Teng Guo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Teng Guo has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
Yu Guo
College of Chemistry and Materials Engineering, Anhui Science and Technology University, Bengbu, China
3 shared publicationsZhifu Liu
The Key Laboratory of Inorganic Functional Materials and Devices, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai, China
3 shared publicationsJunhua Chen
Anhui Science and Technology University
2 shared publicationsZhenzhen Hui
College of Chemistry and Materials Engineering, Anhui Science and Technology University, Bengbu, China
2 shared publicationsZhijie Ding
Anhui Science and Technology University
2 shared publicationsGuang Zhu
Anhui Key Laboratory of Spin Electron and Nanomaterials (Cultivating Base) Suzhou College 234000 Suzhou China
1 shared publication
Latest Publications
- 10 February 2021
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 50 (4) , 2476-2481
Li6NiNb2O9 Compound with Rock-Salt Crystal Structure and Its Microwave Dielectric Properties
- 10 February 2021
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 50 (4) , 2476-2481
Li6NiNb2O9 Compound with Rock-Salt Crystal Structure and Its Microwave Dielectric Properties
- 12 September 2018
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 29 (21) , 18628-18633
Microwave dielectric properties of NaBaPO4 ceramics with fast sintering properties
- 12 September 2018
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 29 (21) , 18628-18633
Microwave dielectric properties of NaBaPO4 ceramics with fast sintering properties
- 20 April 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (15) , 11515-11520
SrZn2(PO4)2–TiO2 composite microwave dielectric ceramics with wide tunability range for temperature coefficient of resonant frequency
- 20 April 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (15) , 11515-11520
SrZn2(PO4)2–TiO2 composite microwave dielectric ceramics with wide tunability range for temperature coefficient of resonant frequency
- 17 February 2016
- Published by Taylor & Francis in Ferroelectrics
- Vol. 492 (1) , 91-102
Microwave Dielectric Properties of AZn2(PO4)2(A = Sr, Ba) Ceramics
Crystal structures, microstructure and microwave dielectric properties were investigated for dense ceramics with single phase of AZn2(PO4)2 (A = Sr, Ba). It was found that crystal structures with large difference can be obtained in SrZn2(PO4)2 and BaZn2(PO4)2, which leads distinct variation of sintering and microwave dielectric properties, in which SrZn2(PO4)2 ceramics has ϵ = 6.29, Q × f = 21600 GHz (10.9 GHz) and τf = − 70.4 ppm/°C when sintering temperature was 940°C, and can be co-fired with copper electrode in N2 atmosphere; while the BaZn2(PO4)2 ceramics could be sintered at a relative higher temperature, 1000°C but higher τf value was obtained, with microwave dielectric properties as ϵ = 7.72, Q × f = 17000 GHz (9.9 GHz) and τf = − 41.1 ppm/°C.
- 17 February 2016
- Published by Taylor & Francis in Ferroelectrics
- Vol. 492 (1) , 91-102
Microwave Dielectric Properties of AZn2(PO4)2(A = Sr, Ba) Ceramics
Crystal structures, microstructure and microwave dielectric properties were investigated for dense ceramics with single phase of AZn2(PO4)2 (A = Sr, Ba). It was found that crystal structures with large difference can be obtained in SrZn2(PO4)2 and BaZn2(PO4)2, which leads distinct variation of sintering and microwave dielectric properties, in which SrZn2(PO4)2 ceramics has ϵ = 6.29, Q × f = 21600 GHz (10.9 GHz) and τf = − 70.4 ppm/°C when sintering temperature was 940°C, and can be co-fired with copper electrode in N2 atmosphere; while the BaZn2(PO4)2 ceramics could be sintered at a relative higher temperature, 1000°C but higher τf value was obtained, with microwave dielectric properties as ϵ = 7.72, Q × f = 17000 GHz (9.9 GHz) and τf = − 41.1 ppm/°C.
- 4 September 2015
- Published by Wiley in Rare Metals
- Vol. 41 (4) , 1357-1363
Magneto‐electric behaviors of La 0.67− x Nd x Sr 0.33 MnO 3 system
The polycrystalline samples La 0.67− x Nd x Sr 0.33 MnO 3 ( x = 0.1, 0.2, 0.3, 0.4, 0.5) were prepared by standard solid‐state reaction method, and the M – T curves, electron spin resonance (ESR) curves, infrared spectra, Raman spectra, ρ – T curves and MR– T curves of the compounds above were measured. The results show that single phase can be obtained at different Nd substitution ratios, and with the increase in Nd doping, the magnetic structure of the system transforms from long‐range ferromagnetic order to spin cluster glass state and antiferromagnetic state; and the phase separation appears in the samples with x = 0.3 and 0.4. The transport property exhibits variation with the increase in Nd doping, and the electric behavior of the sample transforms (from metal state to insulator–metal transition, and then insulator state) is accompanied by colossal magnetoresistance (CMR) effect, which can be attributed to the different couplings of sublattices induced by Nd doping and the interface tunneling effect related to the spin.
- 4 September 2015
- Published by Wiley in Rare Metals
- Vol. 41 (4) , 1357-1363
Magneto‐electric behaviors of La 0.67− x Nd x Sr 0.33 MnO 3 system
The polycrystalline samples La 0.67− x Nd x Sr 0.33 MnO 3 ( x = 0.1, 0.2, 0.3, 0.4, 0.5) were prepared by standard solid‐state reaction method, and the M – T curves, electron spin resonance (ESR) curves, infrared spectra, Raman spectra, ρ – T curves and MR– T curves of the compounds above were measured. The results show that single phase can be obtained at different Nd substitution ratios, and with the increase in Nd doping, the magnetic structure of the system transforms from long‐range ferromagnetic order to spin cluster glass state and antiferromagnetic state; and the phase separation appears in the samples with x = 0.3 and 0.4. The transport property exhibits variation with the increase in Nd doping, and the electric behavior of the sample transforms (from metal state to insulator–metal transition, and then insulator state) is accompanied by colossal magnetoresistance (CMR) effect, which can be attributed to the different couplings of sublattices induced by Nd doping and the interface tunneling effect related to the spin.
- 1 November 2010
- Published by Taylor & Francis in Ferroelectrics
- Vol. 407 (1) , 84-92
Effect of Sr/P Ratio on the Microwave Dielectric Properties of Sr 2 P 2 O 7 Ceramics
A pyrophosphate compound, Sr2P2O7, and a mixture, (1-x)Sr2P2O7-xSr3(PO4)2 (x < 0.06) were prepared by the solid-state reaction method. The phase evolution and microwave dielectric properties of Sr2P2O7 ceramics were investigated, and the change of dielectric properties was discussed when a minor phase, Sr3(PO4)2 introduced. The results show a mixed phase of Sr2P2O7 and Sr3(PO4)2 could be obtained when the molar ratio of Sr/P > 1:1 in the raw material, and when the content of Sr3(PO4)2 increased, the τ f values of samples increased. In particular, when x = 0.060, good microwave dielectric properties were achieved: ϵr = 7.9, Q × f = 17200 GHz (at 9.9 GHz) and τ f = +2.09 ppm/°C.
- 1 November 2010
- Published by Taylor & Francis in Ferroelectrics
- Vol. 407 (1) , 84-92
Effect of Sr/P Ratio on the Microwave Dielectric Properties of Sr 2 P 2 O 7 Ceramics
A pyrophosphate compound, Sr2P2O7, and a mixture, (1-x)Sr2P2O7-xSr3(PO4)2 (x < 0.06) were prepared by the solid-state reaction method. The phase evolution and microwave dielectric properties of Sr2P2O7 ceramics were investigated, and the change of dielectric properties was discussed when a minor phase, Sr3(PO4)2 introduced. The results show a mixed phase of Sr2P2O7 and Sr3(PO4)2 could be obtained when the molar ratio of Sr/P > 1:1 in the raw material, and when the content of Sr3(PO4)2 increased, the τ f values of samples increased. In particular, when x = 0.060, good microwave dielectric properties were achieved: ϵr = 7.9, Q × f = 17200 GHz (at 9.9 GHz) and τ f = +2.09 ppm/°C.