Stanislav S. Gornostayev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Stanislav S. Gornostayev has a total of 51 co-authors. Here are the top co-authors by number of shared publications:
Jouko J. Härkki
Tyrskyvuori 2 E 74; Espoo 02320 Finland
6 shared publicationsTimo M. J. Fabritius
University of Oulu Pentti Kaiteran katu 1, 90014 Oulu Finland
6 shared publicationsJyrki J. Heino
University of Oulu Pentti Kaiteran katu 1, 90014 Oulu Finland
4 shared publicationsTimo Fabritius
Process Metallurgy Research Unit University of Oulu BOX 4300, Oulu, 90014 Finland
4 shared publicationsEetu‐Pekka Heikkinen
Process Metallurgy Research Unit University of Oulu BOX 4300, Oulu, 90014 Finland
3 shared publicationsJyrki Heino
Process Metallurgy Research Unit University of Oulu BOX 4300, Oulu, 90014 Finland
3 shared publications
Latest Publications
- 27 February 2019
- Published by Wiley in Steel Research International
- Vol. 90 (6)
Occurrence and Behavior of Phosphorus‐Bearing Minerals in Metallurgical Coke
The behavior of phosphorus‐bearing minerals is characterized from coking coals to the feed coke and the blast furnace (BF) coke using scanning electron microscope and thermodynamic calculations. In coals, they are represented mostly by apatite (major phase, used for thermodynamic calculations), crandallite, gorceixite, goyazite, monazite and xenotime. Apatite fully transforms to Ca4P2O9 and Ca3P2O8 at coking temperatures. In the samples of BF coke, phosphorus‐bearing phases are 5–30 μm in size. In the case of a closed system (inside pieces of coke, no gas), phosphorus is presented in the BF in the form of Ca4P2O9 and Ca3P2O8 up to 1250 °C. Above this temperature, it is transformed to Fe3P (stable until 1495 °C). A further rise in temperature leads to the transformation of Fe3P to Fe2P (stable up to 1930 °C − tuyere level of the BF). In the case of an open system with intensive flow of BF gas, the formation of Fe3P from Ca4P2O9 and Ca3P2O8 starts at 1178 °C. The Fe2P appears near 1494–1495 °C, and after that it goes to a molten state.
- 27 February 2019
- Published by Wiley in Steel Research International
- Vol. 90 (6)
Occurrence and Behavior of Phosphorus‐Bearing Minerals in Metallurgical Coke
The behavior of phosphorus‐bearing minerals is characterized from coking coals to the feed coke and the blast furnace (BF) coke using scanning electron microscope and thermodynamic calculations. In coals, they are represented mostly by apatite (major phase, used for thermodynamic calculations), crandallite, gorceixite, goyazite, monazite and xenotime. Apatite fully transforms to Ca4P2O9 and Ca3P2O8 at coking temperatures. In the samples of BF coke, phosphorus‐bearing phases are 5–30 μm in size. In the case of a closed system (inside pieces of coke, no gas), phosphorus is presented in the BF in the form of Ca4P2O9 and Ca3P2O8 up to 1250 °C. Above this temperature, it is transformed to Fe3P (stable until 1495 °C). A further rise in temperature leads to the transformation of Fe3P to Fe2P (stable up to 1930 °C − tuyere level of the BF). In the case of an open system with intensive flow of BF gas, the formation of Fe3P from Ca4P2O9 and Ca3P2O8 starts at 1178 °C. The Fe2P appears near 1494–1495 °C, and after that it goes to a molten state.
- 8 February 2018
- Published by Wiley in Steel Research International
- Vol. 89 (4)
Occurrence and Behavior of Sulfur‐Bearing Minerals in Metallurgical Coke
The behavior of sulfur‐bearing minerals is characterized from coking coals to the feed coke and the blast furnace (BF) coke using field emission scanning electron microscope and thermodynamic calculations. In coals, they are represented by sulfides (pyrite, sphalerite, galena, chalcopyrite, and arsenopyrite) and sulfates (anhydrite and barite). During coking process, the minerals undergo phase transformations, but sulfur will be retained in the coke in mineral form for most of the minerals until the end of the coking process. Depending on the initial mineral in the coal, sulfur‐bearing minerals will be transformed at the end of coking process into the following phases: pyrrhotite, wurtzite, Cu–Fe–S melt, CaS, and BaS. The amount of sulfur that will be kept in the coke in mineral form increases in the following order: galena → pyrite → sphalerite → arsenopyrite → chalcopyrite → anhydrite → barite. Intensive gas flow under BF conditions facilitates liberation of sulfur from mineral phases in the Fe–S and Zn–S system. CaS and BaS are the most stable sulfur‐bearing phases formed after sulfur‐bearings minerals. The coals with elevated amounts of anhydrite and barite, or with high concentrations of Ca and Ba combined with S should be avoided for coking purposes. Complete elimination of mineral‐related sulfur from coke under BF conditions occurs above 2000 °C.
- 8 February 2018
- Published by Wiley in Steel Research International
- Vol. 89 (4)
Occurrence and Behavior of Sulfur‐Bearing Minerals in Metallurgical Coke
The behavior of sulfur‐bearing minerals is characterized from coking coals to the feed coke and the blast furnace (BF) coke using field emission scanning electron microscope and thermodynamic calculations. In coals, they are represented by sulfides (pyrite, sphalerite, galena, chalcopyrite, and arsenopyrite) and sulfates (anhydrite and barite). During coking process, the minerals undergo phase transformations, but sulfur will be retained in the coke in mineral form for most of the minerals until the end of the coking process. Depending on the initial mineral in the coal, sulfur‐bearing minerals will be transformed at the end of coking process into the following phases: pyrrhotite, wurtzite, Cu–Fe–S melt, CaS, and BaS. The amount of sulfur that will be kept in the coke in mineral form increases in the following order: galena → pyrite → sphalerite → arsenopyrite → chalcopyrite → anhydrite → barite. Intensive gas flow under BF conditions facilitates liberation of sulfur from mineral phases in the Fe–S and Zn–S system. CaS and BaS are the most stable sulfur‐bearing phases formed after sulfur‐bearings minerals. The coals with elevated amounts of anhydrite and barite, or with high concentrations of Ca and Ba combined with S should be avoided for coking purposes. Complete elimination of mineral‐related sulfur from coke under BF conditions occurs above 2000 °C.
- Open Access
Effect of Charcoal and Kraft-Lignin Addition on Coke Compression Strength and Reactivity
The aim of this research was to investigate the effects of charcoal and Kraft-lignin additions on the structure, cold compression strength, and reactivity of bio-cokes produced at the laboratory scale. Bio-cokes were prepared by adding charcoal and Kraft-lignin (2.5, 5.0, 7.5, and 10.0 wt %) to medium-volatile coal and coking the mixture with controlled heating rate (3.5 °C/min) up to 1200 °C. In addition, four particle sizes of charcoal were added with a 5 wt % addition rate to investigate the effect of particle size on the compression strength and reactivity. Thermogravimetric analysis was used to evaluate the pyrolysis behavior of coal and biomasses. Optical microscopy was used to investigate the interaction of coal and biomass components. It was found that by controlling the amount of charcoal and Kraft-lignin in the coal blend, the compression strength of the bio-cokes remains at an acceptable level compared to the reference coke without biomass addition. The cold compression strength of the charcoal bio-cokes was higher compared to Kraft-lignin bio-cokes. The reactivity of the bio-cokes with charcoal addition was markedly higher compared to reference coke and Kraft-lignin bio-cokes, mainly due to the differences in the physical properties of the parental biomass. By increasing the bulk density of the coal/biomass charge, the cold compression strength of the bio-cokes can be improved substantially.
Open AccessEffect of Charcoal and Kraft-Lignin Addition on Coke Compression Strength and Reactivity
The aim of this research was to investigate the effects of charcoal and Kraft-lignin additions on the structure, cold compression strength, and reactivity of bio-cokes produced at the laboratory scale. Bio-cokes were prepared by adding charcoal and Kraft-lignin (2.5, 5.0, 7.5, and 10.0 wt %) to medium-volatile coal and coking the mixture with controlled heating rate (3.5 °C/min) up to 1200 °C. In addition, four particle sizes of charcoal were added with a 5 wt % addition rate to investigate the effect of particle size on the compression strength and reactivity. Thermogravimetric analysis was used to evaluate the pyrolysis behavior of coal and biomasses. Optical microscopy was used to investigate the interaction of coal and biomass components. It was found that by controlling the amount of charcoal and Kraft-lignin in the coal blend, the compression strength of the bio-cokes remains at an acceptable level compared to the reference coke without biomass addition. The cold compression strength of the charcoal bio-cokes was higher compared to Kraft-lignin bio-cokes. The reactivity of the bio-cokes with charcoal addition was markedly higher compared to reference coke and Kraft-lignin bio-cokes, mainly due to the differences in the physical properties of the parental biomass. By increasing the bulk density of the coal/biomass charge, the cold compression strength of the bio-cokes can be improved substantially.
- 29 June 2017
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- Vol. 56 (3) , 252-258
Effect of micro-pores on cracks formation in metallurgical coke
The relationships of micro-pores and cracks in metallurgical coke have been investigated by optical microscope and field emission scanning electron microscope, using surface section samples. The pores have circular, elliptical and irregular shapes with smooth outlines, formed during the thermoplastic stage of the coking process. They often associate with connecting cracks between neighbouring pores. In case of elliptical pores, the connecting cracks are usually oriented along the longer axis of the pore. The connecting cracks can be developed between the pores, depending on their size and the distance between them. The coke with a large number of small pores rather than with a small number of larger pores will have lower strength due to the increased amount of connecting cracks. When compared with circular pores, elliptical and flattened pores have a lower ability to resist load pressure. Nano-sized pores have polygonal outlines, indicating an ‘explosion’-type formation in the solidified matrix. GRAPHICAL ABSTRACT
- 29 June 2017
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- Vol. 56 (3) , 252-258
Effect of micro-pores on cracks formation in metallurgical coke
The relationships of micro-pores and cracks in metallurgical coke have been investigated by optical microscope and field emission scanning electron microscope, using surface section samples. The pores have circular, elliptical and irregular shapes with smooth outlines, formed during the thermoplastic stage of the coking process. They often associate with connecting cracks between neighbouring pores. In case of elliptical pores, the connecting cracks are usually oriented along the longer axis of the pore. The connecting cracks can be developed between the pores, depending on their size and the distance between them. The coke with a large number of small pores rather than with a small number of larger pores will have lower strength due to the increased amount of connecting cracks. When compared with circular pores, elliptical and flattened pores have a lower ability to resist load pressure. Nano-sized pores have polygonal outlines, indicating an ‘explosion’-type formation in the solidified matrix. GRAPHICAL ABSTRACT
- 4 December 2015
- Published by Wiley in Steel Research International
- Vol. 87 (9) , 1144-1153
Behavior of Alkali‐Bearing Minerals in Coking and Blast Furnace Processes
The distribution, structural, and textural features, and behavior of alkali‐bearing (K and Na) minerals are characterized from coking coals to feed coke and blast furnace (BF) coke. In coals, they are mostly represented by phyllosilicates (illite, montmorillonite, biotite, and muscovite) and feldspars. During the coking process, phyllosilicates retain a layered texture of their aggregates. Under coking conditions, feldspars keep the original outlines of mineral grains and bulk composition. There are no substantial changes in the volume of mineral grains and these alkali‐bearing minerals have no physical effect on the coke matrix at coking temperatures. Thermodynamic calculations have shown that there are two major alkali‐bearing mineral phases left in the system toward the end of the coking process – albite and leucite. Under BF conditions, Na is fully transferred to the molten phase above 1000 °C, while K partly occurs in leucite up to 1434 °C. The formation of intercalation compounds under BF conditions starts at 1127–1136 °C. Since K is referred to as a main intercalate phase in coke, then attention should primarily be focused on the presence of K‐bearing minerals in coking coals. The quality of coals is assessed by the amount of K‐bearing phyllosilicates and K‐feldspars.
- 4 December 2015
- Published by Wiley in Steel Research International
- Vol. 87 (9) , 1144-1153
Behavior of Alkali‐Bearing Minerals in Coking and Blast Furnace Processes
The distribution, structural, and textural features, and behavior of alkali‐bearing (K and Na) minerals are characterized from coking coals to feed coke and blast furnace (BF) coke. In coals, they are mostly represented by phyllosilicates (illite, montmorillonite, biotite, and muscovite) and feldspars. During the coking process, phyllosilicates retain a layered texture of their aggregates. Under coking conditions, feldspars keep the original outlines of mineral grains and bulk composition. There are no substantial changes in the volume of mineral grains and these alkali‐bearing minerals have no physical effect on the coke matrix at coking temperatures. Thermodynamic calculations have shown that there are two major alkali‐bearing mineral phases left in the system toward the end of the coking process – albite and leucite. Under BF conditions, Na is fully transferred to the molten phase above 1000 °C, while K partly occurs in leucite up to 1434 °C. The formation of intercalation compounds under BF conditions starts at 1127–1136 °C. Since K is referred to as a main intercalate phase in coke, then attention should primarily be focused on the presence of K‐bearing minerals in coking coals. The quality of coals is assessed by the amount of K‐bearing phyllosilicates and K‐feldspars.
- Open Access
- 1 December 2015
- Published by Elsevier in Separation and Purification Technology
- Vol. 156, 724-737
Improvement of phosphorus removal from iron ore using combined microwave pretreatment and ultrasonic treatment
- 1 December 2015
- Published by Elsevier in Separation and Purification Technology
- Vol. 156, 724-737
Open AccessImprovement of phosphorus removal from iron ore using combined microwave pretreatment and ultrasonic treatment
- 9 July 2015
- Published by Springer Nature in International Journal of Minerals, Metallurgy and Materials
- Vol. 22 (7) , 697-703
Fe-Si particles on the surface of blast furnace coke
- 9 July 2015
- Published by Springer Nature in International Journal of Minerals, Metallurgy and Materials
- Vol. 22 (7) , 697-703
Fe-Si particles on the surface of blast furnace coke
- 3 October 2014
- Published by Springer Nature in International Journal of Minerals, Metallurgy and Materials
- Vol. 21 (10) , 969-973
Textural changes in metallurgical coke prepared with polyethylene
- 3 October 2014
- Published by Springer Nature in International Journal of Minerals, Metallurgy and Materials
- Vol. 21 (10) , 969-973
Textural changes in metallurgical coke prepared with polyethylene
- 28 April 2014
- Published by Wiley in Steel Research International
- Vol. 85 (12) , 1608-1619
The Hot Strength of Industrial Cokes – Evaluation of Coke Properties that Affect Its High‐Temperature Strength
The strength of coke at high temperatures is of major importance for efficient blast furnace operation. Despite this, there is little information regarding the hot strength of coke. In this research, the hot strength of three industrial European coke grades was studied using a Gleeble thermomechanical simulator. The hot strength was analyzed at three different temperatures: room temperature, 1600 and 1750 °C by measuring the compressive strength of roughly 50 coke samples at each temperature. A significant decrease in strength was observed for all three coke grades at high temperatures. Notable differences between the coke grades in compressive strength were observed at room temperature. At high temperatures, differences were observed in strength and deformation behavior; however, the order of magnitude of strength remained the same. The deformation behavior at high temperatures was also studied and discussed based on stress–strain curves. Several structural properties of coke such as total porosity, pore size distribution, pore shape factor, amount of inerts, and degree of graphitization were determined in order to explain the obtained strength results. Both hot and room temperature compressive strength values were compared to industrial strength tests and discussed. The reliability of the results was evaluated with statistical analyses.
- 28 April 2014
- Published by Wiley in Steel Research International
- Vol. 85 (12) , 1608-1619
The Hot Strength of Industrial Cokes – Evaluation of Coke Properties that Affect Its High‐Temperature Strength
The strength of coke at high temperatures is of major importance for efficient blast furnace operation. Despite this, there is little information regarding the hot strength of coke. In this research, the hot strength of three industrial European coke grades was studied using a Gleeble thermomechanical simulator. The hot strength was analyzed at three different temperatures: room temperature, 1600 and 1750 °C by measuring the compressive strength of roughly 50 coke samples at each temperature. A significant decrease in strength was observed for all three coke grades at high temperatures. Notable differences between the coke grades in compressive strength were observed at room temperature. At high temperatures, differences were observed in strength and deformation behavior; however, the order of magnitude of strength remained the same. The deformation behavior at high temperatures was also studied and discussed based on stress–strain curves. Several structural properties of coke such as total porosity, pore size distribution, pore shape factor, amount of inerts, and degree of graphitization were determined in order to explain the obtained strength results. Both hot and room temperature compressive strength values were compared to industrial strength tests and discussed. The reliability of the results was evaluated with statistical analyses.
- 2 April 2013
- Published by Wiley in Steel Research International
- Vol. 84 (11) , 1104-1109
Mineral Related CO2and H2O Emissions during the Production of Metallurgical Coke
- 2 April 2013
- Published by Wiley in Steel Research International
- Vol. 84 (11) , 1104-1109
Mineral Related CO2and H2O Emissions during the Production of Metallurgical Coke