KZKonstantin K. Zabello

Konstantin K. Zabello

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Konstantin K. Zabello has a total of 25 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Radiation Power of a Short High-Current Vacuum Arc at High Current Densities

    by Yury A. Barinov, Konstantin K. Zabello, Alexander A. Logachev, Irina N. Poluyanova, E. V. Sherstnev, Alexander A. Bogdanov, Sergey M. Shkol'NIk

    The radiation of a vacuum arc was measured in the spectral region 200 nm ≤ λ ≤ 1100 nm. The arc was initiated in the center of the cathode by breaking the current in the auxiliary circuit and was fed by the rectangular current pulse with a duration of 10 ms. The interelectrode gap was fixed at h = 4 mm, and the butt 2r = 30-mm CuCr30 electrodes were used. The arc was stabilized by an external uniform axial magnetic field (AMF). The radiation was coming out of the vacuum chamber through quartz ultraviolet (KU)-1 quartz window. The radiation detector was a silicon photodiode with a diameter of d = 1.2 mm. It was located on an axis intersecting the axis of symmetry of the discharge in the center of the interelectrode gap. The distance from the diode to the axis of symmetry was L = 1340 mm. After amplification, the signal from the diode was recorded on an oscilloscope. The measurements were made in a range of currents from 10 to 25 kA in order to cover the modes with the anodic activity. It was found that under the conditions of these experiments, the anode activity begins to manifest itself at the end of the pulse, starting with currents exceeding 15 kA. As the current increases, the activity begins closer to the beginning of the pulse. Considering the type of the spectral sensitivity of the diode, two series of measurements were made--measurements without a filter and through a yellow filter ZhS-10 that cuts off radiation with λ ≤ 400 nm. The results obtained made it possible to analyze the dependence of the radiation power on the arc current. The results showed that at high current densities in the developed vacuum arc with anodic activity, a significant part of the power is transferred by radiation. At the end of a pulse with a current of ≈ 25 kA, the radiation power is $P_{{uv}}$ ≈ 150 kW, while in the discharge, $P_{a} $ ≈ 800 kW is released. That is, at high current densities at the end of the pulse, the radiation power reaches almost 20% of the power released in the arc at this time. Estimates of lateral losses due to radiation are made.


  • Development and Current–Voltage Characteristic of Arc on AMF Contacts at Different Opening Speeds

    by Alexander A. Logachev, Irina N. Poluyanova, Konstantin K. Zabello, Sergey M. Shkol'NIk

    This article presents the results of the investigation of high-current vacuum arcs (HCVAs) on axial magnetic field (AMF) contacts at an average opening speed of 2 m/s and the comparison of the obtained results with similar results received earlier at a lower average opening speed of 1 m/s. We compared the voltage oscillograms and the current–voltage characteristics (CVCs), as well as the arc development process of the discharges at different opening speeds. The discharge was ignited by opening the contacts in a demountable vacuum chamber and was fed with the half-sine current pulse of 10 ms in duration. For analyzing the arc development processes, high-speed video recording of the arc column and the cathode surface was conducted throughout the entire current pulse. We discovered that the process looks similar for both the investigated contact speeds: a discharge is initiated at one or more points and covers the entire contact surface in a few milliseconds. Only quantitative differences are observed due to a higher arc voltage and, accordingly, energy input at a higher speed of contact movement. The CVC of the developed arc in both cases turned out to be linear in a wide range of currents. The analysis of the CVC showed that, in the developed arc, the ratio of the resistance of the column to its length does not depend on the length of the gap and the opening speed of the contacts. Thus, we can assume that the plasma parameters in the column change little with an increase in the current and in the opening speed of contacts. This assumption is supported by the results of a discussion of the literature on the CVC of HCVAs.


  • Thermal Effect on AMF Electrodes at Different Opening Speeds

    by Konstantin K. Zabello, Irina N. Poluyanova, Alexander A. Logachev, Yury A. Barinov, Sergey M. Shkol'Nik

    The erosion and thermal states at current zero for the axial magnetic field (AMF) electrodes after high-current vacuum arcs (HCVAs) were studied at an average opening speed of 2 m/s. The results obtained are compared with similar results received earlier at an average opening speed of 1 m/s. The discharge was ignited in a demountable vacuum chamber by opening the contacts and was fed with the half-sine current pulse of 10 ms in duration. To determine the thermal state of the surface of the electrodes at zero current, a Phantom MIRO M310 high-speed video camera with a Carl Zeiss 100 mm F2 lens was used. In addition, the surface of the electrodes after the arc exposure was photographed by a Canon camera. The study showed that at the same current an increase of the opening speed leads to an increase in the thermal effect on the electrodes. Besides, the work revealed that at high opening speed (HOS) the process of appearances of erosion traces on the cathodes and, especially, on the anodes, is significantly different. The estimations made in the work showed that the difference in erosion traces on the anode is associated not only with an increase in the thermal effect but also with a change in the momentum transferred to the anode by cathode jets due to jets relaxation in the interaction with the secondary anode plasma in a long arc.


  • Cathode Surface State and Cathode Temperature Distribution After Current Zero of Different AMF-Contacts

    by Alexander A. Logachev, Irina N. Poluyanova, Konstantin K. Zabello, Yury A. Barinov, Sergey M. Shkol'NIk

    The objective of this paper is to compare the state of cathode surface of different axial magnetic field (AMF) contact systems (CSs) during arcing and after arc extinction. The arcs were ignited by opening of electrodes and were fed by sine half-wave current pulses with a duration of 10 ms. Investigations were performed in the range of arc currents up to the levels of guaranteed failure. The measurements were done by a high-speed Phantom M310 video camera. The cathode surface state during arcing was studied using a set of neutral density filters. It was discovered that melting of a part of the cathode surface during arc burning takes place in high-current vacuum arcs. A changing relief in the form of hillocks and hollows forms on the melted surface. We found out that there are two components in droplet erosion of the cathode, when its surface is partially melted: in addition to droplets formed directly in the cathode spot (which can be called droplets of the first type), the liquid part of the surface also emits droplets (which can be called droplets of the second type) significantly different in their sizes and velocities. The formation mechanisms of droplets of the first and the second type are different. The cathode surface temperature distribution immediately after current zero was obtained by comparing the results of cathode surface filming to the results of calibrated band-lamp filming in identical conditions. Reflection of anode radiation from cathode surface was analyzed by mathematical simulation. The filming was carried out using an interference filter. We found that the distribution of the cathode surface temperature is substantially nonuniform. The axial region is the most heated. We conclude that in all investigated CSs with the same amplitude value of the current, the temperature of the most heated parts of the cathode surface is significantly lower than the temperature of the most heated parts of the anode surface. Analysis of obtained results shows that switching failure can be provoked by the cathode and by the anode processes depending on CS design.


  • Droplet Erosion of a Cathode in a High-Current Vacuum Arc

    by K. K. Zabello, A. A. Logachev, I. N. Poluyanova, S. M. Shkol’NIk

    It is shown that high-current vacuum arcs accompanied by partial melting of the cathode surface and its droplet erosion can generate, in addition to the well-known droplets formed immediately...


  • Капельная эрозия катода в сильноточной вакуумной дуге

    by К.к. Забелло, А.а. Логачёв, И.н. Полуянова, С.м. Школьник

    It is shown that high-current vacuum arcs accompanied by partial melting of the cathode surface and its droplet erosion can generate, in addition to the well-known droplets formed immediately in the cathode spot (first type droplets), a second component of erosion. The liquid part of the cathode surface can emit droplets with significantly different sizes and velocities, which may be called second type droplets. The mechanisms of the formation of first and second type droplets are also substantially different.

  • Average current per vacuum-arc cathode spot and spot velocity in a magnetic field on a CuCr50/50 nanocomposite

    by K. K. Zabello, I. N. Poluyanova, V. V. Yakovlev, S. M. Shkol’NIk

    It has been shown that such cathode spot characteristics as the average current per spot and its dependence on tangential magnetic-field induction Bt and the spot velocity and its dependence on Bt for


  • Measurements of Thermal Radiation Brightness of Anode Surface After Current Zero for a Range of Current Levels

    by Irina N. Poluyanova, Konstantin K. Zabello, Alexander A. Logatchev, Vitaliy V. Yakovlev, Sergey M. Shkol'NIk

    Overheating of electrode surfaces during arc burning is considered to be the main reason of a breakdown after kiloampere arc extinction. The greatest interest in this connection is the most energy-loaded electrode-the anode. The aim of this paper is to measure the distributions of thermal radiation brightness of anode surface just after current zero for a range of arc currents from successfully interrupted levels up to the levels of guaranteed failure. The measurements allow us to determine the anode surface temperature distributions and trace the anode cooling. The measurements were done by a high-speed video camera Phantom M310 equipped with a Carl Zeiss 100/2 macro lens. The anode surface temperature distribution was obtained by comparison of the results of anode surface filming and the results of calibrated band-lamp filming in identical conditions. The measurements were done for CuCr 70/30 electrodes with a diameter of 64 mm generating axial magnetic field for the currents up to the interruption limit. The cooling was traced over the time interval, during which the absolute majority of breakdowns takes place at the TRV application for the given contact system.


  • Influence of current ripple on the tungsten cathode erosion

    by N. K. Mitrofanov, K. K. Zabello, V. A. Nemchinsky, S. M. Shkol’NIk