Hanqin Liang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hanqin Liang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Yongfeng Xia
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
12 shared publicationsDongxu Yao
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
11 shared publications- Jinwei Yin
State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai, 200050, China
11 shared publications Kaihui Zuo
State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai, 200050, China
11 shared publications- Yu‐Ping Zeng
State Key Laboratory of High‐Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
10 shared publications - Weide Wang
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China
5 shared publications
Latest Publications
- 17 September 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 20 (1) , 465-474
Enhanced thermal conductivity and flexural strength of sintered reaction‐bonded silicon nitride with addition of (Y0.96Eu0.04)2O3
Sintered reaction‐bonded silicon nitride (SRBSN) with high thermal conductivity was obtained using (Y0.96Eu0.04)2O3 and MgO as sintering additives. Green compacts were nitrided at 1400°C for 4 h. Post‐sintering was carried out at 1850 and 1900°C for 4 h, respectively. In reaction‐bonded silicon nitride (RBSN) doped with Y2O3 and MgO, the β‐Si3N4 content and nitridation degree were 51.1% and 93.8%, respectively. However, the β‐Si3N4 content and nitridation degree were 72.6% and 96.7% in a nitrided compact doped with (Y0.96Eu0.04)2O3 and MgO. After post‐sintering, the phase composition, microstructure, mechanical properties, and thermal conductivity were investigated. After sintering at 1900°C for 4 h, the thermal conductivity of SRBSN doped with (Y0.96Eu0.04)2O3 and MgO was increased by 16.5% compared to that of the samples doped with Y2O3 and MgO. The highest hardness of 1639 HV and the good flexural strength of 776.4 MPa were also achieved in the sample doped with 2‐mol.% (Y0.96Eu0.04)2O3 and 5‐mol.% MgO.
- 17 September 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 20 (1) , 465-474
Enhanced thermal conductivity and flexural strength of sintered reaction‐bonded silicon nitride with addition of (Y0.96Eu0.04)2O3
Sintered reaction‐bonded silicon nitride (SRBSN) with high thermal conductivity was obtained using (Y0.96Eu0.04)2O3 and MgO as sintering additives. Green compacts were nitrided at 1400°C for 4 h. Post‐sintering was carried out at 1850 and 1900°C for 4 h, respectively. In reaction‐bonded silicon nitride (RBSN) doped with Y2O3 and MgO, the β‐Si3N4 content and nitridation degree were 51.1% and 93.8%, respectively. However, the β‐Si3N4 content and nitridation degree were 72.6% and 96.7% in a nitrided compact doped with (Y0.96Eu0.04)2O3 and MgO. After post‐sintering, the phase composition, microstructure, mechanical properties, and thermal conductivity were investigated. After sintering at 1900°C for 4 h, the thermal conductivity of SRBSN doped with (Y0.96Eu0.04)2O3 and MgO was increased by 16.5% compared to that of the samples doped with Y2O3 and MgO. The highest hardness of 1639 HV and the good flexural strength of 776.4 MPa were also achieved in the sample doped with 2‐mol.% (Y0.96Eu0.04)2O3 and 5‐mol.% MgO.
- 1 February 2021
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 855, 157451
Enhanced thermal conductivity in Si3N4 ceramics prepared by using ZrH2 as an oxygen getter
- 1 February 2021
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 855, 157451
Enhanced thermal conductivity in Si3N4 ceramics prepared by using ZrH2 as an oxygen getter
- 27 December 2020
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 18 (3) , 830-837
Effects of surfactant and particle size on the microstructure and strength of Si3N4 foams with high porosity
The highly porous Si 3 N 4 ceramic foams were prepared by direct foaming with mixed surfactants. The surface tension and viscosity of slurries were tailored by different carbon chain length of surfactants and different mean Si 3 N 4 particle size to achieve the pore size controlling. The nearly linear relationship between the pore size and the ratio of surface tension to viscosity was observed, which indicates that the pore size could be precisely tailored by the slurry properties. Si 3 N 4 ceramic foams with porosity of nearly 94%, mean pore size of 110–230 µm, and compressive strength of 1.24–3.51 MPa were obtained.
- 27 December 2020
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 18 (3) , 830-837
Effects of surfactant and particle size on the microstructure and strength of Si3N4 foams with high porosity
The highly porous Si 3 N 4 ceramic foams were prepared by direct foaming with mixed surfactants. The surface tension and viscosity of slurries were tailored by different carbon chain length of surfactants and different mean Si 3 N 4 particle size to achieve the pore size controlling. The nearly linear relationship between the pore size and the ratio of surface tension to viscosity was observed, which indicates that the pore size could be precisely tailored by the slurry properties. Si 3 N 4 ceramic foams with porosity of nearly 94%, mean pore size of 110–230 µm, and compressive strength of 1.24–3.51 MPa were obtained.
- 7 July 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (11) , 6565-6574
Microstructure and gas permeation performance of porous silicon nitride ceramics with unidirectionally aligned channels
Porous Si 3 N 4 ceramics with unidirectionally aligned channels were prepared via freezing ceramics suspension with distinct solid contents under different freezing temperatures. The samples obtained using lower solid content in ceramic suspension at higher freezing temperature exhibit larger Darcian and non‐Darcian constants due to their higher open porosity, larger pore size and lower tortuosity. Moreover the investigation on individual contributions of viscous energy losses and inertial energy losses on the total pressure drop during permeation process indicates that with decreasing the solid content or the freezing temperature the viscous energy losses increase but the inertial energy losses decrease for samples owing to the differences in their pore structures. It is worth mentioning that porous Si 3 N 4 ceramics with unidirectionally aligned channels exhibit larger Darcian and non‐Darcian constants than those with similar pore size distributions and open porosity owing to their lower tortuosity, thus rendering them appropriate for filters and membrane supports.
- 7 July 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (11) , 6565-6574
Microstructure and gas permeation performance of porous silicon nitride ceramics with unidirectionally aligned channels
Porous Si 3 N 4 ceramics with unidirectionally aligned channels were prepared via freezing ceramics suspension with distinct solid contents under different freezing temperatures. The samples obtained using lower solid content in ceramic suspension at higher freezing temperature exhibit larger Darcian and non‐Darcian constants due to their higher open porosity, larger pore size and lower tortuosity. Moreover the investigation on individual contributions of viscous energy losses and inertial energy losses on the total pressure drop during permeation process indicates that with decreasing the solid content or the freezing temperature the viscous energy losses increase but the inertial energy losses decrease for samples owing to the differences in their pore structures. It is worth mentioning that porous Si 3 N 4 ceramics with unidirectionally aligned channels exhibit larger Darcian and non‐Darcian constants than those with similar pore size distributions and open porosity owing to their lower tortuosity, thus rendering them appropriate for filters and membrane supports.
- 7 June 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5990-5998
The sound absorption performance of the highly porous silica ceramics prepared using freeze casting method
Highly porous silica ceramics with unidirectional pores were prepared using the freeze casting method. By adjusting the solid content and freezing temperature, the porosity of the ceramics was tailored in the range of 78.20%‐84.59% and pore size in the range of 8.4‐71.4 μm, respectively. Sound absorption properties of porous silica ceramics was studied and the effect of structural factors was systematically investigated. The results showed that higher porosity and smaller pores of the porous ceramics favored the sound absorption in the entire sound wave frequency. By backing the sample with small pore size porous ceramics, the sound absorption property was enhanced, particularly in the low and medium frequency range, thus the sound absorption peak shifted towards lower frequency. The presence of air gap in the back would also favor sound absorption in low and medium frequency range. The as‐fabricated porous silica ceramics owed excellent sound absorption properties due to their unidirectional pores and low flow resistances.
- 7 June 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5990-5998
The sound absorption performance of the highly porous silica ceramics prepared using freeze casting method
Highly porous silica ceramics with unidirectional pores were prepared using the freeze casting method. By adjusting the solid content and freezing temperature, the porosity of the ceramics was tailored in the range of 78.20%‐84.59% and pore size in the range of 8.4‐71.4 μm, respectively. Sound absorption properties of porous silica ceramics was studied and the effect of structural factors was systematically investigated. The results showed that higher porosity and smaller pores of the porous ceramics favored the sound absorption in the entire sound wave frequency. By backing the sample with small pore size porous ceramics, the sound absorption property was enhanced, particularly in the low and medium frequency range, thus the sound absorption peak shifted towards lower frequency. The presence of air gap in the back would also favor sound absorption in low and medium frequency range. The as‐fabricated porous silica ceramics owed excellent sound absorption properties due to their unidirectional pores and low flow resistances.
- 2 June 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5891-5899
Effect of the binary nonoxide additives on the densification behavior and thermal conductivity of Si 3 N 4 ceramics
Binary nonoxide additives ZrSi 2 ‐MgSiN 2 were applied to obtain Si 3 N 4 ceramics with high thermal conductivity by gas pressure sintering. The shrinkage behaviors during sintering were investigated by in situ dilatometry. Although densification was retarded due to a higher N/O ratio in the liquid phase, the incorporation of oxygen was inhibited because of the lower oxygen content in the liquid phase. The substitution of oxide additives by nonoxide additives eliminated native SiO 2 and induced a nitrogen‐rich liquid, resulting in purified Si 3 N 4 grains, reduced glassy phase, and enhanced Si 3 N 4 ‐Si 3 N 4 contiguity. Ultimately, a thermal conductivity of 117.32 W m −1 K −1 was achieved using ZrSi 2 ‐MgSiN 2 as sintering additives, increased by 32% compared to those doped with ZrO 2 ‐MgO.
- 2 June 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5891-5899
Effect of the binary nonoxide additives on the densification behavior and thermal conductivity of Si 3 N 4 ceramics
Binary nonoxide additives ZrSi 2 ‐MgSiN 2 were applied to obtain Si 3 N 4 ceramics with high thermal conductivity by gas pressure sintering. The shrinkage behaviors during sintering were investigated by in situ dilatometry. Although densification was retarded due to a higher N/O ratio in the liquid phase, the incorporation of oxygen was inhibited because of the lower oxygen content in the liquid phase. The substitution of oxide additives by nonoxide additives eliminated native SiO 2 and induced a nitrogen‐rich liquid, resulting in purified Si 3 N 4 grains, reduced glassy phase, and enhanced Si 3 N 4 ‐Si 3 N 4 contiguity. Ultimately, a thermal conductivity of 117.32 W m −1 K −1 was achieved using ZrSi 2 ‐MgSiN 2 as sintering additives, increased by 32% compared to those doped with ZrO 2 ‐MgO.
- 27 May 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5567-5572
Improved thermal conductivity of β‐Si 3 N 4 ceramics by lowering SiO 2 /Y 2 O 3 ratio using YH 2 as sintering additive
A two‐step sintering process was conducted to produce β‐Si 3 N 4 ceramics with high thermal conductivity. During the first step, native SiO 2 was eliminated, and Y 2 O 3 was in situ generated by a metal hydride reduction process, resulting in a high Y 2 O 3 /SiO 2 ratio. The substitution YH 2 for Y 2 O 3 endow Si 3 N 4 ceramics with an increase of 29% in thermal conductivity from 95.3 to 123 W m −1 K −1 after sintered at 1900°C for 12 hours despite an inferior sinterability. This was primarily attributed to the purified enlarged grains, devitrified grain boundary phase, and reduced lattice oxygen content in the YH 2 ‐MgO‐doped material.
- 27 May 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (10) , 5567-5572
Improved thermal conductivity of β‐Si 3 N 4 ceramics by lowering SiO 2 /Y 2 O 3 ratio using YH 2 as sintering additive
A two‐step sintering process was conducted to produce β‐Si 3 N 4 ceramics with high thermal conductivity. During the first step, native SiO 2 was eliminated, and Y 2 O 3 was in situ generated by a metal hydride reduction process, resulting in a high Y 2 O 3 /SiO 2 ratio. The substitution YH 2 for Y 2 O 3 endow Si 3 N 4 ceramics with an increase of 29% in thermal conductivity from 95.3 to 123 W m −1 K −1 after sintered at 1900°C for 12 hours despite an inferior sinterability. This was primarily attributed to the purified enlarged grains, devitrified grain boundary phase, and reduced lattice oxygen content in the YH 2 ‐MgO‐doped material.
- 1 January 2020
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 813, 152203
The effect of annealing temperature on flexural strength, dielectric loss and thermal conductivity of Si3N4 ceramics
- 1 January 2020
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 813, 152203
The effect of annealing temperature on flexural strength, dielectric loss and thermal conductivity of Si3N4 ceramics
- 10 November 2019
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (3) , 2090-2100
ZrSi 2 –MgO as novel additives for high thermal conductivity of β‐Si 3 N 4 ceramics
A novel ZrSi 2 –MgO system was used as sintering additive for fabricating high thermal conductivity silicon nitride ceramics by gas pressure sintering at 1900°C for 12 hours. By keeping the total amount of additives at 7 mol% and adjusting the amount of ZrSi 2 in the range of 0‐7 mol%, the effect of ZrSi 2 addition on sintering behaviors and thermal conductivity of silicon nitride were investigated. It was found that binary additives ZrSi 2 –MgO were effective for the densification of Si 3 N 4 ceramics. XRD observations demonstrated that ZrSi 2 reacted with native silica on the Si 3 N 4 surface to generate ZrO 2 and β‐Si 3 N 4 grains. TEM and in situ dilatometry confirmed that the as formed ZrO 2 collaborated with MgO and Si 3 N 4 to form Si–Zr–Mg–O–N liquid phase promoting the densification of Si 3 N 4 . Abnormal grain growth was promoted by in situ generated β‐Si 3 N 4 grains. Consequently, compared to ZrO 2 ‐doped materials, the addition of ZrSi 2 led to enlarged grains, extremely thin grain boundary film and high contiguity of Si 3 N 4 –Si 3 N 4 grains. Ultimately, the thermal conductivity increased by 34.6% from 84.58 to 113.91 W·(m·K) −1 when ZrO 2 was substituted by ZrSi 2 .
- 10 November 2019
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (3) , 2090-2100
ZrSi 2 –MgO as novel additives for high thermal conductivity of β‐Si 3 N 4 ceramics
A novel ZrSi 2 –MgO system was used as sintering additive for fabricating high thermal conductivity silicon nitride ceramics by gas pressure sintering at 1900°C for 12 hours. By keeping the total amount of additives at 7 mol% and adjusting the amount of ZrSi 2 in the range of 0‐7 mol%, the effect of ZrSi 2 addition on sintering behaviors and thermal conductivity of silicon nitride were investigated. It was found that binary additives ZrSi 2 –MgO were effective for the densification of Si 3 N 4 ceramics. XRD observations demonstrated that ZrSi 2 reacted with native silica on the Si 3 N 4 surface to generate ZrO 2 and β‐Si 3 N 4 grains. TEM and in situ dilatometry confirmed that the as formed ZrO 2 collaborated with MgO and Si 3 N 4 to form Si–Zr–Mg–O–N liquid phase promoting the densification of Si 3 N 4 . Abnormal grain growth was promoted by in situ generated β‐Si 3 N 4 grains. Consequently, compared to ZrO 2 ‐doped materials, the addition of ZrSi 2 led to enlarged grains, extremely thin grain boundary film and high contiguity of Si 3 N 4 –Si 3 N 4 grains. Ultimately, the thermal conductivity increased by 34.6% from 84.58 to 113.91 W·(m·K) −1 when ZrO 2 was substituted by ZrSi 2 .
- 1 June 2019
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 39 (6) , 2036-2041
High porosity Ca-α-SiAlON ceramics with rod-like grains fabricated by freeze casting and pressureless sintering
- 1 June 2019
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 39 (6) , 2036-2041
High porosity Ca-α-SiAlON ceramics with rod-like grains fabricated by freeze casting and pressureless sintering