Fugang Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Fugang Chen has a total of 65 co-authors. Here are the top co-authors by number of shared publications:
Yong Zhao
8 shared publicationsWenqiang Zhao
7 shared publicationsTieqiao Zhang
6 shared publicationsXiaoli Wang
5 shared publicationsJie Wang
4 shared publicationsLanting Zhang
4 shared publications
Latest Publications
- 20 November 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1048
Advances in La/Ce-containing Nd-Fe-B permanent magnets: A comprehensive review
- 20 November 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1048
Advances in La/Ce-containing Nd-Fe-B permanent magnets: A comprehensive review
- 24 November 2023
- Published by Elsevier in Journal of Rare Earths
- Vol. 43 (2) , 304-311
Design and preparation of a sintered Nd-Y-Fe-B magnet with high magnetic properties via multi-main-phase process and subsequent grain boundary diffusion
- 24 November 2023
- Published by Elsevier in Journal of Rare Earths
- Vol. 43 (2) , 304-311
Design and preparation of a sintered Nd-Y-Fe-B magnet with high magnetic properties via multi-main-phase process and subsequent grain boundary diffusion
- Open Access
Effect of Alternating Magnetic Field on the Organization and Corrosion Resistance of 2205 Duplex Stainless Steel Narrow-Gap Laser-MIG Hybrid Weld Head
In this study, an alternating magnetic field is applied in the narrow-gap laser-MIG hybrid welding of 2205 duplex stainless steel with a thickness of 25 mm to achieve the purpose of balancing the ration of the two phases, refining the grains and improving the corrosion resistance. With the help of OM, EBSD, TEM, and other microstructural analysis methods, the organization evolution of a 2205 duplex stainless steel narrow-gap laser arc hybrid weld under the effect of alternating magnetic field is revealed. The corrosion resistance of the welded joints is investigated by electrochemical tests. The results show that the use of a 40 mT applied alternating magnetic field can not only effectively inhibit the generation of porosity and unfused defects in the weld, but also that the addition of an alternating magnetic field improves the ratio of austenite to ferrite in the weld, and the ratio of the two phases is increased from 0.657 without a magnetic field to 0.850. The weld grain preferential orientation is affected by the magnetic field, and the weld austenite grains are shifted from the Goss texture to the Copper texture. Under the electromagnetic stirring effect of the applied magnetic field, the average austenite grain size decreased from 4.15 μm to 3.82 μm, and the average ferrite grain size decreased from 4.99 μm to 4.08 μm. In addition, the effect of the alternating magnetic field increases the density of twins in the organization. Electrochemical test results show that the addition of an alternating magnetic field increases the corrosion potential by 75.2 mV and the pitting potential by 134.5 mV, which indicates that the corrosion resistance of the cover-welded specimens is improved by the effect of an alternating magnetic field. The improvement in corrosion resistance mainly depends on the austenite grain refinement and the increase in the austenite content.
Open AccessEffect of Alternating Magnetic Field on the Organization and Corrosion Resistance of 2205 Duplex Stainless Steel Narrow-Gap Laser-MIG Hybrid Weld Head
In this study, an alternating magnetic field is applied in the narrow-gap laser-MIG hybrid welding of 2205 duplex stainless steel with a thickness of 25 mm to achieve the purpose of balancing the ration of the two phases, refining the grains and improving the corrosion resistance. With the help of OM, EBSD, TEM, and other microstructural analysis methods, the organization evolution of a 2205 duplex stainless steel narrow-gap laser arc hybrid weld under the effect of alternating magnetic field is revealed. The corrosion resistance of the welded joints is investigated by electrochemical tests. The results show that the use of a 40 mT applied alternating magnetic field can not only effectively inhibit the generation of porosity and unfused defects in the weld, but also that the addition of an alternating magnetic field improves the ratio of austenite to ferrite in the weld, and the ratio of the two phases is increased from 0.657 without a magnetic field to 0.850. The weld grain preferential orientation is affected by the magnetic field, and the weld austenite grains are shifted from the Goss texture to the Copper texture. Under the electromagnetic stirring effect of the applied magnetic field, the average austenite grain size decreased from 4.15 μm to 3.82 μm, and the average ferrite grain size decreased from 4.99 μm to 4.08 μm. In addition, the effect of the alternating magnetic field increases the density of twins in the organization. Electrochemical test results show that the addition of an alternating magnetic field increases the corrosion potential by 75.2 mV and the pitting potential by 134.5 mV, which indicates that the corrosion resistance of the cover-welded specimens is improved by the effect of an alternating magnetic field. The improvement in corrosion resistance mainly depends on the austenite grain refinement and the increase in the austenite content.
- 5 January 2023
- Published by Elsevier in Intermetallics
- Vol. 154
Improving the magnetic properties of sintered Nd-Ce-Fe-B magnets via grain boundary diffusion with Pr60Tb10Cu30 alloy
- 5 January 2023
- Published by Elsevier in Intermetallics
- Vol. 154
Improving the magnetic properties of sintered Nd-Ce-Fe-B magnets via grain boundary diffusion with Pr60Tb10Cu30 alloy
- 26 November 2022
- Published by Elsevier in Journal of Rare Earths
- Vol. 42 (1) , 116-120
Effect of annealing temperature on magnetic properties of a sintered Nd-Fe-B magnet after grain boundary diffusion with Dy70Cu30 alloy
- 26 November 2022
- Published by Elsevier in Journal of Rare Earths
- Vol. 42 (1) , 116-120
Effect of annealing temperature on magnetic properties of a sintered Nd-Fe-B magnet after grain boundary diffusion with Dy70Cu30 alloy
- Open Access
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Synergistic Evolution Mechanism of the Atomic/Nano Scale Structural Heterogeneity of Fe-Based Metallic Glasses at Relaxation and the Effect on Magnetic Properties
Metallic glasses are structurally heterogeneous on the atomic and nano scales. However, few investigations have been conducted on how these two different scales of structural heterogeneity co-evolve during annealing. In this work, the atomic and nanoscale structure heterogeneity evolution accompanying the magnetic softness was systematically discussed based on the literature and our previous synchrotron X-ray diffraction (XRD) and atomic force microscopy (AFM) results. We revealed the synergistic evolution mechanism of structural heterogeneities on the atomic and nano scales during annealing via the insight of percolation theory from the point of view of the local five-fold symmetry of the clusters. The results indicate that the reduction of atomic-scale structural heterogeneities during annealing is accompanied by an increase in the degree of local five-fold symmetry of the clusters and an alteration in their connection patterns. As the local five-fold symmetry of clusters in Fe-based metallic glasses reaches the percolation threshold, the nanoscale liquid-like regions tend to transform into solid-like regions. The great degree of percolation causes the pronounced weakening of the nanoscale structural heterogeneities accompanying changes in the shape and number of the liquid-like regions. The reduction of the liquid-like region causes a reduction in vertical anisotropy and magnetic softening due to a more uniform and less free volume within the sub-circular liquid-like region.
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessSynergistic Evolution Mechanism of the Atomic/Nano Scale Structural Heterogeneity of Fe-Based Metallic Glasses at Relaxation and the Effect on Magnetic Properties
Metallic glasses are structurally heterogeneous on the atomic and nano scales. However, few investigations have been conducted on how these two different scales of structural heterogeneity co-evolve during annealing. In this work, the atomic and nanoscale structure heterogeneity evolution accompanying the magnetic softness was systematically discussed based on the literature and our previous synchrotron X-ray diffraction (XRD) and atomic force microscopy (AFM) results. We revealed the synergistic evolution mechanism of structural heterogeneities on the atomic and nano scales during annealing via the insight of percolation theory from the point of view of the local five-fold symmetry of the clusters. The results indicate that the reduction of atomic-scale structural heterogeneities during annealing is accompanied by an increase in the degree of local five-fold symmetry of the clusters and an alteration in their connection patterns. As the local five-fold symmetry of clusters in Fe-based metallic glasses reaches the percolation threshold, the nanoscale liquid-like regions tend to transform into solid-like regions. The great degree of percolation causes the pronounced weakening of the nanoscale structural heterogeneities accompanying changes in the shape and number of the liquid-like regions. The reduction of the liquid-like region causes a reduction in vertical anisotropy and magnetic softening due to a more uniform and less free volume within the sub-circular liquid-like region.