Wei Luo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Wei Luo has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
- Yong Sheng Khoo
Solar Energy Research Institute of Singapore, Singapore
5 shared publications - Armin Gerhard Aberle
National University of Singapore
4 shared publications - Dirk Jordan
National Laboratory of the Rockies, Golden, CO (United States)
3 shared publications - Seeram Ramakrishna
Department of Mechanical Engineering Tsinghua University Beijing China
3 shared publications Aung Myint Khaing
Solar Energy Research Institute of Singapore National University of Singapore Singapore
2 shared publications- Carlos David Rodriguez Gallegos
National University of Singapore (NUS)
2 shared publications
Latest Publications
- Open Access
- 18 February 2024
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 32 (7) , 481-491
Long‐term outdoor study of an organic photovoltaic module for building integration
Organic photovoltaics (OPV) has attracted tremendous attention as a promising alternative to silicon wafer‐based technologies for building integration. While significant progress has been achieved on the power conversion efficiency of OPV technologies, their field stability is rarely studied. This work investigates the field performance and reliability of a large‐area OPV module designed for building integration in tropical Singapore for 4.5 years. The device suffered more than 14% degradation in power at the standard testing conditions from the initial performance, largely due to losses in fill factor (−12% relative). During the monitoring period, it exhibited comparable performance to more conventional silicon PV technologies, with an average specific energy yield of about 4 kWh/kWp/day and an average performance ratio of 0.96. Excellent performance at low light conditions was also observed. However, its field performance was heavily impacted by soiling, which typically led to a 5 to 10% loss in the current output after several months. Further, the device's outdoor performance also showed a three‐stage degradation process, including (1) an initial slow degradation in the first 2 years (about −1%/year), (2) a stable period with negligible performance loss from Years 2 to 3.5, and (3) a rapid degradation in the last year (about −5%/year).
- 18 February 2024
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 32 (7) , 481-491
Open AccessLong‐term outdoor study of an organic photovoltaic module for building integration
Organic photovoltaics (OPV) has attracted tremendous attention as a promising alternative to silicon wafer‐based technologies for building integration. While significant progress has been achieved on the power conversion efficiency of OPV technologies, their field stability is rarely studied. This work investigates the field performance and reliability of a large‐area OPV module designed for building integration in tropical Singapore for 4.5 years. The device suffered more than 14% degradation in power at the standard testing conditions from the initial performance, largely due to losses in fill factor (−12% relative). During the monitoring period, it exhibited comparable performance to more conventional silicon PV technologies, with an average specific energy yield of about 4 kWh/kWp/day and an average performance ratio of 0.96. Excellent performance at low light conditions was also observed. However, its field performance was heavily impacted by soiling, which typically led to a 5 to 10% loss in the current output after several months. Further, the device's outdoor performance also showed a three‐stage degradation process, including (1) an initial slow degradation in the first 2 years (about −1%/year), (2) a stable period with negligible performance loss from Years 2 to 3.5, and (3) a rapid degradation in the last year (about −5%/year).
- 25 October 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 14 (1) , 140-148
Measurement and Simulation of Moisture Ingress in PV Modules in Various Climates
Moisture plays a critical role in the degradation process of photovoltaic (PV) modules in field conditions. A commonly used approach is to evaluate the properties of PV materials by conducting tests in climatic chambers, and then apply the Fickian diffusion model in simulations to replicate field conditions, however, without experimental verification. This study describes an experimental setup for in situ measurement of moisture in fielded minimodules, using miniature temperature and humidity sensors encapsulated within the modules. Five identical setups are deployed in different climatic regions around the world, enabling a quantitative evaluation of moisture diffusion in the field and a comparison of different climates. The relative humidity measured beside the cell follow weekly weather trends due to breathable backsheet, whereas the sensors in front of the cell react much slower to outside changes and follow seasonal trends. We show that a single 2-D simulation, which is a standard practice in published studies, is insufficient to accurately depict moisture diffusion in front of the cell. Therefore, a two-stage 2-D simulation model, combining Fickian diffusion in vertical and horizontal cross section with carefully set boundary conditions, was introduced. A comparison with measurement results showed the simulation approach to be a good compromise between the simulation accuracy and speed. Finally, the results underscore the significance of understanding the local microclimate surrounding the modules, including the interface between air and backsheet, which is necessary for precise moisture diffusion simulations.
- 25 October 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 14 (1) , 140-148
Measurement and Simulation of Moisture Ingress in PV Modules in Various Climates
Moisture plays a critical role in the degradation process of photovoltaic (PV) modules in field conditions. A commonly used approach is to evaluate the properties of PV materials by conducting tests in climatic chambers, and then apply the Fickian diffusion model in simulations to replicate field conditions, however, without experimental verification. This study describes an experimental setup for in situ measurement of moisture in fielded minimodules, using miniature temperature and humidity sensors encapsulated within the modules. Five identical setups are deployed in different climatic regions around the world, enabling a quantitative evaluation of moisture diffusion in the field and a comparison of different climates. The relative humidity measured beside the cell follow weekly weather trends due to breathable backsheet, whereas the sensors in front of the cell react much slower to outside changes and follow seasonal trends. We show that a single 2-D simulation, which is a standard practice in published studies, is insufficient to accurately depict moisture diffusion in front of the cell. Therefore, a two-stage 2-D simulation model, combining Fickian diffusion in vertical and horizontal cross section with carefully set boundary conditions, was introduced. A comparison with measurement results showed the simulation approach to be a good compromise between the simulation accuracy and speed. Finally, the results underscore the significance of understanding the local microclimate surrounding the modules, including the interface between air and backsheet, which is necessary for precise moisture diffusion simulations.
- Open Access
- 25 March 2023
- Published by Wiley
Long-term Outdoor Study of Organic Photovoltaics for Building Integration
Organic photovoltaics (OPV) has attracted tremendous attention as a promising alternative to silicon wafer-based technologies for building integration. While significant progress has been achieved on the power conversion efficiency of OPV technologies, their field stability is rarely studied. This work investigates the field performance and reliability of a large-area OPV module designed for BIPV application in the tropical region of Singapore for 4.5 years. The device suffered more than 14% degradation in power at the standard testing conditions from the initial performance, largely due to losses in fill factor (-12% relative). During the monitoring period, it exhibited comparable performance to more conventional silicon PV technologies, with an average specific energy yield of about 4 kWh/kWp/day and an average performance ratio of 0.96. Excellent performance at low light conditions was also observed. However, its field performance was heavily impacted by soiling, which typically led to a 5 to 10% loss in the current output after several months. Further, the device’s outdoor performance also showed a three-stage degradation process, including (1) an initial slow degradation in the first two years (about -1%/year), (2) a stable period with negligible performance loss from year 2 to year 3.5 and (3) a rapid degradation in the last year (about -5%/year).
- 25 March 2023
- Published by Wiley
Open AccessLong-term Outdoor Study of Organic Photovoltaics for Building Integration
Organic photovoltaics (OPV) has attracted tremendous attention as a promising alternative to silicon wafer-based technologies for building integration. While significant progress has been achieved on the power conversion efficiency of OPV technologies, their field stability is rarely studied. This work investigates the field performance and reliability of a large-area OPV module designed for BIPV application in the tropical region of Singapore for 4.5 years. The device suffered more than 14% degradation in power at the standard testing conditions from the initial performance, largely due to losses in fill factor (-12% relative). During the monitoring period, it exhibited comparable performance to more conventional silicon PV technologies, with an average specific energy yield of about 4 kWh/kWp/day and an average performance ratio of 0.96. Excellent performance at low light conditions was also observed. However, its field performance was heavily impacted by soiling, which typically led to a 5 to 10% loss in the current output after several months. Further, the device’s outdoor performance also showed a three-stage degradation process, including (1) an initial slow degradation in the first two years (about -1%/year), (2) a stable period with negligible performance loss from year 2 to year 3.5 and (3) a rapid degradation in the last year (about -5%/year).
- 27 September 2022
- Published by Elsevier in Transportation Geotechnics
- Vol. 37, 100862
Mitigation of subway-induced low-frequency vibrations using a wave impeding block
- 27 September 2022
- Published by Elsevier in Transportation Geotechnics
- Vol. 37, 100862
Mitigation of subway-induced low-frequency vibrations using a wave impeding block
- Open Access
- 25 March 2021
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 29 (6) , 573-602
International collaboration framework for the calculation of performance loss rates: Data quality, benchmarks, and trends (towards a uniform methodology)
The IEA PVPS Task 13 group, experts who focus on photovoltaic performance, operation, and reliability from several leading R&D centers, universities, and industrial companies, is developing a framework for the calculation of performance loss rates of a large number of commercial and research photovoltaic (PV) power plants and their related weather data coming across various climatic zones. The general steps to calculate the performance loss rate are (i) input data cleaning and grading; (ii) data filtering; (iii) performance metric selection, corrections, and aggregation; and finally, (iv) application of a statistical modeling method to determine the performance loss rate value. In this study, several high‐quality power and irradiance datasets have been shared, and the participants of the study were asked to calculate the performance loss rate of each individual system using their preferred methodologies. The data are used for benchmarking activities and to define capabilities and uncertainties of all the various methods. The combination of data filtering, metrics (performance ratio or power based), and statistical modeling methods are benchmarked in terms of (i) their deviation from the average value and (ii) their uncertainty, standard error, and confidence intervals. It was observed that careful data filtering is an essential foundation for reliable performance loss rate calculations. Furthermore, the selection of the calculation steps filter/metric/statistical method is highly dependent on one another, and the steps should not be assessed individually.
- 25 March 2021
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 29 (6) , 573-602
Open AccessInternational collaboration framework for the calculation of performance loss rates: Data quality, benchmarks, and trends (towards a uniform methodology)
The IEA PVPS Task 13 group, experts who focus on photovoltaic performance, operation, and reliability from several leading R&D centers, universities, and industrial companies, is developing a framework for the calculation of performance loss rates of a large number of commercial and research photovoltaic (PV) power plants and their related weather data coming across various climatic zones. The general steps to calculate the performance loss rate are (i) input data cleaning and grading; (ii) data filtering; (iii) performance metric selection, corrections, and aggregation; and finally, (iv) application of a statistical modeling method to determine the performance loss rate value. In this study, several high‐quality power and irradiance datasets have been shared, and the participants of the study were asked to calculate the performance loss rate of each individual system using their preferred methodologies. The data are used for benchmarking activities and to define capabilities and uncertainties of all the various methods. The combination of data filtering, metrics (performance ratio or power based), and statistical modeling methods are benchmarked in terms of (i) their deviation from the average value and (ii) their uncertainty, standard error, and confidence intervals. It was observed that careful data filtering is an essential foundation for reliable performance loss rate calculations. Furthermore, the selection of the calculation steps filter/metric/statistical method is highly dependent on one another, and the steps should not be assessed individually.
- 10 April 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (4) , 935-939
Investigation of Potential-Induced Degradation in Bifacial n-PERL Modules
A potential-induced degradation (PID) test method for bifacial double-glass silicon modules is first recommended for studying PID effects at the particular side of interest (the front or rear). This could be achieved by maintaining the same electric potential between solar cells and the untargeted module surface. Using the recommended test method, PID effects on the rear of n-type bifacial passivated emitter rear locally-diffused (bifacial n-PERL) devices (n-base passivated with silicon nitride) are studied. The rear of the n-PERL modules exhibits excellent stability under negative-bias conditions (relative to the ground). However, a huge power loss is observed when they are stressed with + 1000 V, likely due to PID-polarization occurring at the rear. The PID damage is recoverable by illuminating the rear module surface with artificial light. Most of the power loss can even be regenerated by several flashes on the module rear side from a solar simulator.
- 10 April 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (4) , 935-939
Investigation of Potential-Induced Degradation in Bifacial n-PERL Modules
A potential-induced degradation (PID) test method for bifacial double-glass silicon modules is first recommended for studying PID effects at the particular side of interest (the front or rear). This could be achieved by maintaining the same electric potential between solar cells and the untargeted module surface. Using the recommended test method, PID effects on the rear of n-type bifacial passivated emitter rear locally-diffused (bifacial n-PERL) devices (n-base passivated with silicon nitride) are studied. The rear of the n-PERL modules exhibits excellent stability under negative-bias conditions (relative to the ground). However, a huge power loss is observed when they are stressed with + 1000 V, likely due to PID-polarization occurring at the rear. The PID damage is recoverable by illuminating the rear module surface with artificial light. Most of the power loss can even be regenerated by several flashes on the module rear side from a solar simulator.
- 18 October 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (1) , 206-212
Reducing Interanalyst Variability in Photovoltaic Degradation Rate Assessments
The economic return on investment of a commercial photovoltaic system depends greatly on its performance over the long term and, hence, its degradation rate. Many methods have been proposed for assessing system degradation rates from outdoor performance data. However, comparing reported values from one analyst and research group to another requires a common baseline of performance; consistency between methods and analysts can be a challenge. An interlaboratory study was conducted involving different volunteer analysts reporting on the same photovoltaic performance data using different methodologies. Initial variability of the reported degradation rates was so high that analysts could not come to a consensus whether a system degraded or not. More consistent values are received when written guidance is provided to each analyst. Further improvements in analyst variance was accomplished by using the free open-source software RdTools, allowing a reduction in variance between analysts by more than two orders of magnitude over the first round, where multiple analysis methods are allowed. This article highlights many pitfalls in conducting “routine” degradation analysis, and it addresses some of the factors that must be considered when comparing degradation results reported by different analysts or methods.
- 18 October 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 10 (1) , 206-212
Reducing Interanalyst Variability in Photovoltaic Degradation Rate Assessments
The economic return on investment of a commercial photovoltaic system depends greatly on its performance over the long term and, hence, its degradation rate. Many methods have been proposed for assessing system degradation rates from outdoor performance data. However, comparing reported values from one analyst and research group to another requires a common baseline of performance; consistency between methods and analysts can be a challenge. An interlaboratory study was conducted involving different volunteer analysts reporting on the same photovoltaic performance data using different methodologies. Initial variability of the reported degradation rates was so high that analysts could not come to a consensus whether a system degraded or not. More consistent values are received when written guidance is provided to each analyst. Further improvements in analyst variance was accomplished by using the free open-source software RdTools, allowing a reduction in variance between analysts by more than two orders of magnitude over the first round, where multiple analysis methods are allowed. This article highlights many pitfalls in conducting “routine” degradation analysis, and it addresses some of the factors that must be considered when comparing degradation results reported by different analysts or methods.
- 2 November 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (1) , 266-271
Analysis of the Long-Term Performance Degradation of Crystalline Silicon Photovoltaic Modules in Tropical Climates
The long-term performance degradation of five different types of commercial crystalline silicon (c-Si) photovoltaic (PV) modules (one sample for each type) in the tropics, or more specifically the tropical rainforest climate “Af” by the Köppen climate classification (Singapore), is investigated over a period of seven years, based on outdoor I–V measurements at 10-s intervals. The degradation rates of these c-Si PV modules, based on the temperature-corrected performance ratio, range from –0.03 to –0.47%/year, which satisfy the products’ performance warranty. Further analysis of the short-circuit current (I $_\text{sc}$ ), open-circuit voltage, and fill factor for these modules shows that the performance degradation is mainly attributed to the I $_\text{sc}$ loss. The possible causes of the module performance deterioration are also discussed.- 2 November 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (1) , 266-271
Analysis of the Long-Term Performance Degradation of Crystalline Silicon Photovoltaic Modules in Tropical Climates
The long-term performance degradation of five different types of commercial crystalline silicon (c-Si) photovoltaic (PV) modules (one sample for each type) in the tropics, or more specifically the tropical rainforest climate “Af” by the Köppen climate classification (Singapore), is investigated over a period of seven years, based on outdoor I–V measurements at 10-s intervals. The degradation rates of these c-Si PV modules, based on the temperature-corrected performance ratio, range from –0.03 to –0.47%/year, which satisfy the products’ performance warranty. Further analysis of the short-circuit current (I $_\text{sc}$ ), open-circuit voltage, and fill factor for these modules shows that the performance degradation is mainly attributed to the I $_\text{sc}$ loss. The possible causes of the module performance deterioration are also discussed.- 22 June 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 8 (5) , 1168-1173
Investigation of the Impact of Illumination on the Polarization-Type Potential-Induced Degradation of Crystalline Silicon Photovoltaic Modules
Accelerated potential-induced degradation (PID) testing of photovoltaic modules is conventionally conducted in the dark and at high temperature and humidity levels without considering the influence of illumination. This study investigates the impact of illumination on the polarization-type PID (PID-p) on two different types of encapsulated (glass/backsheet) crystalline silicon solar cells: 1) n-type bifacial passivated emitter rear totally diffused (the front side is facing glass and PID-stressed); and 2) p-type bifacial passivated emitter and rear cell (the rear side is facing glass and PID-stressed). The samples are stressed under the conditions of −1000 V, 40 °C, and 40% relative humidity and at different irradiance levels (xenon lamps). While the type-A modules show no reduction in PID-p sensitivity under illumination up to 800 W/m2, PID-p in the type-B modules is arrested by the light at an irradiance level as low as 10 W/m2. Furthermore, PID-degraded type-B modules (degradation induced in the dark) exhibit a rapid recovery (full recovery in 20 min) upon exposure to light (40 W/m2). External quantum efficiency measurements on the type-B modules show that ultraviolet from 300 to 400 nm is mainly responsible for the fast recovery.
- 22 June 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 8 (5) , 1168-1173
Investigation of the Impact of Illumination on the Polarization-Type Potential-Induced Degradation of Crystalline Silicon Photovoltaic Modules
Accelerated potential-induced degradation (PID) testing of photovoltaic modules is conventionally conducted in the dark and at high temperature and humidity levels without considering the influence of illumination. This study investigates the impact of illumination on the polarization-type PID (PID-p) on two different types of encapsulated (glass/backsheet) crystalline silicon solar cells: 1) n-type bifacial passivated emitter rear totally diffused (the front side is facing glass and PID-stressed); and 2) p-type bifacial passivated emitter and rear cell (the rear side is facing glass and PID-stressed). The samples are stressed under the conditions of −1000 V, 40 °C, and 40% relative humidity and at different irradiance levels (xenon lamps). While the type-A modules show no reduction in PID-p sensitivity under illumination up to 800 W/m2, PID-p in the type-B modules is arrested by the light at an irradiance level as low as 10 W/m2. Furthermore, PID-degraded type-B modules (degradation induced in the dark) exhibit a rapid recovery (full recovery in 20 min) upon exposure to light (40 W/m2). External quantum efficiency measurements on the type-B modules show that ultraviolet from 300 to 400 nm is mainly responsible for the fast recovery.
- 5 June 2018
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 26 (10) , 859-867
Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules
This paper elucidates the behavior and underlying mechanism of potential‐induced degradation (PID) on the rear side of p‐type monocrystalline silicon bifacial passivated emitter and rear cell (PERC) photovoltaic modules. At 50°C, 30% relative humidity, and −1000 V bias to the solar cells with aluminium foil on the rear glass surface, the rear‐side performance of bifacial PERC modules at standard testing conditions degraded dramatically after 40 hours with a 40.4%, 36.2%, and 7.2% loss in maximum power (Pmpp), short‐circuit current (Isc), and open‐circuit voltage (Voc), respectively. The front‐side standard testing condition performance, on the other hand, showed less degradation; Pmpp, Isc, and Voc dropped by 12.0%, 5.2%, and 5.3%, respectively. However, negligible degradation was observed when the solar cells were positively biased. Based on I‐V characteristics, electroluminescence, external quantum efficiency measurements, and the effective minority‐carrier lifetime simulation, the efficiency loss is shown to be caused by the surface polarization effect; positive charges are attracted to the passivation/antireflection stack on the rear surface and reduce its field effect passivation performance. Extended PID testing to 100 hours showed an increase in device performances (relative to 40 hours) due to the formation of an inversion layer along the rear surface. In addition, replacing ethylene‐vinyl acetate copolymer with polyolefin elastomer films significantly slows down the progression of PID, whereas a glass/transparent backsheet design effectively protects the rear side of bifacial PERC modules from PID. Furthermore, PID on the rear side of bifacial PERC modules is fully recoverable, and light greatly promotes recovery of the observed PID.
- 5 June 2018
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 26 (10) , 859-867
Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules
This paper elucidates the behavior and underlying mechanism of potential‐induced degradation (PID) on the rear side of p‐type monocrystalline silicon bifacial passivated emitter and rear cell (PERC) photovoltaic modules. At 50°C, 30% relative humidity, and −1000 V bias to the solar cells with aluminium foil on the rear glass surface, the rear‐side performance of bifacial PERC modules at standard testing conditions degraded dramatically after 40 hours with a 40.4%, 36.2%, and 7.2% loss in maximum power (Pmpp), short‐circuit current (Isc), and open‐circuit voltage (Voc), respectively. The front‐side standard testing condition performance, on the other hand, showed less degradation; Pmpp, Isc, and Voc dropped by 12.0%, 5.2%, and 5.3%, respectively. However, negligible degradation was observed when the solar cells were positively biased. Based on I‐V characteristics, electroluminescence, external quantum efficiency measurements, and the effective minority‐carrier lifetime simulation, the efficiency loss is shown to be caused by the surface polarization effect; positive charges are attracted to the passivation/antireflection stack on the rear surface and reduce its field effect passivation performance. Extended PID testing to 100 hours showed an increase in device performances (relative to 40 hours) due to the formation of an inversion layer along the rear surface. In addition, replacing ethylene‐vinyl acetate copolymer with polyolefin elastomer films significantly slows down the progression of PID, whereas a glass/transparent backsheet design effectively protects the rear side of bifacial PERC modules from PID. Furthermore, PID on the rear side of bifacial PERC modules is fully recoverable, and light greatly promotes recovery of the observed PID.