microstructure have not been characterized. This is particularly germane to the broad utilization of electrospun implants in tissue engineering. These implants need to retain their initial nanoscale topography while simultaneously preserving clinically critical mechanical properties. We examined the suture‐driven microstructural deformation of polycaprolactone electrospun to form both square and tubular SRS samples. The impact of fiber orientation (generally parallel or random orientation, orthogonally aligned) on the SRS of these vascular tissue equivalents was analyzed and compared to native and decellularized porcine vasculature. The initial state of the fiber clearly dictates the overall efficiency of scaffold utilization. SRS values for as‐spun fibers at a thickness of 300 μm were found to be in the range of 1.59–4.78 N for the three orientations. Unexpectedly, random fibers provided the optimal SRS values based on both resistance to suture motion and the percentage of scaffold involvement. A “V‐shaped” failure morphology is observed for both electrospun scaffolds and native tissue during SRS testing. Post‐test fiber alignment in the tensile direction was visible in all initial fiber orientations similar to that of native tissue. These findings are significant as they allow us to employ new, counterintuitive biomimetic design criteria for nanofiber‐based scaffolds in which reliable mechanical integration with the surrounding tissues via suture‐based methods is important. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 104B: 1525–1534, 2016.