Yiming Jiang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yiming Jiang has a total of 101 co-authors. Here are the top co-authors by number of shared publications:
Jin Li
21 shared publications- Yangting Sun
Department of Materials Science, State Key Laboratory of Molecular Engineering of Polymers, Fudan University, Shanghai 200438, People’s Republic of China
8 shared publications - Yuanyuan Liu
Department of Materials Science, Fudan University, Shanghai 200433, China
8 shared publications Nianwei Dai
Department of Materials Science, Fudan University, Shanghai, People’s Republic of China
7 shared publicationsJ. Li
Department of Materials Science Fudan University Shanghai 200433 P. R. China
5 shared publicationsJun Wu
Corrosion Laboratory, Department of Materials Science, Fudan University, Shanghai 200433, People's Republic of China
4 shared publications
Latest Publications
- 26 March 2026
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 228
The surface mechanism of a gradient nanostructure in mitigating hydrogen-promoted pitting corrosion
- 26 March 2026
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 228
The surface mechanism of a gradient nanostructure in mitigating hydrogen-promoted pitting corrosion
- Top Cited PapersOpen Access
- 19 January 2026
- Published by Elsevier in Corrosion Communications
- Vol. 24, 29-36
Pitting behavior of austenitic stainless steel welded joints-A review
- 19 January 2026
- Published by Elsevier in Corrosion Communications
- Vol. 24, 29-36
Top Cited PapersOpen AccessPitting behavior of austenitic stainless steel welded joints-A review
- Open Access
- 2 May 2023
- Published by Wiley in Materials and Corrosion
- Vol. 74 (5) , 653
Cover Picture: Materials and Corrosion. 5/2023
- 2 May 2023
- Published by Wiley in Materials and Corrosion
- Vol. 74 (5) , 653
Open AccessCover Picture: Materials and Corrosion. 5/2023
- 28 November 2022
- Published by Wiley in Materials and Corrosion
- Vol. 74 (5) , 660-669
Influence of the machined surface roughness on the pitting behavior of 304 stainless steel
The relationship between specimens with different machined surface roughness and pitting resistance was explored using the critical pitting temperature (CPT), critical pitting potential (Ep), and FeCl3 pitting immersion tests. Compared with the arithmetic mean deviation of the surface contour (Ra), the depth–width ratio could characterize the mathematical relationship between the machined surface roughness and pitting parameters more simply. With an increase in the depth–width ratio, the CPT and Ep of 304 stainless steel decreased, the average corrosion rate increased, the number of pits decreased, and the pit sizes increased. A larger depth–width ratio led to a larger effective diffusion length of metal cations in the pits, thus, the critical pitting criteria could be reached easily, which resulted in the reduction of the pitting resistance of 304 stainless steel.
- 28 November 2022
- Published by Wiley in Materials and Corrosion
- Vol. 74 (5) , 660-669
Influence of the machined surface roughness on the pitting behavior of 304 stainless steel
The relationship between specimens with different machined surface roughness and pitting resistance was explored using the critical pitting temperature (CPT), critical pitting potential (Ep), and FeCl3 pitting immersion tests. Compared with the arithmetic mean deviation of the surface contour (Ra), the depth–width ratio could characterize the mathematical relationship between the machined surface roughness and pitting parameters more simply. With an increase in the depth–width ratio, the CPT and Ep of 304 stainless steel decreased, the average corrosion rate increased, the number of pits decreased, and the pit sizes increased. A larger depth–width ratio led to a larger effective diffusion length of metal cations in the pits, thus, the critical pitting criteria could be reached easily, which resulted in the reduction of the pitting resistance of 304 stainless steel.
- 2 February 2020
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 55 (3) , 232-240
Enhancement in intergranular corrosion resistance of the stabilised ultra-pure 430LX ferritic stainless steel by tin addition
The intergranular corrosion (IGC) susceptibility of the Ti–Nb-stabilised ultra-pure 430LX FSSs with 0–0.47 wt-% tin addition was investigated using double loop electrochemical potentiokinetic reactivation (DL-EPR) and oxalic acid etch tests. The result of DL-EPR test reveals that IGC resistance increases with the increase in tin content. The specimens with different contents of tin exhibit the same microstructural evolution based on oxalic acid etch test. M23C6 precipitates form along grain boundaries, inducing Cr-depleted zones and finally resulting in the susceptibility to IGC. Tin addition gives rise to the formation of SnO2 on the FSSs surface, thus inhibiting the attack of corrosive ions towards Cr-depleted zones.
- 2 February 2020
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 55 (3) , 232-240
Enhancement in intergranular corrosion resistance of the stabilised ultra-pure 430LX ferritic stainless steel by tin addition
The intergranular corrosion (IGC) susceptibility of the Ti–Nb-stabilised ultra-pure 430LX FSSs with 0–0.47 wt-% tin addition was investigated using double loop electrochemical potentiokinetic reactivation (DL-EPR) and oxalic acid etch tests. The result of DL-EPR test reveals that IGC resistance increases with the increase in tin content. The specimens with different contents of tin exhibit the same microstructural evolution based on oxalic acid etch test. M23C6 precipitates form along grain boundaries, inducing Cr-depleted zones and finally resulting in the susceptibility to IGC. Tin addition gives rise to the formation of SnO2 on the FSSs surface, thus inhibiting the attack of corrosive ions towards Cr-depleted zones.
- 16 January 2020
- Published by Wiley in Materials and Corrosion
- Vol. 71 (7) , 1102-1112
High‐temperature corrosion behaviors of typical nickel alloy coatings in a simulated boiler coal ash/gas environment in the Zhundong region
The high‐temperature corrosion behaviors of five nickel alloy coatings used in coal‐fired boilers in the Zhundong region (Xinjiang province) were investigated in simulated coal ash and coal‐combusted flue gas environment at 650°C for 250 and 500 hr. The samples were analyzed by weight gain experiment, X‐ray diffraction test, and scanning electron microscopy technique with energy‐dispersive spectroscopy. The results indicated that the corrosion level is in the order of NiCrMo13 ≈ Hastelloy C‐276 (276) > NiCrBSi > Inconel 718 (718) > 45CT. The compositions of the corrosion scale in five nickel alloy coatings mainly consist of NiO, Ni3S2, and Cr2O3. The enrichment of Cr in the corrosion scale in 45CT, 718, and NiCrBSi coatings inhibits the formation of oxide and sulfide on the coating surface. The presence of W and Mo in nickel alloy coatings accelerates the formation of corrosion products, thus weakening the corrosion resistance of NiCrMo13 and 276 in simulated coal ash and coal‐combusted flue gas environment.
- 16 January 2020
- Published by Wiley in Materials and Corrosion
- Vol. 71 (7) , 1102-1112
High‐temperature corrosion behaviors of typical nickel alloy coatings in a simulated boiler coal ash/gas environment in the Zhundong region
The high‐temperature corrosion behaviors of five nickel alloy coatings used in coal‐fired boilers in the Zhundong region (Xinjiang province) were investigated in simulated coal ash and coal‐combusted flue gas environment at 650°C for 250 and 500 hr. The samples were analyzed by weight gain experiment, X‐ray diffraction test, and scanning electron microscopy technique with energy‐dispersive spectroscopy. The results indicated that the corrosion level is in the order of NiCrMo13 ≈ Hastelloy C‐276 (276) > NiCrBSi > Inconel 718 (718) > 45CT. The compositions of the corrosion scale in five nickel alloy coatings mainly consist of NiO, Ni3S2, and Cr2O3. The enrichment of Cr in the corrosion scale in 45CT, 718, and NiCrBSi coatings inhibits the formation of oxide and sulfide on the coating surface. The presence of W and Mo in nickel alloy coatings accelerates the formation of corrosion products, thus weakening the corrosion resistance of NiCrMo13 and 276 in simulated coal ash and coal‐combusted flue gas environment.
- 9 September 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (13) , C454-C467
Distinction in Corrosion Behaviors of Duplex Stainless Steel 2205 Induced by Different Waveform Alternating Voltages Interference
Anisotropic corrosion behaviors of duplex stainless steel induced by different waveform alternating voltage (AV) interferences have never been elucidated. The results of FeCl3 pitting immersion tests reveal that the critical pitting temperature (CPT) of 2205 samples is decreased with the interferences of three waveform AV signals. For the AV with equal root mean square (RMS) value on electrode samples, the triangular wave induces much stronger etching on DSS 2205 than the sinusoidal and square ones. However, the sinusoidal and triangular AV interferences trigger the most severe pitting corrosion in high-temperature solution (>50°C). The weight loss induced by pitting corrosion is greater than that by strong etching on samples. Regarding the etching behavior, the austenite in the duplex phase exhibits an inferior corrosion resistance and is preferentially dissolved.
- 9 September 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (13) , C454-C467
Distinction in Corrosion Behaviors of Duplex Stainless Steel 2205 Induced by Different Waveform Alternating Voltages Interference
Anisotropic corrosion behaviors of duplex stainless steel induced by different waveform alternating voltage (AV) interferences have never been elucidated. The results of FeCl3 pitting immersion tests reveal that the critical pitting temperature (CPT) of 2205 samples is decreased with the interferences of three waveform AV signals. For the AV with equal root mean square (RMS) value on electrode samples, the triangular wave induces much stronger etching on DSS 2205 than the sinusoidal and square ones. However, the sinusoidal and triangular AV interferences trigger the most severe pitting corrosion in high-temperature solution (>50°C). The weight loss induced by pitting corrosion is greater than that by strong etching on samples. Regarding the etching behavior, the austenite in the duplex phase exhibits an inferior corrosion resistance and is preferentially dissolved.
- 26 April 2019
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 32 (10) , 1219-1226
Crevice Corrosion Behaviors Between CFRP and Stainless Steel 316L for Automotive Applications
- 26 April 2019
- Published by Elsevier in Acta Metallurgica Sinica (English Letters)
- Vol. 32 (10) , 1219-1226
Crevice Corrosion Behaviors Between CFRP and Stainless Steel 316L for Automotive Applications
- 8 April 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (7) , 076569
Pitting inhibition of newly developed lean duplex stainless steel 2002 in NaCl solution by a green inhibitor
The pitting inhibition of sodium lignosulphonate (SL) on newly developed lean duplex stainless steel (LDSS) 2002 in 3.5% NaCl was assessed by using various electrochemical methods. The electrochemical results reveal that the critical pitting temperature (CPT) of LDSS 2002 decreases with increase in inhibitor concentration. The breakdown potential (Eb) also decreases with inhibitor addition and the initiation of metastable pits is effectively suppressed. The potentiostatic pulse technique (PPT) shows that the propagation of pitting and initiation of pitting location can slightly be influenced by addition of SL. The adsorption of SL on the LDSS 2002 surface in 3.5% NaCl solution follows the Langmuir adsorption isotherm and the adsorption accords with both physical and chemical adsorption process. Meanwhile, the presence of SL acts as a barrier to the adsorption and/or penetration of chloride ion into the passive film, thereby inhibiting the pit initiation and growth.
- 8 April 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (7) , 076569
Pitting inhibition of newly developed lean duplex stainless steel 2002 in NaCl solution by a green inhibitor
The pitting inhibition of sodium lignosulphonate (SL) on newly developed lean duplex stainless steel (LDSS) 2002 in 3.5% NaCl was assessed by using various electrochemical methods. The electrochemical results reveal that the critical pitting temperature (CPT) of LDSS 2002 decreases with increase in inhibitor concentration. The breakdown potential (Eb) also decreases with inhibitor addition and the initiation of metastable pits is effectively suppressed. The potentiostatic pulse technique (PPT) shows that the propagation of pitting and initiation of pitting location can slightly be influenced by addition of SL. The adsorption of SL on the LDSS 2002 surface in 3.5% NaCl solution follows the Langmuir adsorption isotherm and the adsorption accords with both physical and chemical adsorption process. Meanwhile, the presence of SL acts as a barrier to the adsorption and/or penetration of chloride ion into the passive film, thereby inhibiting the pit initiation and growth.
- Open Access
Effect of Surface Roughness on Pitting Corrosion of 2205 Duplex Stainless Steel Investigated by Electrochemical Noise Measurements
The influence of surface roughness on the pitting corrosion behaviour of 2205 duplex stainless steel (DSS) in a chloride-containing environment was investigated using electrochemical noise (EN) techniques and morphology observation. A rougher surface condition increased the frequency of pit initiation because of the increase in more occluded pit sites. Rough surface finish also accelerated pit growth by increasing the actual dissolution rate in the pit. Metastable pits on rougher surfaces had longer lifetimes and grew to larger sizes, as their inner chemical environment was more easily maintained. However back-scatter images showed that pitting initiates on DSS 2205 regardless of the roughness condition.
Open AccessEffect of Surface Roughness on Pitting Corrosion of 2205 Duplex Stainless Steel Investigated by Electrochemical Noise Measurements
The influence of surface roughness on the pitting corrosion behaviour of 2205 duplex stainless steel (DSS) in a chloride-containing environment was investigated using electrochemical noise (EN) techniques and morphology observation. A rougher surface condition increased the frequency of pit initiation because of the increase in more occluded pit sites. Rough surface finish also accelerated pit growth by increasing the actual dissolution rate in the pit. Metastable pits on rougher surfaces had longer lifetimes and grew to larger sizes, as their inner chemical environment was more easily maintained. However back-scatter images showed that pitting initiates on DSS 2205 regardless of the roughness condition.