Ankur V. Bansod
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ankur V. Bansod has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
Awanikumar P. Patil
Department of MME, Visvesvaraya National Institute of Technology, Nagpur, India
9 shared publications- Sourabh Shukla
Mechanical Engineering Department, G H Raisoni College of Engineering, Nagpur, India
8 shared publications - Awanikumar P. Patil
Visvesvaraya National Institute of Technology
7 shared publications - Abhijeet Premkumar Moon
Research and Development, Tata Steel Ltd., Jamshedpur, India
3 shared publications - Gabriel Gahiga
Department of Mechanical Engineering, Vel Tech Rangarajan Dr Sagunthala R&D Institute of Science and Technology, Avadi, Chennai, 600062, India
2 shared publications Nilay N Khobragade
Government College of Engineering Amravati, Amravati, Maharashtra, INDIA
2 shared publications
Latest Publications
- Open Access
- 21 March 2026
- Published by Jan Evangelista Purkyne University in Usti nad Labem in Manufacturing Technology
- Vol. 26 (1) , 78-87
Design and Life of a Ball Valve as per the ASME BPVC Section VIII by the Elastic Stress Analysis Method
- 21 March 2026
- Published by Jan Evangelista Purkyne University in Usti nad Labem in Manufacturing Technology
- Vol. 26 (1) , 78-87
Open AccessDesign and Life of a Ball Valve as per the ASME BPVC Section VIII by the Elastic Stress Analysis Method
- Open Access
- 1 March 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (3) , 036514
Effect of martensitic reversal and grain size on the corrosion and wear behaviour of Cr-Mn steel
In this study, the effect of corrosion and wear behaviour of Cr-Mn steel on fine grains were investigated. The sample were solution annealed (SA) for 1 h at 1050 °C and then cold rolled (CW) to 30%. Further the cold rolled sample were thermally aged (CW + TA) 900 °C for four hours. The findings showed that under the 10 N applied load, wear resistance increased with an increase in hardness and martensite fraction of the cold worked (CW) samples. However, the Cr-Mn steel had the superior wear resistance after thermal ageing (TA). In microstructural examination deformation bands can also be visible in cold work samples. The analysis implies that the γ-phase is apparent across all peaks within the spectra of SA samples. In instances involving 30% cold work, prominent α′ martensite peaks were observed, accompanied by minimal ε-martensite peaks. Electrochemical impedance spectroscopy (EIS) analysis discloses a reduction in impedance and a concurrent increase in the defect density of the passive film. The CW+TA structure with good inclusive performances created an early constant hardened layer, which didn’t delaminate and peel off prematurely, thereby effectively increasing the wear resistance, according to analysis of the wear mechanism. The results also concluded that the corrosion resistance of CW sample decreases due to SIM formation, however CW+TA sample provide better corrosion resistance due to smaller and refined grain size.
- 1 March 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (3) , 036514
Open AccessEffect of martensitic reversal and grain size on the corrosion and wear behaviour of Cr-Mn steel
In this study, the effect of corrosion and wear behaviour of Cr-Mn steel on fine grains were investigated. The sample were solution annealed (SA) for 1 h at 1050 °C and then cold rolled (CW) to 30%. Further the cold rolled sample were thermally aged (CW + TA) 900 °C for four hours. The findings showed that under the 10 N applied load, wear resistance increased with an increase in hardness and martensite fraction of the cold worked (CW) samples. However, the Cr-Mn steel had the superior wear resistance after thermal ageing (TA). In microstructural examination deformation bands can also be visible in cold work samples. The analysis implies that the γ-phase is apparent across all peaks within the spectra of SA samples. In instances involving 30% cold work, prominent α′ martensite peaks were observed, accompanied by minimal ε-martensite peaks. Electrochemical impedance spectroscopy (EIS) analysis discloses a reduction in impedance and a concurrent increase in the defect density of the passive film. The CW+TA structure with good inclusive performances created an early constant hardened layer, which didn’t delaminate and peel off prematurely, thereby effectively increasing the wear resistance, according to analysis of the wear mechanism. The results also concluded that the corrosion resistance of CW sample decreases due to SIM formation, however CW+TA sample provide better corrosion resistance due to smaller and refined grain size.
- Open Access
- 1 March 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (3) , 036513
Influence of filler wire on metallurgical, mechanical, and corrosion behaviour of 430 ferritic stainless steel using a fusion welding process
The advantage of ferritic stainless steels (FSS’s) over austenitic stainless steels is that they are less expensive alloys. This is due to low or negligible nickel in its alloying element which makes the steel affordable. This type of steel is highly recommended against chloride attack and is also machinable to produce various components for engineering applications. This study examines the effect of various fillers on 430 ferritic stainless steel (FSS). The austenitic (308) and ferritic (410) grades of filler were used to study the weldability, microstructure, mechanical properties, and corrosion resistance using tungsten inert gas welding. The findings showed the emergence of various complex phases in both the weld sample. The sample welded with 410 filler shows acicular ferrite, martensite and austenite. Whereas, austenite and vermicular ferrite are observed in the sample welded with 308 filler. Based on compositions and solidification modes, the mechanical properties of welded joints also vary. It was found that ferritic mode solidified welds dominated in terms of qualities, which was found in 410 filler. In the chloride solution, the behaviour of the pitting corrosion resistance of each weld varied. The sample welded with 410 was superior corrosion resistance. This is due to more δ-ferrite in the weld sample. Whereas, 308 showed poorer resistance against the simulated seawater solution. In 410 welds, a greater degree of sensitization was observed, as compared to 308 welds.
- 1 March 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (3) , 036513
Open AccessInfluence of filler wire on metallurgical, mechanical, and corrosion behaviour of 430 ferritic stainless steel using a fusion welding process
The advantage of ferritic stainless steels (FSS’s) over austenitic stainless steels is that they are less expensive alloys. This is due to low or negligible nickel in its alloying element which makes the steel affordable. This type of steel is highly recommended against chloride attack and is also machinable to produce various components for engineering applications. This study examines the effect of various fillers on 430 ferritic stainless steel (FSS). The austenitic (308) and ferritic (410) grades of filler were used to study the weldability, microstructure, mechanical properties, and corrosion resistance using tungsten inert gas welding. The findings showed the emergence of various complex phases in both the weld sample. The sample welded with 410 filler shows acicular ferrite, martensite and austenite. Whereas, austenite and vermicular ferrite are observed in the sample welded with 308 filler. Based on compositions and solidification modes, the mechanical properties of welded joints also vary. It was found that ferritic mode solidified welds dominated in terms of qualities, which was found in 410 filler. In the chloride solution, the behaviour of the pitting corrosion resistance of each weld varied. The sample welded with 410 was superior corrosion resistance. This is due to more δ-ferrite in the weld sample. Whereas, 308 showed poorer resistance against the simulated seawater solution. In 410 welds, a greater degree of sensitization was observed, as compared to 308 welds.
- 25 January 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 31 (6) , 4318-4334
The Effect of Cold Work and Thermal Aging on Intergranular and Transgranular Corrosion Failure of High Manganese Austenitic Stainless Steel
- 25 January 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 31 (6) , 4318-4334
The Effect of Cold Work and Thermal Aging on Intergranular and Transgranular Corrosion Failure of High Manganese Austenitic Stainless Steel
- 1 January 2021
- Published by Elsevier in Materials Today: Proceedings
- Vol. 37, 580-583
Effect of doping on thermo-optical properties of vanadium oxide sputtered thin films
- 1 January 2021
- Published by Elsevier in Materials Today: Proceedings
- Vol. 37, 580-583
Effect of doping on thermo-optical properties of vanadium oxide sputtered thin films
- 18 April 2020
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 67 (3) , 281-293
Electrochemical evaluation of cr-mn austenitic stainless steel in aqueous sulphuric acid and influence of thiocyanate ions
Purpose: Low nickel austenitic stainless steel (ASS) has attracted much attention worldwide because of its economical price. This study aims to investigate the effect of different corrosive environments on the corrosion behavior of chrome-manganese (Cr-Mn) ASS. The tests were carried out as a function of H2SO4 concentrations, temperature and addition of ammonium thiocyanate (NH4SCN) (0.01 M). Potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) techniques were used to study the corrosion behavior of Cr-Mn ASS. It was observed that with increasing H2SO4 concentration, temperature and with the addition of NH4SCN solution, icorr, icrit and ipassive values increased. EIS data show decreasing charge transfer resistance value with increasing concentration and temperature. Higher corrosion rate with increasing temperature and concentration of H2SO4 is related to the anions (SO42−), which is responsible for reducing the stability of passive films. With the presence of 0.01 M NH4SCN thiocyanate (SCN− anion), there is a higher dilution of the passive film resulting in a higher corrosion rate. Energy-dispersive spectroscopy (EDS) analysis reveals the adsorption of sulfur on the surface in NH4SCN containing a solution. The significant presence of counter ions and the adsorbed sulfur species on the steel surface play a vital role in corrosion behavior. Design/methodology/approach: All the experiments were performed on a 3 mm thick sheet of Cr-Mn ASS (202 ASS) in hot rolled condition. The samples were then annealed at 1,050°C for 1 h, followed by water quenching. For microstructural examination, they were electrochemically etched in 10 Wt.% oxalic acid solution at 1 amp for 90 s. A computer-controlled Potentiostat (Biologic VMP-300) was used. After the cell was set up, the working electrode (WE) was electrostatically cleaned at −1 V vs saturated calomel electrode (SCE) for 30 s to remove the air-formed film. Then, WE were allowed to attain stable open circuit potential (OCP) for 1 h, following by the EIS test and potentiodynamic polarization test. The polarization test was started from a cathodic potential (−1.2 V vs SCE) and continued up to an anodic potential (1.6 V vs SCE) a scan rate of 0.1667 mV/s. EIS experiment was conducted on the same instrument by using a sinusoidal AC signal of 10 mV in a frequency range of 1,000,000 to 0.01 Hz at OCP. Findings: Potentiodynamic polarization graph shows that with the increase in sulphuric acid concentration. Increasing temperature from 20°C to 80°C in 0.5 M H2SO4 solution increases the corrosion rate (icorr) of Cr-Mn ASS. On the addition of 0.01 M NH4SCN to the sulfuric acid solution (0.1, 0.5 and 1 M) the corrosion rate increases drastically almost four to five times. EDS and XRD analysis shows the presence of sulfur over the oxide film and preferential site for dissolution of Cr and Mn at the steel surface when NH4SCN is added to the sulfuric acid solution. Originality/value: A study on the corrosion behavior of Cr-Mn ASS is scanty according to the author’s knowledge. Therefore, the present study will investigate the corrosion behavior of Cr-Mn ASS on SO4−2 anions, temperature and the addition of SCN− ion in sulfuric acid.
- 18 April 2020
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 67 (3) , 281-293
Electrochemical evaluation of cr-mn austenitic stainless steel in aqueous sulphuric acid and influence of thiocyanate ions
Purpose: Low nickel austenitic stainless steel (ASS) has attracted much attention worldwide because of its economical price. This study aims to investigate the effect of different corrosive environments on the corrosion behavior of chrome-manganese (Cr-Mn) ASS. The tests were carried out as a function of H2SO4 concentrations, temperature and addition of ammonium thiocyanate (NH4SCN) (0.01 M). Potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) techniques were used to study the corrosion behavior of Cr-Mn ASS. It was observed that with increasing H2SO4 concentration, temperature and with the addition of NH4SCN solution, icorr, icrit and ipassive values increased. EIS data show decreasing charge transfer resistance value with increasing concentration and temperature. Higher corrosion rate with increasing temperature and concentration of H2SO4 is related to the anions (SO42−), which is responsible for reducing the stability of passive films. With the presence of 0.01 M NH4SCN thiocyanate (SCN− anion), there is a higher dilution of the passive film resulting in a higher corrosion rate. Energy-dispersive spectroscopy (EDS) analysis reveals the adsorption of sulfur on the surface in NH4SCN containing a solution. The significant presence of counter ions and the adsorbed sulfur species on the steel surface play a vital role in corrosion behavior. Design/methodology/approach: All the experiments were performed on a 3 mm thick sheet of Cr-Mn ASS (202 ASS) in hot rolled condition. The samples were then annealed at 1,050°C for 1 h, followed by water quenching. For microstructural examination, they were electrochemically etched in 10 Wt.% oxalic acid solution at 1 amp for 90 s. A computer-controlled Potentiostat (Biologic VMP-300) was used. After the cell was set up, the working electrode (WE) was electrostatically cleaned at −1 V vs saturated calomel electrode (SCE) for 30 s to remove the air-formed film. Then, WE were allowed to attain stable open circuit potential (OCP) for 1 h, following by the EIS test and potentiodynamic polarization test. The polarization test was started from a cathodic potential (−1.2 V vs SCE) and continued up to an anodic potential (1.6 V vs SCE) a scan rate of 0.1667 mV/s. EIS experiment was conducted on the same instrument by using a sinusoidal AC signal of 10 mV in a frequency range of 1,000,000 to 0.01 Hz at OCP. Findings: Potentiodynamic polarization graph shows that with the increase in sulphuric acid concentration. Increasing temperature from 20°C to 80°C in 0.5 M H2SO4 solution increases the corrosion rate (icorr) of Cr-Mn ASS. On the addition of 0.01 M NH4SCN to the sulfuric acid solution (0.1, 0.5 and 1 M) the corrosion rate increases drastically almost four to five times. EDS and XRD analysis shows the presence of sulfur over the oxide film and preferential site for dissolution of Cr and Mn at the steel surface when NH4SCN is added to the sulfuric acid solution. Originality/value: A study on the corrosion behavior of Cr-Mn ASS is scanty according to the author’s knowledge. Therefore, the present study will investigate the corrosion behavior of Cr-Mn ASS on SO4−2 anions, temperature and the addition of SCN− ion in sulfuric acid.
- 4 November 2019
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 66 (6) , 757-767
Effect of thermal aging on IGC of cold worked Cr-Mn austenitic stainless steel
Purpose: The purpose of this study is to investigate the effect of prior cold work after annealing and thermal ageing on intergranular corrosion or sensitization of Cr-Mn austenitic stainless steel (ASS) is necessary. Such a study is particularly important because ASS are mostly used and welded in mill-annealed condition, which is equivalent to fully annealed material with some cold worked (CW).Design/methodology/approach: The effect of 15% CW of 202 ASS were investigated using microstructural (optical microscope), mechanical (grain size and hardness) and electrochemical methods (double loop electrochemical reactivation [DLEPR]) followed by thermal ageing (800°C, 900°C and 1000°C).Findings: X-ray diffraction analysis shows the presence of martensite in CW samples. The increase in martensite formation (800°C and 900°C) can be observed with the variation of thermal ageing (TA) duration (1, 2 and 3 h). However, there was decreased in the formation of martensite at the temperature of 1000°C because of martensitic reversal. The DLEPR test result shows higher degree of sensitization (DOS) for 800°C and 900°C but for 1000°C, there was re-homogenization of samples which leads to lower DOS (thermal ageing for 1, 2 and 3 h).Originality/value: For 300 series steel, there are various literature available for the effect of cold work on mechanical properties and DOS. However, no one has investigated the effect of cold work and thermal ageing on the sensitization of 202 Cr-Mn ASS.
- 4 November 2019
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 66 (6) , 757-767
Effect of thermal aging on IGC of cold worked Cr-Mn austenitic stainless steel
Purpose: The purpose of this study is to investigate the effect of prior cold work after annealing and thermal ageing on intergranular corrosion or sensitization of Cr-Mn austenitic stainless steel (ASS) is necessary. Such a study is particularly important because ASS are mostly used and welded in mill-annealed condition, which is equivalent to fully annealed material with some cold worked (CW).Design/methodology/approach: The effect of 15% CW of 202 ASS were investigated using microstructural (optical microscope), mechanical (grain size and hardness) and electrochemical methods (double loop electrochemical reactivation [DLEPR]) followed by thermal ageing (800°C, 900°C and 1000°C).Findings: X-ray diffraction analysis shows the presence of martensite in CW samples. The increase in martensite formation (800°C and 900°C) can be observed with the variation of thermal ageing (TA) duration (1, 2 and 3 h). However, there was decreased in the formation of martensite at the temperature of 1000°C because of martensitic reversal. The DLEPR test result shows higher degree of sensitization (DOS) for 800°C and 900°C but for 1000°C, there was re-homogenization of samples which leads to lower DOS (thermal ageing for 1, 2 and 3 h).Originality/value: For 300 series steel, there are various literature available for the effect of cold work on mechanical properties and DOS. However, no one has investigated the effect of cold work and thermal ageing on the sensitization of 202 Cr-Mn ASS.
- Open Access
- 1 January 2019
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 22 (1)
Microstructure, Mechanical and Electrochemical Evaluation of Dissimilar low Ni SS and 304 SS using Different Filler Materials
This study investigates the effect of dissimilar metal welding of low nickel stainless steel (SS) and 304 SS employing tungsten inert gas (TIG) welding process by using three different filler materials (316L, 308L and 310 SS). Microstructural, mechanical properties and corrosion behavior in 3.5% NaCl solution was studied. The microstructural investigation revealed the formation of δ-ferrite and γ-austenite in the weld (welded by 316L and 308L filler). The Higher δ-ferrite content was found more in 316L weld zone. Whereas samples welded by 310 SS filler showed the columnar structure in the weld zone. Relatively wider heat affected zone (HAZ) was measured on Cr-Mn SS side as compared to 304 SS side. Impact fracture surface of all the welded samples exhibited dimple appearance. Corrosion studies showed better pitting corrosion resistance in 316L SS welded sample due to the beneficial effect of δ-ferrite and also the addition of molybdenum (Mo). Electrochemical impedance spectroscopy (EIS) revealed higher polarization resistance (Rp) in 316L SS as compared to other fillers. Galvanic current density was found to be higher in Cr-Mn SS as compared to 304 SS when coupled with different welded samples.
- 1 January 2019
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 22 (1)
Open AccessMicrostructure, Mechanical and Electrochemical Evaluation of Dissimilar low Ni SS and 304 SS using Different Filler Materials
This study investigates the effect of dissimilar metal welding of low nickel stainless steel (SS) and 304 SS employing tungsten inert gas (TIG) welding process by using three different filler materials (316L, 308L and 310 SS). Microstructural, mechanical properties and corrosion behavior in 3.5% NaCl solution was studied. The microstructural investigation revealed the formation of δ-ferrite and γ-austenite in the weld (welded by 316L and 308L filler). The Higher δ-ferrite content was found more in 316L weld zone. Whereas samples welded by 310 SS filler showed the columnar structure in the weld zone. Relatively wider heat affected zone (HAZ) was measured on Cr-Mn SS side as compared to 304 SS side. Impact fracture surface of all the welded samples exhibited dimple appearance. Corrosion studies showed better pitting corrosion resistance in 316L SS welded sample due to the beneficial effect of δ-ferrite and also the addition of molybdenum (Mo). Electrochemical impedance spectroscopy (EIS) revealed higher polarization resistance (Rp) in 316L SS as compared to other fillers. Galvanic current density was found to be higher in Cr-Mn SS as compared to 304 SS when coupled with different welded samples.
- 25 September 2018
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 65 (6) , 605-615
Effect of heat on microstructural, mechanical and electrochemical evaluation of tungsten inert gas welding of low-nickel ASS
Purpose: The purpose of the study is to evaluate Cr-Mn ASS weld using different heat inputs for its microstructure, mechanical properties and electrochemical behavior. The microstructural examination used optical and scanning electron microscopy. It was observed that ferrite content decreases with increasing heat input. The length of dendrites, inter-dendritic space and volume of lathy ferrite increase with increasing heat input. The increasing heat input caused grain coarsening near the fusion boundary and produced wider heat-affected zone (HAZ). It also decreases hardness and tensile strength. This is attributed to formation of more δ ferrite in the weld. The electrochemical evaluation suggested that the δ ferrite helps in improving the pitting potential in 3.5 per cent NaCl solution saturated with CO2. Whereas in 0.5-M H2SO4 + 0.003-M NaF solution, higher passivation current density was observed because of dissolution of dferrite. The interphase corrosion resistance decreased with increasing heat input. Design/methodology/approach: The Cr-Mn austenitic stainless steel or low-nickel ASS was procured in form of 3-mm sheets in rolled condition. The tungsten inert gas welding was performed at three different heat inputs (100 A, 120 A and 140 A), argon as shielding gas with a flow rate of 15 L/min. Different welded regions were observed using optical microscope and scanning electron microscope. Electrochemicals test were performed in solutions containing 3.5 per cent NaCl with saturated CO2 solution and 0.5 M sulfuric acid + 0.003 M NaF at a scan rate of 0.1667 mV/s at room temperature (30 °C ± 1 °C) using a potentiostat. Findings: The test steel Cr-Mn ASS is suitable with the selected electrode (308 L) and it produces no defects. Vermicular ferrite and lathy ferrite form in welds of various heat inputs. The increase in heat input reduces the formation of lathy ferrite. The width of HAZ and un-mixed zone increases with increase in heat input. The weld zone of low heat input (LHI) has the highest hardness and tensile strength because of higher δ ferrite content and small grain size in the weld zone. The hardness at high heat input (HHI) is found to be lowest because of grain coarsening in the weld. With increase in δ ferrite, the pitting resistance increases. In 0.5-M sulfuric acid + 0.003-M NaF, the increase in ferrite content reduces the passivation current density. Interphase corrosion resistance increases with increase in δ ferrite content as higher per cent degree of sensitization was observed in LHI welds as compared to medium heat input and HHI welds. Originality/value: This work focuses on welding of ASS by tungsten inert gas welding at different heat inputs. Welding is a critical process for joining metals in most of the fabrication industries and proper heat input is required for getting desired microstructure in the weld metal. This would highly affect the strength and corrosion behavior of the alloy. This paper would give an understanding of how the change in heat input by tungsten inert gas welding affects the microstructural and corrosion behavior in the weld metal.
- 25 September 2018
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- Vol. 65 (6) , 605-615
Effect of heat on microstructural, mechanical and electrochemical evaluation of tungsten inert gas welding of low-nickel ASS
Purpose: The purpose of the study is to evaluate Cr-Mn ASS weld using different heat inputs for its microstructure, mechanical properties and electrochemical behavior. The microstructural examination used optical and scanning electron microscopy. It was observed that ferrite content decreases with increasing heat input. The length of dendrites, inter-dendritic space and volume of lathy ferrite increase with increasing heat input. The increasing heat input caused grain coarsening near the fusion boundary and produced wider heat-affected zone (HAZ). It also decreases hardness and tensile strength. This is attributed to formation of more δ ferrite in the weld. The electrochemical evaluation suggested that the δ ferrite helps in improving the pitting potential in 3.5 per cent NaCl solution saturated with CO2. Whereas in 0.5-M H2SO4 + 0.003-M NaF solution, higher passivation current density was observed because of dissolution of dferrite. The interphase corrosion resistance decreased with increasing heat input. Design/methodology/approach: The Cr-Mn austenitic stainless steel or low-nickel ASS was procured in form of 3-mm sheets in rolled condition. The tungsten inert gas welding was performed at three different heat inputs (100 A, 120 A and 140 A), argon as shielding gas with a flow rate of 15 L/min. Different welded regions were observed using optical microscope and scanning electron microscope. Electrochemicals test were performed in solutions containing 3.5 per cent NaCl with saturated CO2 solution and 0.5 M sulfuric acid + 0.003 M NaF at a scan rate of 0.1667 mV/s at room temperature (30 °C ± 1 °C) using a potentiostat. Findings: The test steel Cr-Mn ASS is suitable with the selected electrode (308 L) and it produces no defects. Vermicular ferrite and lathy ferrite form in welds of various heat inputs. The increase in heat input reduces the formation of lathy ferrite. The width of HAZ and un-mixed zone increases with increase in heat input. The weld zone of low heat input (LHI) has the highest hardness and tensile strength because of higher δ ferrite content and small grain size in the weld zone. The hardness at high heat input (HHI) is found to be lowest because of grain coarsening in the weld. With increase in δ ferrite, the pitting resistance increases. In 0.5-M sulfuric acid + 0.003-M NaF, the increase in ferrite content reduces the passivation current density. Interphase corrosion resistance increases with increase in δ ferrite content as higher per cent degree of sensitization was observed in LHI welds as compared to medium heat input and HHI welds. Originality/value: This work focuses on welding of ASS by tungsten inert gas welding at different heat inputs. Welding is a critical process for joining metals in most of the fabrication industries and proper heat input is required for getting desired microstructure in the weld metal. This would highly affect the strength and corrosion behavior of the alloy. This paper would give an understanding of how the change in heat input by tungsten inert gas welding affects the microstructural and corrosion behavior in the weld metal.
- 23 July 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (5) , 056508
Microstructural, mechanical and intergranular corrosion behavior of cold work and thermal ageing of low nickel austenitic stainless steel
In the present investigation, microstructural, mechanical and electrochemical properties of cold rolled Cr-Mn austenitic stainless steel were studied. Heat treatment (800 °C, 900 °C, 950 °C and 1000 °C) and thermal ageing (one, two and three hours) of surface were investigated using an optical microscope, scanning electron microscope. Mechanical characteristics like hardness and tensile strength were evaluated. Electrochemical test were carried out using double loop electrochemical potentio kinetic reactivation tests (DLEPR) for finding the degree of sensitivity (DOS). The results showed that without cold rolled, thermal aged for one, two and three hours, there was high sensitization at the temperature of 850 °C and 900 °C, but at the temperature of 950 °C and 1000 °C there was re-homogenization. The grain size increased with increase in temperature. With cold rolled samples, there was a reduction in grain size, increased in strength and hardness in the samples, which is due to the formations of strain induced martensite (SIM). With the increase in thermal duration (1, 2 and 3 hours) there was an increase in martensite formation at temperature of 850 °C and 900 °C. At temperature of 950 °C and 1000 °C, work hardening diminished. Also, it was observed that increase in strain induces martensite which in turn increases degree of sensitization (% DOS).
- 23 July 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (5) , 056508
Microstructural, mechanical and intergranular corrosion behavior of cold work and thermal ageing of low nickel austenitic stainless steel
In the present investigation, microstructural, mechanical and electrochemical properties of cold rolled Cr-Mn austenitic stainless steel were studied. Heat treatment (800 °C, 900 °C, 950 °C and 1000 °C) and thermal ageing (one, two and three hours) of surface were investigated using an optical microscope, scanning electron microscope. Mechanical characteristics like hardness and tensile strength were evaluated. Electrochemical test were carried out using double loop electrochemical potentio kinetic reactivation tests (DLEPR) for finding the degree of sensitivity (DOS). The results showed that without cold rolled, thermal aged for one, two and three hours, there was high sensitization at the temperature of 850 °C and 900 °C, but at the temperature of 950 °C and 1000 °C there was re-homogenization. The grain size increased with increase in temperature. With cold rolled samples, there was a reduction in grain size, increased in strength and hardness in the samples, which is due to the formations of strain induced martensite (SIM). With the increase in thermal duration (1, 2 and 3 hours) there was an increase in martensite formation at temperature of 850 °C and 900 °C. At temperature of 950 °C and 1000 °C, work hardening diminished. Also, it was observed that increase in strain induces martensite which in turn increases degree of sensitization (% DOS).