Sigbjørn Grini
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Sigbjørn Grini has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Clas Persson
Department of Physics/Centre for Materials Science and Nanotechnology University of Oslo P.O. Box 1048, Blindern N-0316 Oslo Norway
4 shared publicationsNils Ross
Department of Physics/Centre for Materials Science and Nanotechnology University of Oslo P.O. Box 1048, Blindern N-0316 Oslo Norway
4 shared publicationsCharlotte Platzer-Björkman
Ångström Solar Center Division of Solid State Electronics Uppsala University Uppsala 75120 Sweden
3 shared publicationsLasse Vines
Department of Physics/Centre for Materials Science and Nanotechnology University of Oslo P.O. Box 1048, Blindern N-0316 Oslo Norway
3 shared publications- Lasse Vines
University of Oslo
2 shared publications Mattias Thuvander
Department of Physics Chalmers University of Technology 41296 Göteborg Sweden
2 shared publications
Latest Publications
- Open Access
- 12 June 2020
- Published by Wiley in Physica Status Solidi (b)
- Vol. 257 (6)
Dynamic Impurity Redistributions in Kesterite Absorbers
- 12 June 2020
- Published by Wiley in Physica Status Solidi (b)
- Vol. 257 (6)
Open AccessDynamic Impurity Redistributions in Kesterite Absorbers
- Open Access
- 26 March 2020
- Published by Wiley in Physica Status Solidi (b)
- Vol. 257 (6)
Dynamic Impurity Redistributions in Kesterite Absorbers
Cu2ZnSn(S,Se)4 is a promising nontoxic earth‐abundant solar cell absorber. To optimize the thin films for solar cell device performance, postdeposition treatments at temperatures below the crystallization temperature are normally performed, which alter the surface and bulk properties. The polycrystalline thin films contain relatively high concentrations of impurities, such as sodium, oxygen and hydrogen. During the treatments, these impurities migrate and likely agglomerate at lattice defects or interfaces. Herein, impurity redistribution after air annealing for temperatures up to 200 °C and short heavy water treatments are studied. In addition, nonuniformities of the sodium distribution on a nanometer and micrometer scale are characterized by atom probe tomography and secondary ion mass spectrometry, respectively. Sodium and oxygen correlate to a greater extent after heat treatments, supporting strong binding between the two impurities. Redistributions of these impurities occur even at room temperature over longer time periods. Heavy water treatments confirm out‐diffusion of sodium with more incorporation of oxygen and hydrogen. It is observed that the increased hydrogen content does not originate from the heavy water. The existence of an “ice‐like” layer on top of the Cu2ZnSnS4 layer is proposed.
- 26 March 2020
- Published by Wiley in Physica Status Solidi (b)
- Vol. 257 (6)
Open AccessDynamic Impurity Redistributions in Kesterite Absorbers
Cu2ZnSn(S,Se)4 is a promising nontoxic earth‐abundant solar cell absorber. To optimize the thin films for solar cell device performance, postdeposition treatments at temperatures below the crystallization temperature are normally performed, which alter the surface and bulk properties. The polycrystalline thin films contain relatively high concentrations of impurities, such as sodium, oxygen and hydrogen. During the treatments, these impurities migrate and likely agglomerate at lattice defects or interfaces. Herein, impurity redistribution after air annealing for temperatures up to 200 °C and short heavy water treatments are studied. In addition, nonuniformities of the sodium distribution on a nanometer and micrometer scale are characterized by atom probe tomography and secondary ion mass spectrometry, respectively. Sodium and oxygen correlate to a greater extent after heat treatments, supporting strong binding between the two impurities. Redistributions of these impurities occur even at room temperature over longer time periods. Heavy water treatments confirm out‐diffusion of sodium with more incorporation of oxygen and hydrogen. It is observed that the increased hydrogen content does not originate from the heavy water. The existence of an “ice‐like” layer on top of the Cu2ZnSnS4 layer is proposed.
- Open Access
- 4 June 2019
- Published by Wiley in Advanced Energy Materials
- Vol. 9 (27)
Strong Interplay between Sodium and Oxygen in Kesterite Absorbers: Complex Formation, Incorporation, and Tailoring Depth Distributions
Sodium and oxygen are prevalent impurities in kesterite solar cells. Both elements are known to strongly impact performance of the kesterite devices and can be connected to efficiency improvements seen after heat treatments. The sodium distribution in the kesterite absorber is commonly reported, whereas the oxygen distribution has received less attention. Here, a direct relationship between sodium and oxygen in kesterite absorbers is established using secondary ion mass spectrometry and explained by defect analyses within the density functional theory. The calculations reveal a binding energy of 0.76 eV between the substitutional defects NaCu and OS in the nearest neighbor configuration, indicating an abundance of NaO complexes in kesterite absorbers at relevant temperatures. Oxygen incorporation is studied by introducing isotopic 18O at different stages of the Cu2ZnSnS4/Mo/soda‐lime glass baseline processing. It is observed that oxygen from the Mo back contact and contaminations during the sulfurization are primary contributors to the oxygen distribution. Indeed, unintentional oxygen incorporation leads to immobilization of sodium. This results in a strong correlation between sodium and oxygen, in excellent agreement with the theoretical calculations. Consequently, oxygen availability should be monitored to optimize postdeposition heat treatments to control impurities in kesterite absorbers and ultimately, the solar cell efficiency.
- 4 June 2019
- Published by Wiley in Advanced Energy Materials
- Vol. 9 (27)
Open AccessStrong Interplay between Sodium and Oxygen in Kesterite Absorbers: Complex Formation, Incorporation, and Tailoring Depth Distributions
Sodium and oxygen are prevalent impurities in kesterite solar cells. Both elements are known to strongly impact performance of the kesterite devices and can be connected to efficiency improvements seen after heat treatments. The sodium distribution in the kesterite absorber is commonly reported, whereas the oxygen distribution has received less attention. Here, a direct relationship between sodium and oxygen in kesterite absorbers is established using secondary ion mass spectrometry and explained by defect analyses within the density functional theory. The calculations reveal a binding energy of 0.76 eV between the substitutional defects NaCu and OS in the nearest neighbor configuration, indicating an abundance of NaO complexes in kesterite absorbers at relevant temperatures. Oxygen incorporation is studied by introducing isotopic 18O at different stages of the Cu2ZnSnS4/Mo/soda‐lime glass baseline processing. It is observed that oxygen from the Mo back contact and contaminations during the sulfurization are primary contributors to the oxygen distribution. Indeed, unintentional oxygen incorporation leads to immobilization of sodium. This results in a strong correlation between sodium and oxygen, in excellent agreement with the theoretical calculations. Consequently, oxygen availability should be monitored to optimize postdeposition heat treatments to control impurities in kesterite absorbers and ultimately, the solar cell efficiency.
- 1 November 2018
- Published by Elsevier in Thin Solid Films
- Vol. 665, 159-163
Low temperature incorporation of selenium in Cu2ZnSnS4: Diffusion and nucleation
- 1 November 2018
- Published by Elsevier in Thin Solid Films
- Vol. 665, 159-163
Low temperature incorporation of selenium in Cu2ZnSnS4: Diffusion and nucleation
- Open Access
- 21 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 8 (4) , 1132-1141
Selenium Inclusion in Cu2ZnSn(S,Se)4Solar Cell Absorber Precursors for Optimized Grain Growth
Cu$_{2}$ZnSn(S,Se)$_{4}$ precursors are fabricated by compound cosputtering from metal sulfide and selenide targets, and annealed in mixed argon, sulfur, and selenium atmosphere at temperatures between 540 and 580 $^\circ$C and at pressures between 24 and 47 kPa. We produce solar cell devices from these absorbers that range from 2.0% to 9.0% power conversion efficiency. We extensively characterize the morphology and elemental composition of the absorbers, and are able to closely relate the annealing conditions, precursor sulfur–selenium content, device performance, and absorber quality. We develop a qualitative model which relates the sulfur–selenium distribution in the precursor and the relative partial pressures of sulfur and selenium during the annealing process to the absorber properties. We show that selenium inclusion in the precursor allows more rapid recrystallization of the absorber at lower temperature. Alternating stacking of sulfur and selenium containing precursor material leads to differential rates of recrystallization, which allows some control over the morphology of the annealed absorber and Zn(S,Se) secondary phase segregation in that absorber. We further show that selenium containing precursors can be used to fabricate the superior devices relative to sulfur-only precursors, when the annealing phase space is subject to severe practical restrictions.
- 21 May 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 8 (4) , 1132-1141
Open AccessSelenium Inclusion in Cu2ZnSn(S,Se)4Solar Cell Absorber Precursors for Optimized Grain Growth
Cu$_{2}$ZnSn(S,Se)$_{4}$ precursors are fabricated by compound cosputtering from metal sulfide and selenide targets, and annealed in mixed argon, sulfur, and selenium atmosphere at temperatures between 540 and 580 $^\circ$C and at pressures between 24 and 47 kPa. We produce solar cell devices from these absorbers that range from 2.0% to 9.0% power conversion efficiency. We extensively characterize the morphology and elemental composition of the absorbers, and are able to closely relate the annealing conditions, precursor sulfur–selenium content, device performance, and absorber quality. We develop a qualitative model which relates the sulfur–selenium distribution in the precursor and the relative partial pressures of sulfur and selenium during the annealing process to the absorber properties. We show that selenium inclusion in the precursor allows more rapid recrystallization of the absorber at lower temperature. Alternating stacking of sulfur and selenium containing precursor material leads to differential rates of recrystallization, which allows some control over the morphology of the annealed absorber and Zn(S,Se) secondary phase segregation in that absorber. We further show that selenium containing precursors can be used to fabricate the superior devices relative to sulfur-only precursors, when the annealing phase space is subject to severe practical restrictions.