Igor M. Chernev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Igor M. Chernev has a total of 72 co-authors. Here are the top co-authors by number of shared publications:
- Konstantin Nickolaevich Galkin
Institute of Automation and Control Processes, FEB RAS 1 , 5 Radio St., Vladivostok 690041
15 shared publications Nikolay G. Galkin
Institute of Automation and Control Processes FEB RAS, Radio St. 5, Vladivostok 690041, Russia
9 shared publications- Dmitrii L. Goroshko
Institute of Automation and Control Processes, Far Eastern Branch, Russian Academy of Sciences, Vladivostok, Russia
8 shared publications - Alexander Vladimirovich Shevlyagin
Institute of Automation and Control Processes, Far Eastern Branch, Russian Academy of Sciences, Vladivostok, Russia
5 shared publications - Evgeniy Anatolievich Chusovitin
Institute of Automation and Control Processes
5 shared publications - Evgenii Petrovich Subbotin
Institute of Automation and Control Processes, Far Eastern Branch, Russian Academy of Sciences, Vladivostok, Russia
4 shared publications
Latest Publications
- 15 December 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (1)
Crystal structure and thermoelectric efficiency of FeSi films on Si substrates: Shunting effects and first-principles calculations of lattice thermal conductivity
The crystal structure and thermoelectric parameters (conductivity, Seebeck coefficient, and power factor) of ultrathin (3–3.5 nm) stoichiometric monoclinic FeSi (m-FeSi) films and cubic FeSi (c-FeSi) films, as well as thin (14–49 nm) cubic FeSi (c-FeSi) films, were determined in the temperature range of 100–450 K. Single-phase FeSi films exhibit a metal-semiconductor transition at temperatures below 200 K due to the Kondo effect, metallic conductivity at temperatures below 30 K, and demonstrate a noticeable Seebeck effect in the range of 100–450 K. The thermoelectric parameters were calculated using a two-layer model for FeSi thin films and taking into account the film-to-substrate resistance ratio to minimize the substrate shunting effect. The 20–49 nm thick c-FeSi films (grown by molecular beam epitaxy) exhibit nearly the lowest resistivity, a positive Seebeck coefficient (30–85 μV/K), and a power factor [0.3–1.0 mW/(m K2)] in the range of 120–470 K. The phonon band structure and lattice thermal conductivity were calculated for both bulk c-FeSi and its nanowires. It was found that the lattice thermal conductivity of nanowires is four to ten times lower than that of bulk c-FeSi. The dimensionless thermoelectric figure of merit (ZT) of the thin FeSi films was estimated: the maximum ZT = 0.03–0.05 at 200–470 K was achieved for a 20 nm thick p-type c-FeSi film. This c-FeSi film was doped with boron atoms from the p+ layer of the Si substrate.
- 15 December 2025
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (1)
Crystal structure and thermoelectric efficiency of FeSi films on Si substrates: Shunting effects and first-principles calculations of lattice thermal conductivity
The crystal structure and thermoelectric parameters (conductivity, Seebeck coefficient, and power factor) of ultrathin (3–3.5 nm) stoichiometric monoclinic FeSi (m-FeSi) films and cubic FeSi (c-FeSi) films, as well as thin (14–49 nm) cubic FeSi (c-FeSi) films, were determined in the temperature range of 100–450 K. Single-phase FeSi films exhibit a metal-semiconductor transition at temperatures below 200 K due to the Kondo effect, metallic conductivity at temperatures below 30 K, and demonstrate a noticeable Seebeck effect in the range of 100–450 K. The thermoelectric parameters were calculated using a two-layer model for FeSi thin films and taking into account the film-to-substrate resistance ratio to minimize the substrate shunting effect. The 20–49 nm thick c-FeSi films (grown by molecular beam epitaxy) exhibit nearly the lowest resistivity, a positive Seebeck coefficient (30–85 μV/K), and a power factor [0.3–1.0 mW/(m K2)] in the range of 120–470 K. The phonon band structure and lattice thermal conductivity were calculated for both bulk c-FeSi and its nanowires. It was found that the lattice thermal conductivity of nanowires is four to ten times lower than that of bulk c-FeSi. The dimensionless thermoelectric figure of merit (ZT) of the thin FeSi films was estimated: the maximum ZT = 0.03–0.05 at 200–470 K was achieved for a 20 nm thick p-type c-FeSi film. This c-FeSi film was doped with boron atoms from the p+ layer of the Si substrate.
- 1 December 2025
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 64 (12) , 12SP02
Mg 2 Si and ε -FeSi contacts for SWIR narrowband Si based photodetectors
This study investigates the performance of Al/ n -Si/Mg 2 Si and Al/ n -Si/ ε -FeSi self-filtered Schottky photodetectors for SWIR applications. The Mg 2 Si-based structure demonstrates superior spectral stability, with a fixed photoresponse peak at 1045 nm (FWHM 120–140 nm) and intensity 30 mA W −1 , 105 mA W −1 and 195 mA W −1 at 0 V, 1 V and 5 V respectively. The Al/ n -Si/ ε -FeSi detector shows narrowband behavior only at above 2 V applied bias with peak at ∼1040 nm and intensity 92 mA W −1 and 272 mA W −1 at 2 V and 5 V bias, respectively
- 1 December 2025
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 64 (12) , 12SP02
Mg 2 Si and ε -FeSi contacts for SWIR narrowband Si based photodetectors
This study investigates the performance of Al/ n -Si/Mg 2 Si and Al/ n -Si/ ε -FeSi self-filtered Schottky photodetectors for SWIR applications. The Mg 2 Si-based structure demonstrates superior spectral stability, with a fixed photoresponse peak at 1045 nm (FWHM 120–140 nm) and intensity 30 mA W −1 , 105 mA W −1 and 195 mA W −1 at 0 V, 1 V and 5 V respectively. The Al/ n -Si/ ε -FeSi detector shows narrowband behavior only at above 2 V applied bias with peak at ∼1040 nm and intensity 92 mA W −1 and 272 mA W −1 at 2 V and 5 V bias, respectively
- 1 December 2024
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 88 (S3) , S322-S324
Laser Micromechanical Sensor for Measurement of the Mass of Bacterial Cell Colonies
We presented results of applying an adaptive interferometry technique, based on dynamic holograms recorded in photorefractive crystal, to accurately determine the mass of biofilm bacteria colonies by the measuring of microcantilever frequency shift. During the experimental testing, biofilms of Escherichia coli were grown on the surface of a cantilever previously coated with a BaF2 film. The proposed experimental setup is completely non-contact due to using an optical method of excitation and detection of cantilever oscillations. Based on the measured shift in the resonant frequency, the mass of the biofilm grown on the cantilever was calculated to be (2.072 ± 0.003) × 10–9 gram.
- 1 December 2024
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 88 (S3) , S322-S324
Laser Micromechanical Sensor for Measurement of the Mass of Bacterial Cell Colonies
We presented results of applying an adaptive interferometry technique, based on dynamic holograms recorded in photorefractive crystal, to accurately determine the mass of biofilm bacteria colonies by the measuring of microcantilever frequency shift. During the experimental testing, biofilms of Escherichia coli were grown on the surface of a cantilever previously coated with a BaF2 film. The proposed experimental setup is completely non-contact due to using an optical method of excitation and detection of cantilever oscillations. Based on the measured shift in the resonant frequency, the mass of the biofilm grown on the cantilever was calculated to be (2.072 ± 0.003) × 10–9 gram.
- 27 December 2023
- Published by Elsevier in Computational Materials Science
- Vol. 233
New monoclinic ground state of FeSi
- 27 December 2023
- Published by Elsevier in Computational Materials Science
- Vol. 233
New monoclinic ground state of FeSi
- 1 December 2023
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 87 (S3) , S370-S374
FeSi and CrSi2 Thin Films as Transparent Conductive Layers for VIS/SWIR Sensitive Mg2Si Films Grown on Si
Mg2Si film 350–600 nm thick was formed on Si(111) substrate by ultrafast reactive deposition of Mg. Then 10–15 nm thick films of FeSi or CrSi2 were grown as cover layers on Mg2Si by codeposition of Fe/Si or Cr/Si. In comparison with bare Mg2Si/Si film, the measured transparency losses in 0.1–1.1 eV range are ∼17–25 and 10–35% for the samples with the FeSi and CrSi2 layers, respectively. The measured at room temperature resistivity is ∼0.24 mΩ cm for FeSi and 1.7 mΩ cm for CrSi2. The photoresponse of structures FeSi/Mg2Si/Si and CrSi2/Mg2Si/Si illuminated with the light filtered by a silicon plate demonstrate the spectral sensitivity in the range 980–1200 nm and peak intensity ∼255 and ∼620 μA/W respectively.
- 1 December 2023
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 87 (S3) , S370-S374
FeSi and CrSi2 Thin Films as Transparent Conductive Layers for VIS/SWIR Sensitive Mg2Si Films Grown on Si
Mg2Si film 350–600 nm thick was formed on Si(111) substrate by ultrafast reactive deposition of Mg. Then 10–15 nm thick films of FeSi or CrSi2 were grown as cover layers on Mg2Si by codeposition of Fe/Si or Cr/Si. In comparison with bare Mg2Si/Si film, the measured transparency losses in 0.1–1.1 eV range are ∼17–25 and 10–35% for the samples with the FeSi and CrSi2 layers, respectively. The measured at room temperature resistivity is ∼0.24 mΩ cm for FeSi and 1.7 mΩ cm for CrSi2. The photoresponse of structures FeSi/Mg2Si/Si and CrSi2/Mg2Si/Si illuminated with the light filtered by a silicon plate demonstrate the spectral sensitivity in the range 980–1200 nm and peak intensity ∼255 and ∼620 μA/W respectively.
- 8 July 2023
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 964
Thick p-type Mg2Si film on Si: Growth, structure and transport properties
- 8 July 2023
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 964
Thick p-type Mg2Si film on Si: Growth, structure and transport properties
- Open Access
- 30 June 2021
- Published by Colloquium in Himičeskaâ fizika i mezoskopiâ
- Vol. 23 (2)
Mechanisms of Conductivity and Thermoelectric Properties of Semimetallic CaSi and CASi2 Films on Si(100) and Si(111) Substrates
- 30 June 2021
- Published by Colloquium in Himičeskaâ fizika i mezoskopiâ
- Vol. 23 (2)
Open AccessMechanisms of Conductivity and Thermoelectric Properties of Semimetallic CaSi and CASi2 Films on Si(100) and Si(111) Substrates
- 1 September 2018
- Published by Trans Tech Publications, Ltd. in Defect and Diffusion Forum
- Vol. 386, 3-8
Comparison of the Structural, Optical and Thermoelectrical Properties of Ca Silicide Films with Variable Composition on Si Substrates
The growth, structure, optical, electrical and thermoelectric properties of calcium silicides of various compositions on silicon substrates with (100) and (111) orientations were experimentally studied. It was found that when the atoms of Ca and Si are co-deposited on atomically clean silicon, the basis phases in the composition of the formed films depends on the substrate temperature and the annealing temperature: Ca2Si (TSi = 20°C, Tann = 330°C), CaSi (TSi = 190-320°C, Tann = 330°C) and CaSi2 (TSi = 500°C). It was established that the Ca2Si phase is a direct-gap semiconductor with a band gap of 0.82±0.02 eV, large contribution of defect levels to the absorption coefficient at energies 0.25 - 0.50 eV and huge transmission up 90% in the far IR region. In CaSi-based films the high transmission (30-40%) up to 25 μm was observed, which corresponds to a semimetal with a constant density of states near the Fermi level. It was found that CaSi-based films have the maximum Seebeck coefficient and the power factor (up to 430 μV/K and up to 1.14 × 10-6 W/(K2m), respectively) at 330K. CaSi2 films with CaSi2 lattice stretching and epitaxial ordering relative to the Si (100) substrate exhibit semimetal properties, with very high conductivity and light transparency (up 12%) in the photon energy range 0.06 - 0.65 eV.
- 1 September 2018
- Published by Trans Tech Publications, Ltd. in Defect and Diffusion Forum
- Vol. 386, 3-8
Comparison of the Structural, Optical and Thermoelectrical Properties of Ca Silicide Films with Variable Composition on Si Substrates
The growth, structure, optical, electrical and thermoelectric properties of calcium silicides of various compositions on silicon substrates with (100) and (111) orientations were experimentally studied. It was found that when the atoms of Ca and Si are co-deposited on atomically clean silicon, the basis phases in the composition of the formed films depends on the substrate temperature and the annealing temperature: Ca2Si (TSi = 20°C, Tann = 330°C), CaSi (TSi = 190-320°C, Tann = 330°C) and CaSi2 (TSi = 500°C). It was established that the Ca2Si phase is a direct-gap semiconductor with a band gap of 0.82±0.02 eV, large contribution of defect levels to the absorption coefficient at energies 0.25 - 0.50 eV and huge transmission up 90% in the far IR region. In CaSi-based films the high transmission (30-40%) up to 25 μm was observed, which corresponds to a semimetal with a constant density of states near the Fermi level. It was found that CaSi-based films have the maximum Seebeck coefficient and the power factor (up to 430 μV/K and up to 1.14 × 10-6 W/(K2m), respectively) at 330K. CaSi2 films with CaSi2 lattice stretching and epitaxial ordering relative to the Si (100) substrate exhibit semimetal properties, with very high conductivity and light transparency (up 12%) in the photon energy range 0.06 - 0.65 eV.
- 25 July 2016
- Published by AIP Publishing in Applied Physics Letters
- Vol. 109 (4) , 043902
On the way to enhance the optical absorption of a-Si in NIR by embedding Mg2Si thin film
Mg2Si thin film was embedded in amorphous silicon matrix by solid phase epitaxy. The structure and optical properties were investigated by electron energy loss, X-ray photoelectron, Raman, and photo thermal deflection spectroscopy measurements. It was found that in the photon energy range of 0.8–1.7 eV, the light absorption of the structure with magnesium silicide (Mg2Si) film embedded in a-Si(i) matrix is 1.5 times higher than that for the same structure without Mg2Si.
- 25 July 2016
- Published by AIP Publishing in Applied Physics Letters
- Vol. 109 (4) , 043902
On the way to enhance the optical absorption of a-Si in NIR by embedding Mg2Si thin film
Mg2Si thin film was embedded in amorphous silicon matrix by solid phase epitaxy. The structure and optical properties were investigated by electron energy loss, X-ray photoelectron, Raman, and photo thermal deflection spectroscopy measurements. It was found that in the photon energy range of 0.8–1.7 eV, the light absorption of the structure with magnesium silicide (Mg2Si) film embedded in a-Si(i) matrix is 1.5 times higher than that for the same structure without Mg2Si.
- 1 March 2016
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 247, 158-167
The Structure and Magnetic Properties of Bronze, Stainless still and Alloy Layers Formed by Direct Laser Welding on Nonmagnetic Substrates
Investigations of crystal structure, microstructure and composition of laser welded coatings of bronze, IN625, PGSR-4 and stainless steel alloys on non-magnetic substrates have shown that from the raw alloy powders (wire) the additional crystalline phases are extracted with new compositions and sizes of units of microns, which randomly distributed in the coating volume. Due to formation of additional phases with increased electron concentration magnetic hysteresis loops have appeared at 4 K and 300 K for all welded coatings. Bronze and stainless steel coatings have demonstrated soft ferromagnetic properties with two type of magnetic domains with small magnetization that resulted in small value of saturation magnetization (Ms = 60-146 emu/cm3 at 300 K and Ms = 107-241 emu/cm3 at 4 K) and low values of coercive force (40 – 90 Oe) at 300 K and (50-170 Oe) at 4 K. En existence of one type of ferromagnetic domains with middle Curie temperatures (230-270 K) in laser welded IN625 and PGSR-4 coatings has determined soft ferromagnetic nature of magnetism at low temperature (Ms =274 – 398 emu/cm3) and transition in paramagnetic conditions at 300 K due to main contribution only paramagnetic grains with different composition.
- 1 March 2016
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 247, 158-167
The Structure and Magnetic Properties of Bronze, Stainless still and Alloy Layers Formed by Direct Laser Welding on Nonmagnetic Substrates
Investigations of crystal structure, microstructure and composition of laser welded coatings of bronze, IN625, PGSR-4 and stainless steel alloys on non-magnetic substrates have shown that from the raw alloy powders (wire) the additional crystalline phases are extracted with new compositions and sizes of units of microns, which randomly distributed in the coating volume. Due to formation of additional phases with increased electron concentration magnetic hysteresis loops have appeared at 4 K and 300 K for all welded coatings. Bronze and stainless steel coatings have demonstrated soft ferromagnetic properties with two type of magnetic domains with small magnetization that resulted in small value of saturation magnetization (Ms = 60-146 emu/cm3 at 300 K and Ms = 107-241 emu/cm3 at 4 K) and low values of coercive force (40 – 90 Oe) at 300 K and (50-170 Oe) at 4 K. En existence of one type of ferromagnetic domains with middle Curie temperatures (230-270 K) in laser welded IN625 and PGSR-4 coatings has determined soft ferromagnetic nature of magnetism at low temperature (Ms =274 – 398 emu/cm3) and transition in paramagnetic conditions at 300 K due to main contribution only paramagnetic grains with different composition.