Edson Edain González Arredondo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Edson Edain González Arredondo has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Ricardo Rangel
División de Estudios de Posgrado de la Facultad de Ingeniería Química, Universidad Michoacana de San Nicolás de Hidalgo, Morelia, Mexico
3 shared publications - Armando Ramos Corona
Cinvestav Unidad Mérida Carretera Antigua a Progreso Km. 6
2 shared publications - Javier Lara-Romero
Facultad de Ingeniería Química, Universidad Michoacana de San Nicolás de Hidalgo, Morelia, Mexico
2 shared publications - Juan José Alvarado Gil
Applied Physics Department, Cinvestav-Unidad Mérida, Mérida, México
2 shared publications A. Solís-Garcia
1 shared publicationA. Solís-García
1 shared publication
Latest Publications
- Open Access
- 30 July 2026
- Published by Universidad Autonoma Metropolitana in AZCATL
- Vol. 04 (08) , 22-25
Películas delgadas: coberturas increíbles que transforman la vida
En los últimos años, el desarrollo tecnológico ha transformado profundamente nuestra vida diaria. Los teléfonos celulares, los lentes con recubrimiento antirreflejante o los paneles solares son ejemplos de ello. Aunque parecen muy distintos, todos comparten un punto clave: los recubrimientos llamados películas delgadas. Estas capas, casi invisibles para el ojo humano, se depositan sobre distintos materiales para modificar sus propiedades, por ejemplo, permiten que conduzcan mejor la electricidad, reflejen menos la luz o capten energía solar con mayor eficacia. Gracias a estas películas delgadas, muchos dispositivos modernos funcionan tal como los conocemos hoy en día.
- 30 July 2026
- Published by Universidad Autonoma Metropolitana in AZCATL
- Vol. 04 (08) , 22-25
Open AccessPelículas delgadas: coberturas increíbles que transforman la vida
En los últimos años, el desarrollo tecnológico ha transformado profundamente nuestra vida diaria. Los teléfonos celulares, los lentes con recubrimiento antirreflejante o los paneles solares son ejemplos de ello. Aunque parecen muy distintos, todos comparten un punto clave: los recubrimientos llamados películas delgadas. Estas capas, casi invisibles para el ojo humano, se depositan sobre distintos materiales para modificar sus propiedades, por ejemplo, permiten que conduzcan mejor la electricidad, reflejen menos la luz o capten energía solar con mayor eficacia. Gracias a estas películas delgadas, muchos dispositivos modernos funcionan tal como los conocemos hoy en día.
- Open Access
Manufacturing and Physicochemical Characterization of {Pt, Ir}/CeRuO2 Solid Solutions Tested in CO Oxidation
Nanoparticle powders of a Ce1−xRuxO2 mixed oxide (3.0% w/w), were synthesized to be used as catalytic supports, on which Pt and Ir nanoparticles were deposited as the active phase. The catalytic supports were prepared through a route involving microwave heating, while the Pt or Ir nanoparticles were incorporated via the wet incipient method. The {Pt, Ir/Ce1−xRuxO2} catalytic systems were successfully tested as catalysts for low-temperature CO oxidation. To provide adequate support to our results, the compounds were characterized by SEM, EDS, XRD, DRS-UV-vis, and XPS techniques. In addition, BET isotherms were carried out to determine specific surface area features. The CO oxidation evolution was tested in the range of 25–350 °C. Both Pt and Ir supported Ce1−xRuxO2 catalysts that remarkably improved the CO oxidation, reaching and sustaining 100% conversion from 125 °C onwards. Remarkably, the mixed oxide support, by itself, showed outstanding performance, achieving 100% conversion to CO2, at a temperature of 225 °C.
Open AccessManufacturing and Physicochemical Characterization of {Pt, Ir}/CeRuO2 Solid Solutions Tested in CO Oxidation
Nanoparticle powders of a Ce1−xRuxO2 mixed oxide (3.0% w/w), were synthesized to be used as catalytic supports, on which Pt and Ir nanoparticles were deposited as the active phase. The catalytic supports were prepared through a route involving microwave heating, while the Pt or Ir nanoparticles were incorporated via the wet incipient method. The {Pt, Ir/Ce1−xRuxO2} catalytic systems were successfully tested as catalysts for low-temperature CO oxidation. To provide adequate support to our results, the compounds were characterized by SEM, EDS, XRD, DRS-UV-vis, and XPS techniques. In addition, BET isotherms were carried out to determine specific surface area features. The CO oxidation evolution was tested in the range of 25–350 °C. Both Pt and Ir supported Ce1−xRuxO2 catalysts that remarkably improved the CO oxidation, reaching and sustaining 100% conversion from 125 °C onwards. Remarkably, the mixed oxide support, by itself, showed outstanding performance, achieving 100% conversion to CO2, at a temperature of 225 °C.
- 1 June 2022
- Published by Elsevier in Catalysis Today
- Vol. 392-393, 3-12
Pt and Ir supported on mixed Ce0.97Ru0.03O2 oxide as low-temperature CO oxidation catalysts
- 1 June 2022
- Published by Elsevier in Catalysis Today
- Vol. 392-393, 3-12
Pt and Ir supported on mixed Ce0.97Ru0.03O2 oxide as low-temperature CO oxidation catalysts
- 1 September 2020
- Published by Elsevier in Molecular Catalysis
- Vol. 493
FTIR investigation under reaction conditions during CO oxidation over Ru(x)-CeO2 catalysts
- 1 September 2020
- Published by Elsevier in Molecular Catalysis
- Vol. 493
FTIR investigation under reaction conditions during CO oxidation over Ru(x)-CeO2 catalysts
- Open Access
{CeO2/Bi2Mo1−xRuxO6} and {Au/Bi2Mo1−xRuxO6} Catalysts for Low-Temperature CO Oxidation
Nowadays, one of the most important challenges that humanity faces is to find alternative ways of reducing pollutant emissions. CeO2/Bi2Mo1−xRuxO6 and Au/Bi2Mo1−xRuxO6 catalysts were prepared to efficiently transform carbon monoxide (CO) to carbon dioxide (CO2) at low temperatures. The systems were prepared in a two-step process. First, Bi2Mo1−xRuxO6 supports were synthesized through the hydrothermal procedure under microwave heating. Then, CeO2 was deposited on Bi2Mo1−xRuxO6 using the wet impregnation method, while the incipient impregnation method was selected to deposit gold nanoparticles. The CeO2/Bi2Mo1−xRuxO6 and Au/Bi2Mo1−xRuxO6 catalysts were characterized using SEM microscopy and XRD. Furthermore, energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and Raman spectroscopy were used. Tests were carried out for the supported catalysts in CO oxidation, and high conversion values, nearing 100%, was observed in a temperature range of 100 to 250 °C. The results showed that the best system was the Au/Bi2Mo0.95Ru0.05O6 catalyst, with CO oxidation starting at 50 °C and reaching 100% conversion at 186 °C.
Open Access{CeO2/Bi2Mo1−xRuxO6} and {Au/Bi2Mo1−xRuxO6} Catalysts for Low-Temperature CO Oxidation
Nowadays, one of the most important challenges that humanity faces is to find alternative ways of reducing pollutant emissions. CeO2/Bi2Mo1−xRuxO6 and Au/Bi2Mo1−xRuxO6 catalysts were prepared to efficiently transform carbon monoxide (CO) to carbon dioxide (CO2) at low temperatures. The systems were prepared in a two-step process. First, Bi2Mo1−xRuxO6 supports were synthesized through the hydrothermal procedure under microwave heating. Then, CeO2 was deposited on Bi2Mo1−xRuxO6 using the wet impregnation method, while the incipient impregnation method was selected to deposit gold nanoparticles. The CeO2/Bi2Mo1−xRuxO6 and Au/Bi2Mo1−xRuxO6 catalysts were characterized using SEM microscopy and XRD. Furthermore, energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and Raman spectroscopy were used. Tests were carried out for the supported catalysts in CO oxidation, and high conversion values, nearing 100%, was observed in a temperature range of 100 to 250 °C. The results showed that the best system was the Au/Bi2Mo0.95Ru0.05O6 catalyst, with CO oxidation starting at 50 °C and reaching 100% conversion at 186 °C.