Andre L. G. Prette
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Andre L. G. Prette has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Marcio Celso Fredel
Ceramic and Composite Materials Research Group (CERMAT), Department of Mechanical Engineering, Federal University of Santa Catarina (UFSC), Florianopolis 88040-900, SC, Brazil
3 shared publications - Rishi Raj
Department of Mechanical Engineering Materials Science and Engineering University of Colorado Boulder Boulder Colorado USA
2 shared publications - Vincenzo Maria Sglavo
University of Trento, Trento, Italy
2 shared publications A Will
Frenzelit Werke GmbH, 95460 Bad Berneck, Germany
1 shared publicationAna Paula M. Casadei
Departament of Mechanical Engineering, Federal University of Santa Catarina, UFSC, Florianópolis, Brazil
1 shared publicationCarlos R. Rambo
Departament of Mechanical Engineering, Federal University of Santa Catarina, UFSC, Florianópolis, Brazil
1 shared publication
Latest Publications
- 1 August 2019
- Published by Elsevier in Acta Materialia
- Vol. 174, 271-278
Effect of boundary conditions on reduction during early stage flash sintering of YSZ
- 1 August 2019
- Published by Elsevier in Acta Materialia
- Vol. 174, 271-278
Effect of boundary conditions on reduction during early stage flash sintering of YSZ
- Open Access
- 13 December 2013
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 47 (1) , 012053
Polycarbosilazane passivation on graphite foil used as gasket seal
Gasket seals are often used in industry and laboratories where a leak-proof installation is needed in order to avoid loss of products or dangerous materials. Many of products transported inside tubes are at relatively high temperatures excluding polymeric gaskets. In the same line, many of transported materials contain solvents which can attack polymer sealings, therefore limiting their use. An alternative is to use graphite joints as sealings. These joints are a sandwich of graphite foil and stainless steel mesh as forming core. The problem that raises using graphite in contact with steel is that at temperatures of about 500 °C an interdiffusion of carbon on the steel structure occurs which produces adhesion of the graphite gasket on the metallic flange. Therefore this adhesion increases the time to change each gasket, since rests of previously adhered graphite has to be removed from the flange. In order to avoid the adhesion of the graphite on the flange, polycarbosilazane precursor was used as protective finishing on the graphite foil surface. After thermal transformation of the polymer into the corresponding PDC finishing, it acts in two manners: It avoids the direct contact between the carbon and the steel and it allows the sealing of liquids and gases. Adhesion tests were done and showed that the foils passivated with PDCs did not adhere to the steel flange. Moreover, the production methods and products are compatible to industrial environment and processes. The results found here show that the time to change the gasket in industry can be clearly reduced by using the PDC finishing on graphite gasket.
- 13 December 2013
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 47 (1) , 012053
Open AccessPolycarbosilazane passivation on graphite foil used as gasket seal
Gasket seals are often used in industry and laboratories where a leak-proof installation is needed in order to avoid loss of products or dangerous materials. Many of products transported inside tubes are at relatively high temperatures excluding polymeric gaskets. In the same line, many of transported materials contain solvents which can attack polymer sealings, therefore limiting their use. An alternative is to use graphite joints as sealings. These joints are a sandwich of graphite foil and stainless steel mesh as forming core. The problem that raises using graphite in contact with steel is that at temperatures of about 500 °C an interdiffusion of carbon on the steel structure occurs which produces adhesion of the graphite gasket on the metallic flange. Therefore this adhesion increases the time to change each gasket, since rests of previously adhered graphite has to be removed from the flange. In order to avoid the adhesion of the graphite on the flange, polycarbosilazane precursor was used as protective finishing on the graphite foil surface. After thermal transformation of the polymer into the corresponding PDC finishing, it acts in two manners: It avoids the direct contact between the carbon and the steel and it allows the sealing of liquids and gases. Adhesion tests were done and showed that the foils passivated with PDCs did not adhere to the steel flange. Moreover, the production methods and products are compatible to industrial environment and processes. The results found here show that the time to change the gasket in industry can be clearly reduced by using the PDC finishing on graphite gasket.
- Top Cited Papers
- 1 February 2011
- Published by Elsevier in Journal of Power Sources
- Vol. 196 (4) , 2061-2065
Flash-sintering of Co2MnO4 spinel for solid oxide fuel cell applications
- 1 February 2011
- Published by Elsevier in Journal of Power Sources
- Vol. 196 (4) , 2061-2065
Top Cited PapersFlash-sintering of Co2MnO4 spinel for solid oxide fuel cell applications
- Top Cited Papers
- 14 January 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (2) , 316-319
Flash‐Sintering of Cubic Yttria‐Stabilized Zirconia at 750°C for Possible Use in SOFC Manufacturing
We show that cubic 8 mol% yttria (8YSZ) can be sintered at 750°C with the application of DC electrical fields; in comparison the lowest sintering temperature for 3YSZ was 850°C. Furthermore, cubic zirconia exhibits the onset of flash sintering at 30 V/cm, whereas 3YSZ begins flash sintering at 60 V/cm. However, the volume specific power dissipation for the onset of flash sintering remains similar at ∼10 mW/mm3. The easier sintering of 8YSZ is ascribed to its higher ionic conductivity.
- 14 January 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (2) , 316-319
Top Cited PapersFlash‐Sintering of Cubic Yttria‐Stabilized Zirconia at 750°C for Possible Use in SOFC Manufacturing
We show that cubic 8 mol% yttria (8YSZ) can be sintered at 750°C with the application of DC electrical fields; in comparison the lowest sintering temperature for 3YSZ was 850°C. Furthermore, cubic zirconia exhibits the onset of flash sintering at 30 V/cm, whereas 3YSZ begins flash sintering at 60 V/cm. However, the volume specific power dissipation for the onset of flash sintering remains similar at ∼10 mW/mm3. The easier sintering of 8YSZ is ascribed to its higher ionic conductivity.
- 9 November 2009
- Published by Wiley
- p. 169-177
Manufacturing of Porous PPLA‐HA Composite Scaffolds by Sintering for Bone Tissue Engineering
- 9 November 2009
- Published by Wiley
- p. 169-177
Manufacturing of Porous PPLA‐HA Composite Scaffolds by Sintering for Bone Tissue Engineering
- 9 November 2009
- Published by Wiley
- p. 33-37
Application of Semiconductor Ceramic Glazes to High‐Voltage Ceramic Insulators
- 9 November 2009
- Published by Wiley
- p. 33-37
Application of Semiconductor Ceramic Glazes to High‐Voltage Ceramic Insulators
- 19 August 2008
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 591-593, 521-525
Developing of Ceramic Roof Tiles Process by Powder Pressing and Firing in Roller Kiln
In this work, it was investigated the behavior of a ceramic composition in pressing and firing process, related to its pyroplasticity, to permit the production of roof tiles in roller kiln. Experiments were realized varying the parameters of pressing, sintering and composition, adding a refractory material. With this study, it became possible to select the optimal parameters of pressing and firing, and to start the pilot industrial tests. The developed process has advantages, in the process and the final product, related with the standard process (extrusion and firing in tunnel kiln). The process is energetically more efficient, because there are no movable in the kiln. It was measured a flexural strength above 40 MPa with 12mm thickness, saving material. Also, the product has a higher quality in size, shape and dimensional precision (linear thermal shrinkage lower than 1,5%); tonality, porosity (water absorption lower than 10%), and frost resistance.
- 19 August 2008
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 591-593, 521-525
Developing of Ceramic Roof Tiles Process by Powder Pressing and Firing in Roller Kiln
In this work, it was investigated the behavior of a ceramic composition in pressing and firing process, related to its pyroplasticity, to permit the production of roof tiles in roller kiln. Experiments were realized varying the parameters of pressing, sintering and composition, adding a refractory material. With this study, it became possible to select the optimal parameters of pressing and firing, and to start the pilot industrial tests. The developed process has advantages, in the process and the final product, related with the standard process (extrusion and firing in tunnel kiln). The process is energetically more efficient, because there are no movable in the kiln. It was measured a flexural strength above 40 MPa with 12mm thickness, saving material. Also, the product has a higher quality in size, shape and dimensional precision (linear thermal shrinkage lower than 1,5%); tonality, porosity (water absorption lower than 10%), and frost resistance.