Hitonobu Koike
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hitonobu Koike has a total of 57 co-authors. Here are the top co-authors by number of shared publications:
- Katsuyuki Kida
University of Toyama
43 shared publications Edson Costa Santos
Kyushu University
24 shared publicationsTakashi Honda
Kyushu University
21 shared publicationsYuji Kashima
17 shared publicationsJustyna Rozwadowska
Kyushu University
16 shared publicationsKenji Kanemasu
Yoshinori Industry
16 shared publications
Latest Publications
- 22 November 2021
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 904, 243-249
Influence on Tribological Behavior of PEEK Composite Film Layer on PEEK-PTFE Bearings with Artificial Defect in Dry Condition
In order to explore influence on tribological behavior of PEEK composite film layer in PEEK-PTFE composite radial alumina ball bearings, rolling contact fatigue tests were performed by using the PEEK bearing’s inner rings with the artificial defects in dry condition. When rotation speed and applied load were 600 rpm and 98 N, the number of cycles of the PEEK-PTFE bearings reached 1.0×107 fatigue cycles. The artificial defects with 0.02 mm depth on the raceway surface of the PEEK inner ring was covered with PEEK composite film accumulation.
- 22 November 2021
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 904, 243-249
Influence on Tribological Behavior of PEEK Composite Film Layer on PEEK-PTFE Bearings with Artificial Defect in Dry Condition
In order to explore influence on tribological behavior of PEEK composite film layer in PEEK-PTFE composite radial alumina ball bearings, rolling contact fatigue tests were performed by using the PEEK bearing’s inner rings with the artificial defects in dry condition. When rotation speed and applied load were 600 rpm and 98 N, the number of cycles of the PEEK-PTFE bearings reached 1.0×107 fatigue cycles. The artificial defects with 0.02 mm depth on the raceway surface of the PEEK inner ring was covered with PEEK composite film accumulation.
- 1 August 2020
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 858, 95-100
Observation of Tribological Wear on PEEK Shaft with Artificial Defect under Radial Rolling Sliding Point Contact
This paper’s aim is to develop the tribological repair method in PEEK (Poly-ether-ether-ketone) polymer mechanical parts with surface damage. The radial rolling sliding contact tests were carried out by using a machined PEEK shaft with an artificial defect as surface damage. An alumina ball and a PTFE composite pin contacted a PEEK shaft specimen under cyclic compressive stress with friction. The particle as solid lubricant from a PTFE composite pin filled up the crevice of the artificial defect. After that, the artificial defect was covered with the deformed microgrooves on the PEEK shaft surface. Due to adhesion by compressive stress and friction, the crevice of the artificial defect was closed. In a running-in process, the artificial defect could be reduced by the adhesion repair.
- 1 August 2020
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 858, 95-100
Observation of Tribological Wear on PEEK Shaft with Artificial Defect under Radial Rolling Sliding Point Contact
This paper’s aim is to develop the tribological repair method in PEEK (Poly-ether-ether-ketone) polymer mechanical parts with surface damage. The radial rolling sliding contact tests were carried out by using a machined PEEK shaft with an artificial defect as surface damage. An alumina ball and a PTFE composite pin contacted a PEEK shaft specimen under cyclic compressive stress with friction. The particle as solid lubricant from a PTFE composite pin filled up the crevice of the artificial defect. After that, the artificial defect was covered with the deformed microgrooves on the PEEK shaft surface. Due to adhesion by compressive stress and friction, the crevice of the artificial defect was closed. In a running-in process, the artificial defect could be reduced by the adhesion repair.
- 29 July 2019
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 814, 314-319
Observation of Tribological Fatigue Fracture on PEEK Shaft with Artificial Defect under One-Point Rolling Contact by Using 2.5D Layer Method
In order to explore the mechanism of tribological fatigue fracture in PEEK (Poly-ether-ether-ketone) polymer mechanical element application, one-point contact type RCF (rolling contact fatigue) tests were carried out by using a PEEK shaft with an artificial defect. An alumina ball contacted a PEEK shaft specimen under maximum Hertzian stress 380 MPa. Flaking and internal fatigue crack propagation under the rolling track of the tested PEEK shaft were investigated through 2.5D layer observation method. The main fatigue crack occurred near the artificial defect on the rolling track of the PEEK shaft, and propagated into depth direction. In addition, the main fatigue crack branched due to internal shear stress. The branching crack as internal fatigue crack propagated into the ball’s rolling direction. After the linkage of the branching crack and another semicircular surface crack, the horseshoe-shaped flaking as tribological fatigue fracture occurred on the rolling track of the PEEK shaft.
- 29 July 2019
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 814, 314-319
Observation of Tribological Fatigue Fracture on PEEK Shaft with Artificial Defect under One-Point Rolling Contact by Using 2.5D Layer Method
In order to explore the mechanism of tribological fatigue fracture in PEEK (Poly-ether-ether-ketone) polymer mechanical element application, one-point contact type RCF (rolling contact fatigue) tests were carried out by using a PEEK shaft with an artificial defect. An alumina ball contacted a PEEK shaft specimen under maximum Hertzian stress 380 MPa. Flaking and internal fatigue crack propagation under the rolling track of the tested PEEK shaft were investigated through 2.5D layer observation method. The main fatigue crack occurred near the artificial defect on the rolling track of the PEEK shaft, and propagated into depth direction. In addition, the main fatigue crack branched due to internal shear stress. The branching crack as internal fatigue crack propagated into the ball’s rolling direction. After the linkage of the branching crack and another semicircular surface crack, the horseshoe-shaped flaking as tribological fatigue fracture occurred on the rolling track of the PEEK shaft.
- Open Access
- 1 March 2017
- Published by SAGE Publications in Materials Science and Technology
- Vol. 33 (5) , 623-628
Increased fatigue strength of partially stabilised zirconia achieved by shot peening
The effects of shot peening (SP) on the fatigue strength of partially stabilised zirconia were studied. Smooth specimens and specimens containing a surface pre-crack with depths in the range 35–110 μm were subjected to SP. The cyclic fatigue tests were performed using a three-point bending setup. SP introduced compressive residual stresses on the specimens and improved their fatigue strengths. The shot peened specimens with pre-crack depths ≤ 50 μm fractured outside the pre-crack area and exhibited considerably high fatigue limits, equivalent to those of the shot peened smooth specimens. Therefore, the pre-cracks with depths ≤ 50 μm could be rendered harmless by SP, which was confirmed by the theoretical estimations based on fracture mechanics.
- 1 March 2017
- Published by SAGE Publications in Materials Science and Technology
- Vol. 33 (5) , 623-628
Open AccessIncreased fatigue strength of partially stabilised zirconia achieved by shot peening
The effects of shot peening (SP) on the fatigue strength of partially stabilised zirconia were studied. Smooth specimens and specimens containing a surface pre-crack with depths in the range 35–110 μm were subjected to SP. The cyclic fatigue tests were performed using a three-point bending setup. SP introduced compressive residual stresses on the specimens and improved their fatigue strengths. The shot peened specimens with pre-crack depths ≤ 50 μm fractured outside the pre-crack area and exhibited considerably high fatigue limits, equivalent to those of the shot peened smooth specimens. Therefore, the pre-cracks with depths ≤ 50 μm could be rendered harmless by SP, which was confirmed by the theoretical estimations based on fracture mechanics.
- 1 August 2016
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 703, 187-191
Backlash Evaluation of Hybrid UHMWPE-PEEK Bushes in a Small Robot Joint System
In our previous work, we designed a new joint system for humanoid sized robot. This system consists of a servomotor, a harmonic drive and a link unit. This link unit includes three components; polymer bushes, a metal cam plate and a metal camshaft. However elastic deformation of all-polymer bushes can cause a large backlash in the system. In the present work, a new bush was developed and its fatigue behavior was investigated.
- 1 August 2016
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 703, 187-191
Backlash Evaluation of Hybrid UHMWPE-PEEK Bushes in a Small Robot Joint System
In our previous work, we designed a new joint system for humanoid sized robot. This system consists of a servomotor, a harmonic drive and a link unit. This link unit includes three components; polymer bushes, a metal cam plate and a metal camshaft. However elastic deformation of all-polymer bushes can cause a large backlash in the system. In the present work, a new bush was developed and its fatigue behavior was investigated.
- 1 October 2015
- Published by Elsevier in Tribology International
- Vol. 90, 77-83
Wear of hybrid radial bearings (PEEK ring-PTFE retainer and alumina balls) under dry rolling contact
- 1 October 2015
- Published by Elsevier in Tribology International
- Vol. 90, 77-83
Wear of hybrid radial bearings (PEEK ring-PTFE retainer and alumina balls) under dry rolling contact
- 21 July 2015
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 24 (9) , 3573-3578
Increase in Strength of Partially Stabilized Zirconia After Shot Peening
- 21 July 2015
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 24 (9) , 3573-3578
Increase in Strength of Partially Stabilized Zirconia After Shot Peening
- 1 January 2015
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Materials and Mechanics Conference
- Vol. 2015, _OS1208-47
OS1208-473 Improvement of wear property of Si_3N_4 using shot-peening
- 1 January 2015
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Materials and Mechanics Conference
- Vol. 2015, _OS1208-47
OS1208-473 Improvement of wear property of Si_3N_4 using shot-peening
- 1 July 2014
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 597, 353-357
Measurement of Sliding Wear of Shot-Peened Partially Stabilized Zirconia Plate
In this paper the wear performance between Partially Stabilized Zirconia (PSZ) plate and silicon nitride ball under dry conditions was investigaed. The wear durability of PSZ with shot peening was higher than that of PSZ without shot peening in the sliding wear test under low Hertzian contact pressure. By shot peening, the transformation from tetragonal to monocryclinic phase with compressive residual stress occurred locally on the PSZ surface. Due to this transformation, the wear durability on the surface of the PSZ plate was improved.
- 1 July 2014
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 597, 353-357
Measurement of Sliding Wear of Shot-Peened Partially Stabilized Zirconia Plate
In this paper the wear performance between Partially Stabilized Zirconia (PSZ) plate and silicon nitride ball under dry conditions was investigaed. The wear durability of PSZ with shot peening was higher than that of PSZ without shot peening in the sliding wear test under low Hertzian contact pressure. By shot peening, the transformation from tetragonal to monocryclinic phase with compressive residual stress occurred locally on the PSZ surface. Due to this transformation, the wear durability on the surface of the PSZ plate was improved.
- 31 March 2014
- Published by Taylor & Francis in Materials Research Innovations
- Vol. 18 (sup1) , S1-38
Measurement of fatigue and wear of PEEK bush and A7075 cam plate in humanoid robot joints
- 31 March 2014
- Published by Taylor & Francis in Materials Research Innovations
- Vol. 18 (sup1) , S1-38
Measurement of fatigue and wear of PEEK bush and A7075 cam plate in humanoid robot joints