Evan M. White
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Evan M. White has a total of 47 co-authors. Here are the top co-authors by number of shared publications:
- Jason Locklin
Department of Chemistry, University of Georgia, Athens, GA 30602, USA
8 shared publications Jessica Horn
New Materials Institute, University of Georgia, Athens, GA 30602, USA
4 shared publicationsAustin F. Wright
New Materials Institute
3 shared publications- Adam M. Feist
BRiGHT, Technical University of Denmark Kgs. Lyngby Denmark
2 shared publications Benjamin Crawford
Department of Chemistry, University of Georgia, Athens, Georgia 30602, United States
2 shared publicationsBranson W. Ritchie
New Materials Institute, University of Georgia, Athens, Georgia 30602, United States
2 shared publications
Latest Publications
- Open Access
- 27 May 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (22) , 23025-23034
Impact Modification of Poly(3-hydroxybutyrate) and Poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) with Terratek FX1515 and Terratek GDH-B1FA
Poly(3-hydroxybutyrate) (PHB) and poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (PHB-co-HHx) are promising alternatives to polyolefins due to their similar processing temperatures and mechanical properties. However, these polymers exhibit brittle failure and poor impact performance, limiting their uses for certain applications. In this work, industrially compostable impact modifiers Terratek FX1515 (FX1515) and Terratek GDH-B1FA (GDH-B1FA) were blended with PHB and PHB-co-HHx at 10, 20, and 30% w/w loadings to assess the mechanical performance of these polymers. Blends containing both impact modifiers show remarkable improvement in the tensile and Izod impact properties of both polymers. The impact strength of PHB-co-HHx blends increases from 2.50 ± 0.09 to 13.81 ± 1.91 kJ/m2 (30% FX1515) and 59.23 ± 1.27 kJ/m2 (30% GDH-B1FA), whereas PHB blends showed moderate improvement from 2.37 ± 0.07 to 4.07 ± 0.18 kJ/m2 (30% FX1515) and 4.79 ± 0.46 kJ/m2 (30% GDH-B1FA). Further analysis of the impact surfaces using scanning electron microscopy, dynamic mechanical analysis, and interfacial tension revealed that the better performance of GDH-B1FA blends was due to its inherent elastomeric properties, large domain size, and good compatibility at the polymer–polymer interface. Additionally, biodegradation testing of the neat polymers, impact modifiers, and blends (ASTM D5338, industrial composting) shows that the polymers and impact-modified blends are capable of composting fully within 120 days.
- 27 May 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (22) , 23025-23034
Open AccessImpact Modification of Poly(3-hydroxybutyrate) and Poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) with Terratek FX1515 and Terratek GDH-B1FA
Poly(3-hydroxybutyrate) (PHB) and poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (PHB-co-HHx) are promising alternatives to polyolefins due to their similar processing temperatures and mechanical properties. However, these polymers exhibit brittle failure and poor impact performance, limiting their uses for certain applications. In this work, industrially compostable impact modifiers Terratek FX1515 (FX1515) and Terratek GDH-B1FA (GDH-B1FA) were blended with PHB and PHB-co-HHx at 10, 20, and 30% w/w loadings to assess the mechanical performance of these polymers. Blends containing both impact modifiers show remarkable improvement in the tensile and Izod impact properties of both polymers. The impact strength of PHB-co-HHx blends increases from 2.50 ± 0.09 to 13.81 ± 1.91 kJ/m2 (30% FX1515) and 59.23 ± 1.27 kJ/m2 (30% GDH-B1FA), whereas PHB blends showed moderate improvement from 2.37 ± 0.07 to 4.07 ± 0.18 kJ/m2 (30% FX1515) and 4.79 ± 0.46 kJ/m2 (30% GDH-B1FA). Further analysis of the impact surfaces using scanning electron microscopy, dynamic mechanical analysis, and interfacial tension revealed that the better performance of GDH-B1FA blends was due to its inherent elastomeric properties, large domain size, and good compatibility at the polymer–polymer interface. Additionally, biodegradation testing of the neat polymers, impact modifiers, and blends (ASTM D5338, industrial composting) shows that the polymers and impact-modified blends are capable of composting fully within 120 days.
- Open Access
- 30 April 2024
- Published by Springer Nature in Nature Communications
- Vol. 15 (1) , 1-15
Biocomposite thermoplastic polyurethanes containing evolved bacterial spores as living fillers to facilitate polymer disintegration
The field of hybrid engineered living materials seeks to pair living organisms with synthetic materials to generate biocomposite materials with augmented function since living systems can provide highly-programmable and complex behavior. Engineered living materials have typically been fabricated using techniques in benign aqueous environments, limiting their application. In this work, biocomposite fabrication is demonstrated in which spores from polymer-degrading bacteria are incorporated into a thermoplastic polyurethane using high-temperature melt extrusion. Bacteria are engineered using adaptive laboratory evolution to improve their heat tolerance to ensure nearly complete cell survivability during manufacturing at 135 °C. Furthermore, the overall tensile properties of spore-filled thermoplastic polyurethanes are substantially improved, resulting in a significant improvement in toughness. The biocomposites facilitate disintegration in compost in the absence of a microbe-rich environment. Finally, embedded spores demonstrate a rationally programmed function, expressing green fluorescent protein. This research provides a scalable method to fabricate advanced biocomposite materials in industrially-compatible processes.
- 30 April 2024
- Published by Springer Nature in Nature Communications
- Vol. 15 (1) , 1-15
Open AccessBiocomposite thermoplastic polyurethanes containing evolved bacterial spores as living fillers to facilitate polymer disintegration
The field of hybrid engineered living materials seeks to pair living organisms with synthetic materials to generate biocomposite materials with augmented function since living systems can provide highly-programmable and complex behavior. Engineered living materials have typically been fabricated using techniques in benign aqueous environments, limiting their application. In this work, biocomposite fabrication is demonstrated in which spores from polymer-degrading bacteria are incorporated into a thermoplastic polyurethane using high-temperature melt extrusion. Bacteria are engineered using adaptive laboratory evolution to improve their heat tolerance to ensure nearly complete cell survivability during manufacturing at 135 °C. Furthermore, the overall tensile properties of spore-filled thermoplastic polyurethanes are substantially improved, resulting in a significant improvement in toughness. The biocomposites facilitate disintegration in compost in the absence of a microbe-rich environment. Finally, embedded spores demonstrate a rationally programmed function, expressing green fluorescent protein. This research provides a scalable method to fabricate advanced biocomposite materials in industrially-compatible processes.
- Open Access
Biocomposite Thermoplastic Polyurethanes Containing Evolved Bacterial Spores as Living Fillers to Facilitate Polymer Disintegration
The field of engineered living materials (ELMs) seeks to pair living organisms with synthetic materials to generate biocomposite materials with augmented function since living systems can provide highly-programmable and complex behavior. ELMs have typically been fabricated using techniques in benign aqueous environments, limiting their application. In this work, biocomposite fabrication was demonstrated in which spores from polymer-degrading bacteria were incorporated into a thermoplastic polyurethane (TPU) using high-temperature melt processing. Bacteria were engineered using adaptive laboratory evolution to improve their heat tolerance to ensure nearly complete cell survivability during manufacturing at 135 °C. Furthermore, the overall tensile properties of spore-filled TPUs were substantially improved, resulting in a significant improvement in toughness. The biocomposites facilitated disintegration in compost in the absence of a microbe-rich environment. Finally, spores retained a programmed function, expressing green fluorescent protein. This research provides a scalable method to fabricate advanced biocomposite materials in industrially-compatible processes.
Open AccessBiocomposite Thermoplastic Polyurethanes Containing Evolved Bacterial Spores as Living Fillers to Facilitate Polymer Disintegration
The field of engineered living materials (ELMs) seeks to pair living organisms with synthetic materials to generate biocomposite materials with augmented function since living systems can provide highly-programmable and complex behavior. ELMs have typically been fabricated using techniques in benign aqueous environments, limiting their application. In this work, biocomposite fabrication was demonstrated in which spores from polymer-degrading bacteria were incorporated into a thermoplastic polyurethane (TPU) using high-temperature melt processing. Bacteria were engineered using adaptive laboratory evolution to improve their heat tolerance to ensure nearly complete cell survivability during manufacturing at 135 °C. Furthermore, the overall tensile properties of spore-filled TPUs were substantially improved, resulting in a significant improvement in toughness. The biocomposites facilitated disintegration in compost in the absence of a microbe-rich environment. Finally, spores retained a programmed function, expressing green fluorescent protein. This research provides a scalable method to fabricate advanced biocomposite materials in industrially-compatible processes.
- 5 November 2021
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 23 (23) , 9658-9668
Semi-aromatic biobased polyesters derived from lignin and cyclic carbonates
Synthesis, characterization, and compostability of several biobased polyesters with a wide array of thermoplastic and elastic properties are described.
- 5 November 2021
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 23 (23) , 9658-9668
Semi-aromatic biobased polyesters derived from lignin and cyclic carbonates
Synthesis, characterization, and compostability of several biobased polyesters with a wide array of thermoplastic and elastic properties are described.
- 12 August 2021
- Published by American Chemical Society (ACS) in Environmental Science & Technology
- Vol. 55 (17) , 11646-11656
Comparative Study of the Biological Degradation of Poly(3-Hydroxybutyrate-co-3-Hydroxyhexanoate) Microbeads in Municipal Wastewater in Environmental and Controlled Laboratory Conditions
From April to June 2019, poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (P3(HA)) microbead samples were exposed to an operational wastewater reclamation facility (WWRF) in an aerobic aeration basin in Athens, Georgia. Samples were withdrawn from the facility over a 13-week timeframe, and the particles were examined by Raman microscopy and thermogravimetric analysis/mass spectroscopy (TGA/MS) coupled with differential scanning calorimetry (DSC). The activated sludge from this facility was also used as an inoculum to examine carbon mineralization under controlled respirometry experiments to corroborate biological degradation rates determined from both the environmental and laboratory approach. Respirometry, Raman microscopy, and TGA/MS-DSC methods all measured similar biodegradation timelines for microbeads bound to an epoxy substrate, indicating that the three methods are temporally comparable and may be used to measure material biological degradation. Samples of epoxy-bound P3(HA) microbeads, free microbeads, the P3(HA) film, and poly(lactic acid) (PLA) film demonstrated carbon mineralization of 90.0, 89.4, 95.0, and 8.15%, respectively, relative to the cellulose positive control. Using a modified Gompertz growth model, the biological degradation rate coefficients (Rm) were determined for cellulose, P3(HA) film, epoxy-bound P3(HA) microbeads, and free P3(HA) microbeads and found to be 31.6, 30.2, 17.5, and 18.7 mL CO2·g–1·day–1, respectively. Moreover, P3(HA) microbeads can efficiently mineralize in WWRF infrastructure at a rate comparable to cellulose.
- 12 August 2021
- Published by American Chemical Society (ACS) in Environmental Science & Technology
- Vol. 55 (17) , 11646-11656
Comparative Study of the Biological Degradation of Poly(3-Hydroxybutyrate-co-3-Hydroxyhexanoate) Microbeads in Municipal Wastewater in Environmental and Controlled Laboratory Conditions
From April to June 2019, poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (P3(HA)) microbead samples were exposed to an operational wastewater reclamation facility (WWRF) in an aerobic aeration basin in Athens, Georgia. Samples were withdrawn from the facility over a 13-week timeframe, and the particles were examined by Raman microscopy and thermogravimetric analysis/mass spectroscopy (TGA/MS) coupled with differential scanning calorimetry (DSC). The activated sludge from this facility was also used as an inoculum to examine carbon mineralization under controlled respirometry experiments to corroborate biological degradation rates determined from both the environmental and laboratory approach. Respirometry, Raman microscopy, and TGA/MS-DSC methods all measured similar biodegradation timelines for microbeads bound to an epoxy substrate, indicating that the three methods are temporally comparable and may be used to measure material biological degradation. Samples of epoxy-bound P3(HA) microbeads, free microbeads, the P3(HA) film, and poly(lactic acid) (PLA) film demonstrated carbon mineralization of 90.0, 89.4, 95.0, and 8.15%, respectively, relative to the cellulose positive control. Using a modified Gompertz growth model, the biological degradation rate coefficients (Rm) were determined for cellulose, P3(HA) film, epoxy-bound P3(HA) microbeads, and free P3(HA) microbeads and found to be 31.6, 30.2, 17.5, and 18.7 mL CO2·g–1·day–1, respectively. Moreover, P3(HA) microbeads can efficiently mineralize in WWRF infrastructure at a rate comparable to cellulose.
- 25 February 2021
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 3 (3) , 1652-1663
Blends of Poly(butylene glutarate) and Poly(lactic acid) with Enhanced Ductility and Composting Performance
- 25 February 2021
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 3 (3) , 1652-1663
Blends of Poly(butylene glutarate) and Poly(lactic acid) with Enhanced Ductility and Composting Performance
- 5 February 2021
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 9 (7) , 2736-2744
Respirometry and Cell Viability Studies for Sustainable Polyesters and Their Hydrolysis Products
- 5 February 2021
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 9 (7) , 2736-2744
Respirometry and Cell Viability Studies for Sustainable Polyesters and Their Hydrolysis Products
- 21 August 2019
- Published by American Chemical Society (ACS) in ACS Chemical Biology
- Vol. 14 (9) , 1921-1929
Fully Synthetic Heparan Sulfate-Based Neural Tissue Construct That Maintains the Undifferentiated State of Neural Stem Cells
Heparin and heparan sulfate (HS) are attractive components for constructing biomaterials due to their ability to recruit and regulate the activity of growth factors. The structural and functional heterogeneity of naturally derived heparin and HS is, however, an impediment for the preparation of biomaterials for regenerative medicine. To address this problem, we have prepared hydrogels modified by well-defined synthetic HS-derived disaccharides. Human induced pluripotent cell-derived neural stem cells (HIP-NSCs) encapsulated in a polyethylene glycol-based hydrogel modified by a pendent HS disaccharide that is a known ligand for fibroblast growth factor-2 (FGF-2) exhibited a significant increase in proliferation and self-renewal. This observation is important because evidence is emerging that undifferentiated stems cells can yield significant therapeutic benefits via their paracrine signaling mechanisms. Our data indicate that the HS disaccharide protects FGF-2, which has a very short biological half-live, from degradation. It is anticipated that, by careful selection of a synthetic HS oligosaccharide, it will be possible to control retention and release of specific growth factor, which in turn will provide control over cell fate.
- 21 August 2019
- Published by American Chemical Society (ACS) in ACS Chemical Biology
- Vol. 14 (9) , 1921-1929
Fully Synthetic Heparan Sulfate-Based Neural Tissue Construct That Maintains the Undifferentiated State of Neural Stem Cells
Heparin and heparan sulfate (HS) are attractive components for constructing biomaterials due to their ability to recruit and regulate the activity of growth factors. The structural and functional heterogeneity of naturally derived heparin and HS is, however, an impediment for the preparation of biomaterials for regenerative medicine. To address this problem, we have prepared hydrogels modified by well-defined synthetic HS-derived disaccharides. Human induced pluripotent cell-derived neural stem cells (HIP-NSCs) encapsulated in a polyethylene glycol-based hydrogel modified by a pendent HS disaccharide that is a known ligand for fibroblast growth factor-2 (FGF-2) exhibited a significant increase in proliferation and self-renewal. This observation is important because evidence is emerging that undifferentiated stems cells can yield significant therapeutic benefits via their paracrine signaling mechanisms. Our data indicate that the HS disaccharide protects FGF-2, which has a very short biological half-live, from degradation. It is anticipated that, by careful selection of a synthetic HS oligosaccharide, it will be possible to control retention and release of specific growth factor, which in turn will provide control over cell fate.
- 17 August 2018
- Published by American Chemical Society (ACS) in Environmental Science & Technology
- Vol. 52 (18) , 10307-10316
Ingested Micronizing Plastic Particle Compositions and Size Distributions within Stranded Post-Hatchling Sea Turtles
From July 2015 to November 2016, 96 post-hatchling sea turtles were collected from 118 km of Atlantic coastline in Florida, USA, including loggerhead, green, and hawksbill sea turtle species. Forty-five of the recovered turtles were rehabilitated and released, but the remaining 52 died and were frozen. At necropsy, the gastrointestinal tracts of most the turtles contained visible plastic, and collected particles of 27 individuals were chemically characterized by Raman microscopy as polyethylene, polypropylene, polyethylene terephthalate, and polystyrene. Mesoparticle plastic fragments 1.0 to 8.7 mm, microparticle fragments 20 to 1000 µm, and nanoparticles 5 to 169 nm were identified in the turtles. Polyethylene and polypropylene were the most common plastics ingested from specimens representing 54.1% and 23.7% of the total observed mesoparticles and 11.7% and 21.0% of the total observed microparticles, respectively. A plastic-to-body mass ratio of 2.07 mg/g was determined for this group. The authors suggest that ingestion of micronizing plastic by post-hatchling sea turtles is likely a substantial risk to survival of these endangered and threatened species. This study also provides some of the first evidence for the formation of nanoscopic plastic particles that we theorize forms in the post-hatchling and juvenile environment and are present post-ingestion.
- 17 August 2018
- Published by American Chemical Society (ACS) in Environmental Science & Technology
- Vol. 52 (18) , 10307-10316
Ingested Micronizing Plastic Particle Compositions and Size Distributions within Stranded Post-Hatchling Sea Turtles
From July 2015 to November 2016, 96 post-hatchling sea turtles were collected from 118 km of Atlantic coastline in Florida, USA, including loggerhead, green, and hawksbill sea turtle species. Forty-five of the recovered turtles were rehabilitated and released, but the remaining 52 died and were frozen. At necropsy, the gastrointestinal tracts of most the turtles contained visible plastic, and collected particles of 27 individuals were chemically characterized by Raman microscopy as polyethylene, polypropylene, polyethylene terephthalate, and polystyrene. Mesoparticle plastic fragments 1.0 to 8.7 mm, microparticle fragments 20 to 1000 µm, and nanoparticles 5 to 169 nm were identified in the turtles. Polyethylene and polypropylene were the most common plastics ingested from specimens representing 54.1% and 23.7% of the total observed mesoparticles and 11.7% and 21.0% of the total observed microparticles, respectively. A plastic-to-body mass ratio of 2.07 mg/g was determined for this group. The authors suggest that ingestion of micronizing plastic by post-hatchling sea turtles is likely a substantial risk to survival of these endangered and threatened species. This study also provides some of the first evidence for the formation of nanoscopic plastic particles that we theorize forms in the post-hatchling and juvenile environment and are present post-ingestion.