Wen Cheng Chang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Wen Cheng Chang has a total of 145 co-authors. Here are the top co-authors by number of shared publications:
- Huang-Wei Chang
National Chung Cheng University
28 shared publications H. W. Chang
Department of Physics, National Chung Cheng University 1 , Chia-Yi 621, Taiwan
23 shared publicationsC. W. Chang
National Chung Cheng University 1 Department of Physics Chia-Yi, Taiwan 621, Republic of China
18 shared publicationsC. C. Hsieh
Department of Physics, National Chung Cheng University 2 , Chia-Yi, 621 Taiwan, Republic of China
16 shared publicationsC. H. Chiu
New Materials Research and Development Department, China Steel Corp. 2 , Kaohsiung 812, Taiwan
14 shared publicationsC.H. Chiu
Department of Physics, National Chung Cheng University, Taiwan, ROC
8 shared publications
Latest Publications
- 1 October 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (10) , 2101305
Magnetic Properties and Microstructure of Melt Spun SmFe 12 Ribbons With V Substitution and B-Doping
- 1 October 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (10) , 2101305
Magnetic Properties and Microstructure of Melt Spun SmFe 12 Ribbons With V Substitution and B-Doping
- 20 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Comparison on the Coercivity Enhancement of Hot-Deformed NdFeB Magnets by Doping Ce80M20-xZnx (M = Cu or Al; x = 0–20) Alloy Powders
Coercivity enhancement of hot-deformed (HD) NdFeB magnets by doping low-cost Ce 80 M 20-x Zn x (M= Cu, Al; x= 0-20) alloy powders is compared. By doping Ce 80 M 20-x Zn x powders, coercivity ( i H c ) is increased from 15.0 kOe for the as-upset magnet to 17.2-18.5 kOe for M=Cu, and 17.0-19.1 kOe for M = Al, respectively. Compared to the magnet doped with Ce 80 Al 20 ( i H c = 17.0 kOe), the magnet doped with Ce 80 Al 10 Zn 10 exhibits higher i H c of 19.1 kOe. Besides, grain morphology of the magnet doped with Ce 80 Al 10 Zn 10 is more platelet-like than that doped with Ce 80 Al 20 . The platelet grain morphology contributes to the good (00L) texture, and thus higher remanence is obtained. Microstructure and element analysis show Ce, Al, Cu, and Zn prefer to distribute at grain boundary, which can strengthen the decoupling effect between adjacent Nd 2 Fe 14 B (2:14:1) grains. Almost unchanged Curie temperature (T C ) of 2:14:1 phase for the magnet doped with Ce 80 Al 10 Zn 10 also indicates Ce mostly distributes at grain boundary. The effect of doping Ce-Al-Zn-containing alloys on the coercivity enhancement and mechanism for HD NdFeB magnets are also discussed in this work.
- 20 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Comparison on the Coercivity Enhancement of Hot-Deformed NdFeB Magnets by Doping Ce80M20-xZnx (M = Cu or Al; x = 0–20) Alloy Powders
Coercivity enhancement of hot-deformed (HD) NdFeB magnets by doping low-cost Ce 80 M 20-x Zn x (M= Cu, Al; x= 0-20) alloy powders is compared. By doping Ce 80 M 20-x Zn x powders, coercivity ( i H c ) is increased from 15.0 kOe for the as-upset magnet to 17.2-18.5 kOe for M=Cu, and 17.0-19.1 kOe for M = Al, respectively. Compared to the magnet doped with Ce 80 Al 20 ( i H c = 17.0 kOe), the magnet doped with Ce 80 Al 10 Zn 10 exhibits higher i H c of 19.1 kOe. Besides, grain morphology of the magnet doped with Ce 80 Al 10 Zn 10 is more platelet-like than that doped with Ce 80 Al 20 . The platelet grain morphology contributes to the good (00L) texture, and thus higher remanence is obtained. Microstructure and element analysis show Ce, Al, Cu, and Zn prefer to distribute at grain boundary, which can strengthen the decoupling effect between adjacent Nd 2 Fe 14 B (2:14:1) grains. Almost unchanged Curie temperature (T C ) of 2:14:1 phase for the magnet doped with Ce 80 Al 10 Zn 10 also indicates Ce mostly distributes at grain boundary. The effect of doping Ce-Al-Zn-containing alloys on the coercivity enhancement and mechanism for HD NdFeB magnets are also discussed in this work.
- 12 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Improvement of Magnetic Property for Melt Spun CeCo5 Ribbons Due to Fe and C-Doping
Improvement of hard magnetic property for melt spun CeCo 5 ribbons by doping proper Fe and C is demonstrated. Low magnetic properties, remanence (B r ) of 4.2 kG, coercivity ( i H c ) of 1.6 kOe and energy product ((BH) max ) of 1.8 MGOe, are found for binary CeCo 5 ribbons due to extremely large size of grains, even prepared at high wheel speed of 40 m/s. i H c is largely enhanced to 12.8 kOe by doping C and 15.0 kOe by co-doping Fe and C, and therefore, (BH) max is increased to 3.5 MGOe and 5.1 MGOe, respectively. The coercivity achieved in this work is superior to those reported ever before, and (BH) max is also larger than the theoretical value of 4.7 MGOe for isotropic CeCo 5 alloy. XRD and TMA results reveal Fe and C enter into 1:5 phase to modify lattice constant and increase T C , and the increased c/a ratio of 1:5 phase may improve H a and contribute to enhance the coercivity. Microstructure analysis indicates the grain size is effectively refined by doping C and co-doping Fe and C. Fine microstructure for C-containing ribbons contributes to attain high coercivity of 12.8-15.0 kOe. Besides, Fe-doping may increase the magnetization of 1:5 phase, and therefore improve the remanence and (BH) max . The results of this work suggest that magnetic properties of CeCo 5 ribbons could be improved by modification of 1:5 crystal and microstructure refinement due to proper Fe and C-codoping.
- 12 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Improvement of Magnetic Property for Melt Spun CeCo5 Ribbons Due to Fe and C-Doping
Improvement of hard magnetic property for melt spun CeCo 5 ribbons by doping proper Fe and C is demonstrated. Low magnetic properties, remanence (B r ) of 4.2 kG, coercivity ( i H c ) of 1.6 kOe and energy product ((BH) max ) of 1.8 MGOe, are found for binary CeCo 5 ribbons due to extremely large size of grains, even prepared at high wheel speed of 40 m/s. i H c is largely enhanced to 12.8 kOe by doping C and 15.0 kOe by co-doping Fe and C, and therefore, (BH) max is increased to 3.5 MGOe and 5.1 MGOe, respectively. The coercivity achieved in this work is superior to those reported ever before, and (BH) max is also larger than the theoretical value of 4.7 MGOe for isotropic CeCo 5 alloy. XRD and TMA results reveal Fe and C enter into 1:5 phase to modify lattice constant and increase T C , and the increased c/a ratio of 1:5 phase may improve H a and contribute to enhance the coercivity. Microstructure analysis indicates the grain size is effectively refined by doping C and co-doping Fe and C. Fine microstructure for C-containing ribbons contributes to attain high coercivity of 12.8-15.0 kOe. Besides, Fe-doping may increase the magnetization of 1:5 phase, and therefore improve the remanence and (BH) max . The results of this work suggest that magnetic properties of CeCo 5 ribbons could be improved by modification of 1:5 crystal and microstructure refinement due to proper Fe and C-codoping.
- Open Access
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025226
High-coercivity heavy-rare-earth-free NdFeB sintered magnets developed by doping Ce85Al15 and grain boundary diffusion with Pr70Cu15Al15
Traditional NdFeB sintered magnets with coercivity larger than 20 kOe, called super-high (SH) level, usually contains considerable amount of high-cost heavy rare earth (HRE), such as Dy or Tb. In this work, high coercivity of 21.4 kOe, which corresponds to SH level, is achieved for HRE-free NdFeB magnet by doping with Ce85Al15 (CeAl) alloy and grain boundary diffusion (GBD) with Pr70Cu15Al15 (PrCuAl) alloy powders, where Ce/RE ratio is about 15% within the magnet. After GBD treatment with PrCuAl on Ce-containing NdFeB magnets, the formation of Pr-containing shell at 2:14:1 grain surface can increase the local magnetic anisotropy filed and therefore enhance the coercivity. Most of Cu and Al, and parts of Ce and Pr appear at grain boundary and triple junction, which can reduce the magnetization of grain boundary phase, strengthen the decoupling effect between grains and thus contribute to high coercivity. This study provides a cost-effective way to obtain high coercivity for HRE-free NdFeB sintered magnet via doping Ce85Al15 and then GBD with Pr70Cu15Al15.
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025226
Open AccessHigh-coercivity heavy-rare-earth-free NdFeB sintered magnets developed by doping Ce85Al15 and grain boundary diffusion with Pr70Cu15Al15
Traditional NdFeB sintered magnets with coercivity larger than 20 kOe, called super-high (SH) level, usually contains considerable amount of high-cost heavy rare earth (HRE), such as Dy or Tb. In this work, high coercivity of 21.4 kOe, which corresponds to SH level, is achieved for HRE-free NdFeB magnet by doping with Ce85Al15 (CeAl) alloy and grain boundary diffusion (GBD) with Pr70Cu15Al15 (PrCuAl) alloy powders, where Ce/RE ratio is about 15% within the magnet. After GBD treatment with PrCuAl on Ce-containing NdFeB magnets, the formation of Pr-containing shell at 2:14:1 grain surface can increase the local magnetic anisotropy filed and therefore enhance the coercivity. Most of Cu and Al, and parts of Ce and Pr appear at grain boundary and triple junction, which can reduce the magnetization of grain boundary phase, strengthen the decoupling effect between grains and thus contribute to high coercivity. This study provides a cost-effective way to obtain high coercivity for HRE-free NdFeB sintered magnet via doping Ce85Al15 and then GBD with Pr70Cu15Al15.
- Open Access
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025308
Directional growth effect on magneto-mechanical properties of Fe81Al19 alloy
Directional growth effect on magneto-mechanical properties of Fe81Al19 alloy is studied. The ideal model of heat flux for directional solidification (DS) technique is proposed, and the tuned A/L (the ratio of cross-sectional area and length for the ingot) and ΔT (temperature difference) are adopted to increase heat flux (q). The experimental result shows that the increase of q effectively promotes the degree of (011)[100] Goss texture and therefore helps to form an oriented stripe domain structure. Large λ100 of 93.8 ppm attained for this optimized Fe81Al19 alloy prepared by DS method is very close to that of the Fe81Al19 single crystal (95.0 ppm). For the optimized DS prepared Fe81Al19 alloy, high magnetostriction sensitivity (dλ/dH) of 0.45 ppm/Oe leads to huge ΔEs/E0 of ∼10% and attractive ΔE/E0 of 8.2% at small H = 0.25 kOe. The above remarkable magneto-mechanical properties, low cost of Fe81Al19, and simple process of DS favor for applications. This work proposes an ideal model to emphasize the importance of heat flux in DS, and experimentally attains the remarkable magneto-mechanical properties for Fe81Al19 alloy prepared by DS.
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025308
Open AccessDirectional growth effect on magneto-mechanical properties of Fe81Al19 alloy
Directional growth effect on magneto-mechanical properties of Fe81Al19 alloy is studied. The ideal model of heat flux for directional solidification (DS) technique is proposed, and the tuned A/L (the ratio of cross-sectional area and length for the ingot) and ΔT (temperature difference) are adopted to increase heat flux (q). The experimental result shows that the increase of q effectively promotes the degree of (011)[100] Goss texture and therefore helps to form an oriented stripe domain structure. Large λ100 of 93.8 ppm attained for this optimized Fe81Al19 alloy prepared by DS method is very close to that of the Fe81Al19 single crystal (95.0 ppm). For the optimized DS prepared Fe81Al19 alloy, high magnetostriction sensitivity (dλ/dH) of 0.45 ppm/Oe leads to huge ΔEs/E0 of ∼10% and attractive ΔE/E0 of 8.2% at small H = 0.25 kOe. The above remarkable magneto-mechanical properties, low cost of Fe81Al19, and simple process of DS favor for applications. This work proposes an ideal model to emphasize the importance of heat flux in DS, and experimentally attains the remarkable magneto-mechanical properties for Fe81Al19 alloy prepared by DS.
- Open Access
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025202
Coercivity enhancement of hot-deformed NdFeB magnets by in situ two-end-diffusion with R70Cu30 alloy powders (R = NdPr and Ce)
We hereby present a simple process, called in situ two-end diffusion (TED), to reach coercivity enhancement with almost unchanged energy product for hot deformed (HD) NdFeB magnets. Coercivity of the HD magnets is increased from 15.1 to 18.7 kOe for the magnet TED with (Nd0.75Pr0.25)70Cu30 (NdPrCu), which is larger than 17.6 kOe for the magnet directly doped with 2 wt. % NdPrCu alloy. Besides, the magnet TED with NdPrCu exhibits good (00L) texture and therefore could support high (BH)max of 43.0 MGOe. In addition, the magnet TED with Ce70Cu30 (CeCu) exhibit superior magnetic properties of Br = 12.8 kG, iHc = 18.0 kOe and (BH)max = 40.7 MGOe to those of traditional doping with CeCu (Br = 11.7 kG, iHc = 16.4 kOe and (BH)max = 34.2 MGOe). For TED process, low-melting CeCu can infiltrate into the center of the magnet, and most Ce distribute at grain boundary. The distribution of Ce and Cu at grain boundary can reduce the magnetization of grain boundary phase, strengthen the decoupling effect between grains and contribute to the coercivity enhancement. This work demonstrates TED with low-melting HRE-free alloys is a simple method to effectively enhance coercivity and keep high Br and (BH)max for HD NdFeB magnets.
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025202
Open AccessCoercivity enhancement of hot-deformed NdFeB magnets by in situ two-end-diffusion with R70Cu30 alloy powders (R = NdPr and Ce)
We hereby present a simple process, called in situ two-end diffusion (TED), to reach coercivity enhancement with almost unchanged energy product for hot deformed (HD) NdFeB magnets. Coercivity of the HD magnets is increased from 15.1 to 18.7 kOe for the magnet TED with (Nd0.75Pr0.25)70Cu30 (NdPrCu), which is larger than 17.6 kOe for the magnet directly doped with 2 wt. % NdPrCu alloy. Besides, the magnet TED with NdPrCu exhibits good (00L) texture and therefore could support high (BH)max of 43.0 MGOe. In addition, the magnet TED with Ce70Cu30 (CeCu) exhibit superior magnetic properties of Br = 12.8 kG, iHc = 18.0 kOe and (BH)max = 40.7 MGOe to those of traditional doping with CeCu (Br = 11.7 kG, iHc = 16.4 kOe and (BH)max = 34.2 MGOe). For TED process, low-melting CeCu can infiltrate into the center of the magnet, and most Ce distribute at grain boundary. The distribution of Ce and Cu at grain boundary can reduce the magnetization of grain boundary phase, strengthen the decoupling effect between grains and contribute to the coercivity enhancement. This work demonstrates TED with low-melting HRE-free alloys is a simple method to effectively enhance coercivity and keep high Br and (BH)max for HD NdFeB magnets.
- 3 May 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (19) , 8800-8817
Phase modification and magnetic property improvement in melt spun LaCo5-based ribbons
- 3 May 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (19) , 8800-8817
Phase modification and magnetic property improvement in melt spun LaCo5-based ribbons
- 9 February 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 58 (8) , 1-5
Fabrication of Non-Contact Magnetic Screws by Additive Manufacturing
Magnetic screws are characterized by their noncontact features, thus eliminating the disadvantage of friction loss inherent in traditional screws. Some applications require spiral-shaped screws; however, commercially available magnets are rarely spiral in shape. To obtain spiral-shaped screws, manufactures require molds or the magnets are spliced to desired shape. Unfortunately, these two fabrication processes both have drawbacks, which include, discontinuity in the magnetic flux, high cost, and reduced efficiency. This article therefore presents alternative approach that involves the design and fabrication of spiral magnetic screws via 3-D printing with magnetic materials. The prototypes were fabricated using two 3-D printing techniques, pellet deposit melting (PDM) and hybrid soft magnet selective laser melting (SLM). Finite element method is adopted to simulate and validate the fabricated magnetic screw. Experiment results, using the PDM fabricated magnets and the hybrid soft magnet SLM combined with commercial sintered NdFeB magnet are also provided, along with, verification of the design characteristics and the simulation results.
- 9 February 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 58 (8) , 1-5
Fabrication of Non-Contact Magnetic Screws by Additive Manufacturing
Magnetic screws are characterized by their noncontact features, thus eliminating the disadvantage of friction loss inherent in traditional screws. Some applications require spiral-shaped screws; however, commercially available magnets are rarely spiral in shape. To obtain spiral-shaped screws, manufactures require molds or the magnets are spliced to desired shape. Unfortunately, these two fabrication processes both have drawbacks, which include, discontinuity in the magnetic flux, high cost, and reduced efficiency. This article therefore presents alternative approach that involves the design and fabrication of spiral magnetic screws via 3-D printing with magnetic materials. The prototypes were fabricated using two 3-D printing techniques, pellet deposit melting (PDM) and hybrid soft magnet selective laser melting (SLM). Finite element method is adopted to simulate and validate the fabricated magnetic screw. Experiment results, using the PDM fabricated magnets and the hybrid soft magnet SLM combined with commercial sintered NdFeB magnet are also provided, along with, verification of the design characteristics and the simulation results.
- 18 January 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 58 (8) , 1-5
Magnetic Properties of Ce₈₅Al₁₅ Doped NdFeB Sintered Magnet by Grain Boundary Diffusion of Tb₇₀Cu₃₀ Powders
Magnetic properties’ modification and coercivity enhancement of NdFeB sintered magnets prepared by the dual-alloy (DA) sintering together with grain boundary diffusion (GBD) treatment are demonstrated. For the original NdFeB magnet, ( BH ) max of 51.4 MGOe and ${_{i}}H_{\mathrm {c}}$ of 14.9 kOe are obtained. For the magnet made with the same composition as the former but doped with Ce 85 Al 15 (CeAl) powders, magnetic isolation due to the distribution of Ce and Al at GB increases the coercivity effectively, yet few Ce entering into grain interior decreases $B_{\mathrm {r}}$ , ( BH ) max , and Curie temperature slightly. In addition, the coercivity of the above magnets can be further enhanced to 22.7–25.1 kOe by GBD with different amounts of Tb 70 Cu 30 (TbCu) powders. The clear core–shell structure, which consists of (Nd, Tb) 2 Fe 14 B phase with higher magnetocrystalline anisotropy field ( $H_{\mathrm {A}}$ ) as the shell and Nd 2 Fe 14 B phase as the core, is observed. CeAl helps to form a continuous and smooth GB. The diffusion source of TbCu could infiltrate into the magnet along such smooth GB and form a homogeneous core–shell structure. As a result, coercivity is remarkably enhanced from 14.9 kOe for DA sintered magnet with 2 wt% CeAl to 25.1 kOe for the magnet GBD with TbCu. Most importantly, various levels of NdFeB magnets, such as 52M, 35–50SH, and 45UH, could be easily attained by modifying the amounts of CeAl for DA sintered magnets and/or GBD with TbCu powders.
- 18 January 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 58 (8) , 1-5
Magnetic Properties of Ce₈₅Al₁₅ Doped NdFeB Sintered Magnet by Grain Boundary Diffusion of Tb₇₀Cu₃₀ Powders
Magnetic properties’ modification and coercivity enhancement of NdFeB sintered magnets prepared by the dual-alloy (DA) sintering together with grain boundary diffusion (GBD) treatment are demonstrated. For the original NdFeB magnet, ( BH ) max of 51.4 MGOe and ${_{i}}H_{\mathrm {c}}$ of 14.9 kOe are obtained. For the magnet made with the same composition as the former but doped with Ce 85 Al 15 (CeAl) powders, magnetic isolation due to the distribution of Ce and Al at GB increases the coercivity effectively, yet few Ce entering into grain interior decreases $B_{\mathrm {r}}$ , ( BH ) max , and Curie temperature slightly. In addition, the coercivity of the above magnets can be further enhanced to 22.7–25.1 kOe by GBD with different amounts of Tb 70 Cu 30 (TbCu) powders. The clear core–shell structure, which consists of (Nd, Tb) 2 Fe 14 B phase with higher magnetocrystalline anisotropy field ( $H_{\mathrm {A}}$ ) as the shell and Nd 2 Fe 14 B phase as the core, is observed. CeAl helps to form a continuous and smooth GB. The diffusion source of TbCu could infiltrate into the magnet along such smooth GB and form a homogeneous core–shell structure. As a result, coercivity is remarkably enhanced from 14.9 kOe for DA sintered magnet with 2 wt% CeAl to 25.1 kOe for the magnet GBD with TbCu. Most importantly, various levels of NdFeB magnets, such as 52M, 35–50SH, and 45UH, could be easily attained by modifying the amounts of CeAl for DA sintered magnets and/or GBD with TbCu powders.
- 13 December 2021
- Published by AIP Publishing in Applied Physics Letters
- Vol. 119 (24) , 242402
Large stress-induced anisotropy in soft magnetic films for synthetic spin valves
We obtain a large in-plane magnetic uniaxial anisotropy in the soft magnetic Fe60Co20B20 (FeCoB) thin films prepared by rotational sputtering. The anisotropy field (Ha) of 75 to 175 Oe was found in the films with wide ranged thickness from 2.5 to 100 nm, which was attributed to the magnetoelastic energy in association with anisotropic tensile stress. This stress-induced anisotropy has outstanding thermal stability that survives up to 350 °C in the annealing process. The similar large uniaxial anisotropy can be realized in other soft magnetic thin films, such as Fe, Co, Ni, FeCo, and NiFe, with the same synthesis technique. The anisotropic FeCoB film was used as a free layer in a synthetic spin valve. A linear resistance change against external field with a range wider than ±100 Oe together with a significantly reduced coercivity of ∼1.1 Oe (∼8.5 Oe in the case with isotropic free layer) was observed in the transfer curve. The results of this work not only confirm the feasibility of films with large stress-induced magnetic anisotropy as a functional layer in spin-valve devices but also demonstrate a simple synthesis route to induce the magnetic anisotropy, which provides an additional control parameter for the spintronic device design.
- 13 December 2021
- Published by AIP Publishing in Applied Physics Letters
- Vol. 119 (24) , 242402
Large stress-induced anisotropy in soft magnetic films for synthetic spin valves
We obtain a large in-plane magnetic uniaxial anisotropy in the soft magnetic Fe60Co20B20 (FeCoB) thin films prepared by rotational sputtering. The anisotropy field (Ha) of 75 to 175 Oe was found in the films with wide ranged thickness from 2.5 to 100 nm, which was attributed to the magnetoelastic energy in association with anisotropic tensile stress. This stress-induced anisotropy has outstanding thermal stability that survives up to 350 °C in the annealing process. The similar large uniaxial anisotropy can be realized in other soft magnetic thin films, such as Fe, Co, Ni, FeCo, and NiFe, with the same synthesis technique. The anisotropic FeCoB film was used as a free layer in a synthetic spin valve. A linear resistance change against external field with a range wider than ±100 Oe together with a significantly reduced coercivity of ∼1.1 Oe (∼8.5 Oe in the case with isotropic free layer) was observed in the transfer curve. The results of this work not only confirm the feasibility of films with large stress-induced magnetic anisotropy as a functional layer in spin-valve devices but also demonstrate a simple synthesis route to induce the magnetic anisotropy, which provides an additional control parameter for the spintronic device design.