Zhanzhan Tang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Zhanzhan Tang has a total of 64 co-authors. Here are the top co-authors by number of shared publications:
- Wei Zhang
School of Civil Engineering, Fujian University of Technology, Fuzhou, 350118, China
7 shared publications - Hanqing Zhuge
School of Civil Engineering and Architecture, Zhejiang University of Science and Technology, Hangzhou 310023, China
6 shared publications Xu Xie
4 shared publications- Hanyang Xue
Department of Civil Engineering, College of Civil Science and Engineering, Yangzhou University, Yangzhou 225127, China
3 shared publications Jianbing Yu
College of Civil Science and Engineering, Yangzhou University
3 shared publicationsStanislav Pospíšil
3 shared publications
Latest Publications
- Open Access
- 1 January 2026
- Published by Tech Science Press in Structural Durability & Health Monitoring
- Vol. 20 (4) , 1-10
Ultimate Strength Evaluation of Urban Underground UPVC Pipelines Considering Effects of High-Temperatures
The outstanding performance of unplasticized polyvinyl chloride (UPVC) has led to its widespread use in urban underground pipeline systems. However, understanding the effects of high-temperature industrial wastewater on the buried pipes is very complicated. To investigate the influence of industrial wastewater on the safety of pipes, the mechanical properties were tested using the material specimens. The changes in mechanical properties caused by the environmental temperature and heat cycles were experimentally analyzed. Empirical formulas to predict the mechanical parameters of UPVC pipe material were proposed. The ultimate strength of underground urban pipes was numerically studied by the parametric analysis. Results show that the maximum stress and ductility of UPVC pipe material decrease significantly as the ambient temperature and heat cycle increase. The ultimate strength of the underground pipe decreases exponentially with the increase in the ambient temperature. Both the temperature amplitude and the number of heat cycles have significant influences on the performance of the underground pipes.
- 1 January 2026
- Published by Tech Science Press in Structural Durability & Health Monitoring
- Vol. 20 (4) , 1-10
Open AccessUltimate Strength Evaluation of Urban Underground UPVC Pipelines Considering Effects of High-Temperatures
The outstanding performance of unplasticized polyvinyl chloride (UPVC) has led to its widespread use in urban underground pipeline systems. However, understanding the effects of high-temperature industrial wastewater on the buried pipes is very complicated. To investigate the influence of industrial wastewater on the safety of pipes, the mechanical properties were tested using the material specimens. The changes in mechanical properties caused by the environmental temperature and heat cycles were experimentally analyzed. Empirical formulas to predict the mechanical parameters of UPVC pipe material were proposed. The ultimate strength of underground urban pipes was numerically studied by the parametric analysis. Results show that the maximum stress and ductility of UPVC pipe material decrease significantly as the ambient temperature and heat cycle increase. The ultimate strength of the underground pipe decreases exponentially with the increase in the ambient temperature. Both the temperature amplitude and the number of heat cycles have significant influences on the performance of the underground pipes.
- Open Access
- 10 August 2023
- Published by MDPI AG in Applied Sciences
- Vol. 13 (16) , 9108
Research on Seismic Performance and Reinforcement Methods for Self-Centering Rocking Steel Bridge Piers
To study the seismic performance of self-centering circular-section rocking steel bridge piers whose functions can be restored after an earthquake, a high-precision finite element (FE) analysis model of such a bridge piers was established. The hysteresis behavior of concrete-infilled and hollow rocking steel bridge piers was compared. In response to the characteristics of the local deformation of the wall plates and elliptical deformation of the bottom surface, two reinforcement methods for the pier bottom, namely thickening the wall plate and adding longitudinal stiffeners in the plastic zone of the pier bottom, were proposed. The pseudo static analysis of bridge piers was carried out considering the effects of overall design parameters and reinforcement parameters of the pier bottom. The results indicate that the FE model used in this paper can obtain accurate horizontal load-displacement curves of rocking steel bridge piers. The hysteresis curves of the rocking steel bridge piers and infilled concrete rocking steel bridge piers is close, and directly using hollow steel bridge piers can improve the economic efficiency of the design. Compared to adding longitudinal stiffeners, the reinforcement form of thickened wall plates at the pier bottom has a better effect in improving the seismic performance of bridge piers. The reinforcement of the pier bottom has little effect on the energy dissipation capacity of the bridge pier, but it helps to reduce residual displacement and improve lateral stiffness.
- 10 August 2023
- Published by MDPI AG in Applied Sciences
- Vol. 13 (16) , 9108
Open AccessResearch on Seismic Performance and Reinforcement Methods for Self-Centering Rocking Steel Bridge Piers
To study the seismic performance of self-centering circular-section rocking steel bridge piers whose functions can be restored after an earthquake, a high-precision finite element (FE) analysis model of such a bridge piers was established. The hysteresis behavior of concrete-infilled and hollow rocking steel bridge piers was compared. In response to the characteristics of the local deformation of the wall plates and elliptical deformation of the bottom surface, two reinforcement methods for the pier bottom, namely thickening the wall plate and adding longitudinal stiffeners in the plastic zone of the pier bottom, were proposed. The pseudo static analysis of bridge piers was carried out considering the effects of overall design parameters and reinforcement parameters of the pier bottom. The results indicate that the FE model used in this paper can obtain accurate horizontal load-displacement curves of rocking steel bridge piers. The hysteresis curves of the rocking steel bridge piers and infilled concrete rocking steel bridge piers is close, and directly using hollow steel bridge piers can improve the economic efficiency of the design. Compared to adding longitudinal stiffeners, the reinforcement form of thickened wall plates at the pier bottom has a better effect in improving the seismic performance of bridge piers. The reinforcement of the pier bottom has little effect on the energy dissipation capacity of the bridge pier, but it helps to reduce residual displacement and improve lateral stiffness.
- 18 July 2023
- Published by Elsevier in Construction and Building Materials
- Vol. 398
Experimental study on mechanical properties of basalt Fiber-Clay lime mortar and application in brick masonry
- 18 July 2023
- Published by Elsevier in Construction and Building Materials
- Vol. 398
Experimental study on mechanical properties of basalt Fiber-Clay lime mortar and application in brick masonry
- Open Access
Experimental Study on Shear-Peeling Debonding Behavior of BFRP Sheet-to-Steel Interfaces
In order to study the failure mode and debonding behavior of the interface between BFRP (basalt fiber reinforced polymer) sheet and structural steel under mixed-mode loading conditions, eighteen specimens with different initial angles were tested in this study. The specimens were designed with different initial angles to ensure that the interface performed under mixed-mode loading conditions. The relations between the bond strengths, failure modes, and initial angles were investigated. A new evaluation method to predict the interfacial bond strength under shear-peeling loading mode was proposed. The test results show that specimens with a smaller initial angle are more likely to exhibit a shear debonding failure at the interface between the steel plate and adhesive. In contrast, specimens with a larger initial angle are more likely to exhibit peeling of the interface. The ultimate tensile strength of the specimen is higher with a smaller initial angle. The results predicted by the proposed method are in good agreement with the experimental results.
Open AccessExperimental Study on Shear-Peeling Debonding Behavior of BFRP Sheet-to-Steel Interfaces
In order to study the failure mode and debonding behavior of the interface between BFRP (basalt fiber reinforced polymer) sheet and structural steel under mixed-mode loading conditions, eighteen specimens with different initial angles were tested in this study. The specimens were designed with different initial angles to ensure that the interface performed under mixed-mode loading conditions. The relations between the bond strengths, failure modes, and initial angles were investigated. A new evaluation method to predict the interfacial bond strength under shear-peeling loading mode was proposed. The test results show that specimens with a smaller initial angle are more likely to exhibit a shear debonding failure at the interface between the steel plate and adhesive. In contrast, specimens with a larger initial angle are more likely to exhibit peeling of the interface. The ultimate tensile strength of the specimen is higher with a smaller initial angle. The results predicted by the proposed method are in good agreement with the experimental results.
- Open Access
Mechanical Properties of Low Carbon Alloy Steel with Consideration of Prior Fatigue and Plastic Damages
Mechanical properties, including the fatigue behavior of metals, are usually determined from damage-free specimens, but it is not well known how these properties change with respect to prior damages; hence, the present work aims to understand the remaining mechanical properties of low carbon alloy steel Q345q with pre-damages. Low-cycle fatigue tests on the damage free specimens, tensile tests on the low-cycle fatigue damaged specimens, and fatigue tests on the plastic deformed specimens were carried out, respectively. The low-cycle fatigue life prediction formula was proposed. The influences of different kinds of pre-damages on the residual mechanical properties were analyzed. Results show that the stable hysteretic loops in the low-cycle fatigue tests are well-stacked. The material illustrates Masing behavior, and it has a good energy dissipation capacity. The ductility of the low-cycle fatigue-damaged materials decreases significantly in comparison with the undamaged ones. The low-cycle fatigue lives of Q345q steel are almost unaffected, so long as the pre-applied tensile strain is lower than 10%.
Open AccessMechanical Properties of Low Carbon Alloy Steel with Consideration of Prior Fatigue and Plastic Damages
Mechanical properties, including the fatigue behavior of metals, are usually determined from damage-free specimens, but it is not well known how these properties change with respect to prior damages; hence, the present work aims to understand the remaining mechanical properties of low carbon alloy steel Q345q with pre-damages. Low-cycle fatigue tests on the damage free specimens, tensile tests on the low-cycle fatigue damaged specimens, and fatigue tests on the plastic deformed specimens were carried out, respectively. The low-cycle fatigue life prediction formula was proposed. The influences of different kinds of pre-damages on the residual mechanical properties were analyzed. Results show that the stable hysteretic loops in the low-cycle fatigue tests are well-stacked. The material illustrates Masing behavior, and it has a good energy dissipation capacity. The ductility of the low-cycle fatigue-damaged materials decreases significantly in comparison with the undamaged ones. The low-cycle fatigue lives of Q345q steel are almost unaffected, so long as the pre-applied tensile strain is lower than 10%.
- 8 June 2022
- Published by Elsevier in Journal of Constructional Steel Research
- Vol. 195, 107358
Effects of pre-fatigue damages on ultimate strength of steel columns: From material to structure
- 8 June 2022
- Published by Elsevier in Journal of Constructional Steel Research
- Vol. 195, 107358
Effects of pre-fatigue damages on ultimate strength of steel columns: From material to structure
- Open Access
- 8 June 2022
- Published by MDPI AG in Applied Sciences
- Vol. 12 (12) , 5838
Fiber Model Considering the Local Instability Effect and Its Application to the Seismic Analysis of Eccentrically Compressed Steel Piers
To propose a seismic response calculation model for eccentrically compressed steel piers that can consider the local instability effect and horizontal bidirectional earthquake actions, in-plane and out-of-plane pseudo-static numerical simulation and bidirectional seismic response analysis are performed to study the applicability of the improved fiber model. The comparison results with the refined hybrid-element model show that the improved fiber model can accurately simulate the hysteretic performance of eccentrically compressed steel piers in the in-plane or out-of-plane directions and can be used to calculate the structural seismic requirements under the bidirectional action of rarely met earthquakes.
- 8 June 2022
- Published by MDPI AG in Applied Sciences
- Vol. 12 (12) , 5838
Open AccessFiber Model Considering the Local Instability Effect and Its Application to the Seismic Analysis of Eccentrically Compressed Steel Piers
To propose a seismic response calculation model for eccentrically compressed steel piers that can consider the local instability effect and horizontal bidirectional earthquake actions, in-plane and out-of-plane pseudo-static numerical simulation and bidirectional seismic response analysis are performed to study the applicability of the improved fiber model. The comparison results with the refined hybrid-element model show that the improved fiber model can accurately simulate the hysteretic performance of eccentrically compressed steel piers in the in-plane or out-of-plane directions and can be used to calculate the structural seismic requirements under the bidirectional action of rarely met earthquakes.
- Open Access
Experimental and Numerical Study of Combined High and Low Cycle Fatigue Performance of Low Alloy Steel and Engineering Application
The fatigue behaviors of metals are different under different in-service environment and loading conditions. This study was devoted to investigating the combined effects of high and low cycle fatigue loads on the performance of the low alloy steel Q345. Three kinds of experiments were carried out, including the pure high cycle fatigue (HCF) tests, the pure low cycle fatigue (LCF) tests, and the combined high and low cycle fatigue (HLCF) tests. The prediction formulae were proposed for the combined high and low cycle fatigue failure. Scanning electron microscopy (SEM) and stereo microscope were used to analyze the microstructure and fracture morphology due to different fatigue loads. Case study on the combined high and low cycle fatigue damage of a steel arch bridge was carried out based on the FE method and the proposed formula. The results show that the LCF life decreases evidently due to the prior HCF damages. The HLCF fracture surface is relatively flat near the crack initiation side, and rugged at the other half part. The fatigue damages at the bridge joints increase significantly with consideration of the pre-fatigue damages caused by traffic load. In the 100th anniversary of service, the fatigue damage index without considering the HCF pre-damage is only about 50% of the coupled damage value.
Open AccessExperimental and Numerical Study of Combined High and Low Cycle Fatigue Performance of Low Alloy Steel and Engineering Application
The fatigue behaviors of metals are different under different in-service environment and loading conditions. This study was devoted to investigating the combined effects of high and low cycle fatigue loads on the performance of the low alloy steel Q345. Three kinds of experiments were carried out, including the pure high cycle fatigue (HCF) tests, the pure low cycle fatigue (LCF) tests, and the combined high and low cycle fatigue (HLCF) tests. The prediction formulae were proposed for the combined high and low cycle fatigue failure. Scanning electron microscopy (SEM) and stereo microscope were used to analyze the microstructure and fracture morphology due to different fatigue loads. Case study on the combined high and low cycle fatigue damage of a steel arch bridge was carried out based on the FE method and the proposed formula. The results show that the LCF life decreases evidently due to the prior HCF damages. The HLCF fracture surface is relatively flat near the crack initiation side, and rugged at the other half part. The fatigue damages at the bridge joints increase significantly with consideration of the pre-fatigue damages caused by traffic load. In the 100th anniversary of service, the fatigue damage index without considering the HCF pre-damage is only about 50% of the coupled damage value.