Chandra Sekhar Gahan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Chandra Sekhar Gahan has a total of 59 co-authors. Here are the top co-authors by number of shared publications:
Himanshi Garg
Department of Microbiology School of Life Sciences Central University of Rajasthan NH‐8, Bandarsindri, Tehsil Kishangarh, District Ajmer 305817 Rajasthan India
6 shared publications- Åke Sandström
Div. of Sustainable Process Engineering, Luleå University of Technology, SE-971 87 Luleå, Sweden
6 shared publications Neha Nagar
Department of Microbiology, School of Life Sciences, Central University of Rajasthan, Rajasthan, India
5 shared publications- Neha Nagar
Department of Microbiology, School of Life Sciences, Central University of Rajasthan, Ajmer, India
4 shared publications Shatakshi Tiwari
Central University of Rajasthan
4 shared publicationsSugandha Aachhera
Central University of Rajasthan
4 shared publications
Latest Publications
- 17 July 2026
- Published by Springer Nature
- p. 241-269
Electronic Waste Management in Megacities: A Review
- 17 July 2026
- Published by Springer Nature
- p. 241-269
Electronic Waste Management in Megacities: A Review
- 7 January 2026
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 12 (2) , 1346-1362
Innovative Approach in Fed-Batch Bioleaching of Zinc Sulfide Concentrate Using Iron-Oxidizing Microorganisms Under Controlled Redox Potential
- 7 January 2026
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 12 (2) , 1346-1362
Innovative Approach in Fed-Batch Bioleaching of Zinc Sulfide Concentrate Using Iron-Oxidizing Microorganisms Under Controlled Redox Potential
- Open Access
- 28 July 2025
- Published by Slovak University of Agriculture in Nitra in Journal of microbiology, biotechnology and food sciences
- p. e12378
TWO-STEP LEACHING OF METAL VALUES FROM DISCARDED MOBILE PHONE PRINTED CIRCUIT BOARD USING BIOGENIC FERRIC ION WITH COPPER LEACHING KINETICS
Discarded mobile phone printed circuit boards (mobile phone PCBs), a prominent component of electronic waste, represent a significant secondary resource for metal recovery. Mobile phone PCBs contain significant amounts of copper and other critical metals, making them a good option for bioleaching, which is a sustainable and environmentally friendly alternative to conventional metal extraction methods. However, slow reaction kinetics often hinder bioleaching, limiting its industrial-scale applicability. This study utilized mixed culture consortia of iron oxidizing microorganisms dominated by Leptospirillum ferriphilum, which were chemolithotrophic microbes thriving in highly acidic conditions and high ferric iron concentrations responsible for enhanced copper recovery through a two-step bioleaching process. All the bioleaching experiments were conducted at a controlled temperature of 35±5 ℃ and pH controlled to 1.5 with a Pulp Density (P.D.) of 10% while varying biogenic ferric iron concentrations from 9–18 g/L, which served as the main lixiviant for metal extraction. The results demonstrated that increasing biogenic ferric iron concentration significantly improved copper recovery and reduced leaching time. In the first leaching step, 50-83% copper extraction efficiencies were achieved at biogenic ferric iron concentrations of 9-18 g/L. During the second leaching step, copper extraction exceeded 99% within 5.5-3.5 days for the corresponding ferric concentrations. The elevated biogenic ferric iron levels facilitated this rapid and efficient copper extraction, accelerating the leaching kinetics. Post-leaching analyses, including XRF, SEM-EDS, and XRD, confirmed >95% copper recovery following solid-liquid separation. The study highlights the effectiveness of the two-step bioleaching process and underscores the potential of biogenic ferric iron in overcoming the limitations of traditional bioleaching methods. This research demonstrates a fast, simple, and sustainable bioleaching method for the efficient recovery of copper from mobile phone PCBs, offering a promising pathway for industrial applications in e-waste management and contributing to the circular economy.
- 28 July 2025
- Published by Slovak University of Agriculture in Nitra in Journal of microbiology, biotechnology and food sciences
- p. e12378
Open AccessTWO-STEP LEACHING OF METAL VALUES FROM DISCARDED MOBILE PHONE PRINTED CIRCUIT BOARD USING BIOGENIC FERRIC ION WITH COPPER LEACHING KINETICS
Discarded mobile phone printed circuit boards (mobile phone PCBs), a prominent component of electronic waste, represent a significant secondary resource for metal recovery. Mobile phone PCBs contain significant amounts of copper and other critical metals, making them a good option for bioleaching, which is a sustainable and environmentally friendly alternative to conventional metal extraction methods. However, slow reaction kinetics often hinder bioleaching, limiting its industrial-scale applicability. This study utilized mixed culture consortia of iron oxidizing microorganisms dominated by Leptospirillum ferriphilum, which were chemolithotrophic microbes thriving in highly acidic conditions and high ferric iron concentrations responsible for enhanced copper recovery through a two-step bioleaching process. All the bioleaching experiments were conducted at a controlled temperature of 35±5 ℃ and pH controlled to 1.5 with a Pulp Density (P.D.) of 10% while varying biogenic ferric iron concentrations from 9–18 g/L, which served as the main lixiviant for metal extraction. The results demonstrated that increasing biogenic ferric iron concentration significantly improved copper recovery and reduced leaching time. In the first leaching step, 50-83% copper extraction efficiencies were achieved at biogenic ferric iron concentrations of 9-18 g/L. During the second leaching step, copper extraction exceeded 99% within 5.5-3.5 days for the corresponding ferric concentrations. The elevated biogenic ferric iron levels facilitated this rapid and efficient copper extraction, accelerating the leaching kinetics. Post-leaching analyses, including XRF, SEM-EDS, and XRD, confirmed >95% copper recovery following solid-liquid separation. The study highlights the effectiveness of the two-step bioleaching process and underscores the potential of biogenic ferric iron in overcoming the limitations of traditional bioleaching methods. This research demonstrates a fast, simple, and sustainable bioleaching method for the efficient recovery of copper from mobile phone PCBs, offering a promising pathway for industrial applications in e-waste management and contributing to the circular economy.
- 21 January 2022
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 8 (1) , 333-342
Bioleaching of Zinc Sulfide Concentrate in Redox-Controlled Fed-Batch Process Compared to Redox Non-controlled Batch Process
- 21 January 2022
- Published by Springer Nature in Journal of Sustainable Metallurgy
- Vol. 8 (1) , 333-342
Bioleaching of Zinc Sulfide Concentrate in Redox-Controlled Fed-Batch Process Compared to Redox Non-controlled Batch Process
- 8 September 2021
- Published by Springer Nature in Ecotoxicology
- Vol. 31 (4) , 615-625
A study on the biosorption kinetics of Cu (II) and Zn (II) ions from aqueous phase (sulphate medium) using waste sawdust generated from Acacia nilotica wood carpentry
In the present study, the natural biosorption capacity of Acacia nilotica sawdust (wood biomass) was studied for the removal of copper (Cu) and zinc (Zn) heavy metal ions. The process was optimized for several important factors such as pH, contact time, biomass amount, and metal ion concentration. The maximum biosorption of Zn onto Acacia nilotica sawdust was 66.092% at pH 7.0, contact time 20 min, biomass concentration 0.4 g, and initial Zn concentration 8.4 mg/L. The maximum Cu biosorption to Acacia nilotica sawdust was 66.097% at pH 4, contact time 45 min, biomass 0.8 g, initial metal ion concentration 27 mg/L. The experimental data were analyzed by two different adsorption isotherms i.e. Langmuir and Freundlich models. Based on the regression coefficient the Freundlich isotherm model showed the best fit for Zn whereas Cu metal ion adsorption gave a favorable fit for Langmuir isotherm. Both metal ions followed pseudo-second-order kinetics in the adsorption process using sawdust of Acacia nilotica.
- 8 September 2021
- Published by Springer Nature in Ecotoxicology
- Vol. 31 (4) , 615-625
A study on the biosorption kinetics of Cu (II) and Zn (II) ions from aqueous phase (sulphate medium) using waste sawdust generated from Acacia nilotica wood carpentry
In the present study, the natural biosorption capacity of Acacia nilotica sawdust (wood biomass) was studied for the removal of copper (Cu) and zinc (Zn) heavy metal ions. The process was optimized for several important factors such as pH, contact time, biomass amount, and metal ion concentration. The maximum biosorption of Zn onto Acacia nilotica sawdust was 66.092% at pH 7.0, contact time 20 min, biomass concentration 0.4 g, and initial Zn concentration 8.4 mg/L. The maximum Cu biosorption to Acacia nilotica sawdust was 66.097% at pH 4, contact time 45 min, biomass 0.8 g, initial metal ion concentration 27 mg/L. The experimental data were analyzed by two different adsorption isotherms i.e. Langmuir and Freundlich models. Based on the regression coefficient the Freundlich isotherm model showed the best fit for Zn whereas Cu metal ion adsorption gave a favorable fit for Langmuir isotherm. Both metal ions followed pseudo-second-order kinetics in the adsorption process using sawdust of Acacia nilotica.
- 27 May 2021
- Published by Wiley in Environmental Quality Management
- Vol. 31 (4) , 63-73
Comparative biosorption kinetics study of Ni and Zn metal ions from the aqueous phase in sulfate medium by the wooden biomass of Dalbergia sissoo
- 27 May 2021
- Published by Wiley in Environmental Quality Management
- Vol. 31 (4) , 63-73
Comparative biosorption kinetics study of Ni and Zn metal ions from the aqueous phase in sulfate medium by the wooden biomass of Dalbergia sissoo
- 25 February 2021
- Published by Springer Nature in 3 Biotech
- Vol. 11 (3) , 1-13
Effect of pulp density on the bioleaching of metals from petroleum refinery spent catalyst
Bioleaching is one of the well-known methods of metal recovery with Environmental benefits. This process has been extensively used for combating improper waste management issues along with metal reclamation. The aim of this study is to bioleach spent petroleum refinery catalyst at variant pulp densities (PD) (5, 10 and 15%) using microorganisms in acidic pH (1.5–1.6) and mesophilic temperature (30–35 °C). The study includes leaching yields of metals like nickel, molybdenum, copper and aluminum. The three bioleaching experiments with different pulp densities yielded a maximum of more than 90% nickel, 73% copper, 87% molybdenum and 24% aluminum. The results are validated 5, 10, and 15% pulp density and the result is validated with pH, Redox potential, microbial population, sulphate concentration and ferrous iron, concentration. The time saving due to faster nickel dissolution using iron and sulphur oxidizing microorganisms would be economical for the bioleaching process.
- 25 February 2021
- Published by Springer Nature in 3 Biotech
- Vol. 11 (3) , 1-13
Effect of pulp density on the bioleaching of metals from petroleum refinery spent catalyst
Bioleaching is one of the well-known methods of metal recovery with Environmental benefits. This process has been extensively used for combating improper waste management issues along with metal reclamation. The aim of this study is to bioleach spent petroleum refinery catalyst at variant pulp densities (PD) (5, 10 and 15%) using microorganisms in acidic pH (1.5–1.6) and mesophilic temperature (30–35 °C). The study includes leaching yields of metals like nickel, molybdenum, copper and aluminum. The three bioleaching experiments with different pulp densities yielded a maximum of more than 90% nickel, 73% copper, 87% molybdenum and 24% aluminum. The results are validated 5, 10, and 15% pulp density and the result is validated with pH, Redox potential, microbial population, sulphate concentration and ferrous iron, concentration. The time saving due to faster nickel dissolution using iron and sulphur oxidizing microorganisms would be economical for the bioleaching process.
- Open Access
- 1 January 2021
- Published by Syncsci Publishing Pte., Ltd. in Chemical Reports
- Vol. 3 (1) , 177-187
Characterization of different types of petroleum refinery spent catalyst followed by microbial mediated leaching of metal values
The present study aims for characterization and classification of five different spent petroleum refinery catalysts followed by metal recovery via bioleaching. The nomenclature given to the different spent catalyst (SC) is SC1, SC2, SC3, SC4 and SC5 collected from an Indian petroleum refinery. All spent catalysts were crushed and ground prior to their characterization by X-Ray Fluorescence for chemical composition followed by X-Ray Diffraction and Scanning Electron Microscopy-Energy Dispersive X-Ray Spectroscopy for their mineralogy. Further, all five spent catalysts were classified based upon their chemical composition and mineralogy. Metal recovery from the spent catalysts was carried out by bioleaching by a mixed microbial consortium of iron and Sulphur oxidizing microorganisms. Most of the spent catalysts showed very significant metal recovery with respect to Ni, Cu, Cr, Mo, Zn, Sr and Ti. The study provides a possible metal recovery route via bioleaching for further testing and scaling up.
- 1 January 2021
- Published by Syncsci Publishing Pte., Ltd. in Chemical Reports
- Vol. 3 (1) , 177-187
Open AccessCharacterization of different types of petroleum refinery spent catalyst followed by microbial mediated leaching of metal values
The present study aims for characterization and classification of five different spent petroleum refinery catalysts followed by metal recovery via bioleaching. The nomenclature given to the different spent catalyst (SC) is SC1, SC2, SC3, SC4 and SC5 collected from an Indian petroleum refinery. All spent catalysts were crushed and ground prior to their characterization by X-Ray Fluorescence for chemical composition followed by X-Ray Diffraction and Scanning Electron Microscopy-Energy Dispersive X-Ray Spectroscopy for their mineralogy. Further, all five spent catalysts were classified based upon their chemical composition and mineralogy. Metal recovery from the spent catalysts was carried out by bioleaching by a mixed microbial consortium of iron and Sulphur oxidizing microorganisms. Most of the spent catalysts showed very significant metal recovery with respect to Ni, Cu, Cr, Mo, Zn, Sr and Ti. The study provides a possible metal recovery route via bioleaching for further testing and scaling up.
- Open Access
Bench scale microbial catalysed leaching of mobile phone PCBs with an increasing pulp density
- 21 September 2019
- Published by Springer Nature in International Journal of Environmental Science and Technology
- Vol. 17 (6) , 3165-3176
Bioleaching of waste mobile phone printed circuit board in controlled redox potential compared to non-controlled redox potential
- 21 September 2019
- Published by Springer Nature in International Journal of Environmental Science and Technology
- Vol. 17 (6) , 3165-3176
Bioleaching of waste mobile phone printed circuit board in controlled redox potential compared to non-controlled redox potential