Triwikantoro Triwikantoro
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Triwikantoro Triwikantoro has a total of 117 co-authors. Here are the top co-authors by number of shared publications:
- Suminar Pratapa
Department of Physics, Faculty of Science and Data Analytics, Institut Teknologi Sepuluh Nopember (ITS), Surabaya, Indonesia
11 shared publications Darminto
10 shared publications- Malik Anjelh Baqiya
Institut Teknologi Sepuluh Nopember
6 shared publications - Darminto
Department of Physics, Faculty of Science and Data Analytics, Institut Teknologi Sepuluh Nopember, Surabaya, Indonesia
5 shared publications Mashuri
5 shared publications- Mochamad Zainuri
Institut Teknologi Sepuluh Nopember
5 shared publications
Latest Publications
- 18 November 2025
- Published by Trans Tech Publications, Ltd. in Journal of Metastable and Nanocrystalline Materials
- Vol. 42, 35-43
Influence of Crucible Materials and Pre-Treatments on Nanocrystalline Na2ZrO3 Formation during Zirconia Recovery for Dental Applications
The structures of sodium zirconate were studied in this research, which formed after the alkali fusion process. In this process, zircon is decomposed using sodium hydroxide (NaOH) at high temperatures to separate zirconium from impurities, resulting in high-purity zirconia which has potential as a dental material. The study aims to control the formation of Na 2 ZrO 3 phase and to minimize the reactions between Zircon, NaOH, and crucible materials, such as porcelain, silicon carbide (SiC), and alumina to prevent contamination. To enhance reaction efficiency, a pre-treatment process was introduced, including wet milling and NaOH leaching. Then, the pre-treated zircon sand was reacted with NaOH in a 1 ZrSiO 4 : 6 NaOH molar ratio. Results showed color changes in the crucibles, indicating interactions between crucible materials and NaOH. But there is no change observed in alumina crucible which means that it is not reacted with either NaOH or ZrSiO 4 . Different pre-treatment and crucible materials influenced the crystal size of Na 2 ZrO 3 phase which give the lowest crystal size of 24.69 nm when using porcelain crucible. After the recovery process was finished high-purity full tetragonal zirconia phase is achieved which can be further processed as a artificial dental application. In artificial tooth application, pure zirconia with high strength is needed, thus controlling crystal and grain sizes is a crucial factor which affect the properties.
- 18 November 2025
- Published by Trans Tech Publications, Ltd. in Journal of Metastable and Nanocrystalline Materials
- Vol. 42, 35-43
Influence of Crucible Materials and Pre-Treatments on Nanocrystalline Na2ZrO3 Formation during Zirconia Recovery for Dental Applications
The structures of sodium zirconate were studied in this research, which formed after the alkali fusion process. In this process, zircon is decomposed using sodium hydroxide (NaOH) at high temperatures to separate zirconium from impurities, resulting in high-purity zirconia which has potential as a dental material. The study aims to control the formation of Na 2 ZrO 3 phase and to minimize the reactions between Zircon, NaOH, and crucible materials, such as porcelain, silicon carbide (SiC), and alumina to prevent contamination. To enhance reaction efficiency, a pre-treatment process was introduced, including wet milling and NaOH leaching. Then, the pre-treated zircon sand was reacted with NaOH in a 1 ZrSiO 4 : 6 NaOH molar ratio. Results showed color changes in the crucibles, indicating interactions between crucible materials and NaOH. But there is no change observed in alumina crucible which means that it is not reacted with either NaOH or ZrSiO 4 . Different pre-treatment and crucible materials influenced the crystal size of Na 2 ZrO 3 phase which give the lowest crystal size of 24.69 nm when using porcelain crucible. After the recovery process was finished high-purity full tetragonal zirconia phase is achieved which can be further processed as a artificial dental application. In artificial tooth application, pure zirconia with high strength is needed, thus controlling crystal and grain sizes is a crucial factor which affect the properties.
- Open Access
- 25 January 2025
- Published by Universitas Gadjah Mada in Indonesian Journal of Chemistry
- Vol. 25 (1) , 100-109
Enhanced Optical Properties of ZnO-TiO2 Films Through Co-Sensitization with Multiple Natural Dyes
The ZnO-TiO2 films were co-sensitized with single, double, and triple natural dyes, leading to distinct effects on the optical properties. ZnO (wurtzite) and TiO2 (anatase) were prepared from commercial powders and the XRD results revealed that the crystallite size is 158 and 443 nm, respectively. The UV absorbance of ZnO powder shows significant peaks at wavelengths of 255 and 345 nm, with a band gap energy of 3.07 eV. Meanwhile, TiO2 powder exhibits a maximum peak at 325 nm and possesses a band gap energy of 3.16 eV. The extraction of natural dyes (Moringa oleifera, Biancaea sappan, Matricaria chamomilla, Rosa, and Chrysanthemum) was carried out using a cost-effective and simple method involving immersion in ethanol for 2 × 24 h followed by filtration. FTIR test results show the presence of O–H, C–H, C=C, and C–O functional groups. The results of coating the ZnO-TiO2 film with natural dyes show that the UV spectrum peaks are higher than the visible light wavelength. Co-sensitization of double natural dyes demonstrated different effects on the ZnO-TiO2 film, i.e., achieved panchromatic absorption mainly in the UV wavelength spectrum.
- 25 January 2025
- Published by Universitas Gadjah Mada in Indonesian Journal of Chemistry
- Vol. 25 (1) , 100-109
Open AccessEnhanced Optical Properties of ZnO-TiO2 Films Through Co-Sensitization with Multiple Natural Dyes
The ZnO-TiO2 films were co-sensitized with single, double, and triple natural dyes, leading to distinct effects on the optical properties. ZnO (wurtzite) and TiO2 (anatase) were prepared from commercial powders and the XRD results revealed that the crystallite size is 158 and 443 nm, respectively. The UV absorbance of ZnO powder shows significant peaks at wavelengths of 255 and 345 nm, with a band gap energy of 3.07 eV. Meanwhile, TiO2 powder exhibits a maximum peak at 325 nm and possesses a band gap energy of 3.16 eV. The extraction of natural dyes (Moringa oleifera, Biancaea sappan, Matricaria chamomilla, Rosa, and Chrysanthemum) was carried out using a cost-effective and simple method involving immersion in ethanol for 2 × 24 h followed by filtration. FTIR test results show the presence of O–H, C–H, C=C, and C–O functional groups. The results of coating the ZnO-TiO2 film with natural dyes show that the UV spectrum peaks are higher than the visible light wavelength. Co-sensitization of double natural dyes demonstrated different effects on the ZnO-TiO2 film, i.e., achieved panchromatic absorption mainly in the UV wavelength spectrum.
- 15 January 2025
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 333
Effect of interfacial diffusion on structural, physical, and mechanical properties of ZrSiO4/Al2O3 composites
- 15 January 2025
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 333
Effect of interfacial diffusion on structural, physical, and mechanical properties of ZrSiO4/Al2O3 composites
- Open Access
- 1 May 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (5) , 055002
Ultra-dense (Bi, V, B)-oxide-added zircon ceramics fabricated by liquid-phase assisted spark plasma sintering (SPS)
Ultra-high-density zircon (ZrSiO4) ceramics were prepared using the spark plasma sintering (SPS) technique of zircon nanopowder with the addition of three different sintering agents, i.e., Bi2O3, V2O5and B2O3. The effect of each agent and the SPS parameters (temperature and pressure) on phase composition, microstructure, thermal and mechanical properties of the ceramics were evaluated. The identified crystalline phases of the sintered ceramics were zircon and monoclinic zirconia. The addition of a sintering agent affects the structure of zircon ceramics, i.e. the lattice parameter and the crystallite size. The sintered ceramics reached relative densities up to 99.9% of the theoretical one when V2O5or B2O3was added. SEM observations confirmed the densification of the zircon ceramics. We found the ceramics exhibited thermal conductivity ranging from 0.39 to 0.61 Wm−1K−1at 373 K while the coefficient of thermal expansion was 2.3–4.0 × 10−6/°C and the Vickers hardness was obtained to be 9.52–12.66 GPa. The Young’s (E), bulk (B), and shear (G) moduli, Poisson’s ratio ν, Pugh’s ratioB/G, and the ratio of of the ceramics are in a range of 240 − 288 GPa, 207 − 267 GPa, 91 − 109 Pa, 1.95 − 2.45, and 0.011 − 0.019 respectively. We found that high-density, quasi-ductile zircon ceramics can be synthesized at a low sintering temperature and short holding time.- 1 May 2023
- Published by IOP Publishing in Materials Research Express
- Vol. 10 (5) , 055002
Open AccessUltra-dense (Bi, V, B)-oxide-added zircon ceramics fabricated by liquid-phase assisted spark plasma sintering (SPS)
Ultra-high-density zircon (ZrSiO4) ceramics were prepared using the spark plasma sintering (SPS) technique of zircon nanopowder with the addition of three different sintering agents, i.e., Bi2O3, V2O5and B2O3. The effect of each agent and the SPS parameters (temperature and pressure) on phase composition, microstructure, thermal and mechanical properties of the ceramics were evaluated. The identified crystalline phases of the sintered ceramics were zircon and monoclinic zirconia. The addition of a sintering agent affects the structure of zircon ceramics, i.e. the lattice parameter and the crystallite size. The sintered ceramics reached relative densities up to 99.9% of the theoretical one when V2O5or B2O3was added. SEM observations confirmed the densification of the zircon ceramics. We found the ceramics exhibited thermal conductivity ranging from 0.39 to 0.61 Wm−1K−1at 373 K while the coefficient of thermal expansion was 2.3–4.0 × 10−6/°C and the Vickers hardness was obtained to be 9.52–12.66 GPa. The Young’s (E), bulk (B), and shear (G) moduli, Poisson’s ratio ν, Pugh’s ratioB/G, and the ratio of of the ceramics are in a range of 240 − 288 GPa, 207 − 267 GPa, 91 − 109 Pa, 1.95 − 2.45, and 0.011 − 0.019 respectively. We found that high-density, quasi-ductile zircon ceramics can be synthesized at a low sintering temperature and short holding time. - Open Access
- 27 March 2023
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 13 (15) , 10414-10423
Structures and electric properties of PANI/polymorphic-ZrO2 composites
A polyaniline/zirconia (PANI/ZrO2) composite has been successfully synthesized using an in situ method with HCl used as a doping agent, SDBS as a surfactant and APS as an oxidant.
- 27 March 2023
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 13 (15) , 10414-10423
Open AccessStructures and electric properties of PANI/polymorphic-ZrO2 composites
A polyaniline/zirconia (PANI/ZrO2) composite has been successfully synthesized using an in situ method with HCl used as a doping agent, SDBS as a surfactant and APS as an oxidant.
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2714 (1) , 020001
Morphology and AC conductivity of polyaniline/ZrSiO4 composite prepared by in-situ oxidative polymerization with SDBS as surfactant in acidic medium
This paper reports the synthesis and observations of morphology and A.C. conductivity of polyaniline/ZrSiO4 composites. ZrSiO4 as filler was obtained by refinin
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2714 (1) , 020001
Open AccessMorphology and AC conductivity of polyaniline/ZrSiO4 composite prepared by in-situ oxidative polymerization with SDBS as surfactant in acidic medium
This paper reports the synthesis and observations of morphology and A.C. conductivity of polyaniline/ZrSiO4 composites. ZrSiO4 as filler was obtained by refinin
- 14 April 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 285
Structural, physical and mechanical properties of zirconia-polymorph/alumina composites
- 14 April 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 285
Structural, physical and mechanical properties of zirconia-polymorph/alumina composites
- Open Access
- 1 June 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (6) , 065001
Thickness optimization of a double-layered microwave absorber combining magnetic and dielectric particles
The purpose of this study is to optimize the thickness of the double-layered microwave absorber for obtaining the highest absorption. The graphenic-based carbon compounds and Fe3O4 magnetic particles were combined to fabricate the double-layered absorber. The thickness was optimized by employing a genetic algorithm (GA) to obtain high reflection loss R L min values. These samples at a thickness of 2 mm were measured for reflection loss (RL) with a Vector Network Analyzer (VNA). Input variables, such as relatively complex permeability and relatively complex permittivity, were obtained using a conversion program that uses Nicolson-Ross-Weir (NRW) method from VNA S-parameter values (S11 and S21) data. By entering the permeability and permittivity of the complex relative to GA, the thickness can be optimized to produce high R L min value. Optimization of the double-layer thickness of 12 absorbers produces the optimum thickness of d 1 = 5.99 mm and d 2 = 0.87 mm among the materials combination, which results in a high R L min (−44.69 dB). This optimization is very important for designing double-layer radar absorbing material (RAM) which results in high R L min values.
- 1 June 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (6) , 065001
Open AccessThickness optimization of a double-layered microwave absorber combining magnetic and dielectric particles
The purpose of this study is to optimize the thickness of the double-layered microwave absorber for obtaining the highest absorption. The graphenic-based carbon compounds and Fe3O4 magnetic particles were combined to fabricate the double-layered absorber. The thickness was optimized by employing a genetic algorithm (GA) to obtain high reflection loss R L min values. These samples at a thickness of 2 mm were measured for reflection loss (RL) with a Vector Network Analyzer (VNA). Input variables, such as relatively complex permeability and relatively complex permittivity, were obtained using a conversion program that uses Nicolson-Ross-Weir (NRW) method from VNA S-parameter values (S11 and S21) data. By entering the permeability and permittivity of the complex relative to GA, the thickness can be optimized to produce high R L min value. Optimization of the double-layer thickness of 12 absorbers produces the optimum thickness of d 1 = 5.99 mm and d 2 = 0.87 mm among the materials combination, which results in a high R L min (−44.69 dB). This optimization is very important for designing double-layer radar absorbing material (RAM) which results in high R L min values.
- Open Access
- 5 February 2020
- Published by IntechOpen
Ferrite-Based Nanoparticles Synthesized from Natural Iron Sand as the Fe3+ Ion Source
Ferrite-based nanoparticles, namely, bismuth ferrite (BiFeO3) and calcium ferrite (CaFe4O7), have been synthesized via sol-gel and chemically dissolved method, respectively, employing hematite (α-Fe2O3) as the Fe3+ ion source. Firstly, α-Fe2O3 nanoparticles were prepared from natural iron sand containing mostly magnetite (Fe3O4) phase through coprecipitation technique continued by sintering process at 800°C for 2 h. Higher BiFeO3 phase content was achieved after Bi-Fe gel being annealed at 650°C for 1 h in air atmosphere. Furthermore, major phase of CaFe4O7 was formed with molar ratio of Fe3+/Ca2+ = 6 and sintering temperature of 800°C for 3 h. Interestingly, the powders with dominant CaFe4O7 phase, known as calcium biferrite, exhibit higher ferromagnetism at room temperature. The magnetic properties of the calcium biferrite are comparable to those of barium hexaferrite which can be applied for radar-absorbing material. Meanwhile, BiFeO3 powders also show weak room temperature ferromagnetism. It has also demonstrated that Ni doping in the bismuth ferrite (BiFe1−xNixO3 with x = 0.1) nanoparticles results in enhancement of the magnetic properties. Moreover, a ferroelectric hysteresis loop and a trend of frequency dependence of the dielectric constant have been observed, which were enhanced by Pb doping (Bi1−yPbyFeO3 with y = 0.1). These results suggest a multiferroic behavior in the BiFeO3 nanoparticles.
- 5 February 2020
- Published by IntechOpen
Open AccessFerrite-Based Nanoparticles Synthesized from Natural Iron Sand as the Fe3+ Ion Source
Ferrite-based nanoparticles, namely, bismuth ferrite (BiFeO3) and calcium ferrite (CaFe4O7), have been synthesized via sol-gel and chemically dissolved method, respectively, employing hematite (α-Fe2O3) as the Fe3+ ion source. Firstly, α-Fe2O3 nanoparticles were prepared from natural iron sand containing mostly magnetite (Fe3O4) phase through coprecipitation technique continued by sintering process at 800°C for 2 h. Higher BiFeO3 phase content was achieved after Bi-Fe gel being annealed at 650°C for 1 h in air atmosphere. Furthermore, major phase of CaFe4O7 was formed with molar ratio of Fe3+/Ca2+ = 6 and sintering temperature of 800°C for 3 h. Interestingly, the powders with dominant CaFe4O7 phase, known as calcium biferrite, exhibit higher ferromagnetism at room temperature. The magnetic properties of the calcium biferrite are comparable to those of barium hexaferrite which can be applied for radar-absorbing material. Meanwhile, BiFeO3 powders also show weak room temperature ferromagnetism. It has also demonstrated that Ni doping in the bismuth ferrite (BiFe1−xNixO3 with x = 0.1) nanoparticles results in enhancement of the magnetic properties. Moreover, a ferroelectric hysteresis loop and a trend of frequency dependence of the dielectric constant have been observed, which were enhanced by Pb doping (Bi1−yPbyFeO3 with y = 0.1). These results suggest a multiferroic behavior in the BiFeO3 nanoparticles.
- Open Access
- 1 November 2019
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1373 (1) , 012027
The Crystallization Process of Zr-Based Metallic Glass by the Influence of Heating Rate and Alloy Composition
A study of the crystallization process of Zr-based Metallic Glass by the influence of the heating rate and variation of alloy composition was investigated. The alloys used were Zr68Cu14Ni11Al7, Zr64.5Cu17Ni11Al7.5, and Zr69.5Cu12Ni11Al7.5. Thermal stability was analyzed using DSC (Differential Scanning Calorimetry) with a heating rate of 5°C/min and 10°C/min until the temperature reached 500°C. The three samples were heated with temperature variations of 400°C, 425°C, and 450°C for one hour in air. Crystal growth was observed by XRD test. The DSC curve of the three samples shows that the higher the rate of heating, the shift of the crystallization peak temperature shifts to a higher temperature. At higher temperatures, the crystallization process occurs faster than at lower temperatures. The composition of zirconium contributes to the resistance properties of crystallization. The alloy with the highest zirconium composition has a high resistance to crystallization. The crystalline phase formed is ZrO2 tetragonal in all samples heated at a temperature of 450°C, and there is an intermetallic phase of Zr2Ni identified on Zr64.5Cu17Ni11Al7.5
- 1 November 2019
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1373 (1) , 012027
Open AccessThe Crystallization Process of Zr-Based Metallic Glass by the Influence of Heating Rate and Alloy Composition
A study of the crystallization process of Zr-based Metallic Glass by the influence of the heating rate and variation of alloy composition was investigated. The alloys used were Zr68Cu14Ni11Al7, Zr64.5Cu17Ni11Al7.5, and Zr69.5Cu12Ni11Al7.5. Thermal stability was analyzed using DSC (Differential Scanning Calorimetry) with a heating rate of 5°C/min and 10°C/min until the temperature reached 500°C. The three samples were heated with temperature variations of 400°C, 425°C, and 450°C for one hour in air. Crystal growth was observed by XRD test. The DSC curve of the three samples shows that the higher the rate of heating, the shift of the crystallization peak temperature shifts to a higher temperature. At higher temperatures, the crystallization process occurs faster than at lower temperatures. The composition of zirconium contributes to the resistance properties of crystallization. The alloy with the highest zirconium composition has a high resistance to crystallization. The crystalline phase formed is ZrO2 tetragonal in all samples heated at a temperature of 450°C, and there is an intermetallic phase of Zr2Ni identified on Zr64.5Cu17Ni11Al7.5